Yiyou Tu
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Previous Organizations / Institutes
The organizations / institutes from the scholar's other articles in the past ten years
Research Subjects
Yiyou Tu has a total of 99 co-authors. Here are the top co-authors by number of shared publications:
Jianqing Jiang
12 shared publicationsZhipeng Yuan
10 shared publicationsTing Yuan
9 shared publicationsXuefeng Zhou
School of Materials Science and Engineering, Southeast University 1 , Nanjing 211189, China
7 shared publicationsZenglei Ni
7 shared publicationsWandong Yang
5 shared publications
Latest Publications
- 17 August 2026
- Published by Wiley in Materials and Corrosion
Effect of Shot Peening on the Corrosion Behavior of 304 Austenitic Stainless Steel in Molten Solar Salt
The effect of shot peening on the corrosion behavior of 304 austenitic stainless steel in molten Solar Salt (60 wt% NaNO 3 + 40 wt% KNO 3 ) at 550°C was studied. Shot peening markedly improves the corrosion resistance of 304 austenitic stainless steel. Electrochemical tests show a 35.2% reduction in corrosion rate, with current density decreasing from 0.281 to 0.182 mA cm −2 . After 2000 h of immersion, shot‐peened samples form a thin, compact, and adherent oxide scale with negligible spallation, unlike the porous, cracked scale on untreated steel. The surface deformation layer (~50 μm) introduced by shot peening—characterized by grain refinement, high dislocation density, and dispersed martensite—enhances Cr diffusion to the oxidation front. This promotes Cr enrichment in the inner oxide layer and subsurface Ni accumulation, thereby suppressing Fe oxidation and improving scale protectiveness for Concentrated solar power (CSP) applications.
- 17 August 2026
- Published by Wiley in Materials and Corrosion
Effect of Shot Peening on the Corrosion Behavior of 304 Austenitic Stainless Steel in Molten Solar Salt
The effect of shot peening on the corrosion behavior of 304 austenitic stainless steel in molten Solar Salt (60 wt% NaNO 3 + 40 wt% KNO 3 ) at 550°C was studied. Shot peening markedly improves the corrosion resistance of 304 austenitic stainless steel. Electrochemical tests show a 35.2% reduction in corrosion rate, with current density decreasing from 0.281 to 0.182 mA cm −2 . After 2000 h of immersion, shot‐peened samples form a thin, compact, and adherent oxide scale with negligible spallation, unlike the porous, cracked scale on untreated steel. The surface deformation layer (~50 μm) introduced by shot peening—characterized by grain refinement, high dislocation density, and dispersed martensite—enhances Cr diffusion to the oxidation front. This promotes Cr enrichment in the inner oxide layer and subsurface Ni accumulation, thereby suppressing Fe oxidation and improving scale protectiveness for Concentrated solar power (CSP) applications.
- Open Access
- 19 May 2026
- Published by Wiley in Advanced Engineering Materials
- Vol. 28 (14) , e70931
Investigation of the Influence of Grain Size on the Oxidation and Corrosion Characteristics of 316L Stainless Steel in Static Liquid Lead–Bismuth Eutectic Environment at 500°C
This study systematically investigated how grain size affects the oxidation and corrosion behavior of 316L austenitic stainless steel when exposed to liquid lead–bismuth eutectic (LBE) at 500°C. The corrosion conditions were examined across a range of grain sizes, from 1.4 ± 0.33 to 98.6 ± 5.56 μm. The tests revealed that fine‐grained microstructures exhibited significantly accelerated degradation rates, with an internal oxidation depth that was 79% greater than that of coarse‐grained microstructures. Detailed transmission electron microscopy analysis confirms that grain boundaries act as preferential diffusion paths for oxygen and metal elements. Significant differences in grain boundary density directly induce variations in the internal oxide layer structure of 316L stainless steel, where the quantity and volume fraction of Fe–Ni‐rich phases directly determine the inability of the internal oxide layer in fine‐grained 316L to form a continuous protective scale. These findings provide a critical foundation for optimizing microstructural characteristics under LBE conditions, offering a basis for selecting materials that achieve the optimal balance between corrosion resistance and mechanical integrity in fourth‐generation lead‐cooled reactor containment systems. This work provides actionable recommendations for selecting structural materials for use in heavy liquid metal applications.
- 19 May 2026
- Published by Wiley in Advanced Engineering Materials
- Vol. 28 (14) , e70931
Open AccessInvestigation of the Influence of Grain Size on the Oxidation and Corrosion Characteristics of 316L Stainless Steel in Static Liquid Lead–Bismuth Eutectic Environment at 500°C
This study systematically investigated how grain size affects the oxidation and corrosion behavior of 316L austenitic stainless steel when exposed to liquid lead–bismuth eutectic (LBE) at 500°C. The corrosion conditions were examined across a range of grain sizes, from 1.4 ± 0.33 to 98.6 ± 5.56 μm. The tests revealed that fine‐grained microstructures exhibited significantly accelerated degradation rates, with an internal oxidation depth that was 79% greater than that of coarse‐grained microstructures. Detailed transmission electron microscopy analysis confirms that grain boundaries act as preferential diffusion paths for oxygen and metal elements. Significant differences in grain boundary density directly induce variations in the internal oxide layer structure of 316L stainless steel, where the quantity and volume fraction of Fe–Ni‐rich phases directly determine the inability of the internal oxide layer in fine‐grained 316L to form a continuous protective scale. These findings provide a critical foundation for optimizing microstructural characteristics under LBE conditions, offering a basis for selecting materials that achieve the optimal balance between corrosion resistance and mechanical integrity in fourth‐generation lead‐cooled reactor containment systems. This work provides actionable recommendations for selecting structural materials for use in heavy liquid metal applications.
- Open Access
Effects of Hot Compression on Grain Boundary Evolution and Twin Boundary Characteristics on the Material Properties of Inconel 617 Alloy
The evolution of grain size and special grain boundary in Inconel 617 alloy was analyzed by electron backscatter diffraction (EBSD). It was found that during hot compression, dynamic recrystallization (DRX) occurs, the grain size changes, and a twinning structure is generated, which then affects grain growth. In this paper, the high-angle grain boundaries (HAGBs) and low-angle grain boundaries (LAGBs) under different conditions were studied, and the formation mechanism of special twin boundaries and the proportion of these grain boundaries under different conditions were analyzed. In addition, it was found that the variation in twin boundaries is complex at different temperatures and strain rates, and the formation mechanism of special twin boundaries Σ3, Σ9, and Σ27 is also closely related to temperature and strain rate. Through electrochemical corrosion testing, it was further found that there is a positive relationship between the content of Σ3 and the corrosion resistance of the material. This paper provides theoretical guidance for the microstructural study of Inconel 617 alloy during plastic deformation.
Open AccessEffects of Hot Compression on Grain Boundary Evolution and Twin Boundary Characteristics on the Material Properties of Inconel 617 Alloy
The evolution of grain size and special grain boundary in Inconel 617 alloy was analyzed by electron backscatter diffraction (EBSD). It was found that during hot compression, dynamic recrystallization (DRX) occurs, the grain size changes, and a twinning structure is generated, which then affects grain growth. In this paper, the high-angle grain boundaries (HAGBs) and low-angle grain boundaries (LAGBs) under different conditions were studied, and the formation mechanism of special twin boundaries and the proportion of these grain boundaries under different conditions were analyzed. In addition, it was found that the variation in twin boundaries is complex at different temperatures and strain rates, and the formation mechanism of special twin boundaries Σ3, Σ9, and Σ27 is also closely related to temperature and strain rate. Through electrochemical corrosion testing, it was further found that there is a positive relationship between the content of Σ3 and the corrosion resistance of the material. This paper provides theoretical guidance for the microstructural study of Inconel 617 alloy during plastic deformation.
- Top Cited Papers
Effect of bending deformation on the corrosion behavior of AA4343/AA3xxx/AA4343 multilayer aluminium sheets
- Open Access
- 7 May 2025
- Published by Elsevier in Journal of Materials Research and Technology
- Vol. 36, 8367-8379
Microstructure characterization and corrosion resistance of eutectic and near-eutectic AlCoCrFeNi high-entropy alloys
- 7 May 2025
- Published by Elsevier in Journal of Materials Research and Technology
- Vol. 36, 8367-8379
Open AccessMicrostructure characterization and corrosion resistance of eutectic and near-eutectic AlCoCrFeNi high-entropy alloys