Diah Hari Kusumawati
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Research Subjects
Research Interests
Diah Hari Kusumawati has a total of 34 co-authors. Here are the top co-authors by number of shared publications:
- Munasir Munasir
Physics Department, Universitas Negeri Surabaya, Surabaya, Indonesia
5 shared publications Munasir
4 shared publications- Nugrahani Primary Putri
Department of Physics, Universitas Negeri Surabaya, Surabaya, Indonesia
4 shared publications - Ahmad Taufiq
Department of Physics Universitas Negeri Malang Malang Indonesia
3 shared publications - Nurul Hidayat
Universitas Negeri Malang
3 shared publications - Sunaryono Sunaryono
Universitas Negeri Malang
3 shared publications
Latest Publications
- 24 March 2026
- Published by Wiley in ChemistrySelect
- Vol. 11 (12)
Synergistic Effect of PANI/ZnO Composites for High‐Sensitivity Ammonia Detection
Ammonia (NH 3 ) is a toxic gas that must be detected at low concentrations at room temperature. This study synthesized a polyaniline/zinc oxide (PANI/ZnO) composite via an in situ polymerization method, using ZnO prepared via green synthesis from pineapple peel waste. The composite was then applied to a printed circuit board (PCB) substrate with interdigitation electrodes and characterized using XRD, FTIR, and SEM‐EDX. The sensor test results showed that PANI/ZnO with 0.3 g ZnO added provided the highest sensitivity of 79% at 4 ppm NH 3 , higher than that of pure PANI (61%). The sensor also showed a fast response time (20–29 s), a recovery time of 61–79 s, and good stability in repeated tests. This performance improvement resulted from the synergistic effect of the p–n heterojunction between PANI (p‐type) and ZnO (n‐type). This study confirms that the environmentally friendly PANI/ZnO composite has excellent potential to be developed as a low‐concentration NH 3 sensor at room temperature with sustainable and cost‐effective application prospects.
- 24 March 2026
- Published by Wiley in ChemistrySelect
- Vol. 11 (12)
Synergistic Effect of PANI/ZnO Composites for High‐Sensitivity Ammonia Detection
Ammonia (NH 3 ) is a toxic gas that must be detected at low concentrations at room temperature. This study synthesized a polyaniline/zinc oxide (PANI/ZnO) composite via an in situ polymerization method, using ZnO prepared via green synthesis from pineapple peel waste. The composite was then applied to a printed circuit board (PCB) substrate with interdigitation electrodes and characterized using XRD, FTIR, and SEM‐EDX. The sensor test results showed that PANI/ZnO with 0.3 g ZnO added provided the highest sensitivity of 79% at 4 ppm NH 3 , higher than that of pure PANI (61%). The sensor also showed a fast response time (20–29 s), a recovery time of 61–79 s, and good stability in repeated tests. This performance improvement resulted from the synergistic effect of the p–n heterojunction between PANI (p‐type) and ZnO (n‐type). This study confirms that the environmentally friendly PANI/ZnO composite has excellent potential to be developed as a low‐concentration NH 3 sensor at room temperature with sustainable and cost‐effective application prospects.
- Open Access
- 28 July 2025
- Published by OU Scientific Route in EUREKA: Physics and Engineering
- No. 5,p. 25-36
Adsorption of polyethylene microplastics using Fe3O4 nanoparticles from Tulungagung ilmenite sand
Plastic waste pollution in rivers is an environmental problem caused by the lack of public awareness and concern about throwing waste in waterways. One of the consequences is that plastic waste is difficult to degrade in waters for a long time until microplastics are formed. The type of microplastic waste often found in river waters comes from plastic-based beverage packaging, which is generally polyethylene. The presence of microplastic waste can endanger living things and their environment. Therefore, handling and controlling microplastics in the environment is necessary and urgent. The adsorption method is more appropriate and efficient regarding time, implementation, and cost, and it is environmentally friendly in eliminating microplastics. The material that has the potential to adsorb microplastics is Fe3O4 nanoparticles. This material can be obtained by extracting Tulungagung ilmenite sand through coprecipitation. This simple, inexpensive method uses room temperature and makes it easier to control the size of sample particles. The synthesized Fe3O4 nanoparticles with 15, 17, 19, 21, and 23 mg/ml concentrations were tested for 150 minutes in artificial seawater and mineral water dissolved with low-density polyethylene. The results showed that the removal of polyethylene microplastics in artificial seawater was more efficient than in mineral water, with the highest adsorption efficiency in artificial seawater reaching 97.5% and in mineral water reaching 90.5% at a concentration of Fe3O4 nanoparticles of 23 mg/ml. Thus, Fe3O4 nanoparticles from Tulungagung ilmenite sand can be candidates for microplastic removal applications with a simple technique and have specific application prospects.
- 28 July 2025
- Published by OU Scientific Route in EUREKA: Physics and Engineering
- No. 5,p. 25-36
Open AccessAdsorption of polyethylene microplastics using Fe3O4 nanoparticles from Tulungagung ilmenite sand
Plastic waste pollution in rivers is an environmental problem caused by the lack of public awareness and concern about throwing waste in waterways. One of the consequences is that plastic waste is difficult to degrade in waters for a long time until microplastics are formed. The type of microplastic waste often found in river waters comes from plastic-based beverage packaging, which is generally polyethylene. The presence of microplastic waste can endanger living things and their environment. Therefore, handling and controlling microplastics in the environment is necessary and urgent. The adsorption method is more appropriate and efficient regarding time, implementation, and cost, and it is environmentally friendly in eliminating microplastics. The material that has the potential to adsorb microplastics is Fe3O4 nanoparticles. This material can be obtained by extracting Tulungagung ilmenite sand through coprecipitation. This simple, inexpensive method uses room temperature and makes it easier to control the size of sample particles. The synthesized Fe3O4 nanoparticles with 15, 17, 19, 21, and 23 mg/ml concentrations were tested for 150 minutes in artificial seawater and mineral water dissolved with low-density polyethylene. The results showed that the removal of polyethylene microplastics in artificial seawater was more efficient than in mineral water, with the highest adsorption efficiency in artificial seawater reaching 97.5% and in mineral water reaching 90.5% at a concentration of Fe3O4 nanoparticles of 23 mg/ml. Thus, Fe3O4 nanoparticles from Tulungagung ilmenite sand can be candidates for microplastic removal applications with a simple technique and have specific application prospects.
- Open Access
- 29 March 2024
- Published by OU Scientific Route in EUREKA: Physics and Engineering
- No. 2,p. 178-189
The synthesis of MgO/Zein nanocomposites to improve anti-bacteria characteristics of mouthwash
Mouthwash is an alternative to address problems in the oral cavity, such as caries, periodontal inflammation, and microbial abscesses generally caused by pathogens. However, chlorhexidine contained in the mouthwash was limited concentration, i.e., 0.2 %, due to the side effects caused by these ingredients. Even though chlorhexidine has bactericidal and bacteriostatic properties against various bacteria found in plaque, for this reason, to increase the antibacterial activity of these mouthwashes, it is necessary to add other ingredients to the mouthwash formula, namely MgO/Zein nanocomposites with a composition of 1:4 and 1:5. The method used in this study was the preparation of MgO nanoparticles from dolomite using a solid acid solvent, the results of which were then composited with Zein using alcohol and NaOH. Synthesized samples were characterized using XRD, FTIR, SEM, and TEM. The antibacterial activity of S. aureus and mushrooms C. albicans in mouthwash with a concentration of 0.5 to 2.5 % can be determined by conducting a diffusion test. The results showed that the MgO/Zein nanocomposite fabrication had been successfully carried out and had the following characteristics: having a MgO phase with a polycrystalline cubic structure, having a zein phase with α-helix and β-sheet structures of proteins shows that Zein has an amorphous structure. The results of the antibacterial activity test showed that mouthwash with adding MgO/Zein nanocomposites more effectively inhibited bacterial growth of S. aureus and mushrooms C. albicans. It is known that the MgO/Zein nanocomposite composition 1:4 has the largest inhibition zone in S. aureus bacteria with a concentration of 1.5 % mouthwash and C. albicans fungi with a concentration of 0.5 %, namely 40.17 mm and 8.42 mm
- 29 March 2024
- Published by OU Scientific Route in EUREKA: Physics and Engineering
- No. 2,p. 178-189
Open AccessThe synthesis of MgO/Zein nanocomposites to improve anti-bacteria characteristics of mouthwash
Mouthwash is an alternative to address problems in the oral cavity, such as caries, periodontal inflammation, and microbial abscesses generally caused by pathogens. However, chlorhexidine contained in the mouthwash was limited concentration, i.e., 0.2 %, due to the side effects caused by these ingredients. Even though chlorhexidine has bactericidal and bacteriostatic properties against various bacteria found in plaque, for this reason, to increase the antibacterial activity of these mouthwashes, it is necessary to add other ingredients to the mouthwash formula, namely MgO/Zein nanocomposites with a composition of 1:4 and 1:5. The method used in this study was the preparation of MgO nanoparticles from dolomite using a solid acid solvent, the results of which were then composited with Zein using alcohol and NaOH. Synthesized samples were characterized using XRD, FTIR, SEM, and TEM. The antibacterial activity of S. aureus and mushrooms C. albicans in mouthwash with a concentration of 0.5 to 2.5 % can be determined by conducting a diffusion test. The results showed that the MgO/Zein nanocomposite fabrication had been successfully carried out and had the following characteristics: having a MgO phase with a polycrystalline cubic structure, having a zein phase with α-helix and β-sheet structures of proteins shows that Zein has an amorphous structure. The results of the antibacterial activity test showed that mouthwash with adding MgO/Zein nanocomposites more effectively inhibited bacterial growth of S. aureus and mushrooms C. albicans. It is known that the MgO/Zein nanocomposite composition 1:4 has the largest inhibition zone in S. aureus bacteria with a concentration of 1.5 % mouthwash and C. albicans fungi with a concentration of 0.5 %, namely 40.17 mm and 8.42 mm
- Open Access
- 30 July 2021
- Published by Lembaga Penelitian dan Pemberdayaan Masyarakat - LITPAM in Jurnal Penelitian dan Pengkajian Ilmu Pendidikan: e-Saintika
- Vol. 5 (2) , 168-174
Development of rGO/Fe3O4 Composites as Glucose Biosensors
The rGO/Fe3O4 composite is one type of composites that can be used as a biosensor material, especially glucose sensors. The main ingredients of the composite synthesis are graphite and iron sand. The synthesis process of Fe3O4 was done using the coprecipitation method, while the graphite oxidation process was accomplished using the modified Hummer's method. The composites were formed using the ex-situ wet mixing method. The formed iron sand and graphite were characterized using FTIR and XRD, and it was found that Fe3O4 was formed from the appearance of the Fe-O bond, the oxidation process of graphite was seen from the appearance of the C=O bond, and the detection of Fe peaks corresponded to the cubic crystal plane. Likewise, the composites formed were also characterized using FTIR and XRD for identification of the rGO/Fe3O4 composite formation. It was proven from the presence of Fe-O and C-O bonds and the appearance of an amorphous peak of rGO in the XRD results. The performance of the rGO/Fe3O4 composites as the glucose biosensor was examined by varying the mass of Fe3O4 on the composite, using UV-Vis spectroscopy. The performance of the rGO/Fe3O4 composite biosensor in absorbing glucose reached optimum at a mass variation of 0.3 grams of Fe3O4, as demonstrated by by the lowest absorbance peak with an intensity of 0.0048 at a wavelength of 440 nm, corresponding to glucose entrappment of 7.1 mg/gram.
- 30 July 2021
- Published by Lembaga Penelitian dan Pemberdayaan Masyarakat - LITPAM in Jurnal Penelitian dan Pengkajian Ilmu Pendidikan: e-Saintika
- Vol. 5 (2) , 168-174
Open AccessDevelopment of rGO/Fe3O4 Composites as Glucose Biosensors
The rGO/Fe3O4 composite is one type of composites that can be used as a biosensor material, especially glucose sensors. The main ingredients of the composite synthesis are graphite and iron sand. The synthesis process of Fe3O4 was done using the coprecipitation method, while the graphite oxidation process was accomplished using the modified Hummer's method. The composites were formed using the ex-situ wet mixing method. The formed iron sand and graphite were characterized using FTIR and XRD, and it was found that Fe3O4 was formed from the appearance of the Fe-O bond, the oxidation process of graphite was seen from the appearance of the C=O bond, and the detection of Fe peaks corresponded to the cubic crystal plane. Likewise, the composites formed were also characterized using FTIR and XRD for identification of the rGO/Fe3O4 composite formation. It was proven from the presence of Fe-O and C-O bonds and the appearance of an amorphous peak of rGO in the XRD results. The performance of the rGO/Fe3O4 composites as the glucose biosensor was examined by varying the mass of Fe3O4 on the composite, using UV-Vis spectroscopy. The performance of the rGO/Fe3O4 composite biosensor in absorbing glucose reached optimum at a mass variation of 0.3 grams of Fe3O4, as demonstrated by by the lowest absorbance peak with an intensity of 0.0048 at a wavelength of 440 nm, corresponding to glucose entrappment of 7.1 mg/gram.
- Open Access
- 1 July 2020
- Published by IOP Publishing in Journal of Physics: Conference Series
- Vol. 1569 (4) , 042087
Magnetic Properties of Fe3O4@Graphene: Preparation from Natural Material
This work presents a study of structure and the magnetic behavior of Fe3O4 nanoparticles produced in the extraction process and Magnetic Nanoparticle of Fe3O4 coated by graphene oxide (GO) from natural materials of coconut shells (graphite). Preparation of the core-shell composite Fe3O4@Graphene was carried out with ex-situ process. Superparamagnetic analysis of Fe3O4, and Fe3O4@Graphene using VSM (vibrating sample magnetometer), structure analysis using HRPD, TEM and adsorption of dyes solution in the drink water. Obtained results, along with the thickening of the skin (Graphene that encloses the core particles (Fe3O4), the saturation of the magnetization (Ms) decreases. And the amount of GO composition affects the coating decorated (shell); Fe3O4/Graphene absorptivity increases when walls are thinner.
- 1 July 2020
- Published by IOP Publishing in Journal of Physics: Conference Series
- Vol. 1569 (4) , 042087
Open AccessMagnetic Properties of Fe3O4@Graphene: Preparation from Natural Material
This work presents a study of structure and the magnetic behavior of Fe3O4 nanoparticles produced in the extraction process and Magnetic Nanoparticle of Fe3O4 coated by graphene oxide (GO) from natural materials of coconut shells (graphite). Preparation of the core-shell composite Fe3O4@Graphene was carried out with ex-situ process. Superparamagnetic analysis of Fe3O4, and Fe3O4@Graphene using VSM (vibrating sample magnetometer), structure analysis using HRPD, TEM and adsorption of dyes solution in the drink water. Obtained results, along with the thickening of the skin (Graphene that encloses the core particles (Fe3O4), the saturation of the magnetization (Ms) decreases. And the amount of GO composition affects the coating decorated (shell); Fe3O4/Graphene absorptivity increases when walls are thinner.
- Open Access
- 1 February 2019
- Published by IOP Publishing in Journal of Physics: Conference Series
- Vol. 1171 (1) , 012042
Effect of calcination temperature on characteristics of reduced Graphene Oxide (rGO) made from old coconut shell
- 1 February 2019
- Published by IOP Publishing in Journal of Physics: Conference Series
- Vol. 1171 (1) , 012042
Open AccessEffect of calcination temperature on characteristics of reduced Graphene Oxide (rGO) made from old coconut shell
- Open Access
- 1 September 2018
- Published by IOP Publishing in Journal of Physics: Conference Series
- Vol. 1093 (1) , 012025
Phase Transition of SiO2 Nanoparticles Prepared from Natural Sand: The Calcination Temperature Effect
In this paper, we systematically report the synthesis of nano silica powder from natural silica sand by a continuous process. Extraction of sodium silicate from silica sand was through a hydrothermal process, then sodium silicate was ready to be used as a precursor in the form of silicate slurry by coprecipitation process. The silicate slurry of SiO2.XH2O was then dried in a furnace at 150 C for 4 hours until obtaining a pure white SiO2 powder. At a calcination temperature of 900 °C, the sample was then tested by XRD to analyze the transformation of the crystal phase of SiO2 nanoparticles. Identification of functional group absorption was undertaken by FTIR test, and the particle grain microstructure was analyzed by SEM. At calcination temperature of 900 C, the SiO2 silica nanoparticles experienced a change of phase from amorphous to crystal or amorphous-cristobalite phase; a shift in stiffness for positions of functional group absorption of Si-O stretching or LO functional groups, Si-O stretching or TO, Si-O-Si bending and Si-O-Si rocking and OH-functional groups occurred; the growth of particle grains happened with a spherical and oval trend, with a larger size. SiO2 nanoparticles were successfully synthesized by a continuous method and 900 C calcination temperature had a significant effect on structural phase changes, the formation of siloxane functional groups, silanol, and grain growth on SiO2 nanoparticles.
- 1 September 2018
- Published by IOP Publishing in Journal of Physics: Conference Series
- Vol. 1093 (1) , 012025
Open AccessPhase Transition of SiO2 Nanoparticles Prepared from Natural Sand: The Calcination Temperature Effect
In this paper, we systematically report the synthesis of nano silica powder from natural silica sand by a continuous process. Extraction of sodium silicate from silica sand was through a hydrothermal process, then sodium silicate was ready to be used as a precursor in the form of silicate slurry by coprecipitation process. The silicate slurry of SiO2.XH2O was then dried in a furnace at 150 C for 4 hours until obtaining a pure white SiO2 powder. At a calcination temperature of 900 °C, the sample was then tested by XRD to analyze the transformation of the crystal phase of SiO2 nanoparticles. Identification of functional group absorption was undertaken by FTIR test, and the particle grain microstructure was analyzed by SEM. At calcination temperature of 900 C, the SiO2 silica nanoparticles experienced a change of phase from amorphous to crystal or amorphous-cristobalite phase; a shift in stiffness for positions of functional group absorption of Si-O stretching or LO functional groups, Si-O stretching or TO, Si-O-Si bending and Si-O-Si rocking and OH-functional groups occurred; the growth of particle grains happened with a spherical and oval trend, with a larger size. SiO2 nanoparticles were successfully synthesized by a continuous method and 900 C calcination temperature had a significant effect on structural phase changes, the formation of siloxane functional groups, silanol, and grain growth on SiO2 nanoparticles.
- Open Access
- 1 September 2018
- Published by IOP Publishing in Journal of Physics: Conference Series
- Vol. 1093 (1) , 012015
Synthesis and Characterization of γ-Al2O3/SiO2 Composite Materials
This article reports the synthesis process of γ-alumina/SiO2 composite from aluminium powders and amorphous nanosilica through the means of tetra-methyl-ammonium hydroxide (TMAH) as the mixing medium which produced aluminium hydroxide Al(OH)3 in the form of white powders. The crystal structures, microstructures, and mapping of the atomic constituent of γ-Al2O3 and γ-Al2O3/SiO2 samples were respectively analyzed via X-ray diffraction (XRD), and scanning electron microscopy-energy dispersive X-ray SEM-EDX. At the calcination temperature to 300 °C, the samples still had boehmite phase, and the boehmite phase transformation to γ-alumina phase occurred at temperature of 700-900 °C. The γ-alumina phase began to form at the calcination temperature of 500-700 °C with the crystal structure of (440), (511), (400), (222), (311), and (111). The similar diffraction pattern was also shown by the γ-Al2O3/SiO2 composite for the calcination temperature of 700 °C and 900 °C. The microstructure analysis of the γ-Al2O3/SiO2 showed that SiO2 particles were smaller and round while the γ-Al2O3 particles were bigger and elongated. Additionally, the mapping results showed SiO2 and γ-Al2O3 particles were homogenously distributed.
- 1 September 2018
- Published by IOP Publishing in Journal of Physics: Conference Series
- Vol. 1093 (1) , 012015
Open AccessSynthesis and Characterization of γ-Al2O3/SiO2 Composite Materials
This article reports the synthesis process of γ-alumina/SiO2 composite from aluminium powders and amorphous nanosilica through the means of tetra-methyl-ammonium hydroxide (TMAH) as the mixing medium which produced aluminium hydroxide Al(OH)3 in the form of white powders. The crystal structures, microstructures, and mapping of the atomic constituent of γ-Al2O3 and γ-Al2O3/SiO2 samples were respectively analyzed via X-ray diffraction (XRD), and scanning electron microscopy-energy dispersive X-ray SEM-EDX. At the calcination temperature to 300 °C, the samples still had boehmite phase, and the boehmite phase transformation to γ-alumina phase occurred at temperature of 700-900 °C. The γ-alumina phase began to form at the calcination temperature of 500-700 °C with the crystal structure of (440), (511), (400), (222), (311), and (111). The similar diffraction pattern was also shown by the γ-Al2O3/SiO2 composite for the calcination temperature of 700 °C and 900 °C. The microstructure analysis of the γ-Al2O3/SiO2 showed that SiO2 particles were smaller and round while the γ-Al2O3 particles were bigger and elongated. Additionally, the mapping results showed SiO2 and γ-Al2O3 particles were homogenously distributed.
- Open Access
- 1 May 2018
- Published by IOP Publishing in IOP Conference Series: Materials Science and Engineering
- Vol. 367 (1) , 012010
Structure Analysis of Fe3O4@SiO2 Core Shells Prepared from Amorphous and Crystalline SiO2 Particles
- 1 May 2018
- Published by IOP Publishing in IOP Conference Series: Materials Science and Engineering
- Vol. 367 (1) , 012010
Open AccessStructure Analysis of Fe3O4@SiO2 Core Shells Prepared from Amorphous and Crystalline SiO2 Particles
- Open Access
- 1 March 2018
- Published by IOP Publishing in Journal of Physics: Conference Series
- Vol. 997
Synthesis of polyaniline/cellulose composite as humidity sensor
- 1 March 2018
- Published by IOP Publishing in Journal of Physics: Conference Series
- Vol. 997
Open AccessSynthesis of polyaniline/cellulose composite as humidity sensor