Fengnan Li
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Previous Organizations / Institutes
The organizations / institutes from the scholar's other articles in the past ten years
Research Subjects
Fengnan Li has a total of 55 co-authors. Here are the top co-authors by number of shared publications:
- Hongxing Wang
Key Lab for Physical Electronics and Devices, Ministry of Education, Xi'an Jiaotong University 1 , Xi'an 710049
7 shared publications Wei Wang
Institute of Wide Band Gap Semiconductors, Xi’an Jiaotong University, Xi’an, 710049, China
5 shared publicationsZhangcheng Liu
Institute of Wide Band Gap Semiconductors, Xi’an Jiaotong University, Xi’an, 710049, China
5 shared publications- Jingwen Zhang
Key Laboratory for Physical Electronics and Devices of the Ministry of Education, Xi’an Jiaotong University, Xi’an 710049, China
3 shared publications - Minghui Zhang
Key Lab for physical Electronics and Devices, Ministry of Education, Xi’an Jiaotong University, Xi’an 710049, China
3 shared publications Hong-Xing Wang
2 shared publications
Latest Publications
- Open Access
- 4 December 2019
- Published by Optica Publishing Group in Optics Express
- Vol. 27 (25) , 36750-36756
Characterization of UV photodetector based on ZnO/diamond film
In this study, a ZnO/diamond structure ultraviolet (UV) photodetector was fabricated and investigated. ZnO films with thickness of 50 and 100 nm were deposited on half of diamond substrates by sputtering technique. Then, electrodes were patterned on ZnO and diamond areas to form photodetectors. The photocurrent gain in the UV region has been strongly influenced by ZnO film. ZnO films with thickness of 50 and 100 nm on diamond substrates reaches 14.3 and 308 A/W, respectively. Both of peak responsivities were located at 270 nm. Additionally, two shoulder peaks around 240 nm and 290 nm were observed for ZnO/diamond photodetector, which may stem from diamond and ZnO, respectively.
- 4 December 2019
- Published by Optica Publishing Group in Optics Express
- Vol. 27 (25) , 36750-36756
Open AccessCharacterization of UV photodetector based on ZnO/diamond film
In this study, a ZnO/diamond structure ultraviolet (UV) photodetector was fabricated and investigated. ZnO films with thickness of 50 and 100 nm were deposited on half of diamond substrates by sputtering technique. Then, electrodes were patterned on ZnO and diamond areas to form photodetectors. The photocurrent gain in the UV region has been strongly influenced by ZnO film. ZnO films with thickness of 50 and 100 nm on diamond substrates reaches 14.3 and 308 A/W, respectively. Both of peak responsivities were located at 270 nm. Additionally, two shoulder peaks around 240 nm and 290 nm were observed for ZnO/diamond photodetector, which may stem from diamond and ZnO, respectively.
- Open Access
Ohmic Contact of Pt/Au on Hydrogen-Terminated Single Crystal Diamond
In this study, contact properties of platinum/gold (Pt/Au) on the surface of hydrogen-terminated single crystal diamond (H-SCD) were studied with several treatment conditions. The electrodes of Pt (20 nm)/Au (100 nm) were deposited on H-SCD surface by electron beam evaporation technique. Then, the specific contact resistance (ρc) of the as-fabricated sample was measured by the circular transmission line model, which showed good ohmic properties with the value of 5.65 × 10−4 Ω·cm2. To identify the thermal stability of Pt/Au/H-SCD, the sample was annealed in hydrogen ambient from 200 to 700 °C for 20 min at each temperature. As the temperature increased, ρc demonstrated better thermal stability. In addition, the barrier height was evaluated to be −0.67 ± 0.12 eV by X-ray photoelectron spectroscopy (XPS) technique.
Open AccessOhmic Contact of Pt/Au on Hydrogen-Terminated Single Crystal Diamond
In this study, contact properties of platinum/gold (Pt/Au) on the surface of hydrogen-terminated single crystal diamond (H-SCD) were studied with several treatment conditions. The electrodes of Pt (20 nm)/Au (100 nm) were deposited on H-SCD surface by electron beam evaporation technique. Then, the specific contact resistance (ρc) of the as-fabricated sample was measured by the circular transmission line model, which showed good ohmic properties with the value of 5.65 × 10−4 Ω·cm2. To identify the thermal stability of Pt/Au/H-SCD, the sample was annealed in hydrogen ambient from 200 to 700 °C for 20 min at each temperature. As the temperature increased, ρc demonstrated better thermal stability. In addition, the barrier height was evaluated to be −0.67 ± 0.12 eV by X-ray photoelectron spectroscopy (XPS) technique.
- 16 May 2019
- Published by IOP Publishing in Nanotechnology
- Vol. 30 (32) , 325204
Self-powered diamond ultraviolet photodetector with a transparent Ag nanowire electrode
A novel diamond UV photodetector with a transparent Ag nanowire (NW) electrode was fabricated. A transparent Ag NW network was spin-coated on single crystalline diamond to form a Schottky contact, which had a barrier height of about 1.37 eV obtained by XPS measurements. Meanwhile, multilayered metals of Au/Pt/Ti were evaporated on the diamond sample to form ohmic contacts. Compared to a Au/Pt/Ti-Au/Pt/Ti diamond photodetector, the Au/Pt/Ti-Ag NW diamond photodetector exhibited relatively high responsivity under 220 nm (18 mA W −1 ), high linear dynamic range (41 dB), and short response time (0.12 s for rise time, 0.56 s for decay time). In particular, the Au/Pt/Ti-Ag NW diamond photodetector displayed high photocurrent of about 200 pA at zero-bias, indicating its potential for creating self-powered devices.
- 16 May 2019
- Published by IOP Publishing in Nanotechnology
- Vol. 30 (32) , 325204
Self-powered diamond ultraviolet photodetector with a transparent Ag nanowire electrode
A novel diamond UV photodetector with a transparent Ag nanowire (NW) electrode was fabricated. A transparent Ag NW network was spin-coated on single crystalline diamond to form a Schottky contact, which had a barrier height of about 1.37 eV obtained by XPS measurements. Meanwhile, multilayered metals of Au/Pt/Ti were evaporated on the diamond sample to form ohmic contacts. Compared to a Au/Pt/Ti-Au/Pt/Ti diamond photodetector, the Au/Pt/Ti-Ag NW diamond photodetector exhibited relatively high responsivity under 220 nm (18 mA W −1 ), high linear dynamic range (41 dB), and short response time (0.12 s for rise time, 0.56 s for decay time). In particular, the Au/Pt/Ti-Ag NW diamond photodetector displayed high photocurrent of about 200 pA at zero-bias, indicating its potential for creating self-powered devices.
- 5 December 2017
- Published by Optica Publishing Group in Optics Express
- Vol. 25 (25) , 31586-31594
Fabrication of monolithic diamond photodetector with microlenses
A monolithic diamond photodetector with microlenses is fabricated by etching microlens arrays (MLAs) on single crystal diamond surface and patterning tungsten electrode strips on the edge of these arrays. Firstly, compact MLAs are etched on half of diamond sample surface by thermal reflow method. Secondly, via magnetron sputtering technique, two sets of interdigitated tungsten electrodes are patterned on the sample surface, one set is on the edge of MLAs, the other set is on the planar area. The optoelectronic performances of photodetectors have been investigated and indicated that the photocurrent of microlens photodetector increases by 74.8 percent at 10 V under 220 nm UV light illumination by comparing with that in planar case. Simulations of photodetectors' electrical and optical properties have been carried out, illustrating an improvement of charge collection ability and light absorption efficiency in microlens case. Furthermore, the present device structure can be extended to other semiconductor photodetectors.
- 5 December 2017
- Published by Optica Publishing Group in Optics Express
- Vol. 25 (25) , 31586-31594
Fabrication of monolithic diamond photodetector with microlenses
A monolithic diamond photodetector with microlenses is fabricated by etching microlens arrays (MLAs) on single crystal diamond surface and patterning tungsten electrode strips on the edge of these arrays. Firstly, compact MLAs are etched on half of diamond sample surface by thermal reflow method. Secondly, via magnetron sputtering technique, two sets of interdigitated tungsten electrodes are patterned on the sample surface, one set is on the edge of MLAs, the other set is on the planar area. The optoelectronic performances of photodetectors have been investigated and indicated that the photocurrent of microlens photodetector increases by 74.8 percent at 10 V under 220 nm UV light illumination by comparing with that in planar case. Simulations of photodetectors' electrical and optical properties have been carried out, illustrating an improvement of charge collection ability and light absorption efficiency in microlens case. Furthermore, the present device structure can be extended to other semiconductor photodetectors.
- Open Access
Barrier Heights of Au on Diamond with Different Terminations Determined by X-ray Photoelectron Spectroscopy
Barrier heights of Au on hydrogen-/oxygen-/fluorine-/nitrogen-terminated diamond (H-/O-/F-/N-diamond) have been investigated by X-ray photoelectron spectroscopy. All of the H-/O-/F-/N-diamond surfaces have been formed on different areas of one diamond sample. An Au film with a thickness of 4 nm was evaporated to form Au/diamond contacts. Barrier height values for Au on H-/O-/F-/N-diamond contacts were determined to be −0.19, 1.71, 2.29, and 2.39 eV, respectively. Then, the surface of Au/diamond contacts was treated by 1000 eV Ar+ bombardment with different duration of time, resulting in a pinned barrier height of 1.83 eV independent of contact structures. In the end, the spatial distribution of the energy band diagram has been calculated by solving Poisson’s equation.
Open AccessBarrier Heights of Au on Diamond with Different Terminations Determined by X-ray Photoelectron Spectroscopy
Barrier heights of Au on hydrogen-/oxygen-/fluorine-/nitrogen-terminated diamond (H-/O-/F-/N-diamond) have been investigated by X-ray photoelectron spectroscopy. All of the H-/O-/F-/N-diamond surfaces have been formed on different areas of one diamond sample. An Au film with a thickness of 4 nm was evaporated to form Au/diamond contacts. Barrier height values for Au on H-/O-/F-/N-diamond contacts were determined to be −0.19, 1.71, 2.29, and 2.39 eV, respectively. Then, the surface of Au/diamond contacts was treated by 1000 eV Ar+ bombardment with different duration of time, resulting in a pinned barrier height of 1.83 eV independent of contact structures. In the end, the spatial distribution of the energy band diagram has been calculated by solving Poisson’s equation.
- Open Access
Fabrication of Low Dislocation Density, Single-Crystalline Diamond via Two-Step Epitaxial Lateral Overgrowth
Continuous diamond films with low dislocation density were obtained by two-step epitaxial lateral overgrowth (ELO). Grooves were fabricated by inductively coupled plasma etching. Mo/Pd stripes sputtered in the grooves were used to inhibit the propagation of dislocations originating from the diamond substrate. Coalescent diamond films were achieved by ELO via microwave plasma-enhanced chemical vapor deposition. Etch-pits were formed intentionally to characterize the quality of the epitaxial films and distinguish different growth areas, as dislocations served as preferential sites for etching. In the window regions, a high density of dislocations, displayed as dense etch-pits, was generated. By contrast, the etch-pit density was clearly lower in the overgrowth regions. After the second ELO step, the dislocation density was further decreased. Raman spectroscopy analysis suggested that the lateral overgrowth of diamond is a promising method for achieving low dislocation density films.
Open AccessFabrication of Low Dislocation Density, Single-Crystalline Diamond via Two-Step Epitaxial Lateral Overgrowth
Continuous diamond films with low dislocation density were obtained by two-step epitaxial lateral overgrowth (ELO). Grooves were fabricated by inductively coupled plasma etching. Mo/Pd stripes sputtered in the grooves were used to inhibit the propagation of dislocations originating from the diamond substrate. Coalescent diamond films were achieved by ELO via microwave plasma-enhanced chemical vapor deposition. Etch-pits were formed intentionally to characterize the quality of the epitaxial films and distinguish different growth areas, as dislocations served as preferential sites for etching. In the window regions, a high density of dislocations, displayed as dense etch-pits, was generated. By contrast, the etch-pit density was clearly lower in the overgrowth regions. After the second ELO step, the dislocation density was further decreased. Raman spectroscopy analysis suggested that the lateral overgrowth of diamond is a promising method for achieving low dislocation density films.
- 1 February 2017
- Published by Elsevier in Materials Letters
- Vol. 188, 52-54
Photoelectrical characteristics of ultra thin TiO 2 /diamond photodetector
- 1 February 2017
- Published by Elsevier in Materials Letters
- Vol. 188, 52-54
Photoelectrical characteristics of ultra thin TiO 2 /diamond photodetector
- 10 October 2016
- Published by AIP Publishing in Applied Physics Letters
- Vol. 109 (15) , 153507
Fabrication of three dimensional diamond ultraviolet photodetector through down-top method
Three dimensional diamond ultraviolet (UV) photodetector have been fabricated on diamond epitaxial layer through down-top approach, where diamond epitaxial layer was grown between metal electrodes. A thin diamond epitaxial layer was first grown on high-pressure high-temperature single crystal diamond substrate. Then, the diamond epitaxial layer was covered by interdigitated tungsten electrodes. Furthermore, another diamond epitaxial layer was grown on uncovered area. At last, UV-Ozone treatment was used to oxidize the surface. The optoelectronic performance of the photodetector was characterized, exhibiting a large responsivity and a repeatable transient response behavior. Moreover, down-top process is beneficial for the electrode conductivity stability. Also, an ohmic contact could be formed between tungsten and diamond during growth. The results indicate that down-top process is an efficient way for fabrication of three dimensional diamond photodetectors.
- 10 October 2016
- Published by AIP Publishing in Applied Physics Letters
- Vol. 109 (15) , 153507
Fabrication of three dimensional diamond ultraviolet photodetector through down-top method
Three dimensional diamond ultraviolet (UV) photodetector have been fabricated on diamond epitaxial layer through down-top approach, where diamond epitaxial layer was grown between metal electrodes. A thin diamond epitaxial layer was first grown on high-pressure high-temperature single crystal diamond substrate. Then, the diamond epitaxial layer was covered by interdigitated tungsten electrodes. Furthermore, another diamond epitaxial layer was grown on uncovered area. At last, UV-Ozone treatment was used to oxidize the surface. The optoelectronic performance of the photodetector was characterized, exhibiting a large responsivity and a repeatable transient response behavior. Moreover, down-top process is beneficial for the electrode conductivity stability. Also, an ohmic contact could be formed between tungsten and diamond during growth. The results indicate that down-top process is an efficient way for fabrication of three dimensional diamond photodetectors.