Xianghui Ren
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Xianghui Ren has a total of 6 co-authors. Here are the top co-authors by number of shared publications:
- Bin Xie
School of Mechanical and Automotive Engineering, South China University of Technology, Guangzhou 510641, China
3 shared publications - Jiaxiang Xue
School of Mechanical and Automotive Engineering, South China University of Technology, Guangzhou, China
3 shared publications - Bin Xie
School of Mechanical and Automotive Engineering, South China University of Technology, Guangzhou 510641, China
1 shared publication - Wei Wu
School of Automobile and Transportation Engineering, Guangdong Polytechnic Normal University, Guangzhou, P.R. China
1 shared publication - Zhanhui Zhang
School of Future Technology, Guangzhou Polytechnic University, No. 1342 Shiliang Road, Panyu District, Guangzhou 511483, China
1 shared publication - Zhuangbin Lin
School of Mechanical and Automotive Engineering, South China University of Technology, Guangzhou 510641, China
1 shared publication
Latest Publications
- Open Access
Wire Arc Deposition Additive Manufacturing and Experimental Study of 316L Stainless Steel by CMT + P Process
The cold metal transfer plus pulse (CMT + P) process was performed to produce a 316L vertical wall through the single-channel multi-layer deposition method. The microstructure of different regions on deposited samples was observed by an optical microscope and a scanning electron microscope (SEM). The phase composition of the as-deposited wall was checked by X-ray diffraction, and the element distribution in the structure was analyzed by an energy-dispersive spectrometer. The tensile strength and microhardness of samples were tested, and the fracture morphology was observed by an SEM. Finally, the electrochemical corrosion characteristics of the as-deposited wall in different regions along the building direction were tested. Results from the experiments indicated that the microstructure of metallography showed a layer band. The metallurgical bounding between layers was carried out by dendrite remelting and epitaxial growth. Along the building direction, the alloy of different regions solidified in an ferritic-austenitic (FA) manner, and due to having undergone different heat histories, their SEM microstructures were significantly distinct. The ultimate tensile strength (UTS) and yield strength (YS) of the vertical specimens were higher than those of the horizontal specimens, displaying obvious anisotropy. Due to a large amount of precipitation of precipitated phases in terms of intermetallic compounds in the middle and upper regions, the tensile strength and microhardness along the building direction showed a trend of first decreasing and then increasing. In the bottom region, a small amount of ferrite precipitated in the austenite matrix, while in the middle of the as-deposited wall, the amount of ferrite gradually increased and was distributed in the austenite matrix as a network. However, due to the heat accumulation effect, the ferrite dissolved into austenite in large quantities and the austenite showed an obvious increase in size in the top region. A stable passivation film was caused by a relatively low dislocation density and grain boundary number, and the middle region of the arc as-deposited wall had the best corrosion resistance. The large consumption of chromium (Cr) atoms and material stripping in the top region resulted in the integrity of the passivation film in this region being the weakest, resulting in the lowest corrosion resistance.
Open AccessWire Arc Deposition Additive Manufacturing and Experimental Study of 316L Stainless Steel by CMT + P Process
The cold metal transfer plus pulse (CMT + P) process was performed to produce a 316L vertical wall through the single-channel multi-layer deposition method. The microstructure of different regions on deposited samples was observed by an optical microscope and a scanning electron microscope (SEM). The phase composition of the as-deposited wall was checked by X-ray diffraction, and the element distribution in the structure was analyzed by an energy-dispersive spectrometer. The tensile strength and microhardness of samples were tested, and the fracture morphology was observed by an SEM. Finally, the electrochemical corrosion characteristics of the as-deposited wall in different regions along the building direction were tested. Results from the experiments indicated that the microstructure of metallography showed a layer band. The metallurgical bounding between layers was carried out by dendrite remelting and epitaxial growth. Along the building direction, the alloy of different regions solidified in an ferritic-austenitic (FA) manner, and due to having undergone different heat histories, their SEM microstructures were significantly distinct. The ultimate tensile strength (UTS) and yield strength (YS) of the vertical specimens were higher than those of the horizontal specimens, displaying obvious anisotropy. Due to a large amount of precipitation of precipitated phases in terms of intermetallic compounds in the middle and upper regions, the tensile strength and microhardness along the building direction showed a trend of first decreasing and then increasing. In the bottom region, a small amount of ferrite precipitated in the austenite matrix, while in the middle of the as-deposited wall, the amount of ferrite gradually increased and was distributed in the austenite matrix as a network. However, due to the heat accumulation effect, the ferrite dissolved into austenite in large quantities and the austenite showed an obvious increase in size in the top region. A stable passivation film was caused by a relatively low dislocation density and grain boundary number, and the middle region of the arc as-deposited wall had the best corrosion resistance. The large consumption of chromium (Cr) atoms and material stripping in the top region resulted in the integrity of the passivation film in this region being the weakest, resulting in the lowest corrosion resistance.
- Open Access
- 8 May 2020
- Published by MDPI AG in Applied Sciences
- Vol. 10 (9) , 3284
A Comparative Study of the CMT+P Process on 316L Stainless Steel Additive Manufacturing
Adopting the cold metal transfer plus pulse (CMT + P) process, 316L stainless steel wire was treated with a single channel multi-layer deposition experiment under different linear energy. The microstructures of different regions on the deposited samples were observed by optical microscope and scanning electron microscope, and the element distribution in the structure was analyzed by energy dispersive spectrometer. The mechanical properties and microhardness were measured by tensile test method and microhardness tester, respectively, and the anisotropy of tensile strength in horizontal and vertical directions were calculated. Finally, the fracture morphology of the tensile samples were observed by SEM. Experiment results showed that when the difference between the actual and the optimal wire feeding speed matching the specific welding speed was too large, this led to an unstable deposition process as well as flow and collapse of weld bead metal, thus seriously deteriorating the appearance of the deposition samples. The results from metallographic micrograph showed that rapid heat dissipation of the substrate caused small grains to generate in the bottom region of deposition samples, then gradually grew up to coarse dendrites along the building direction in the middle and top region caused by the continuous heat accumulation during deposition. Tensile test results showed that with the increase of linear energy, the horizontal and vertical tensile strength of the as-deposited samples decreased. In addition, the higher linear energy would deteriorate the microstructure of as-deposited parts, including significantly increasing the tendency of oxidation and material stripping. The microhardness values of the bottom, middle and top regions of the samples fluctuated along the centerline of the cross-section, and the values showed a trend of decreasing first and then rising along the building direction. Meanwhile, the yield strength and tensile strength of each specimen showed obvious anisotropy due to unique grain growth morphology. On the whole, the results from this study prove that CMT+P process is a feasible MIG welding additive manufacturing method for 316L stainless steel.
- 8 May 2020
- Published by MDPI AG in Applied Sciences
- Vol. 10 (9) , 3284
Open AccessA Comparative Study of the CMT+P Process on 316L Stainless Steel Additive Manufacturing
Adopting the cold metal transfer plus pulse (CMT + P) process, 316L stainless steel wire was treated with a single channel multi-layer deposition experiment under different linear energy. The microstructures of different regions on the deposited samples were observed by optical microscope and scanning electron microscope, and the element distribution in the structure was analyzed by energy dispersive spectrometer. The mechanical properties and microhardness were measured by tensile test method and microhardness tester, respectively, and the anisotropy of tensile strength in horizontal and vertical directions were calculated. Finally, the fracture morphology of the tensile samples were observed by SEM. Experiment results showed that when the difference between the actual and the optimal wire feeding speed matching the specific welding speed was too large, this led to an unstable deposition process as well as flow and collapse of weld bead metal, thus seriously deteriorating the appearance of the deposition samples. The results from metallographic micrograph showed that rapid heat dissipation of the substrate caused small grains to generate in the bottom region of deposition samples, then gradually grew up to coarse dendrites along the building direction in the middle and top region caused by the continuous heat accumulation during deposition. Tensile test results showed that with the increase of linear energy, the horizontal and vertical tensile strength of the as-deposited samples decreased. In addition, the higher linear energy would deteriorate the microstructure of as-deposited parts, including significantly increasing the tendency of oxidation and material stripping. The microhardness values of the bottom, middle and top regions of the samples fluctuated along the centerline of the cross-section, and the values showed a trend of decreasing first and then rising along the building direction. Meanwhile, the yield strength and tensile strength of each specimen showed obvious anisotropy due to unique grain growth morphology. On the whole, the results from this study prove that CMT+P process is a feasible MIG welding additive manufacturing method for 316L stainless steel.
- Open Access
Process Optimization on Multilayer Morphology During 316L Double-wire CMT+P Deposition Process
Cold metal transfer (CMT) has been widely used in metal additive manufacturing for its low heat input, less splashing and high efficiency. Wire feeding speed and travelling speed are important processes that affect morphology in CMT deposition. This study optimized the forming process of 30-layer stainless-steel part deposited by double-wire and double-arc CMT plus pulse (CMT+P) process, and investigated the effect of the ratio of wire feeding speed to travelling speed on deposition morphology. The results show that asynchronous arc striking and extinguishing can improve the forming. Moreover, the deposition molding is affected by the interaction of heat input and heat accumulation. With the similar ratio of wire feeding speed to travelling speed and the similar heat input, increasing the wire feeding speed can increase the heat accumulation and the width of sample, and decrease the height. The optimum process interval of wire feeding speed to travelling speed ratio and heat input is 3.9–4.2 and 70–74.8 J/mm, respectively. Although the increasing heat accumulation makes grain coarse and slight decreases mechanical property, the highest deposition rate can be up to 5.4 kg/h, when wire feeding speed and travelling speed are 5 m/min and 120 cm/min, respectively, and the tensile strength and elongation rate of which can reach the basic standard requirements for stainless-steel forgings.
Open AccessProcess Optimization on Multilayer Morphology During 316L Double-wire CMT+P Deposition Process
Cold metal transfer (CMT) has been widely used in metal additive manufacturing for its low heat input, less splashing and high efficiency. Wire feeding speed and travelling speed are important processes that affect morphology in CMT deposition. This study optimized the forming process of 30-layer stainless-steel part deposited by double-wire and double-arc CMT plus pulse (CMT+P) process, and investigated the effect of the ratio of wire feeding speed to travelling speed on deposition morphology. The results show that asynchronous arc striking and extinguishing can improve the forming. Moreover, the deposition molding is affected by the interaction of heat input and heat accumulation. With the similar ratio of wire feeding speed to travelling speed and the similar heat input, increasing the wire feeding speed can increase the heat accumulation and the width of sample, and decrease the height. The optimum process interval of wire feeding speed to travelling speed ratio and heat input is 3.9–4.2 and 70–74.8 J/mm, respectively. Although the increasing heat accumulation makes grain coarse and slight decreases mechanical property, the highest deposition rate can be up to 5.4 kg/h, when wire feeding speed and travelling speed are 5 m/min and 120 cm/min, respectively, and the tensile strength and elongation rate of which can reach the basic standard requirements for stainless-steel forgings.