Chunping Wu
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Chunping Wu has a total of 46 co-authors. Here are the top co-authors by number of shared publications:
Guofu Xu
10 shared publicationsXiaolu Yuan
7 shared publicationsChengwei Zhao
6 shared publicationsChengxin Liu
5 shared publicationsJunjie Dai
5 shared publicationsLejian Yu
5 shared publications
Latest Publications
- 17 November 2026
- Published by Elsevier in Surfaces and Interfaces
Atmosphere-controlled Ti2SnC decomposition and SnO2-rich network formation in Ag/Ti2SnC composites
- 17 November 2026
- Published by Elsevier in Surfaces and Interfaces
Atmosphere-controlled Ti2SnC decomposition and SnO2-rich network formation in Ag/Ti2SnC composites
- 14 September 2026
- Published by Elsevier in Corrosion Science
- Vol. 272
Phase-controlled internal oxidation and solute redistribution in Sb- and Cr-modified Ag-Sn-In-Ni alloys
- 14 September 2026
- Published by Elsevier in Corrosion Science
- Vol. 272
Phase-controlled internal oxidation and solute redistribution in Sb- and Cr-modified Ag-Sn-In-Ni alloys
- 16 July 2026
- Published by Elsevier in Applied Surface Science
- Vol. 748
The oxidation behavior and mechanism of Ag-Sn-In-La-Ni/Te alloy powders
- 16 July 2026
- Published by Elsevier in Applied Surface Science
- Vol. 748
The oxidation behavior and mechanism of Ag-Sn-In-La-Ni/Te alloy powders
- Open Access
- 24 June 2026
- Published by Elsevier in SSRN Electronic Journal
Phase-controlled internal oxidation and solute redistribution in Sb- and Cr-modified Ag-Sn-In-Ni alloys
The internal oxidation of multicomponent Ag-based alloys is controlled not only by oxygen diffusion through the Ag matrix but also by the constitution and reactivity of solute-rich secondary phases. However, the phase-specific roles of minor Sb and Cr additions remain insufficiently clarified. In this work, Ag-6.5Sn-2.5In-0.5Ni-0.5Sb and Ag-6.5Sn-2.5In-0.5Ni-0.5Cr alloys were investigated by high-pressure oxidation, quasi-in-situ oxidation, X-ray diffraction, and electron probe microanalysis. After oxidation at 750 °C in pure O2 under pO2 ≈ 0.9 MPa, full-thickness cross-sectional observations revealed inward oxidation from both surfaces toward the specimen center, leaving a residual Ag-rich unoxidized core. The Cr-containing alloy showed a larger inward oxidation depth than the Sb-containing alloy, suggesting a higher degree of internal oxidation. Quasi-in-situ observations further indicated distinct phase-controlled oxidation features. In the Sb-containing alloy, In and Sn dissolved in the Ag matrix appeared to oxidize preferentially, followed by delayed oxidation of Ni-Sb-Sn-rich secondary phases and accompanied by oxygen ingress and outward redistribution of Sn, Sb, and Ni. In the Cr-containing alloy, Cr-rich regions showed preferential early-stage oxidation, whereas Ni-Sn-rich and mixed Ni-Cr-Sn regions were associated with complex Ni-, Sn-, Cr-, and O-containing oxide configurations at later stages. These results suggest that Sb favors a relatively sequential oxidation pathway, while Cr promotes reactive Cr-bearing regions and multiphase-coupled oxidation. This phase-dependent mechanism provides guidance for tailoring oxide morphology and optimizing high-pressure internal oxidation processing in Ag-SnO2-based electrical contact materials. The findings also highlight the importance of controlling secondary-phase type, distribution, and reactivity during alloy design.
- 24 June 2026
- Published by Elsevier in SSRN Electronic Journal
Open AccessPhase-controlled internal oxidation and solute redistribution in Sb- and Cr-modified Ag-Sn-In-Ni alloys
The internal oxidation of multicomponent Ag-based alloys is controlled not only by oxygen diffusion through the Ag matrix but also by the constitution and reactivity of solute-rich secondary phases. However, the phase-specific roles of minor Sb and Cr additions remain insufficiently clarified. In this work, Ag-6.5Sn-2.5In-0.5Ni-0.5Sb and Ag-6.5Sn-2.5In-0.5Ni-0.5Cr alloys were investigated by high-pressure oxidation, quasi-in-situ oxidation, X-ray diffraction, and electron probe microanalysis. After oxidation at 750 °C in pure O2 under pO2 ≈ 0.9 MPa, full-thickness cross-sectional observations revealed inward oxidation from both surfaces toward the specimen center, leaving a residual Ag-rich unoxidized core. The Cr-containing alloy showed a larger inward oxidation depth than the Sb-containing alloy, suggesting a higher degree of internal oxidation. Quasi-in-situ observations further indicated distinct phase-controlled oxidation features. In the Sb-containing alloy, In and Sn dissolved in the Ag matrix appeared to oxidize preferentially, followed by delayed oxidation of Ni-Sb-Sn-rich secondary phases and accompanied by oxygen ingress and outward redistribution of Sn, Sb, and Ni. In the Cr-containing alloy, Cr-rich regions showed preferential early-stage oxidation, whereas Ni-Sn-rich and mixed Ni-Cr-Sn regions were associated with complex Ni-, Sn-, Cr-, and O-containing oxide configurations at later stages. These results suggest that Sb favors a relatively sequential oxidation pathway, while Cr promotes reactive Cr-bearing regions and multiphase-coupled oxidation. This phase-dependent mechanism provides guidance for tailoring oxide morphology and optimizing high-pressure internal oxidation processing in Ag-SnO2-based electrical contact materials. The findings also highlight the importance of controlling secondary-phase type, distribution, and reactivity during alloy design.
- Open Access
- 22 April 2026
- Published by Elsevier in SSRN Electronic Journal
Distinct effects of Sb and Cr on the internal oxidation behavior and mechanisms of Ag-Sn-In-Ni alloys
The effects of Sb and Cr on the internal oxidation behavior of Ag-6.5Sn-2.5In-0.5Ni-based alloys were investigated using quasi-in-situ oxidation, electron probe microanalysis (EPMA), and X-ray diffraction (XRD). The results showed that Sb and Cr altered the oxidation pathway and phase evolution in distinctly different ways. In Ag-6.5Sn-2.5In-0.5Ni-0.5Sb, the NiSbSn phase was fully oxidized, producing four characteristic oxide morphologies. In Ag-6.5Sn-2.5In-0.5Ni-0.5Cr, the NiSn, Cr(Ni), and NiCrSn phases were completely oxidized, resulting in six oxide types. Quasi-in-situ observations revealed the sequential oxidation of individual phases and the associated microstructural evolution. The difference in oxidation behavior indicates that Sb and Cr play different roles in phase stability, oxidation progression, and oxide distribution, leading to distinct internal oxidation mechanisms. These results provide insight into alloying-element effects on internal oxidation and guidance for the design of Ag-SnO2 electrical contact materials.
- 22 April 2026
- Published by Elsevier in SSRN Electronic Journal
Open AccessDistinct effects of Sb and Cr on the internal oxidation behavior and mechanisms of Ag-Sn-In-Ni alloys
The effects of Sb and Cr on the internal oxidation behavior of Ag-6.5Sn-2.5In-0.5Ni-based alloys were investigated using quasi-in-situ oxidation, electron probe microanalysis (EPMA), and X-ray diffraction (XRD). The results showed that Sb and Cr altered the oxidation pathway and phase evolution in distinctly different ways. In Ag-6.5Sn-2.5In-0.5Ni-0.5Sb, the NiSbSn phase was fully oxidized, producing four characteristic oxide morphologies. In Ag-6.5Sn-2.5In-0.5Ni-0.5Cr, the NiSn, Cr(Ni), and NiCrSn phases were completely oxidized, resulting in six oxide types. Quasi-in-situ observations revealed the sequential oxidation of individual phases and the associated microstructural evolution. The difference in oxidation behavior indicates that Sb and Cr play different roles in phase stability, oxidation progression, and oxide distribution, leading to distinct internal oxidation mechanisms. These results provide insight into alloying-element effects on internal oxidation and guidance for the design of Ag-SnO2 electrical contact materials.
- 26 November 2025
- Published by Elsevier in Applied Surface Science
- Vol. 720
The effects of oxidation methods on microstructure and properties of Ag/SnO2Bi2O3CuO materials
- 26 November 2025
- Published by Elsevier in Applied Surface Science
- Vol. 720
The effects of oxidation methods on microstructure and properties of Ag/SnO2Bi2O3CuO materials
- 5 August 2025
- Published by Elsevier in Journal of Alloys and Compounds
- Vol. 1038
The influence of temperature and atmosphere on microstructure and properties of Ag/Ti3AlC2 compacts
- 5 August 2025
- Published by Elsevier in Journal of Alloys and Compounds
- Vol. 1038
The influence of temperature and atmosphere on microstructure and properties of Ag/Ti3AlC2 compacts
- 7 September 2024
- Published by Springer Nature in Journal of Materials Science: Materials in Electronics
- Vol. 35 (25) , 1-19
Influence of oxidation way on microstructure and oxides distribution of Ag–SnO2Sb2O3 materials
- 7 September 2024
- Published by Springer Nature in Journal of Materials Science: Materials in Electronics
- Vol. 35 (25) , 1-19
Influence of oxidation way on microstructure and oxides distribution of Ag–SnO2Sb2O3 materials
- 27 April 2023
- Published by Springer Nature in Journal of Materials Science: Materials in Electronics
- Vol. 34 (12) , 1-15
Influence of Ni content on arc erosion behavior of Ag/Ni electrical contact materials
- 27 April 2023
- Published by Springer Nature in Journal of Materials Science: Materials in Electronics
- Vol. 34 (12) , 1-15
Influence of Ni content on arc erosion behavior of Ag/Ni electrical contact materials
- Open Access
Influence of Rolling Temperatures on Interface Microstructure and Mechanical Properties of Multi-Pass Rolling TA1/Q235B Explosive Welded Sheets
The effect of rolling temperatures on the interface microstructure and mechanical properties is investigated using 2-mm-thick TA1/Q235B composite sheets, which were prepared after nine passes of hot rolling of explosive welded plates. The results show that the vortex region and the transition layer exist in the interface at the explosive welded plate, while only the transition layer exists in the interface after hot rolling. The transition layer is composed of α-Ti, TiC, Fe, and FeTi, and the thickness increases with the increasing rolling temperature. The microhardness of the explosive welded plate is higher than that of the hot-rolling sheet, and the microhardness of interface are higher than that of matrix metals. The interface shear strength and tensile elongation of the hot-rolled sheet increase with the increasing hot rolling temperature, while the ultimate tensile strength (UTS), yield strength (YS) and Young modulus decrease with the increase of hot rolling temperature. The shear strength of sheets is related to the interfacial compounds, and the tensile strength is mainly affected by the grain morphology of the matrix.
Open AccessInfluence of Rolling Temperatures on Interface Microstructure and Mechanical Properties of Multi-Pass Rolling TA1/Q235B Explosive Welded Sheets
The effect of rolling temperatures on the interface microstructure and mechanical properties is investigated using 2-mm-thick TA1/Q235B composite sheets, which were prepared after nine passes of hot rolling of explosive welded plates. The results show that the vortex region and the transition layer exist in the interface at the explosive welded plate, while only the transition layer exists in the interface after hot rolling. The transition layer is composed of α-Ti, TiC, Fe, and FeTi, and the thickness increases with the increasing rolling temperature. The microhardness of the explosive welded plate is higher than that of the hot-rolling sheet, and the microhardness of interface are higher than that of matrix metals. The interface shear strength and tensile elongation of the hot-rolled sheet increase with the increasing hot rolling temperature, while the ultimate tensile strength (UTS), yield strength (YS) and Young modulus decrease with the increase of hot rolling temperature. The shear strength of sheets is related to the interfacial compounds, and the tensile strength is mainly affected by the grain morphology of the matrix.