Lap-Yan Yeung
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Previous Organizations / Institutes
The organizations / institutes from the scholar's other articles in the past ten years
Research Subjects
Lap-Yan Yeung has a total of 39 co-authors. Here are the top co-authors by number of shared publications:
- Jinlian Hu
Department of Biomedical Engineering, City University of Hong Kong, Kowloon, China
6 shared publications Qinghao Meng
Institute of Textiles and Clothing, Hong Kong Polytechnic University, Kowloon, Hong Kong, People's Republic of China
4 shared publicationsYong Zhu
Institute of Textiles and Clothing, Hong Kong Polytechnic University, Kowloon, Hong Kong, People's Republic of China
4 shared publicationsFenglong Ji
2 shared publicationsJing Lu
Institute of Textiles and Clothing, Hong Kong Polytechnic University, Kowloon, Hong Kong, P.R. China
2 shared publicationsJinlian Hu
2 shared publications
Latest Publications
- Open Access
- 1 July 2025
- Published by SAGE Publications in AATCC Journal of Research
- Vol. 12 (4)
A comprehensive method for the sampling, purification, extraction, and quantification of microplastic fibre release in textile production
The release of microplastics from the textile industry is a significant environmental concern. While the release of microplastics during the laundering process and within wastewater treatment plants has been extensively studied, there is still a pressing need for a standardised sampling protocol to assess microplastic release across various matrices involved in different textile production processes. In this report, we propose a comprehensive sampling protocol targeting four types of samples derived from textile production processes: sludge, wastewater, dust, and air. We also provide a detail method for the extraction and analysis of microplastics from these samples, including the separation of microplastics from collected textile samples through cellulose dissolution, oxidation, and oleophilic extraction processes, as well as heat treatment for air samples. This is followed by automated methods for quantifying microplastic fibres. The proposed protocol provides an efficient, effective, straightforward, cost-effective, and safe approach for analysing and monitoring textile-related microplastics.
- 1 July 2025
- Published by SAGE Publications in AATCC Journal of Research
- Vol. 12 (4)
Open AccessA comprehensive method for the sampling, purification, extraction, and quantification of microplastic fibre release in textile production
The release of microplastics from the textile industry is a significant environmental concern. While the release of microplastics during the laundering process and within wastewater treatment plants has been extensively studied, there is still a pressing need for a standardised sampling protocol to assess microplastic release across various matrices involved in different textile production processes. In this report, we propose a comprehensive sampling protocol targeting four types of samples derived from textile production processes: sludge, wastewater, dust, and air. We also provide a detail method for the extraction and analysis of microplastics from these samples, including the separation of microplastics from collected textile samples through cellulose dissolution, oxidation, and oleophilic extraction processes, as well as heat treatment for air samples. This is followed by automated methods for quantifying microplastic fibres. The proposed protocol provides an efficient, effective, straightforward, cost-effective, and safe approach for analysing and monitoring textile-related microplastics.
- 8 August 2011
- Published by Wiley in Journal of Applied Polymer Science
- Vol. 123 (2) , 749-762
Morphology, reversible phase crystallization, and thermal sensitive shape memory effect of cellulose whisker/SMPU nano‐composites
To investigate the morphology, crystallization properties of reversible phase and thermal sensitive shape memory properties of CW/SMPU (Cellulose Whisker/Shape Memory Polyurethane) nano‐composite, the CW/SMPU nano‐composite having CW contents of 0.1–3.8 wt % were prepared. SEM investigation showed the evolution of reversible phase morphology from spherolite crystallization structure to uniform matrix with tiny CW aggregates with the addition of CW into the SMPU matrix. DSC and isothermal crystallization kinetic method revealed the effect of CW on crystallization properties of reversible phase and fixed phase, suggesting that the effect of CW on the crystallization of hard segment phase is not comparable with thermal history; the more CW causes the higher crystallization rate of reversible phase; the crystallization mechanism of reversible phase in nano‐composite gradually evolves to heterogeneous nucleation and crystal growth in two dimensions with the increase of CW content; the excellent nucleation effect of CW for the reversible phase leads to the drop of activity energy from 134.1 kJ/mol (N‐0), to 95.1 kJ/mol (N‐4). Cyclic tensile tests illustrate the addition of CW content can engender rapid shape fixity ability after a relative short cooling time; the shape fixity ratio of nano‐composite and the control sample after sufficient cooling all can be identically high. © 2011 Wiley Periodicals, Inc. J Appl Polym Sci, 2011
- 8 August 2011
- Published by Wiley in Journal of Applied Polymer Science
- Vol. 123 (2) , 749-762
Morphology, reversible phase crystallization, and thermal sensitive shape memory effect of cellulose whisker/SMPU nano‐composites
To investigate the morphology, crystallization properties of reversible phase and thermal sensitive shape memory properties of CW/SMPU (Cellulose Whisker/Shape Memory Polyurethane) nano‐composite, the CW/SMPU nano‐composite having CW contents of 0.1–3.8 wt % were prepared. SEM investigation showed the evolution of reversible phase morphology from spherolite crystallization structure to uniform matrix with tiny CW aggregates with the addition of CW into the SMPU matrix. DSC and isothermal crystallization kinetic method revealed the effect of CW on crystallization properties of reversible phase and fixed phase, suggesting that the effect of CW on the crystallization of hard segment phase is not comparable with thermal history; the more CW causes the higher crystallization rate of reversible phase; the crystallization mechanism of reversible phase in nano‐composite gradually evolves to heterogeneous nucleation and crystal growth in two dimensions with the increase of CW content; the excellent nucleation effect of CW for the reversible phase leads to the drop of activity energy from 134.1 kJ/mol (N‐0), to 95.1 kJ/mol (N‐4). Cyclic tensile tests illustrate the addition of CW content can engender rapid shape fixity ability after a relative short cooling time; the shape fixity ratio of nano‐composite and the control sample after sufficient cooling all can be identically high. © 2011 Wiley Periodicals, Inc. J Appl Polym Sci, 2011
- 20 October 2008
- Published by Wiley in Journal of Applied Polymer Science
- Vol. 111 (3) , 1156-1164
The influence of heat treatment on the properties of shape memory fibers. II. Tensile properties, dimensional stability, recovery force relaxation, and thermomechanical cyclic properties
Shape memory fibers (SMFs) were prepared via a melt spinning process. The fibers were subject to different heat treatments to eliminate internal stress and structure deficiency caused during the melt spinning process. The influences of heat treatments on the SMF thermal properties, molecular orientation, tensile properties, dimensional stability, recovery force relaxation, and thermomechanical cyclic properties were studied. It was found that the heat treatments increased soft segment crystallinity and phase separation while decreased molecular orientation. The low‐temperature heat treatment increased the breaking elongation, shape fixity ratios, and decreased boiling water shrinkage while shape recovery ratios were decreased. High‐temperature treatment increased both the shape recovery ratios, fixity ratios, recovery stress stability and at the same time decreasing the fiber mechanical strength. The results from differential scanning calorimetry, molecular orientation apparatus, and cyclic tensile testing were used to illustrate the mechanism governing the mechanical properties and shape memory effect. To obtain comprehensive outstanding properties, the SMF is expected to be treated at a high temperature because of the hard segment high glass transition temperature. Unfortunately, the heat treatment could not be conducted at a too high temperature because the SMF became too tacky and soft due to the melting of the soft segment phase. © 2008 Wiley Periodicals, Inc. J Appl Polym Sci, 2009
- 20 October 2008
- Published by Wiley in Journal of Applied Polymer Science
- Vol. 111 (3) , 1156-1164
The influence of heat treatment on the properties of shape memory fibers. II. Tensile properties, dimensional stability, recovery force relaxation, and thermomechanical cyclic properties
Shape memory fibers (SMFs) were prepared via a melt spinning process. The fibers were subject to different heat treatments to eliminate internal stress and structure deficiency caused during the melt spinning process. The influences of heat treatments on the SMF thermal properties, molecular orientation, tensile properties, dimensional stability, recovery force relaxation, and thermomechanical cyclic properties were studied. It was found that the heat treatments increased soft segment crystallinity and phase separation while decreased molecular orientation. The low‐temperature heat treatment increased the breaking elongation, shape fixity ratios, and decreased boiling water shrinkage while shape recovery ratios were decreased. High‐temperature treatment increased both the shape recovery ratios, fixity ratios, recovery stress stability and at the same time decreasing the fiber mechanical strength. The results from differential scanning calorimetry, molecular orientation apparatus, and cyclic tensile testing were used to illustrate the mechanism governing the mechanical properties and shape memory effect. To obtain comprehensive outstanding properties, the SMF is expected to be treated at a high temperature because of the hard segment high glass transition temperature. Unfortunately, the heat treatment could not be conducted at a too high temperature because the SMF became too tacky and soft due to the melting of the soft segment phase. © 2008 Wiley Periodicals, Inc. J Appl Polym Sci, 2009
- 4 August 2008
- Published by Wiley in Polymers for Advanced Technologies
- Vol. 19 (12) , 1745-1753
Shape memory fiber spun with segmented polyurethane ionomer
The effect of cationic groups within hard segments on shape memory polyurethane (SMPU) fibers was studied and the cyclic tensile testing was conducted to assess the shape memory effect. Mechanical properties, hard segment crystallization, and dynamic mechanical properties of SMPU ionomer fibers composed of 1,4‐butanediol (BDO), N‐methyldiethanolamine (NMDA), 4,4′‐methylenebis(phenyl isocyanate) (MDI), and poly(butylene adipate)diol (PBA) were investigated using a universal tensile tester, differential scanning calorimetry (DSC), and dynamic mechanical analysis (DMA). The results demonstrate that only 2 wt% NMDA can significantly change the glass transition temperature of the soft segment phase. DSC shows that the ionic group within hard segments can facilitate the crystallization of hard segments in unsteamed SMPU ionomer fibers. But for steamed fiber specimens, this effect is insignificant. Moreover, the ionic groups in hard segments with different hard segment contents (HSC) have different effects. In unsteamed fibers with 64 wt% HSC, 2 wt% NMDA increases the glass transition of soft segments from 63.5 to 70.6°C. However, in fibers with 55 wt% HSC, the glass transition temperature is lowered from 46.7 to 33.5°C. The post‐treatment, high‐pressure steaming is an effective way to remove the internal stress and subsequently improve the dimensional stability of SMPU ionomer fibers. Copyright © 2008 John Wiley & Sons, Ltd.
- 4 August 2008
- Published by Wiley in Polymers for Advanced Technologies
- Vol. 19 (12) , 1745-1753
Shape memory fiber spun with segmented polyurethane ionomer
The effect of cationic groups within hard segments on shape memory polyurethane (SMPU) fibers was studied and the cyclic tensile testing was conducted to assess the shape memory effect. Mechanical properties, hard segment crystallization, and dynamic mechanical properties of SMPU ionomer fibers composed of 1,4‐butanediol (BDO), N‐methyldiethanolamine (NMDA), 4,4′‐methylenebis(phenyl isocyanate) (MDI), and poly(butylene adipate)diol (PBA) were investigated using a universal tensile tester, differential scanning calorimetry (DSC), and dynamic mechanical analysis (DMA). The results demonstrate that only 2 wt% NMDA can significantly change the glass transition temperature of the soft segment phase. DSC shows that the ionic group within hard segments can facilitate the crystallization of hard segments in unsteamed SMPU ionomer fibers. But for steamed fiber specimens, this effect is insignificant. Moreover, the ionic groups in hard segments with different hard segment contents (HSC) have different effects. In unsteamed fibers with 64 wt% HSC, 2 wt% NMDA increases the glass transition of soft segments from 63.5 to 70.6°C. However, in fibers with 55 wt% HSC, the glass transition temperature is lowered from 46.7 to 33.5°C. The post‐treatment, high‐pressure steaming is an effective way to remove the internal stress and subsequently improve the dimensional stability of SMPU ionomer fibers. Copyright © 2008 John Wiley & Sons, Ltd.
- 28 March 2008
- Published by Wiley in Journal of Applied Polymer Science
- Vol. 109 (1) , 406-411
Preparation of polyurethane nanofibers by electrospinning
Polyurethane (PU) nanofibers were prepared by the electrospinning method. The process parameters, including the applied voltage, feeding rate, and solution concentration, were investigated carefully. The results showed that the resultant nanofibers, electrospun from PU/N,N‐dimethylformamide (DMF) solutions, had ultrafine diameters ranging from about 700 to 50 nm. In addition, it was found that the diameters and morphology of the nanofibers were influenced greatly by the process parameters. In particular, the solution concentration played a main role in influencing the transformation of the polymer solution into ultrafine fibers, and the diameters increased with the solution concentrations increasing. Finally, it was concluded that uniform PU nanofibers without beads or curls could be prepared by electrospinning through good control of the process parameters, such as 5.0–7.0 wt % PU/DMF solutions, 10–15‐kV applied voltages, and 0.06–0.08 mm/min feeding rates. © 2008 Wiley Periodicals, Inc. J Appl Polym Sci, 2008
- 28 March 2008
- Published by Wiley in Journal of Applied Polymer Science
- Vol. 109 (1) , 406-411
Preparation of polyurethane nanofibers by electrospinning
Polyurethane (PU) nanofibers were prepared by the electrospinning method. The process parameters, including the applied voltage, feeding rate, and solution concentration, were investigated carefully. The results showed that the resultant nanofibers, electrospun from PU/N,N‐dimethylformamide (DMF) solutions, had ultrafine diameters ranging from about 700 to 50 nm. In addition, it was found that the diameters and morphology of the nanofibers were influenced greatly by the process parameters. In particular, the solution concentration played a main role in influencing the transformation of the polymer solution into ultrafine fibers, and the diameters increased with the solution concentrations increasing. Finally, it was concluded that uniform PU nanofibers without beads or curls could be prepared by electrospinning through good control of the process parameters, such as 5.0–7.0 wt % PU/DMF solutions, 10–15‐kV applied voltages, and 0.06–0.08 mm/min feeding rates. © 2008 Wiley Periodicals, Inc. J Appl Polym Sci, 2008
- 29 May 2007
- Published by IOP Publishing in Smart Materials and Structures
- Vol. 16 (4) , 969-981
Effect of steaming on shape memory polyurethane fibers with various hard segment contents
- 29 May 2007
- Published by IOP Publishing in Smart Materials and Structures
- Vol. 16 (4) , 969-981
Effect of steaming on shape memory polyurethane fibers with various hard segment contents
- 4 May 2007
- Published by IOP Publishing in Smart Materials and Structures
- Vol. 16 (3) , 830-836
An electro-active shape memory fibre by incorporating multi-walled carbon nanotubes
- 4 May 2007
- Published by IOP Publishing in Smart Materials and Structures
- Vol. 16 (3) , 830-836
An electro-active shape memory fibre by incorporating multi-walled carbon nanotubes
- 24 April 2007
- Published by IOP Publishing in Smart Materials and Structures
- Vol. 16 (3) , 748-753
A prerequisite for the effective transfer of the shape-memory effect to cotton fibers
- 24 April 2007
- Published by IOP Publishing in Smart Materials and Structures
- Vol. 16 (3) , 748-753
A prerequisite for the effective transfer of the shape-memory effect to cotton fibers
- 2 April 2007
- Published by Wiley in Journal of Applied Polymer Science
- Vol. 105 (2) , 765-770
Segment self‐orientational behavior in shape memory polymer thin films probed by Raman spectroscopy
- 2 April 2007
- Published by Wiley in Journal of Applied Polymer Science
- Vol. 105 (2) , 765-770
Segment self‐orientational behavior in shape memory polymer thin films probed by Raman spectroscopy
- 25 September 2006
- Published by IOP Publishing in Smart Materials and Structures
- Vol. 15 (6) , 1547-1554
Smart polymer fibers with shape memory effect
- 25 September 2006
- Published by IOP Publishing in Smart Materials and Structures
- Vol. 15 (6) , 1547-1554
Smart polymer fibers with shape memory effect