    Determining the patterns of phase and structural transformations at carbon­thermal reduction of molybdenum concentrate

    by Stanislav Hryhoriev, Artem Petryshchev, Ganna Shyshkanova, Tetyana Zaytseva, Oleksandr Frydman, Yuliya Petrusha, Andrey Andreev, Alexander Katschan, Mykola Lazutkin, Nina Sinyaeva

    We have studied patterns in the influence of O/C in the charge on the content of C, O2, and Mo in metallized molybdenum concentrate after different temperatures of thermal treatment. it was determined that O/C at 1.75‒2.00 in the charge after treatment at 1,223–1,423 K provides for the content of Mo in metallized molybdenum concentrate at 74.6–78.0 % by weight. The content of C and O2 was 0.5–2.0 % by weight, and 0.6–5.5 % by weight, respectively. At O/C in the charge at 2.50, the products of reduction after heat treatment at 1,323 K consisted of Mo and MoO2. The residual molybdenum-containing oxide component is due to the insufficient amount of a reducing agent. The presence in the phase composition of carbide Mo2C together with Mo was found at O/C in the charge at 1.33, indicating a certain excess of the carbon reducing agent. The most favorable conditions for reduction were ensured at O/C in the charge at the level of 1.83 with a transition of most of the oxides to the metal phase of Mo. We have obtained a spongy structure of the metallized product, which ensures an increased rate of dissolving the obtained molybdenum-containing additive in a liquid metal at alloying. We did not identify in the phase composition any compounds susceptible to sublimation, which predetermines a reduction in the losses of Mo when using an alloying additive.

  • Open Access

    A study of environmentally friendly recycling of technogenic chromium and nickel containing waste by the method of solid phase extraction

    by Stanislav Hryhoriev, Artem Petryshchev, Ganna Shyshkanova, Tetyana Zaytseva, Oleksandr Frydman, Kristina Krupey, Andrey Andreev, Alexander Katschan, Yuliya Petrusha, Dmytro Stepanov

    The study has revealed the regularities of the effect produced by increasing the content of scale of steel 12Cr18Ni10Ti in the charge from 5 to 75 mass % on the contents of the products of carbon thermal reduction of oxide waste of corrosion-resistant steels. The concentration of Ni is increased from 0.8 to 7.0 mass % when the Cr content ranges from 15.9 to 17.1 mass %. The concentration of Cr in the extraction products within the range of 16.1–17.1 mass% is provided with the content of scale of 95Cr18 steel in the charge in the range from 5 to 55 mass %. It has been found that metallization products mainly consist of a solid solution of alloying elements in α-Fe. Fe3O4, Fe3C, and Fe2C were also identified. The microstructure of the extraction products is spongy and disordered. The particles are sintered, with varying Cr and Ni contents in the ranges of 7.47 to 18.03 mass % and 2.97–10.40 mass %, respectively. The study has helped achieve environmentally safe conditions for solid-phase extraction of chrome and nickel containing industrial wastes from the production of corrosion-resistant steels with the return of the alloyed product to the welding industry


  • Open Access

    A study of environmentally safe obtaining of molybdenum-based alloying material by solid phase extraction

    by Stanislav Hryhoriev, Artem Petryshchev, Kristina Krupey, Andrey Andreev, Alexander Katschan, Dmytro Stepanov, Yevheniia Manidina, Vadim Ryzhkov, Nataliia Berenda, Anton Matiukhin

    The study has determined an increase of the degree of thermal carbon extraction of the molybdenum oxide concentrate from 11 % to 97 % with an increase in the processing temperature from 873 K to 1373 K, respectively. A further rise in temperature to 1473 K led to a reduction in the degree of recovery to 89 %. The recovery products after treatment at 873–1073 K mostly consisted of MoO2 with some Mo and Mo2C manifestations. Treatment at 1223–1473 K provided a predominance of Mo and Mo2C as to the oxide component. The microstructure of the recovery products was spongy and disordered with varying degrees of sintering, depending on the processing temperature. The alloying of R6M5 steel with the new molybdenum material in experimental industrial conditions provided an increase in the Mo uptake rate from 88.9 % to 95.0 % compared with the standard technology. Improvement of environmental safety is achieved by replacing carbon monoxide and aluminothermic melting of ferroalloy production of Mo with the latest methods of powder metallurgy.