Yurii S. Nechaev
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Previous Organizations / Institutes
The organizations / institutes from the scholar's other articles in the past ten years
Yurii S. Nechaev has a total of 24 co-authors. Here are the top co-authors by number of shared publications:
N. A. Shurygina
Scientific Center of Metals Science and Physics, Bardin Central Research Institute for Ferrous Metallurgy, Moscow, Russia
10 shared publicationsA. O. Cheretaeva
Institute of Progressive Technologies, Togliatti State University, Togliatti, Russia
7 shared publicationsE. A. Denisov
Physics Department, St. Petersburg State University
7 shared publications- Alisa O. Cheretaeva
Togliatti State University, Togliatti, Russia
6 shared publications N. M. Alexandrova
Scientific Center of Metals Science and Physics, Bardin Central Research Institute for Ferrous Metallurgy, Moscow, Russia
6 shared publicationsE. K. Kostikova
Institute of Applied Mathematical Research, Karelian Research Center, Russian Academy of Sciences, Petrozavodsk, Russia
5 shared publications
Latest Publications
- 1 June 2025
- Published by Pleiades Publishing Ltd in Journal of Surface Investigation: X-Ray, Synchrotron and Neutron Techniques
- Vol. 19 (3) , 598-604
On Clustering in Real Cottrell Nanosegregations in Metallic Materials
By analyzing some known data of 3D atomic force microscopy for metallic materials and a number of other theoretical and experimental results, including data on the dislocation dissolution of cementite in pearlitic and martensitic steels, clustering in real Cottrell atmospheres (nanosegregations) is considered and their characteristics, including the number of impurity atoms per dislocation of atomic length, are determined, which differ significantly from those corresponding to classical theoretical models. In particular, Cottrell boron nanosegregations on edge dislocations in an ordered intermetallic compound FeAl containing 40 at % Al and 0.04 at % B, as well as Cottrell carbon nanosegregations on screw dislocations in martensitic steel, are examined. The presence of Fe3B- and Fe3C-type clustering in such nanosegregations, which is not taken into account in the framework of the classical models of Cottrell atmospheres (clouds), is shown. It is shown that in metallic materials (FeAl–B, Fe–C, Al–Fe, Pd–H) in real atmospheres (nanosegregations) on dislocations a certain clustering takes place (including the formation of boride-like, carbide-like, intermetallic-like, and hydride-like structures), which differs from that of the classical theoretical models of Cottrell atmospheres. In particular, the methodology for determining the impurity diffusion coefficient in the areas of nanosegregations on dislocations in metallic materials is considered using Pd–H, Al–Fe, and Fe–C systems as an example.
- 1 June 2025
- Published by Pleiades Publishing Ltd in Journal of Surface Investigation: X-Ray, Synchrotron and Neutron Techniques
- Vol. 19 (3) , 598-604
On Clustering in Real Cottrell Nanosegregations in Metallic Materials
By analyzing some known data of 3D atomic force microscopy for metallic materials and a number of other theoretical and experimental results, including data on the dislocation dissolution of cementite in pearlitic and martensitic steels, clustering in real Cottrell atmospheres (nanosegregations) is considered and their characteristics, including the number of impurity atoms per dislocation of atomic length, are determined, which differ significantly from those corresponding to classical theoretical models. In particular, Cottrell boron nanosegregations on edge dislocations in an ordered intermetallic compound FeAl containing 40 at % Al and 0.04 at % B, as well as Cottrell carbon nanosegregations on screw dislocations in martensitic steel, are examined. The presence of Fe3B- and Fe3C-type clustering in such nanosegregations, which is not taken into account in the framework of the classical models of Cottrell atmospheres (clouds), is shown. It is shown that in metallic materials (FeAl–B, Fe–C, Al–Fe, Pd–H) in real atmospheres (nanosegregations) on dislocations a certain clustering takes place (including the formation of boride-like, carbide-like, intermetallic-like, and hydride-like structures), which differs from that of the classical theoretical models of Cottrell atmospheres. In particular, the methodology for determining the impurity diffusion coefficient in the areas of nanosegregations on dislocations in metallic materials is considered using Pd–H, Al–Fe, and Fe–C systems as an example.
- 16 July 2024
- Published by The Russian Academy of Sciences in Poverhnostʹ. Rentgenovskie, sinhrotronnye i nejtronnye issledovaniâ
- No. 2,p. 18-25
Calorimetric and Volumetric Studies of Dislocations During Martensitic Transformations in Shape Memory TiNi Alloy
Based on the use of appropriate approaches, methods and results of the analysis of a number of topical problems of physical materials science, an in-depth analysis has been done of calorimetric and volumetric data for direct, reverse and deformation martensitic transformations in a nanostructured Ti49.3Ni50.7 shape memory alloy obtained by cold rolling with simultaneous action of pulsed high-density current. For the first time, by applying a new technique for processing calorimetric spectra (peaks), the staging and “kinetics” of changes in heat content, as well as thermal effects (enthalpies of individual stages) during direct and reverse martensitic transformations during cooling or heating of samples at a constant rate (3 × K/ min) in the range 170–370 K has been done. It is shown, by processing volumetric data, using theoretical values of the dislocation density and elements of the classical theory of dislocations, that in the Ti49.3Ni50.7 shape memory alloy subjected to cold deformation accompanied by the action of a pulsed current, a deformation martensitic transformation occurs, leading to a positive volume effect (∆V/V) ≈ 3 × 10–3), which can be largely due to dislocations. It is shown, by applying the theoretical values of the dislocation density and elements of the classical theory of dislocations, that the possible contributions of dislocations to the enthalpies of direct and reverse martensitic transformations (in the Ti49.3Ni50.7 alloy) can and should be significantly lower in absolute value, but opposite in sign to the observed enthalpies of direct and reverse martensitic transformation in a given alloy. It is shown that the physics of the processes under consideration is contained to a certain extent in scientific discoveries No. 239 “The phenomenon of thermoelastic equilibrium during phase transformations of the martensitic type – the Kurdyumov effect” and No. 339 “The phenomenon of the formation of non-equilibrium grain boundaries in polycrystals when they absorb lattice dislocations”.
- 16 July 2024
- Published by The Russian Academy of Sciences in Poverhnostʹ. Rentgenovskie, sinhrotronnye i nejtronnye issledovaniâ
- No. 2,p. 18-25
Calorimetric and Volumetric Studies of Dislocations During Martensitic Transformations in Shape Memory TiNi Alloy
Based on the use of appropriate approaches, methods and results of the analysis of a number of topical problems of physical materials science, an in-depth analysis has been done of calorimetric and volumetric data for direct, reverse and deformation martensitic transformations in a nanostructured Ti49.3Ni50.7 shape memory alloy obtained by cold rolling with simultaneous action of pulsed high-density current. For the first time, by applying a new technique for processing calorimetric spectra (peaks), the staging and “kinetics” of changes in heat content, as well as thermal effects (enthalpies of individual stages) during direct and reverse martensitic transformations during cooling or heating of samples at a constant rate (3 × K/ min) in the range 170–370 K has been done. It is shown, by processing volumetric data, using theoretical values of the dislocation density and elements of the classical theory of dislocations, that in the Ti49.3Ni50.7 shape memory alloy subjected to cold deformation accompanied by the action of a pulsed current, a deformation martensitic transformation occurs, leading to a positive volume effect (∆V/V) ≈ 3 × 10–3), which can be largely due to dislocations. It is shown, by applying the theoretical values of the dislocation density and elements of the classical theory of dislocations, that the possible contributions of dislocations to the enthalpies of direct and reverse martensitic transformations (in the Ti49.3Ni50.7 alloy) can and should be significantly lower in absolute value, but opposite in sign to the observed enthalpies of direct and reverse martensitic transformation in a given alloy. It is shown that the physics of the processes under consideration is contained to a certain extent in scientific discoveries No. 239 “The phenomenon of thermoelastic equilibrium during phase transformations of the martensitic type – the Kurdyumov effect” and No. 339 “The phenomenon of the formation of non-equilibrium grain boundaries in polycrystals when they absorb lattice dislocations”.
- 1 February 2024
- Published by Pleiades Publishing Ltd in Journal of Surface Investigation: X-Ray, Synchrotron and Neutron Techniques
- Vol. 18 (1) , 135-141
Calorimetric and Volumetric Studies of Dislocations during Martensitic Transformations in TiNi Alloy with Shape Memory
An in-depth analysis of calorimetric and volumetric data for direct, reverse, and deformation martensitic transformations in the nanostructured alloy Ti49.3Ni50.7 with shape memory is carried out. The samples are obtained by cold rolling with the simultaneous action of a high-density pulsed current. A new technique for processing calorimetry spectra is applied, with the help of which, for the first time, the staging and kinetics of changes in the heat content are studied in detail, as well as thermal effects (enthalpy of individual stages) during direct and reverse martensitic transformations occurring under the influence of temperature. By processing volumetric data, using theoretical values of the dislocation density and elements of classical dislocation theory, it is shown that in the Ti49.3Ni50.7 alloy with shape memory subjected to cold plane deformation (rolling) accompanied by the action of a pulsed current, a strain-induced martensitic transformation occurs. This transformation results in a positive volume effect (∆V/V ≈ 3 × 10–3), which can be largely due to dislocations. It is demonstrated that the possible contributions of dislocations to the enthalpy of direct and reverse martensitic transformations in the Ti49.3Ni50.7 alloy can and should be significantly lower in absolute value, but opposite in sign relative to the observed enthalpy of direct and reverse martensitic transformations in this alloy.
- 1 February 2024
- Published by Pleiades Publishing Ltd in Journal of Surface Investigation: X-Ray, Synchrotron and Neutron Techniques
- Vol. 18 (1) , 135-141
Calorimetric and Volumetric Studies of Dislocations during Martensitic Transformations in TiNi Alloy with Shape Memory
An in-depth analysis of calorimetric and volumetric data for direct, reverse, and deformation martensitic transformations in the nanostructured alloy Ti49.3Ni50.7 with shape memory is carried out. The samples are obtained by cold rolling with the simultaneous action of a high-density pulsed current. A new technique for processing calorimetry spectra is applied, with the help of which, for the first time, the staging and kinetics of changes in the heat content are studied in detail, as well as thermal effects (enthalpy of individual stages) during direct and reverse martensitic transformations occurring under the influence of temperature. By processing volumetric data, using theoretical values of the dislocation density and elements of classical dislocation theory, it is shown that in the Ti49.3Ni50.7 alloy with shape memory subjected to cold plane deformation (rolling) accompanied by the action of a pulsed current, a strain-induced martensitic transformation occurs. This transformation results in a positive volume effect (∆V/V ≈ 3 × 10–3), which can be largely due to dislocations. It is demonstrated that the possible contributions of dislocations to the enthalpy of direct and reverse martensitic transformations in the Ti49.3Ni50.7 alloy can and should be significantly lower in absolute value, but opposite in sign relative to the observed enthalpy of direct and reverse martensitic transformations in this alloy.
- 8 December 2023
- Published by Pleiades Publishing Ltd in Journal of Surface Investigation: X-Ray, Synchrotron and Neutron Techniques
- Vol. 17 (6) , 1395-1404
Cottrell Cosegregations of Carbon and Hydrogen: Characteristics and Role in the Strain Aging and Embrittlement of Steels
This study investigates the characteristics of phase-like Cottrell atmospheres, which are carbohydride-like cosegregations of carbon and hydrogen, present at dislocations within the martensitic and ferritic components of high-strength austenitic steel with transformation-induced plasticity. The research addresses concerns related to aging, hydrogen embrittlement, and the degradation of certain steels during operational use. A key focus is placed on the development of an in-depth processing technique and analysis of the thermal-desorption spectra of hydrogen across several steel samples and iron (used as a reference material). The investigation involves employing thermodynamic analysis and a methodology for determining the thermodynamic parameters, including hydrogen concentrations, activation energies, and desorption-process rate constants. Additionally, the study aims to identify the nature of hydrogen traps by analyzing comprehensive thermal-desorption data. These findings are then compared with theoretical data and corresponding information obtained through three-dimensional atomic-probe tomography. The results demonstrate the potential formation of Cottrell carbohydride-like cosegregations of carbon and hydrogen at dislocations in both martensitic and ferritic phases within high-strength austenitic steel exhibiting high plasticity due to transformation. The research provides novel insights into the binding energies of hydrogen associated with carbohydride-like cosegregations of carbon and hydrogen along dislocations in these martensitic and ferritic phases.
- 8 December 2023
- Published by Pleiades Publishing Ltd in Journal of Surface Investigation: X-Ray, Synchrotron and Neutron Techniques
- Vol. 17 (6) , 1395-1404
Cottrell Cosegregations of Carbon and Hydrogen: Characteristics and Role in the Strain Aging and Embrittlement of Steels
This study investigates the characteristics of phase-like Cottrell atmospheres, which are carbohydride-like cosegregations of carbon and hydrogen, present at dislocations within the martensitic and ferritic components of high-strength austenitic steel with transformation-induced plasticity. The research addresses concerns related to aging, hydrogen embrittlement, and the degradation of certain steels during operational use. A key focus is placed on the development of an in-depth processing technique and analysis of the thermal-desorption spectra of hydrogen across several steel samples and iron (used as a reference material). The investigation involves employing thermodynamic analysis and a methodology for determining the thermodynamic parameters, including hydrogen concentrations, activation energies, and desorption-process rate constants. Additionally, the study aims to identify the nature of hydrogen traps by analyzing comprehensive thermal-desorption data. These findings are then compared with theoretical data and corresponding information obtained through three-dimensional atomic-probe tomography. The results demonstrate the potential formation of Cottrell carbohydride-like cosegregations of carbon and hydrogen at dislocations in both martensitic and ferritic phases within high-strength austenitic steel exhibiting high plasticity due to transformation. The research provides novel insights into the binding energies of hydrogen associated with carbohydride-like cosegregations of carbon and hydrogen along dislocations in these martensitic and ferritic phases.
- 1 December 2023
- Published by The Russian Academy of Sciences in Poverhnostʹ. Rentgenovskie, sinhrotronnye i nejtronnye issledovaniâ
- No. 12,p. 90-100
On the Characteristics and Role of Cottrell Co-Segregations of Carbon and Hydrogen in Strain Aging and Embrittlement of a Number of Steels
The work is devoted to the study of the characteristics of Cottrell’s phase-like “atmospheres” (carbohydride-like cosegregations of carbon and hydrogen) on dislocations in the martensitic and ferritic components in high-strength austenitic steel with transformation-induced plasticity due to the problems of aging, hydrogen embrittlement and degradation of a number of steels during operation. Particular attention is paid to in-depth processing (new technique) and analysis of the thermal desorption spectra of hydrogen for a number of steels and iron (as a reference material). The methods of thermodynamic analysis, the methodology for determining the thermodynamic characteristics (hydrogen concentrations, activation energies and rate constants of desorption processes) and the nature of “hydrogen traps” by analyzing the most representative thermal desorption data, comparing with the corresponding data obtained by three-dimensional atomic probe tomography, and also comparisons with the corresponding theoretical data. The conducted studies have shown the possibility of the formation of Cottrell carbohydride-like cosegregations of carbon and hydrogen on dislocations in martensitic and ferritic phases in high-strength austenitic steel with high plasticity induced by transformation, in particular, they made it possible for the first time to determine the binding energies of hydrogen with carbohydride-like cosegregations of carbon and hydrogen on dislocations in martensitic and ferritic phases.
- 1 December 2023
- Published by The Russian Academy of Sciences in Poverhnostʹ. Rentgenovskie, sinhrotronnye i nejtronnye issledovaniâ
- No. 12,p. 90-100
On the Characteristics and Role of Cottrell Co-Segregations of Carbon and Hydrogen in Strain Aging and Embrittlement of a Number of Steels
The work is devoted to the study of the characteristics of Cottrell’s phase-like “atmospheres” (carbohydride-like cosegregations of carbon and hydrogen) on dislocations in the martensitic and ferritic components in high-strength austenitic steel with transformation-induced plasticity due to the problems of aging, hydrogen embrittlement and degradation of a number of steels during operation. Particular attention is paid to in-depth processing (new technique) and analysis of the thermal desorption spectra of hydrogen for a number of steels and iron (as a reference material). The methods of thermodynamic analysis, the methodology for determining the thermodynamic characteristics (hydrogen concentrations, activation energies and rate constants of desorption processes) and the nature of “hydrogen traps” by analyzing the most representative thermal desorption data, comparing with the corresponding data obtained by three-dimensional atomic probe tomography, and also comparisons with the corresponding theoretical data. The conducted studies have shown the possibility of the formation of Cottrell carbohydride-like cosegregations of carbon and hydrogen on dislocations in martensitic and ferritic phases in high-strength austenitic steel with high plasticity induced by transformation, in particular, they made it possible for the first time to determine the binding energies of hydrogen with carbohydride-like cosegregations of carbon and hydrogen on dislocations in martensitic and ferritic phases.
- 1 August 2022
- Published by Pleiades Publishing Ltd in Kinetics and Catalysis
- Vol. 63 (4) , 449-461
On Fundamental Aspects of Solving the Problem of “Super” Storage of Hydrogen in Catalytically Synthetized Graphite Nanofibers
This work considered some fundamental aspects (basics) of solving the long-term (discussed by many researchers for about 25 years) problem of “super” storage (in Maeland’s terminology) of “reversible” hydrogen (about 20–30 wt %) and “irreversible” hydrogen (about 7–10 wt %) in catalytically synthesized graphite nanofibers (GNFs). The problem was formulated in connection with the experimental results (obtained by Rodriguez and Baker’s group), which were patented and published in 1997–2005, and which other researchers could neither reproduce (except, to a certain extent, Gupta’s group (2000–2006)), nor reveal their physics. A deeper study of this important problem and the identification of a number of fundamental (including kinetic and thermodynamic) aspects of solving this problem were made using a modified efficient method for processing and analyzing the hydrogen thermal desorption spectra and their related thermogravimetric and other data. For the first time, the characteristics of the main desorption peak of irreversible hydrogen in graphite nanofibers, which correspond to a first-order kinetic process, were determined both from thermal desorption and thermogravimetric data. These characteristics were the temperature of the highest desorption rate (Tmax = 914–923 K), the activation energy of the desorption process (Q ≈ 40 kJ/mol), the pre-exponential rate constant factor (K0 ≈ 2 × 10–1 s–1), and the amount of the released hydrogen (~8 wt %; i.e., the atomic ratio H : C ≈ 1). The physics of the processes of super sorption of irreversible and reversible hydrogen was analyzed, including the role of hydrogen diffusion processes accompanied by the “reversible” capture of the diffusant by certain sorption sites, the role of the hydrogen spillover effect causing the local atomization of gaseous H2 during the GNFs hydrogenation, and the role of the Kurdyumov phenomenon of thermoelastic phase equilibrium. It was shown that the above extraordinary data on the super storage of hydrogen in GNFs are neither an error, nor a hoax, as most researchers believe. The necessary conditions for reproducing these extraordinary results by other researchers were determined. It was shown, in particular, that Rodriguez and Baker’s group can reproduce the “normal” results (about 0.1–4 wt %) on the storage of hydrogen in GNFs obtained by other researchers.
- 1 August 2022
- Published by Pleiades Publishing Ltd in Kinetics and Catalysis
- Vol. 63 (4) , 449-461
On Fundamental Aspects of Solving the Problem of “Super” Storage of Hydrogen in Catalytically Synthetized Graphite Nanofibers
This work considered some fundamental aspects (basics) of solving the long-term (discussed by many researchers for about 25 years) problem of “super” storage (in Maeland’s terminology) of “reversible” hydrogen (about 20–30 wt %) and “irreversible” hydrogen (about 7–10 wt %) in catalytically synthesized graphite nanofibers (GNFs). The problem was formulated in connection with the experimental results (obtained by Rodriguez and Baker’s group), which were patented and published in 1997–2005, and which other researchers could neither reproduce (except, to a certain extent, Gupta’s group (2000–2006)), nor reveal their physics. A deeper study of this important problem and the identification of a number of fundamental (including kinetic and thermodynamic) aspects of solving this problem were made using a modified efficient method for processing and analyzing the hydrogen thermal desorption spectra and their related thermogravimetric and other data. For the first time, the characteristics of the main desorption peak of irreversible hydrogen in graphite nanofibers, which correspond to a first-order kinetic process, were determined both from thermal desorption and thermogravimetric data. These characteristics were the temperature of the highest desorption rate (Tmax = 914–923 K), the activation energy of the desorption process (Q ≈ 40 kJ/mol), the pre-exponential rate constant factor (K0 ≈ 2 × 10–1 s–1), and the amount of the released hydrogen (~8 wt %; i.e., the atomic ratio H : C ≈ 1). The physics of the processes of super sorption of irreversible and reversible hydrogen was analyzed, including the role of hydrogen diffusion processes accompanied by the “reversible” capture of the diffusant by certain sorption sites, the role of the hydrogen spillover effect causing the local atomization of gaseous H2 during the GNFs hydrogenation, and the role of the Kurdyumov phenomenon of thermoelastic phase equilibrium. It was shown that the above extraordinary data on the super storage of hydrogen in GNFs are neither an error, nor a hoax, as most researchers believe. The necessary conditions for reproducing these extraordinary results by other researchers were determined. It was shown, in particular, that Rodriguez and Baker’s group can reproduce the “normal” results (about 0.1–4 wt %) on the storage of hydrogen in GNFs obtained by other researchers.
- Open Access
On the Problem of “Super” Storage of Hydrogen in Graphite Nanofibers
This article is devoted to some fundamental aspects of “super” storage in graphite nanofibers (GNF) of “reversible” (~20–30 wt.%) and “irreversible” hydrogen (~7–10 wt.%). Extraordinary results for hydrogen “super” storage were previously published by the group of Rodriguez and Baker at the turn of the century, which been unable to be reproduced or explained in terms of physics by other researchers. For the first time, using an efficient method of processing and analysis of hydrogen thermal desorption spectra, the characteristics of the main desorption peak of “irreversible” hydrogen in GNF were determined: the temperature of the highest desorption rate (Tmax = 914–923 K), the activation energy of the desorption process (Q ≈ 40 kJ mol−1), the pre-exponential rate constant factor (K0 ≈ 2 × 10−1 s−1), and the amount of hydrogen released (~8 wt.%). The physics of hydrogen “super” sorption includes hydrogen diffusion, accompanied by the “reversible” capture of the diffusant by certain sorption “centers”; the hydrogen spillover effect, which provides local atomization of gaseous H2 during GNF hydrogenation; and the Kurdjumov phenomenon on thermoelastic phase equilibrium. It is shown that the above-mentioned extraordinary data on the hydrogen “super” storage in GNFs are neither a mistake nor a mystification, as most researchers believe.
Open AccessOn the Problem of “Super” Storage of Hydrogen in Graphite Nanofibers
This article is devoted to some fundamental aspects of “super” storage in graphite nanofibers (GNF) of “reversible” (~20–30 wt.%) and “irreversible” hydrogen (~7–10 wt.%). Extraordinary results for hydrogen “super” storage were previously published by the group of Rodriguez and Baker at the turn of the century, which been unable to be reproduced or explained in terms of physics by other researchers. For the first time, using an efficient method of processing and analysis of hydrogen thermal desorption spectra, the characteristics of the main desorption peak of “irreversible” hydrogen in GNF were determined: the temperature of the highest desorption rate (Tmax = 914–923 K), the activation energy of the desorption process (Q ≈ 40 kJ mol−1), the pre-exponential rate constant factor (K0 ≈ 2 × 10−1 s−1), and the amount of hydrogen released (~8 wt.%). The physics of hydrogen “super” sorption includes hydrogen diffusion, accompanied by the “reversible” capture of the diffusant by certain sorption “centers”; the hydrogen spillover effect, which provides local atomization of gaseous H2 during GNF hydrogenation; and the Kurdjumov phenomenon on thermoelastic phase equilibrium. It is shown that the above-mentioned extraordinary data on the hydrogen “super” storage in GNFs are neither a mistake nor a mystification, as most researchers believe.
- 1 February 2022
- Published by Pleiades Publishing Ltd in Journal of Surface Investigation: X-Ray, Synchrotron and Neutron Techniques
- Vol. 16 (1) , 145-150
On Hydrogen “Superstorage“ in Know-How Activated Graphite Nanofibers
The extraordinary, unreproduced data of Rodriguez, Baker, Gupta on the “superstorage” of “reversible” and “irreversible” hydrogen in activated graphite nanofibers are studied using an effective methodology for processing, analyzing and interpretating the thermal desorption and thermogravimetric spectra of hydrogen. The processing of data obtained by Rodriguez makes it possible to determine (by means of two independent methods) the characteristics of the main desorption peak of “irreversible” hydrogen for the first time, namely, the temperature of the highest desorption rate Tmax = 914–950 K, the desorption activation energy Q = 39 ± 3 kJ/mol, the frequency factor of the rate constant of the desorption process K0 ≈ 0.15 s–1, and the amount of evolved hydrogen ~7 wt % corresponding to an atomic ratio of H/C ≈ 0.9. These results can be considered as irrefutable evidence of the “superstorage” of “irreversible” hydrogen in specially activated graphite nanofibers. There is no peak in the thermal-desorption spectra of graphite nanofibers obtained by Rzepka, who unsuccessfully tried to reproduce the extraordinary results of Rodriguez. The presence of a desorption peak is obviously a characteristic feature (attribute) of specially activated graphite nanofibers, which is necessary for the multiple (at least 10 repeated desorption–adsorption cycles at room temperature) “superstorage” of “reversible” hydrogen in them (in the amount of ~20–30 wt %). The physics of the “superstorage” and processes of desorption–adsorption of “reversible” and “irreversible” hydrogen in graphite nanofibers is discussed. The analysis showed that there is a real possibility of reproducing the extraordinary results obtained by Rodriguez, but only in the case of revealing (disclosing) the know-how technology of the activation treatment of graphite nanofibers.
- 1 February 2022
- Published by Pleiades Publishing Ltd in Journal of Surface Investigation: X-Ray, Synchrotron and Neutron Techniques
- Vol. 16 (1) , 145-150
On Hydrogen “Superstorage“ in Know-How Activated Graphite Nanofibers
The extraordinary, unreproduced data of Rodriguez, Baker, Gupta on the “superstorage” of “reversible” and “irreversible” hydrogen in activated graphite nanofibers are studied using an effective methodology for processing, analyzing and interpretating the thermal desorption and thermogravimetric spectra of hydrogen. The processing of data obtained by Rodriguez makes it possible to determine (by means of two independent methods) the characteristics of the main desorption peak of “irreversible” hydrogen for the first time, namely, the temperature of the highest desorption rate Tmax = 914–950 K, the desorption activation energy Q = 39 ± 3 kJ/mol, the frequency factor of the rate constant of the desorption process K0 ≈ 0.15 s–1, and the amount of evolved hydrogen ~7 wt % corresponding to an atomic ratio of H/C ≈ 0.9. These results can be considered as irrefutable evidence of the “superstorage” of “irreversible” hydrogen in specially activated graphite nanofibers. There is no peak in the thermal-desorption spectra of graphite nanofibers obtained by Rzepka, who unsuccessfully tried to reproduce the extraordinary results of Rodriguez. The presence of a desorption peak is obviously a characteristic feature (attribute) of specially activated graphite nanofibers, which is necessary for the multiple (at least 10 repeated desorption–adsorption cycles at room temperature) “superstorage” of “reversible” hydrogen in them (in the amount of ~20–30 wt %). The physics of the “superstorage” and processes of desorption–adsorption of “reversible” and “irreversible” hydrogen in graphite nanofibers is discussed. The analysis showed that there is a real possibility of reproducing the extraordinary results obtained by Rodriguez, but only in the case of revealing (disclosing) the know-how technology of the activation treatment of graphite nanofibers.
- Open Access
Revealing Hydrogen States in Carbon Structures by Analyzing the Thermal Desorption Spectra
An effective methodology for the detailed analysis of thermal desorption spectra (TDS) of hydrogen in carbon structures at micro- and nanoscale was further developed and applied for a number of TDS data of one heating rate, in particular, for graphite materials irradiated with atomic hydrogen. The technique is based on a preliminary description of hydrogen desorption spectra by symmetric Gaussians with their special processing in the approximation of the first- and the second-order reactions. As a result, the activation energies and the pre-exponential factors of the rate constants of the hydrogen desorption processes are determined, analyzed and interpreted. Some final verification of the results was completed using methods of numerical simulation of thermal desorption peaks (non-Gaussians) corresponding to the first- and the second-order reactions. The main research finding of this work is a further refinement and/or disclosure of poorly studied characteristics and physics of various states of hydrogen in microscale graphite structures after irradiation with atomic hydrogen, and comparison with the related results for nanoscale carbon structures. This is important for understanding the behavior and relationship of hydrogen in a number of cases of high energy carbon-based materials and nanomaterials.
Open AccessRevealing Hydrogen States in Carbon Structures by Analyzing the Thermal Desorption Spectra
An effective methodology for the detailed analysis of thermal desorption spectra (TDS) of hydrogen in carbon structures at micro- and nanoscale was further developed and applied for a number of TDS data of one heating rate, in particular, for graphite materials irradiated with atomic hydrogen. The technique is based on a preliminary description of hydrogen desorption spectra by symmetric Gaussians with their special processing in the approximation of the first- and the second-order reactions. As a result, the activation energies and the pre-exponential factors of the rate constants of the hydrogen desorption processes are determined, analyzed and interpreted. Some final verification of the results was completed using methods of numerical simulation of thermal desorption peaks (non-Gaussians) corresponding to the first- and the second-order reactions. The main research finding of this work is a further refinement and/or disclosure of poorly studied characteristics and physics of various states of hydrogen in microscale graphite structures after irradiation with atomic hydrogen, and comparison with the related results for nanoscale carbon structures. This is important for understanding the behavior and relationship of hydrogen in a number of cases of high energy carbon-based materials and nanomaterials.
- 2 January 2022
- Published by Taylor & Francis in Fullerenes, Nanotubes and Carbon Nanostructures
- Vol. 30 (1) , 211-219
On the real possibility of “super” hydrogen intercalation into graphite nanofibers
In this work, data of Rodriguez-Baker et al. and some others were analyzed and interpreted in relation to the long-term, i.e., about 25 years, problem of “super” storage (intercalation) of “reversible” (at 300 K) hydrogen (∼38 ± 10 wt.%, i.e., the atomic ratio (H/C) ≈ 7 ± 3)), along with “irreversible” hydrogen (∼11 ± 3 wt.% ((H/C) ≈ 1.5 ± 0.4)) into graphite nanofibers (GNFs). For a more in-depth study of the a problem, an effective methodology of processing and analyzing the thermal desorption spectra of hydrogen and the related thermogravimetric data was modified and used. It was shown that the above noted extraordinary data on the “super” storage of hydrogen in GNFs are neither an error nor a hoax, as most researchers believed. The necessary conditions were determined to reproduce this extraordinary data. It has also been shown that the Rodriguez-Baker team can reproduce “normal,” i.e., typical results obtained by other researchers on hydrogen storage in GNFs.
- 2 January 2022
- Published by Taylor & Francis in Fullerenes, Nanotubes and Carbon Nanostructures
- Vol. 30 (1) , 211-219
On the real possibility of “super” hydrogen intercalation into graphite nanofibers
In this work, data of Rodriguez-Baker et al. and some others were analyzed and interpreted in relation to the long-term, i.e., about 25 years, problem of “super” storage (intercalation) of “reversible” (at 300 K) hydrogen (∼38 ± 10 wt.%, i.e., the atomic ratio (H/C) ≈ 7 ± 3)), along with “irreversible” hydrogen (∼11 ± 3 wt.% ((H/C) ≈ 1.5 ± 0.4)) into graphite nanofibers (GNFs). For a more in-depth study of the a problem, an effective methodology of processing and analyzing the thermal desorption spectra of hydrogen and the related thermogravimetric data was modified and used. It was shown that the above noted extraordinary data on the “super” storage of hydrogen in GNFs are neither an error nor a hoax, as most researchers believed. The necessary conditions were determined to reproduce this extraordinary data. It has also been shown that the Rodriguez-Baker team can reproduce “normal,” i.e., typical results obtained by other researchers on hydrogen storage in GNFs.