Sandan Kumar Sharma
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Previous Organizations / Institutes
The organizations / institutes from the scholar's other articles in the past ten years
Research Subjects
Sandan Kumar Sharma has a total of 41 co-authors. Here are the top co-authors by number of shared publications:
- Balabhadrapatruni Venkata Manoj Kumar
TriboCeramics Laboratory Department of Metallurgical and Materials Engineering Indian Institute of Technology (IIT) Roorkee Roorkee India
10 shared publications - Young-Wook Kim
University of Seoul
6 shared publications Amrita Kumari
Department of Metallurgical and Materials Engineering Indian Institute of Technology Patna Bihar India
2 shared publicationsB. Venkata Manoj Kumar
2 shared publications- Debrupa Lahiri
Indian Institute of Technology Roorkee
2 shared publications Divyansh Mittal
Department of Mechanical Engineering Indian Institute of Technology Jodhpur Rajasthan India
2 shared publications
Latest Publications
- 8 April 2026
- Published by Elsevier in Tribology International
- Vol. 221
Grain-refinement-mediated tribo-oxidation and corrosion trade-offs in a dual-phase AlCoCrFeNi high-entropy alloy
- 8 April 2026
- Published by Elsevier in Tribology International
- Vol. 221
Grain-refinement-mediated tribo-oxidation and corrosion trade-offs in a dual-phase AlCoCrFeNi high-entropy alloy
- 1 March 2026
- Published by Wiley in Advanced Engineering Materials
- Vol. 28 (9)
A Comprehensive Review on Processing and Tribological Performance of YAG Transparent Ceramics
Transparent yttrium aluminum garnet (YAG) ceramics are attracting considerable attention owing to their high optical transmittance over a broad spectral range, hardness, and fracture toughness, which make them suitable for tribological applications under extreme service conditions. This article summarizes the main processing routes for YAG transparent ceramics, including powder synthesis, calcination, the use of sintering aids, green body formation, and densification, as well as alternative approaches based on glass formation. It analyses links between processing conditions, microstructure, and mechanical and tribological behavior, with emphasis on how grain size, porosity, or dopants influence mechanical properties and tribological behavior. Available data on the mechanisms of deformation, fracture, and wear under sliding, scratching, and impact loading are reviewed, with special attention given to material removal mechanisms, including ductile‐to‐brittle transitions and crack propagation pathways, which govern tribological behavior. The review concludes with perspectives on processing optimization and dopant engineering to enhance the tribological reliability of YAG ceramics for advanced structural and defense applications.
- 1 March 2026
- Published by Wiley in Advanced Engineering Materials
- Vol. 28 (9)
A Comprehensive Review on Processing and Tribological Performance of YAG Transparent Ceramics
Transparent yttrium aluminum garnet (YAG) ceramics are attracting considerable attention owing to their high optical transmittance over a broad spectral range, hardness, and fracture toughness, which make them suitable for tribological applications under extreme service conditions. This article summarizes the main processing routes for YAG transparent ceramics, including powder synthesis, calcination, the use of sintering aids, green body formation, and densification, as well as alternative approaches based on glass formation. It analyses links between processing conditions, microstructure, and mechanical and tribological behavior, with emphasis on how grain size, porosity, or dopants influence mechanical properties and tribological behavior. Available data on the mechanisms of deformation, fracture, and wear under sliding, scratching, and impact loading are reviewed, with special attention given to material removal mechanisms, including ductile‐to‐brittle transitions and crack propagation pathways, which govern tribological behavior. The review concludes with perspectives on processing optimization and dopant engineering to enhance the tribological reliability of YAG ceramics for advanced structural and defense applications.
- 19 September 2024
- Published by Wiley in International Journal of Applied Ceramic Technology
- Vol. 22 (3)
Dry sliding behavior of transparent yttrium aluminum garnet against 100Cr6 steel balls
Transparent yttrium aluminum garnet (YAG) exhibits high hardness and abrasive resistance, making it a promising candidate for applications involving material contact, such as protective optical elements, windows, domes, and armors. When transparent YAG is employed in such applications, it may be susceptible to degradation due to friction, chemical exposure, or thermal stress. Despite its potential, there is limited research on the tribological behavior of transparent YAG. In the present study, transparent YAG ceramics were fabricated by reaction sintering of high‐purity Al2O3 and Y2O3 powders. The transparent YAG specimens had an average grain size of 20 ± 6 µm and hardness of 1068.98 ± 115.15 HV, and fracture toughness of 1.27 ± .06 MPa.m0.5. The effect of load variation from 5 to 15 N on the tribological behavior of transparent YAG was investigated when slid against chrome steel (100Cr6) balls with a hardness of 815 ± 75 HV. The low coefficient of friction (COF) and wear rate were observed due to the wedge formation (fish‐scale‐like pattern) at the surface when the load was increased from 5 to 10 N. Moreover, tribochemical layer formation, fracture, and material transfer were observed when the load was increased from 10 to 15 N, leading to high COF and increased wear rate.
- 19 September 2024
- Published by Wiley in International Journal of Applied Ceramic Technology
- Vol. 22 (3)
Dry sliding behavior of transparent yttrium aluminum garnet against 100Cr6 steel balls
Transparent yttrium aluminum garnet (YAG) exhibits high hardness and abrasive resistance, making it a promising candidate for applications involving material contact, such as protective optical elements, windows, domes, and armors. When transparent YAG is employed in such applications, it may be susceptible to degradation due to friction, chemical exposure, or thermal stress. Despite its potential, there is limited research on the tribological behavior of transparent YAG. In the present study, transparent YAG ceramics were fabricated by reaction sintering of high‐purity Al2O3 and Y2O3 powders. The transparent YAG specimens had an average grain size of 20 ± 6 µm and hardness of 1068.98 ± 115.15 HV, and fracture toughness of 1.27 ± .06 MPa.m0.5. The effect of load variation from 5 to 15 N on the tribological behavior of transparent YAG was investigated when slid against chrome steel (100Cr6) balls with a hardness of 815 ± 75 HV. The low coefficient of friction (COF) and wear rate were observed due to the wedge formation (fish‐scale‐like pattern) at the surface when the load was increased from 5 to 10 N. Moreover, tribochemical layer formation, fracture, and material transfer were observed when the load was increased from 10 to 15 N, leading to high COF and increased wear rate.
- 3 April 2023
- Published by SAGE Publications in Tribology - Materials, Surfaces & Interfaces
- Vol. 17 (2) , 119-135
Dry sliding wear of ductile and austempered ductile iron: effect of load and sliding speed
In this study, dry sliding wear behaviour of a copper alloyed austempered ductile iron (ADI) consisting of very fine ausferrite, small high carbon austenite blocks, was investigated against 100Cr6 ball using ball-on-disc tribometer. Tribotests were conducted at different loads of 10, 30, 50, and 100 N and speeds between 0.39 to 0.79 m/s. Worn-out surfaces and wear debris revealed tribe-oxidation and abrasive wear as the primary mechanism for material removal at lower loads and low speed (0.39 m/s). With an increase in load and speed, fragmented graphite nodules acted as solid lubricants. Additionally, partial transfer of tribo-oxide onto the counter-body ball, and plastic deformation and strain hardening of ADI matrix lowered the friction coefficient and wear rate at higher loads and speed, to nearly 1/3 and 1/10 as compared with those at lower loads and speed. The superior wear resistance of present ADI is worthy of consideration for transmission parts. GRAPHICAL ABSTRACT
- 3 April 2023
- Published by SAGE Publications in Tribology - Materials, Surfaces & Interfaces
- Vol. 17 (2) , 119-135
Dry sliding wear of ductile and austempered ductile iron: effect of load and sliding speed
In this study, dry sliding wear behaviour of a copper alloyed austempered ductile iron (ADI) consisting of very fine ausferrite, small high carbon austenite blocks, was investigated against 100Cr6 ball using ball-on-disc tribometer. Tribotests were conducted at different loads of 10, 30, 50, and 100 N and speeds between 0.39 to 0.79 m/s. Worn-out surfaces and wear debris revealed tribe-oxidation and abrasive wear as the primary mechanism for material removal at lower loads and low speed (0.39 m/s). With an increase in load and speed, fragmented graphite nodules acted as solid lubricants. Additionally, partial transfer of tribo-oxide onto the counter-body ball, and plastic deformation and strain hardening of ADI matrix lowered the friction coefficient and wear rate at higher loads and speed, to nearly 1/3 and 1/10 as compared with those at lower loads and speed. The superior wear resistance of present ADI is worthy of consideration for transmission parts. GRAPHICAL ABSTRACT
- 28 December 2021
- Published by Wiley in International Journal of Applied Ceramic Technology
- Vol. 19 (3) , 1691-1701
Erosive wear behavior of spark plasma‐sintered SiC–TaC composites
Spark plasma sintering of SiC‐10, 20, or 30 wt% TaC composites was performed at 1800°C. Microstructures of sintered composites revealed uniform dispersion of TaC particles in SiC matrix. With the increase in TaC content, hardness decreased from 25.75 to 23.30 GPa and fracture toughness increased from 3.48 to 3.85 MPa m 1/2 . Erosion testing was performed to evaluate the potential of sintered composites at room temperature and 400°C by a stream of SiC particles impinging at different angles (30°, 60°, or 90°). The erosion rate varied from 25 to 166 mm 3 /kg, with change in TaC content, impingement angle, or temperature. The erosion rate increased as the angle of impingement and temperature increased, but reduced when the TaC concentration increased. Worn surfaces revealed that the material was dominantly removed via fracture of SiC grains and TaC particles pull‐out. SiC‐30 wt% TaC composites exhibited superior erosive wear resistance at low impingement angle and room temperature.
- 28 December 2021
- Published by Wiley in International Journal of Applied Ceramic Technology
- Vol. 19 (3) , 1691-1701
Erosive wear behavior of spark plasma‐sintered SiC–TaC composites
Spark plasma sintering of SiC‐10, 20, or 30 wt% TaC composites was performed at 1800°C. Microstructures of sintered composites revealed uniform dispersion of TaC particles in SiC matrix. With the increase in TaC content, hardness decreased from 25.75 to 23.30 GPa and fracture toughness increased from 3.48 to 3.85 MPa m 1/2 . Erosion testing was performed to evaluate the potential of sintered composites at room temperature and 400°C by a stream of SiC particles impinging at different angles (30°, 60°, or 90°). The erosion rate varied from 25 to 166 mm 3 /kg, with change in TaC content, impingement angle, or temperature. The erosion rate increased as the angle of impingement and temperature increased, but reduced when the TaC concentration increased. Worn surfaces revealed that the material was dominantly removed via fracture of SiC grains and TaC particles pull‐out. SiC‐30 wt% TaC composites exhibited superior erosive wear resistance at low impingement angle and room temperature.
- 14 October 2021
- Published by Springer Nature in Silicon
- Vol. 14 (12) , 7377-7382
Flash Spark Plasma Sintering of SiC: Impact of Additives
- 14 October 2021
- Published by Springer Nature in Silicon
- Vol. 14 (12) , 7377-7382
Flash Spark Plasma Sintering of SiC: Impact of Additives
- Open Access
- 16 March 2018
- Published by Tsinghua University Press in Friction
- Vol. 7 (2) , 129-142
Tribology of WC reinforced SiC ceramics: Influence of counterbody
Hot pressed silicon carbide (SiC) composites prepared with 0, 10, 30 or 50 wt% tungsten carbide (WC) are subjected to dry sliding wear against WC-Co and steel ball. In particular an attempt has been made to answer the following important questions: (i) How does the load (from 5 to 20 N) effect sliding wear behaviour of SiC-ceramics against WC-Co and steel counterbodies? (ii) Is there any effect of WC content on friction and wear characteristics of SiC ceramics? (iii) Does the dominant material removal mechanism of SiC ceramics change with the addition of WC or counterbody? (iv) What is the influence of mechanical properties on the sliding wear? Experimental results indicated that coefficient of friction (COF) for the SiC ceramics varied between 0.66 and 0.33 with change in load and counterbodies. Wear volume for SiC ceramics found approximately 6−10 times more against WC-Co as compared against steel. Wear volume changes from 2.0 × 10–3 mm3 to 1.2 × 10–2 mm3 with change in counterbodies for SiC-(10, 30 or 50 wt%) WC composite at 20 N. SiC ceramics indicated abrasion and composites reveal tribochemical wear as major material removal mechanisms. Wear is influenced by the hardness of counterbody and fracture toughness of SiC-WC composites.
- 16 March 2018
- Published by Tsinghua University Press in Friction
- Vol. 7 (2) , 129-142
Open AccessTribology of WC reinforced SiC ceramics: Influence of counterbody
Hot pressed silicon carbide (SiC) composites prepared with 0, 10, 30 or 50 wt% tungsten carbide (WC) are subjected to dry sliding wear against WC-Co and steel ball. In particular an attempt has been made to answer the following important questions: (i) How does the load (from 5 to 20 N) effect sliding wear behaviour of SiC-ceramics against WC-Co and steel counterbodies? (ii) Is there any effect of WC content on friction and wear characteristics of SiC ceramics? (iii) Does the dominant material removal mechanism of SiC ceramics change with the addition of WC or counterbody? (iv) What is the influence of mechanical properties on the sliding wear? Experimental results indicated that coefficient of friction (COF) for the SiC ceramics varied between 0.66 and 0.33 with change in load and counterbodies. Wear volume for SiC ceramics found approximately 6−10 times more against WC-Co as compared against steel. Wear volume changes from 2.0 × 10–3 mm3 to 1.2 × 10–2 mm3 with change in counterbodies for SiC-(10, 30 or 50 wt%) WC composite at 20 N. SiC ceramics indicated abrasion and composites reveal tribochemical wear as major material removal mechanisms. Wear is influenced by the hardness of counterbody and fracture toughness of SiC-WC composites.
- 1 January 2018
- Published by Elsevier in Materials Today: Proceedings
- Vol. 5 (9) , 17342-17349
Effect of linear velocity on sliding wear behavior of TiCN based cermets
- 1 January 2018
- Published by Elsevier in Materials Today: Proceedings
- Vol. 5 (9) , 17342-17349
Effect of linear velocity on sliding wear behavior of TiCN based cermets
- 1 December 2017
- Published by Elsevier in Ceramics International
- Vol. 43 (18) , 16827-16834
Room and high temperature reciprocated sliding wear behavior of SiC-WC composites
- 1 December 2017
- Published by Elsevier in Ceramics International
- Vol. 43 (18) , 16827-16834
Room and high temperature reciprocated sliding wear behavior of SiC-WC composites
- 1 November 2017
- Published by Elsevier in International Journal of Refractory Metals and Hard Materials
- Vol. 68, 166-171
Effect of impingement angle and WC content on high temperature erosion behavior of SiC-WC composites
- 1 November 2017
- Published by Elsevier in International Journal of Refractory Metals and Hard Materials
- Vol. 68, 166-171
Effect of impingement angle and WC content on high temperature erosion behavior of SiC-WC composites