Lijin Dong
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Lijin Dong has a total of 94 co-authors. Here are the top co-authors by number of shared publications:
Qinying Wang
Southwest Petroleum University School of New Energy and Materials Chengdu
16 shared publicationsLi Liu
Southwest Petroleum University School of New Energy and Materials Chengdu
12 shared publicationsHuaibei Zheng
Chengdu Advanced Metal Materials Industry Technology Research Institute Co., Ltd, Chengdu, China
10 shared publications- Qinying Wang
School of New Energy and Materials, Southwest Petroleum University, Chengdu, China
8 shared publications En-Hou Han
Key Laboratory of Nuclear Materials and Safety Assessment, Institute of Metal Research, Chinese Academy of Sciences, Shenyang, 110016, China
6 shared publicationsXingshou Zhang
School of New Energy and Materials, Southwest Petroleum University, Chengdu, China
6 shared publications
Latest Publications
- 17 November 2026
- Published by Emerald Publishing in Anti-Corrosion Methods and Materials
- p. 1-14
Effect of pre-strain on hydrogen permeation and embrittlement susceptibility of X80 steel under cathodic protection conditions
Purpose: This study aims to investigate the effects of varying pre-strain levels on the hydrogen permeation and embrittlement behavior of X80 pipeline steel in simulated marine environments. Design/methodology/approach: Electrochemical hydrogen permeation tests, slow-strain-rate tensile tests and microstructural characterization were used to study hydrogen permeation kinetics and fracture behavior under varying pre-strain levels and cathodic polarization potentials. Findings: Pre-strain significantly increased the dislocation density and the low-angle grain boundary fraction, while it reduced the effective hydrogen diffusion coefficient and increased subsurface hydrogen concentration and total hydrogen trap density. The hydrogen embrittlement index exhibited a monotonic upward trend with increasingly negative cathodic polarization potential and increasing pre-strain level. As pre-strain increased, the high density of hydrogen traps immobilized diffusible hydrogen. Under applied stress, hydrogen accumulated in stress-concentrated regions via the hydrogen-enhanced localized plasticity mechanism, inducing localized plastic deformation and severely compromising the macroscopic plasticity of X80 steel. Originality/value: This work provides critical insights for ensuring the safe operation of strained X80 pipeline steel under cathodic protection conditions in simulated marine environments.
- 17 November 2026
- Published by Emerald Publishing in Anti-Corrosion Methods and Materials
- p. 1-14
Effect of pre-strain on hydrogen permeation and embrittlement susceptibility of X80 steel under cathodic protection conditions
Purpose: This study aims to investigate the effects of varying pre-strain levels on the hydrogen permeation and embrittlement behavior of X80 pipeline steel in simulated marine environments. Design/methodology/approach: Electrochemical hydrogen permeation tests, slow-strain-rate tensile tests and microstructural characterization were used to study hydrogen permeation kinetics and fracture behavior under varying pre-strain levels and cathodic polarization potentials. Findings: Pre-strain significantly increased the dislocation density and the low-angle grain boundary fraction, while it reduced the effective hydrogen diffusion coefficient and increased subsurface hydrogen concentration and total hydrogen trap density. The hydrogen embrittlement index exhibited a monotonic upward trend with increasingly negative cathodic polarization potential and increasing pre-strain level. As pre-strain increased, the high density of hydrogen traps immobilized diffusible hydrogen. Under applied stress, hydrogen accumulated in stress-concentrated regions via the hydrogen-enhanced localized plasticity mechanism, inducing localized plastic deformation and severely compromising the macroscopic plasticity of X80 steel. Originality/value: This work provides critical insights for ensuring the safe operation of strained X80 pipeline steel under cathodic protection conditions in simulated marine environments.
- 22 September 2026
- Published by SAGE Publications in Corrosion Engineering, Science and Technology: The International Journal of Corrosion Processes and Corrosion Control
Effects of austenitizing time on microstructure and hydrogen environment-assisted cracking behavior of M54 steel
Ferrium M54 steel offers a cost-effective alternative to AerMet 100, achieving comparable strength and toughness through reduced Co content and additions of W, Nb, and Ti. However, hydrogen environment-assisted cracking (HEAC) is a critical concern for the engineering application of this steel. This study investigated the effect of austenitizing time on the microstructure and HEAC behavior of M54 steel. Microstructure analyses through optical microscopy, X-ray diffraction, electron backscatter diffraction, and transmission electron microscopy revealed that extending austenitizing time beyond 75 min led to noticeable grain growth, dissolution of MC carbides and a reduction of the austenite volume fraction. The prior austenite grain boundaries acted as the preferential pathway for hydrogen atoms to diffuse in M54 steel. The hydrogen diffusion coefficient, crack growth rate and HEAC susceptibility exhibited a peak value after austenitizing treatment for 75 min, which may be due to the combined effect of the austenite fraction and prior austenite grain size. This work elucidates how a specific austenitizing treatment can reduce HEAC risks and proposes an optimized austenitizing protocol for M54 steel.
- 22 September 2026
- Published by SAGE Publications in Corrosion Engineering, Science and Technology: The International Journal of Corrosion Processes and Corrosion Control
Effects of austenitizing time on microstructure and hydrogen environment-assisted cracking behavior of M54 steel
Ferrium M54 steel offers a cost-effective alternative to AerMet 100, achieving comparable strength and toughness through reduced Co content and additions of W, Nb, and Ti. However, hydrogen environment-assisted cracking (HEAC) is a critical concern for the engineering application of this steel. This study investigated the effect of austenitizing time on the microstructure and HEAC behavior of M54 steel. Microstructure analyses through optical microscopy, X-ray diffraction, electron backscatter diffraction, and transmission electron microscopy revealed that extending austenitizing time beyond 75 min led to noticeable grain growth, dissolution of MC carbides and a reduction of the austenite volume fraction. The prior austenite grain boundaries acted as the preferential pathway for hydrogen atoms to diffuse in M54 steel. The hydrogen diffusion coefficient, crack growth rate and HEAC susceptibility exhibited a peak value after austenitizing treatment for 75 min, which may be due to the combined effect of the austenite fraction and prior austenite grain size. This work elucidates how a specific austenitizing treatment can reduce HEAC risks and proposes an optimized austenitizing protocol for M54 steel.
- Open Access
- 17 August 2026
- Published by Taylor & Francis in Nuclear Technology
- p. 1-17
Effect of Crack Location on the Mechanical State at the Tip of Stress Corrosion Cracks in Dissimilar Metal Welded Joints
I. The dissimilar metal weld joint (DMWJ) between low-alloy steel SA508 and 316L austenitic stainless steel (SS) piping is a critical component extensively utilized in the primary coolant circuits ...
- 17 August 2026
- Published by Taylor & Francis in Nuclear Technology
- p. 1-17
Open AccessEffect of Crack Location on the Mechanical State at the Tip of Stress Corrosion Cracks in Dissimilar Metal Welded Joints
I. The dissimilar metal weld joint (DMWJ) between low-alloy steel SA508 and 316L austenitic stainless steel (SS) piping is a critical component extensively utilized in the primary coolant circuits ...
- 18 June 2026
- Published by Springer Nature in Journal of Materials Engineering and Performance
- Vol. 35 (34) , 35808-35819
Simulation of Pit Growth Behavior of Nickel-Based Alloy 825 in High-Temperature and High-Pressure CO2 Environments
- 18 June 2026
- Published by Springer Nature in Journal of Materials Engineering and Performance
- Vol. 35 (34) , 35808-35819
Simulation of Pit Growth Behavior of Nickel-Based Alloy 825 in High-Temperature and High-Pressure CO2 Environments
- 26 January 2026
- Published by Springer Nature in Journal of Materials Engineering and Performance
- Vol. 35 (21) , 21425-21439
Effect of Heat Treatment on Microstructure and Stress Corrosion Cracking of M54 Ultra-High Strength Steel
- 26 January 2026
- Published by Springer Nature in Journal of Materials Engineering and Performance
- Vol. 35 (21) , 21425-21439
Effect of Heat Treatment on Microstructure and Stress Corrosion Cracking of M54 Ultra-High Strength Steel
- 25 June 2025
- Published by Elsevier in Corrosion Science
- Vol. 255
Unveiling localized protection and media-dependent degradation mechanism of Inconel 625 coating during tribocorrosion
- 25 June 2025
- Published by Elsevier in Corrosion Science
- Vol. 255
Unveiling localized protection and media-dependent degradation mechanism of Inconel 625 coating during tribocorrosion
- 2 June 2025
- Published by Springer Nature in Journal of Materials Engineering and Performance
- Vol. 34 (24) , 30240-30258
Effect of Temperature on Stress Corrosion Cracking of AerMet 100 Ultra-High-Strength Steel in Simulated Marine Environments
- 2 June 2025
- Published by Springer Nature in Journal of Materials Engineering and Performance
- Vol. 34 (24) , 30240-30258
Effect of Temperature on Stress Corrosion Cracking of AerMet 100 Ultra-High-Strength Steel in Simulated Marine Environments