Олег Александрович Перегудов
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Previous Organizations / Institutes
The organizations / institutes from the scholar's other articles in the past ten years
Олег Александрович Перегудов has a total of 55 co-authors. Here are the top co-authors by number of shared publications:
- Viktor Evgenievich Gromov
Siberian State Industrial University, Novokuznetsk, Russia
35 shared publications - Yurii Fedorovich Ivanov
High Current Electronics Institute, Siberian Branch of the Russian Academy of Sciences, Tomsk, Russia
19 shared publications K. V. Morozov
Siberian State Industrial University
12 shared publications- Sergey V. Konovalov
Siberian State Industrial University
10 shared publications A. B. Yur’EV
Evraz—United West Siberian Metallurgical Combine LLC
4 shared publicationsA. M. Glezer
Bardin Central Research Institute for Ferrous Metallurgy
4 shared publications
Latest Publications
- Open Access
- 28 May 2024
- Published by Altai State Technical University in Фундаментальные проблемы современного материаловедения
- Vol. 21 (2) , 143-152
СТРУКТУРА СЛОЯ БЫСТРОРЕЖУЩЕЙ СТАЛИ С АЗОТОМ, НАПЛАВЛЕННОГО НА ДЕТАЛИ МЕТАЛЛУРГИЧЕСКОГО ОБОРУДОВАНИЯ
Методами современного физического материаловедения исследована структура, микротвердость и трибологические свойства быстрорежущей стали Р18Ю, легированной азотом и алюминием направленной на валки из среднеглеродистой стали 30ХГСА. Плазменная наплавка осуществлена в закрытой среде азота порошковой проволокой. Проведен регулируемый термический цикл для получения равномерного состояния и предотвращенияформирования холодных трещин. Выявлено, что наплавленный слой имеет структуру ячеисто-дендритного типа. Зерна обогащены атомами железа, а границы разделены тонкими прослойками второй фазы, обогащенными атомами хрома, алюминия, вольфрама и ванадия. Внутри центральной части зерен обнаружены включения игольчатого типа длиной 150-730 нм. Четырехкратный высокотемпературный отпуск при 580 °С в течении 1 часа обеспечивает: растворение наноразмерных включений в объеме зерен; способствует более равномерному распределению легирующих элементов; формирует структуру пластинчатого (игольчатого) типа, характерную по морфологическому признаку для игольчатого мартенсита. Выдвинуто и обосновано предположение, что зерна наплавленного слоя сформированы твердым раствором γ-железа (аустенита). Выявлено незначительное снижение микротвердости, износостойкости и коэффициента трения наплавочного слоя после высокотемпературного отпуска. Такое поведение наплавочного материала при высокотемпературном отпуске может быть обусловлено релаксацией термических напряжений, сформированных в слое при наплавке.
- 28 May 2024
- Published by Altai State Technical University in Фундаментальные проблемы современного материаловедения
- Vol. 21 (2) , 143-152
Open AccessСТРУКТУРА СЛОЯ БЫСТРОРЕЖУЩЕЙ СТАЛИ С АЗОТОМ, НАПЛАВЛЕННОГО НА ДЕТАЛИ МЕТАЛЛУРГИЧЕСКОГО ОБОРУДОВАНИЯ
Методами современного физического материаловедения исследована структура, микротвердость и трибологические свойства быстрорежущей стали Р18Ю, легированной азотом и алюминием направленной на валки из среднеглеродистой стали 30ХГСА. Плазменная наплавка осуществлена в закрытой среде азота порошковой проволокой. Проведен регулируемый термический цикл для получения равномерного состояния и предотвращенияформирования холодных трещин. Выявлено, что наплавленный слой имеет структуру ячеисто-дендритного типа. Зерна обогащены атомами железа, а границы разделены тонкими прослойками второй фазы, обогащенными атомами хрома, алюминия, вольфрама и ванадия. Внутри центральной части зерен обнаружены включения игольчатого типа длиной 150-730 нм. Четырехкратный высокотемпературный отпуск при 580 °С в течении 1 часа обеспечивает: растворение наноразмерных включений в объеме зерен; способствует более равномерному распределению легирующих элементов; формирует структуру пластинчатого (игольчатого) типа, характерную по морфологическому признаку для игольчатого мартенсита. Выдвинуто и обосновано предположение, что зерна наплавленного слоя сформированы твердым раствором γ-железа (аустенита). Выявлено незначительное снижение микротвердости, износостойкости и коэффициента трения наплавочного слоя после высокотемпературного отпуска. Такое поведение наплавочного материала при высокотемпературном отпуске может быть обусловлено релаксацией термических напряжений, сформированных в слое при наплавке.
- Open Access
- 20 April 2024
- Published by National University of Science and Technology MISiS in Izvestiya. Ferrous Metallurgy
- Vol. 67 (2) , 185-194
Formation of the gradient of structural-phase states of high-speed steel during surfacing. Part 2. The role of the Mullins–Sekerka instability in formation of crystallization structures
The authors studied the crystallization process of the Fe – W system, which is the basis of heat-resistant high-speed steel used in plasma arc surfacing on the surface of rolls and various cutting tools. The structure of this material consists of two components: cellular and dendritic. Histogram of the structural elements distribution shows the presence of a single maximum. The most probable size takes a value in the range of 10 – 15 μm. The paper considers the morphological instability of crystallization front (the Mullins-Sekerka instability). The model includes the equations of convective thermal conductivity and diffusion. The Stefan conditions for temperature were set at interface of the phases. Linear analysis of this instability is carried out for two cases: when the convective term in the equations of thermal conductivity and diffusion can be neglected; when convection prevails over diffusion processes. In all cases, it was assumed that the value (1 – ks ) was close to zero, which corresponds to a concentration of the alloying element approximately equal to or exceeding the eutectic one, and a short-wave approximation was also used. In the first case, the analytical view of dependence of the wavelength, which accounts for the maximum rate of interface disturbances growth, coincides with generally accepted concepts. In the second case, the value of this wavelength is directly proportional to square root of the interphase boundary velocity. The limits of applicability of these approximations for various mechanisms of crystal growth were determined. In the case of normal growth, both approximations provide an adequate explanation for the formation of structural elements up to 5 μm in size at a crystallization front velocity of about 2 m/s. For the case of growth due to screw dislocations, the wavelength value corresponding to the fastest-growing perturbation mode in the first case coincides with experimental data at a crystallization front velocity of the order of 10–7 m/s, whereas in the convective approximation such a coincidence is observed at 10–4 m/s. Further development of the model consists in simultaneous consideration of the convective and diffusion components. The results obtained will serve as a material for the research of the Mullins–Sekerka instability for two interface boundaries.
- 20 April 2024
- Published by National University of Science and Technology MISiS in Izvestiya. Ferrous Metallurgy
- Vol. 67 (2) , 185-194
Open AccessFormation of the gradient of structural-phase states of high-speed steel during surfacing. Part 2. The role of the Mullins–Sekerka instability in formation of crystallization structures
The authors studied the crystallization process of the Fe – W system, which is the basis of heat-resistant high-speed steel used in plasma arc surfacing on the surface of rolls and various cutting tools. The structure of this material consists of two components: cellular and dendritic. Histogram of the structural elements distribution shows the presence of a single maximum. The most probable size takes a value in the range of 10 – 15 μm. The paper considers the morphological instability of crystallization front (the Mullins-Sekerka instability). The model includes the equations of convective thermal conductivity and diffusion. The Stefan conditions for temperature were set at interface of the phases. Linear analysis of this instability is carried out for two cases: when the convective term in the equations of thermal conductivity and diffusion can be neglected; when convection prevails over diffusion processes. In all cases, it was assumed that the value (1 – ks ) was close to zero, which corresponds to a concentration of the alloying element approximately equal to or exceeding the eutectic one, and a short-wave approximation was also used. In the first case, the analytical view of dependence of the wavelength, which accounts for the maximum rate of interface disturbances growth, coincides with generally accepted concepts. In the second case, the value of this wavelength is directly proportional to square root of the interphase boundary velocity. The limits of applicability of these approximations for various mechanisms of crystal growth were determined. In the case of normal growth, both approximations provide an adequate explanation for the formation of structural elements up to 5 μm in size at a crystallization front velocity of about 2 m/s. For the case of growth due to screw dislocations, the wavelength value corresponding to the fastest-growing perturbation mode in the first case coincides with experimental data at a crystallization front velocity of the order of 10–7 m/s, whereas in the convective approximation such a coincidence is observed at 10–4 m/s. Further development of the model consists in simultaneous consideration of the convective and diffusion components. The results obtained will serve as a material for the research of the Mullins–Sekerka instability for two interface boundaries.
- Open Access
- 5 April 2024
- Published by Altai State University in Izvestiya of Altai State University
- No. 1(135),p. 43-49
Fracture Physics and Phase Transformation of Cementite in Rails under Extreme Operation Conditions
This paper presents the quantitative estimation of carbon atom distribution in cementite particles and elements of defective substructures within the 10 mm depth area of the running surface of rails along the central axis and the symmetry axis of the upper fillet. The estimation is based on the electron microscopic study and X-ray spectral analysis. The subjects of the study are the differentially hardened 100-meter long rails after passing tonnage of 1411 and 1770 million tons of gross weight. There are three mechanisms of cementite plates transformation analyzed in the paper. It is shown that extremely long operation of rails is accompanied by a significant redistribution of carbon atoms in surface layers with depths up to 10 mm. In the initial state, the basic amount of carbon atoms is concentrated in cementite particles. After the extremely long operation period, there are defects in the crystalline structure (dislocations, grain and subgrain boundaries) with the presence of the а-iron in the surface layer and the crystal lattice. An increase of passing tonnage from 1411 to 1770 million tons leads to a distinctive shift of carbon atoms to structural defects of the rail upper fillet. The discussion of the obtained results includes the concepts of bifurcation interstitial structure states in the crystalline structure rotation zones and plastic distortion, along with the analogies of extremely long operation and megaplastic deformations.
- 5 April 2024
- Published by Altai State University in Izvestiya of Altai State University
- No. 1(135),p. 43-49
Open AccessFracture Physics and Phase Transformation of Cementite in Rails under Extreme Operation Conditions
This paper presents the quantitative estimation of carbon atom distribution in cementite particles and elements of defective substructures within the 10 mm depth area of the running surface of rails along the central axis and the symmetry axis of the upper fillet. The estimation is based on the electron microscopic study and X-ray spectral analysis. The subjects of the study are the differentially hardened 100-meter long rails after passing tonnage of 1411 and 1770 million tons of gross weight. There are three mechanisms of cementite plates transformation analyzed in the paper. It is shown that extremely long operation of rails is accompanied by a significant redistribution of carbon atoms in surface layers with depths up to 10 mm. In the initial state, the basic amount of carbon atoms is concentrated in cementite particles. After the extremely long operation period, there are defects in the crystalline structure (dislocations, grain and subgrain boundaries) with the presence of the а-iron in the surface layer and the crystal lattice. An increase of passing tonnage from 1411 to 1770 million tons leads to a distinctive shift of carbon atoms to structural defects of the rail upper fillet. The discussion of the obtained results includes the concepts of bifurcation interstitial structure states in the crystalline structure rotation zones and plastic distortion, along with the analogies of extremely long operation and megaplastic deformations.
- Open Access
- 30 December 2023
- Published by Siberian State Industrial University in Bulletin of the Siberian State Industrial University
- No. 4,p. 9-20
BEHAVIOR OF CEMENTITE IN PERLITE STEEL UNDER DEFORMATION
A brief overview of the latest experimental results of the study of cement as a structural component of perlite, obtained by transmission microscopy methods for various types of deformation is presented. The behavior of lamellar and granular cementite under types of active deformation (forging, stamping, drawing, rolling, long-term operation of rails) has been studied. Studies of granular perlite on samples of carbon eutectoid steel grade U8 containing 0.8% C, 0.18 % Mn, 0.22% Si, 0.17% Cr, 0.12%Ni, 0.10 % Cu are presented. The historical aspect of the origin of the name cementite from the history of the metallographic study of cementite as an independent phase is considered. An example of the practical application of pearlitic steel in the construction of the Akashi-Kaike bridge in Japan (the longest single-span suspension bridge based on huge pearlitic steel cables) is given Attention is paid to the analysis of transformation during various technological processes, its morphology and structural features, and the main mechanisms of destruction are analyzed. It was revealed that with a large missed tonnage, a critical density of defects accumulates in the surface layer, which inhibits the development of reversible elastic deformation and the involvement (development) of the mechanism of plastic distortion. It is suggested that an increase in the service life of rails can be achieved due to a longer preservation of a structure capable of developing reversible deformation processes that exclude the destruction of cementite plates in pearlite colonies with subsequent movement of carbon atoms to defects (dislocations) and the iron lattice region. Представлен краткий обзор последних экспериментальных результатов изучения цементита как структурной составляющей перлита, полученных методов просвечивающей микроскопии при различных видах деформирования. Исследовано поведение пластинчатого и зернистого цементита при видах активной деформации (ковке, штамповке, волочении, прокатке, длительной эксплуатации рельсов). Представлены исследования зернистого перлита на образцах углеродистой эвтектоидной стали марки У8, содержащей 0,8 % С, 0,18 % Mn, 0,22 % Si, 0,17 % Cr, 0,12 %Ni, 0,10 % Cu. Рассмотрен исторический аспект происхождения названия «цементит». Из истории металлографического изучения это вещество рассматривается как самостоятельной фазы. Приведен пример практического применения перлитной стали в конструкции моста Акаси-Кайке в Японии (самый длинный однопролетный подвесной мост, опирающийся на огромные тросы из перлитной стали). Уделено внимание анализу трансформации в ходе различных технологических процессов, его морфологии и структурным особенностям, проанализированы основные механизмы разрушения. Выявлено, что при большом пропущенном тоннаже в поверхностном слое накапливается критическая плотность дефектов, что сдерживает развитие обратимой упругой деформации и вовлечение (развитие) механизма пластической дисторсии. Высказано предположение, что повышение ресурса работы рельсов может быть достигнуто за счет более длительного сохранения структуры, способной к развитию обратимых деформационных процессов, исключающих разрушение цементитных пластин в перлитных колониях с последующим перемещением атомов углерода на дефекты (дислокации) и области решетки -железа.
- 30 December 2023
- Published by Siberian State Industrial University in Bulletin of the Siberian State Industrial University
- No. 4,p. 9-20
Open AccessBEHAVIOR OF CEMENTITE IN PERLITE STEEL UNDER DEFORMATION
A brief overview of the latest experimental results of the study of cement as a structural component of perlite, obtained by transmission microscopy methods for various types of deformation is presented. The behavior of lamellar and granular cementite under types of active deformation (forging, stamping, drawing, rolling, long-term operation of rails) has been studied. Studies of granular perlite on samples of carbon eutectoid steel grade U8 containing 0.8% C, 0.18 % Mn, 0.22% Si, 0.17% Cr, 0.12%Ni, 0.10 % Cu are presented. The historical aspect of the origin of the name cementite from the history of the metallographic study of cementite as an independent phase is considered. An example of the practical application of pearlitic steel in the construction of the Akashi-Kaike bridge in Japan (the longest single-span suspension bridge based on huge pearlitic steel cables) is given Attention is paid to the analysis of transformation during various technological processes, its morphology and structural features, and the main mechanisms of destruction are analyzed. It was revealed that with a large missed tonnage, a critical density of defects accumulates in the surface layer, which inhibits the development of reversible elastic deformation and the involvement (development) of the mechanism of plastic distortion. It is suggested that an increase in the service life of rails can be achieved due to a longer preservation of a structure capable of developing reversible deformation processes that exclude the destruction of cementite plates in pearlite colonies with subsequent movement of carbon atoms to defects (dislocations) and the iron lattice region. Представлен краткий обзор последних экспериментальных результатов изучения цементита как структурной составляющей перлита, полученных методов просвечивающей микроскопии при различных видах деформирования. Исследовано поведение пластинчатого и зернистого цементита при видах активной деформации (ковке, штамповке, волочении, прокатке, длительной эксплуатации рельсов). Представлены исследования зернистого перлита на образцах углеродистой эвтектоидной стали марки У8, содержащей 0,8 % С, 0,18 % Mn, 0,22 % Si, 0,17 % Cr, 0,12 %Ni, 0,10 % Cu. Рассмотрен исторический аспект происхождения названия «цементит». Из истории металлографического изучения это вещество рассматривается как самостоятельной фазы. Приведен пример практического применения перлитной стали в конструкции моста Акаси-Кайке в Японии (самый длинный однопролетный подвесной мост, опирающийся на огромные тросы из перлитной стали). Уделено внимание анализу трансформации в ходе различных технологических процессов, его морфологии и структурным особенностям, проанализированы основные механизмы разрушения. Выявлено, что при большом пропущенном тоннаже в поверхностном слое накапливается критическая плотность дефектов, что сдерживает развитие обратимой упругой деформации и вовлечение (развитие) механизма пластической дисторсии. Высказано предположение, что повышение ресурса работы рельсов может быть достигнуто за счет более длительного сохранения структуры, способной к развитию обратимых деформационных процессов, исключающих разрушение цементитных пластин в перлитных колониях с последующим перемещением атомов углерода на дефекты (дислокации) и области решетки -железа.
- Open Access
- 11 November 2023
- Published by National University of Science and Technology MISiS in Izvestiya. Ferrous Metallurgy
- Vol. 66 (5) , 587-593
Formation of the gradient of structural-phase states of high-speed steel during surfacing. Part 1. Solving the Stefan problem with two movable boundaries
The article considers theoretical study of solidification of the binary iron–tungsten system at a tungsten content of 18 wt. %. Such tungsten content is typical for heat-resistant alloys used in plasma-arc surfacing on the rolls surface. The axisymmetric Stefan thermal problem is solved for two movable cylindrical boundaries that separate three regions. In region 1, the melt is at the melting point; in region 2, the substance is in a two‒phase state, and in region 3 – a solid. The liquidus temperature was set at the interface of regions 1 and 2, and the solidus temperature – at the interface of regions 2 and 3. At these boundaries, a condition for the heat flows balance was given, from which a system of kinetic equations was obtained. This system was solved by numerical methods, without hypothesizing that the fronts of phase transformations move according to the law R ~ t1/2. Solution of the system of kinetic equations shows that the solidus boundary moves almost linearly. The liquidus boundary moves according to the parabolic law. For regions of the micrometer range in size, the processes of phase transformations take place in a time of about 5 ns, whereas for regions of the order of 10 μm in size – in a time of about 50 ms. Dependences of temperature fields on the radial coordinate at various points in time show that with increasing time, the dimensions of region 2 decrease, and as soon as coordinates of the liquidus and solidus boundaries become close, thecrystallization process stops. Further development of the model consists in taking into account the rotation of one of the media. The results obtained will serve as a material for the study of the Mullins-Sekerka two-front instability.
- 11 November 2023
- Published by National University of Science and Technology MISiS in Izvestiya. Ferrous Metallurgy
- Vol. 66 (5) , 587-593
Open AccessFormation of the gradient of structural-phase states of high-speed steel during surfacing. Part 1. Solving the Stefan problem with two movable boundaries
The article considers theoretical study of solidification of the binary iron–tungsten system at a tungsten content of 18 wt. %. Such tungsten content is typical for heat-resistant alloys used in plasma-arc surfacing on the rolls surface. The axisymmetric Stefan thermal problem is solved for two movable cylindrical boundaries that separate three regions. In region 1, the melt is at the melting point; in region 2, the substance is in a two‒phase state, and in region 3 – a solid. The liquidus temperature was set at the interface of regions 1 and 2, and the solidus temperature – at the interface of regions 2 and 3. At these boundaries, a condition for the heat flows balance was given, from which a system of kinetic equations was obtained. This system was solved by numerical methods, without hypothesizing that the fronts of phase transformations move according to the law R ~ t1/2. Solution of the system of kinetic equations shows that the solidus boundary moves almost linearly. The liquidus boundary moves according to the parabolic law. For regions of the micrometer range in size, the processes of phase transformations take place in a time of about 5 ns, whereas for regions of the order of 10 μm in size – in a time of about 50 ms. Dependences of temperature fields on the radial coordinate at various points in time show that with increasing time, the dimensions of region 2 decrease, and as soon as coordinates of the liquidus and solidus boundaries become close, thecrystallization process stops. Further development of the model consists in taking into account the rotation of one of the media. The results obtained will serve as a material for the study of the Mullins-Sekerka two-front instability.
- Open Access
- 30 October 2022
- Published by National University of Science and Technology MISiS in Izvestiya. Ferrous Metallurgy
- Vol. 65 (10) , 683-692
Coatings from high-entropy alloys: State and prospects
The authors made a brief review of recent publications by foreign and domestic researchers on the structure, phase composition, and properties of films and coatings of five-component high-entropy alloys (HEA) on various substrates and modification of the HEA surface by various types of processing. The main methods of applying films and coatings are considered: magnetron sputtering, thermal sputtering, laser sputtering, and electrodeposition. Particular attention is paid to the deposition of coatings on stainless steels and titanium alloys. The positive change in the tribological, strength properties, and corrosion resistance of film coatings in a wide temperature range is analyzed and possible causes of the observed effects are discussed. The role of solid solution strengthening, formation of fine-grained structure, and the formation of oxide layers enriched with one of the HEA components were taken into account. The authors identified new methods for applying coatings from HEA and subsequent processing. Using Nb and Ti doping as an example, their role in increasing microhardness, wear resistance, and reducing the friction coefficient in coatings were revealed. Electrolytic polishing, electroerosive machining, mechanical polishing and their combination are considered among the methods of HEA surface treatment. A number of works propose a method of powder borating to increase the surface strength and wear resistance of HEAs. The paper considers analysis of works on electron-beam processing as one of the promising and high efficient methods of HEA surface hardening.
- 30 October 2022
- Published by National University of Science and Technology MISiS in Izvestiya. Ferrous Metallurgy
- Vol. 65 (10) , 683-692
Open AccessCoatings from high-entropy alloys: State and prospects
The authors made a brief review of recent publications by foreign and domestic researchers on the structure, phase composition, and properties of films and coatings of five-component high-entropy alloys (HEA) on various substrates and modification of the HEA surface by various types of processing. The main methods of applying films and coatings are considered: magnetron sputtering, thermal sputtering, laser sputtering, and electrodeposition. Particular attention is paid to the deposition of coatings on stainless steels and titanium alloys. The positive change in the tribological, strength properties, and corrosion resistance of film coatings in a wide temperature range is analyzed and possible causes of the observed effects are discussed. The role of solid solution strengthening, formation of fine-grained structure, and the formation of oxide layers enriched with one of the HEA components were taken into account. The authors identified new methods for applying coatings from HEA and subsequent processing. Using Nb and Ti doping as an example, their role in increasing microhardness, wear resistance, and reducing the friction coefficient in coatings were revealed. Electrolytic polishing, electroerosive machining, mechanical polishing and their combination are considered among the methods of HEA surface treatment. A number of works propose a method of powder borating to increase the surface strength and wear resistance of HEAs. The paper considers analysis of works on electron-beam processing as one of the promising and high efficient methods of HEA surface hardening.
- Open Access
- 2 October 2022
- Published by National University of Science and Technology MISiS in Izvestiya. Ferrous Metallurgy
- Vol. 65 (9) , 654-661
Evolution of structure of rail steel lamellar pearlite under compression deformation
The article presents the results of analysis of evolution of the defective substructure of rail steel pearlite with lamellar morphology under deformation by uniaxial compression. The strain hardening of the studied steel under such deformation has a multistage character. Deformation of steel is accompanied by fragmentation of pearlite grains, which intensifies as the degree of deformation increases and reaches 0.4 of the studied foil volume at ε = 50 %. Fragments formed in ferrite plates are separated by low-angle boundaries. It was established that the average sizes of ferrite plate fragments decrease from 240 nm (ε = 15 %) to 200 nm (ε = 50 %) with an increase in the deformation degree. Fragmentation of cementite plates was revealed. It was found that the size of the fragments varies within 15 – 20 nm and weakly depends on the degree of steel deformation. Fracture of cementite lamellae, proceeding by their dissolution and cutting by mobile dislocations, was discovered. Carbon atoms that have passed from the crystal lattice of cementite to dislocations are carried out into the interlamellar space and form particles of tertiary cementite, the size of which is 2 – 4 nm. In the process of steel deformation, an inhomogeneous dislocation substructure is formed, which is due to the deceleration of dislocations by cementite particles. It was found that an increase in the deformation degree is accompanied by a decrease in the scalar and excess density of dislocations, which may be due to the escape of dislocations into low-angle boundaries, as well as their annihilation. It was established that the sources of internal stress fields are the interfaces between pearlite grains and colonies, cementite plates in pearlite grains, particles of the second phase located in the volume of ferrite plates.
- 2 October 2022
- Published by National University of Science and Technology MISiS in Izvestiya. Ferrous Metallurgy
- Vol. 65 (9) , 654-661
Open AccessEvolution of structure of rail steel lamellar pearlite under compression deformation
The article presents the results of analysis of evolution of the defective substructure of rail steel pearlite with lamellar morphology under deformation by uniaxial compression. The strain hardening of the studied steel under such deformation has a multistage character. Deformation of steel is accompanied by fragmentation of pearlite grains, which intensifies as the degree of deformation increases and reaches 0.4 of the studied foil volume at ε = 50 %. Fragments formed in ferrite plates are separated by low-angle boundaries. It was established that the average sizes of ferrite plate fragments decrease from 240 nm (ε = 15 %) to 200 nm (ε = 50 %) with an increase in the deformation degree. Fragmentation of cementite plates was revealed. It was found that the size of the fragments varies within 15 – 20 nm and weakly depends on the degree of steel deformation. Fracture of cementite lamellae, proceeding by their dissolution and cutting by mobile dislocations, was discovered. Carbon atoms that have passed from the crystal lattice of cementite to dislocations are carried out into the interlamellar space and form particles of tertiary cementite, the size of which is 2 – 4 nm. In the process of steel deformation, an inhomogeneous dislocation substructure is formed, which is due to the deceleration of dislocations by cementite particles. It was found that an increase in the deformation degree is accompanied by a decrease in the scalar and excess density of dislocations, which may be due to the escape of dislocations into low-angle boundaries, as well as their annihilation. It was established that the sources of internal stress fields are the interfaces between pearlite grains and colonies, cementite plates in pearlite grains, particles of the second phase located in the volume of ferrite plates.
- 1 October 2022
- Published by Allerton Press in Steel in Translation
- Vol. 52 (10) , 899-906
High-Entropy Alloy Coatings: State and Prospects
We have made a brief review of recent foreign and domestic publications, in which the structures, phase compositions, and properties of films and coatings
- 1 October 2022
- Published by Allerton Press in Steel in Translation
- Vol. 52 (10) , 899-906
High-Entropy Alloy Coatings: State and Prospects
We have made a brief review of recent foreign and domestic publications, in which the structures, phase compositions, and properties of films and coatings
- 1 May 2022
- Published by Springer Nature in Russian Physics Journal
- Vol. 65 (1) , 107-113
Structure and Properties of SnO2–In2O3–Ag–N Coatings Formed by a Complex Method on Copper
- 1 May 2022
- Published by Springer Nature in Russian Physics Journal
- Vol. 65 (1) , 107-113
Structure and Properties of SnO2–In2O3–Ag–N Coatings Formed by a Complex Method on Copper
- Open Access
- 17 March 2022
- Published by National University of Science and Technology MISiS in Izvestiya. Ferrous Metallurgy
- Vol. 65 (2) , 134-136
Redistribution of carbon atoms in rails under ultra long-term operation
The article considers quantitative estimation of the relative carbon content in the structure elements of rail head after passed tonnage of 1411 and 1770 mln tons. In the initial state carbon is mainly located in cementite particles and after the operation the defects of crystal structure together with cementite are the places of carbon location. It is shown that the processes of carbon redistribution take place more intensive in surface layers up to 2 mm. Increase in passed tonnage is accompanied by intensive carbon movement on the defects of working fillet structure compared to the tread surface.
- 17 March 2022
- Published by National University of Science and Technology MISiS in Izvestiya. Ferrous Metallurgy
- Vol. 65 (2) , 134-136
Open AccessRedistribution of carbon atoms in rails under ultra long-term operation
The article considers quantitative estimation of the relative carbon content in the structure elements of rail head after passed tonnage of 1411 and 1770 mln tons. In the initial state carbon is mainly located in cementite particles and after the operation the defects of crystal structure together with cementite are the places of carbon location. It is shown that the processes of carbon redistribution take place more intensive in surface layers up to 2 mm. Increase in passed tonnage is accompanied by intensive carbon movement on the defects of working fillet structure compared to the tread surface.