Qiangqiang Liao
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Previous Organizations / Institutes
The organizations / institutes from the scholar's other articles in the past ten years
Qiangqiang Liao has a total of 28 co-authors. Here are the top co-authors by number of shared publications:
Dong Yang
Shanghai Key Laboratory of Materials Protection and Advanced Materials in Electric Power, Shanghai Engineering Research Center of Energy-Saving in Heat Exchange Systems, Shanghai University of Electric Power, Shanghai, 200090, PR China
3 shared publicationsMiaomiao Mu
Shanghai Univ Elect Power, Shanghai Key Lab Mat Protect & Adv Mat Elect Powe, Shanghai 200090, Peoples R China
3 shared publicationsJilei Ye
New Energy Research Institute, Branch of China Electric Power Research Institute Nanjing China
2 shared publicationsYoulang Zhang
Shanghai Key Laboratory of Materials Protection and Advanced Materials in Electric Power, Shanghai Engineering Research Center of Electric Energy ConversionShanghai University of Electric Power Shanghai China
2 shared publicationsAijun Yan
China Datang Corporation Science and Technology Research Institute , Xi’an 710054, Shaanxi , China
1 shared publicationAiqiang Pan
State Grid Shanghai Municipal Electric Power Company Shanghai China
1 shared publication
Latest Publications
- 1 September 2021
- Published by Elsevier in Sustainable Chemistry and Pharmacy
- Vol. 22, 100488
Dithiocarbamate modified glucose as a novel eco-friendly corrosion inhibitor for copper in sodium chloride media
- 1 September 2021
- Published by Elsevier in Sustainable Chemistry and Pharmacy
- Vol. 22, 100488
Dithiocarbamate modified glucose as a novel eco-friendly corrosion inhibitor for copper in sodium chloride media
- 12 December 2019
- Published by Wiley in International Journal of Energy Research
- Vol. 44 (3) , 2337-2344
A fast classification method of retired electric vehicle battery modules and their energy storage application in photovoltaic generation
- 12 December 2019
- Published by Wiley in International Journal of Energy Research
- Vol. 44 (3) , 2337-2344
A fast classification method of retired electric vehicle battery modules and their energy storage application in photovoltaic generation
- 27 December 2018
- Published by Wiley in International Journal of Energy Research
- Vol. 43 (12) , 6461-6474
Economic analysis of an industrial photovoltaic system coupling with battery storage
- 27 December 2018
- Published by Wiley in International Journal of Energy Research
- Vol. 43 (12) , 6461-6474
Economic analysis of an industrial photovoltaic system coupling with battery storage
- 1 October 2018
- Published by American Scientific Publishers in Science of Advanced Materials
- Vol. 10 (10) , 1397-1407
Cycling Degradation of Lithium-Ion Batteries Module from Electric Vehicle
A commercial 26650-type lithium-ion module (15P4S) of LiFePO4/graphite from an electric vehicle was cycled at the charge–discharge rate of 2 C at room temperature (20±2 °C) for 400 times until its state-of-health (SOH) declined below 60%. Its degradation was investigated by capacity fading characterization, electrochemical impedance spectroscopy (EIS), field emission scanning electron microscopy (FE-SEM), energy dispersive X-ray spectroscopy (EDS), X-ray photoelectron spectroscopy (XPS) and X-ray diffraction (XRD). The results show that the battery module's capacity degradation is mainly related to the increase of internal resistance. The patchy image on the aged graphite surface indicates that part of the graphite is detached from the current collector. The rise of P–F and Li–F content connotes the thickening of the SEI film. The (002) peak position in the XRD patterns of the ageing graphite electrode shifts to a low angle direction, suggesting an increase in the graphite layer distance. The appearance of the FePO4 phase in the XRD patterns indicates a reduction in active lithium. Therefore, the capacity loss of the battery module is mainly caused by the performance deterioration of graphite and LiFePO4 materials together.
- 1 October 2018
- Published by American Scientific Publishers in Science of Advanced Materials
- Vol. 10 (10) , 1397-1407
Cycling Degradation of Lithium-Ion Batteries Module from Electric Vehicle
A commercial 26650-type lithium-ion module (15P4S) of LiFePO4/graphite from an electric vehicle was cycled at the charge–discharge rate of 2 C at room temperature (20±2 °C) for 400 times until its state-of-health (SOH) declined below 60%. Its degradation was investigated by capacity fading characterization, electrochemical impedance spectroscopy (EIS), field emission scanning electron microscopy (FE-SEM), energy dispersive X-ray spectroscopy (EDS), X-ray photoelectron spectroscopy (XPS) and X-ray diffraction (XRD). The results show that the battery module's capacity degradation is mainly related to the increase of internal resistance. The patchy image on the aged graphite surface indicates that part of the graphite is detached from the current collector. The rise of P–F and Li–F content connotes the thickening of the SEI film. The (002) peak position in the XRD patterns of the ageing graphite electrode shifts to a low angle direction, suggesting an increase in the graphite layer distance. The appearance of the FePO4 phase in the XRD patterns indicates a reduction in active lithium. Therefore, the capacity loss of the battery module is mainly caused by the performance deterioration of graphite and LiFePO4 materials together.
- 21 August 2017
- Published by Walter de Gruyter GmbH in Corrosion Reviews
- Vol. 35 (6) , 463-471
Synergistic inhibition effect of imidazoline derivative and potassium iodide on carbon steel corrosion in amidosulfuric acid solution
The mixture of 2-undecyl- N -carboxymethyl- N -hydroxyethly imidazoline (UHCI) with potassium iodide (KI) as a corrosion inhibitor for carbon steel in 8% amidosulfuric acid solution was investigated by weight loss test and electrochemical methods. Results show that the combined inhibitor strongly inhibits the corrosion of 20# carbon steel in amidosulfuric acid solution, and the mixture with the mass ratio (UHCI:KI) of 9:1 has the best corrosion inhibition at a total concentration of 0.4%. The impedance spectra of carbon steel electrodes change from one time constant into two time constants when the mixture inhibitor adds into the blank solution, while the polarization curves indicate that the mixture behaves as a mixed type inhibitor. The mixture is found to follow the Langmuir adsorption isotherm, and the mechanism is chemisorption.
- 21 August 2017
- Published by Walter de Gruyter GmbH in Corrosion Reviews
- Vol. 35 (6) , 463-471
Synergistic inhibition effect of imidazoline derivative and potassium iodide on carbon steel corrosion in amidosulfuric acid solution
The mixture of 2-undecyl- N -carboxymethyl- N -hydroxyethly imidazoline (UHCI) with potassium iodide (KI) as a corrosion inhibitor for carbon steel in 8% amidosulfuric acid solution was investigated by weight loss test and electrochemical methods. Results show that the combined inhibitor strongly inhibits the corrosion of 20# carbon steel in amidosulfuric acid solution, and the mixture with the mass ratio (UHCI:KI) of 9:1 has the best corrosion inhibition at a total concentration of 0.4%. The impedance spectra of carbon steel electrodes change from one time constant into two time constants when the mixture inhibitor adds into the blank solution, while the polarization curves indicate that the mixture behaves as a mixed type inhibitor. The mixture is found to follow the Langmuir adsorption isotherm, and the mechanism is chemisorption.
- 28 February 2017
- Published by Springer Nature in Journal of Materials Engineering and Performance
- Vol. 26 (4) , 1751-1757
Corrosion Behavior of Copper-Clad Steel Bars with Unclad Two-End Faces for Grounding Grids in the Red Clay Soil
- 28 February 2017
- Published by Springer Nature in Journal of Materials Engineering and Performance
- Vol. 26 (4) , 1751-1757
Corrosion Behavior of Copper-Clad Steel Bars with Unclad Two-End Faces for Grounding Grids in the Red Clay Soil
- 2 September 2016
- Published by Walter de Gruyter GmbH in Corrosion Reviews
- Vol. 34 (5-6) , 295-304
Electrochemical and XPS studies of alkyl imidazoline on the corrosion inhibition of carbon steel in citric acid solution
The corrosion inhibition behavior of an imidazoline derivative, namely, 2-undecyl- N -carboxymethyl- N -hydroxyethyl imidazoline (UHCI) for carbon steel in 4 wt.% citric acid solutions was characterized by weight loss method and electrochemical techniques in conjunction with X-ray photoelectron spectrometer (XPS) technique. The inhibitor has a good anti-corrosion effect on the carbon steel in 4 wt.% citric acid solutions. The inhibition efficiency increases with UHCI concentrations from 0 up to 0.4 wt.%, yet declines a bit at 0.6 wt.% per contra with further augmentation of concentration. The inhibition efficiency declines with the rise of temperature from 20°C to 95°C, while it rises with the extension of soaking time from 2 h to 24 h. Two N 1s peaks that appeared in XPS spectra give proof of UHCI inhibitor adsorbed on the carbon steel surface.
- 2 September 2016
- Published by Walter de Gruyter GmbH in Corrosion Reviews
- Vol. 34 (5-6) , 295-304
Electrochemical and XPS studies of alkyl imidazoline on the corrosion inhibition of carbon steel in citric acid solution
The corrosion inhibition behavior of an imidazoline derivative, namely, 2-undecyl- N -carboxymethyl- N -hydroxyethyl imidazoline (UHCI) for carbon steel in 4 wt.% citric acid solutions was characterized by weight loss method and electrochemical techniques in conjunction with X-ray photoelectron spectrometer (XPS) technique. The inhibitor has a good anti-corrosion effect on the carbon steel in 4 wt.% citric acid solutions. The inhibition efficiency increases with UHCI concentrations from 0 up to 0.4 wt.%, yet declines a bit at 0.6 wt.% per contra with further augmentation of concentration. The inhibition efficiency declines with the rise of temperature from 20°C to 95°C, while it rises with the extension of soaking time from 2 h to 24 h. Two N 1s peaks that appeared in XPS spectra give proof of UHCI inhibitor adsorbed on the carbon steel surface.