Alexey B. Shubin
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Previous Organizations / Institutes
The organizations / institutes from the scholar's other articles in the past ten years
Research Subjects
Research Interests
Alexey B. Shubin has a total of 45 co-authors. Here are the top co-authors by number of shared publications:
E. A. Pastukhov
Russian Academy of Sciences
9 shared publications- Tatyana V. Kulikova
Vatolin Institute of Metallurgy of the Ural Branch of the Russian Academy of Sciences
6 shared publications - Viktor Anatolyevich Bykov
Institute of Metallurgy, Ural Branch of the Russian Academy of Sciences, Yekaterinburg 620002, Russia
6 shared publications E. A. Popova
5 shared publicationsK. Y. Shunyaev
Russian Academy of Sciences, Urals Branch
5 shared publicationsK. Yu. Shunyaev
Russian Academy of Sciences
5 shared publications
Latest Publications
- 1 June 2026
- Published by Springer Nature in Russian Chemical Bulletin
- Vol. 75 (6) , 1823-1830
Synthesis of diffusion-hardening alloys from a mixture of solid components containing gallium powder
- 1 June 2026
- Published by Springer Nature in Russian Chemical Bulletin
- Vol. 75 (6) , 1823-1830
Synthesis of diffusion-hardening alloys from a mixture of solid components containing gallium powder
- Open Access
Effect of Copper on the Formation of L12 Intermetallic Phases in Al–Cu–X (X = Ti, Zr, Hf) Alloys
Transition metal trialuminides of the Al3X type of groups 4 and 5 of the periodic system have reduced density, high melting points, and corrosion resistance. Aluminides with a cubic lattice of the Al3Sc type can be used as a nucleating phase for aluminum alloys. However, low plasticity and a tetragonal lattice limit their application. In this work, we stabilized the metastable cubic lattice of Al3X-type aluminides by replacing aluminum with copper. The conditions for the formation of L12 metastable aluminides in the Al–Cu–TM (TM: Ti, Zr, Hf) alloys were studied using a wide range of copper concentrations. A high concentration of copper (hypereutectic alloys) is the one of the necessary conditions for the formation of (Al1−xCux)3Ti, (Al1−xCux)3Zr, (Al1−xCux)3Hf aluminides. With an increase in the copper concentration, the number of metastable aluminides sharply increased. The process of their formation strongly depended on the sequence of dissolution of the corresponding components in the melts. The low volume fraction of precipitated titanium aluminides was the result of insufficient supersaturation of α-Al with titanium (at the peritectic temperature) compared to that for alloys with zirconium and hafnium. Under identical synthesis conditions in the crystal lattice of metastable aluminides formed in experimental Al–Cu–Ti, Al–Cu–Zr, Al–Cu–Hf alloys, copper was found to substitute up to 8, 10, and 13 at.% of aluminum, respectively. The crystallographic and dimensional similarities of the lattices in metastable transition metal aluminides and in α-Al suggest their usefulness as modifying additions in aluminum-based alloys.
Open AccessEffect of Copper on the Formation of L12 Intermetallic Phases in Al–Cu–X (X = Ti, Zr, Hf) Alloys
Transition metal trialuminides of the Al3X type of groups 4 and 5 of the periodic system have reduced density, high melting points, and corrosion resistance. Aluminides with a cubic lattice of the Al3Sc type can be used as a nucleating phase for aluminum alloys. However, low plasticity and a tetragonal lattice limit their application. In this work, we stabilized the metastable cubic lattice of Al3X-type aluminides by replacing aluminum with copper. The conditions for the formation of L12 metastable aluminides in the Al–Cu–TM (TM: Ti, Zr, Hf) alloys were studied using a wide range of copper concentrations. A high concentration of copper (hypereutectic alloys) is the one of the necessary conditions for the formation of (Al1−xCux)3Ti, (Al1−xCux)3Zr, (Al1−xCux)3Hf aluminides. With an increase in the copper concentration, the number of metastable aluminides sharply increased. The process of their formation strongly depended on the sequence of dissolution of the corresponding components in the melts. The low volume fraction of precipitated titanium aluminides was the result of insufficient supersaturation of α-Al with titanium (at the peritectic temperature) compared to that for alloys with zirconium and hafnium. Under identical synthesis conditions in the crystal lattice of metastable aluminides formed in experimental Al–Cu–Ti, Al–Cu–Zr, Al–Cu–Hf alloys, copper was found to substitute up to 8, 10, and 13 at.% of aluminum, respectively. The crystallographic and dimensional similarities of the lattices in metastable transition metal aluminides and in α-Al suggest their usefulness as modifying additions in aluminum-based alloys.
- 30 September 2022
- Published by Pleiades Publishing Ltd in Inorganic Materials: Applied Research
- Vol. 13 (5) , 1371-1375
Electrical Contact Material Based on a Copper Powder Clad with a Fe–Cu Pseudo Alloy
A composite material (CM) based on a copper powder clad with a Fe–Cu pseudo alloy (PA) for a working layer of two-layer interrupting electrical contacts was created using pressing, rolling, and sintering. The powder of activated carbon (CA) with the specific surface area of 1000 m2/g served as an arc quenching component, and highly dispersed powders of Al2O3, Fe2Al5, and Fe were used as additional components. The experimental linear dependences of the conductivity and hardness of copper-based composites on the concentration of particular functional additives of CA, PA, Al2O3, and Fe2Al5 were established. The addition of mixtures of these components was used to obtain CMs for the working contact layer of the following compositions (in wt %): 97% Cu + 1% СА + 2% PA and 97.5% Cu + 1% СA + 0.5% PA + 1% Al2O3 with the electrical resistivity of 3.20 and 4.5 μΩ cm and hardness HB of 1030 and 790 MPa, respectively. The dependence of the maximum allowable resistivity of the working layer (ρCM) on the ratio of its thickness to that of the copper layer was calculated for a given conductivity of a two-layer contact at a level of at least 75% of the copper conductivity. The characteristics of the CM with the composition 97% Cu + 1% СА + 2% PA make it possible to create an electrical contact for which the ratio of thicknesses of the working and copper layers is 1 : 1.
- 30 September 2022
- Published by Pleiades Publishing Ltd in Inorganic Materials: Applied Research
- Vol. 13 (5) , 1371-1375
Electrical Contact Material Based on a Copper Powder Clad with a Fe–Cu Pseudo Alloy
A composite material (CM) based on a copper powder clad with a Fe–Cu pseudo alloy (PA) for a working layer of two-layer interrupting electrical contacts was created using pressing, rolling, and sintering. The powder of activated carbon (CA) with the specific surface area of 1000 m2/g served as an arc quenching component, and highly dispersed powders of Al2O3, Fe2Al5, and Fe were used as additional components. The experimental linear dependences of the conductivity and hardness of copper-based composites on the concentration of particular functional additives of CA, PA, Al2O3, and Fe2Al5 were established. The addition of mixtures of these components was used to obtain CMs for the working contact layer of the following compositions (in wt %): 97% Cu + 1% СА + 2% PA and 97.5% Cu + 1% СA + 0.5% PA + 1% Al2O3 with the electrical resistivity of 3.20 and 4.5 μΩ cm and hardness HB of 1030 and 790 MPa, respectively. The dependence of the maximum allowable resistivity of the working layer (ρCM) on the ratio of its thickness to that of the copper layer was calculated for a given conductivity of a two-layer contact at a level of at least 75% of the copper conductivity. The characteristics of the CM with the composition 97% Cu + 1% СА + 2% PA make it possible to create an electrical contact for which the ratio of thicknesses of the working and copper layers is 1 : 1.
- 30 May 2022
- Published by Pleiades Publishing Ltd in Inorganic Materials: Applied Research
- Vol. 13 (3) , 818-822
Two-Layer Copper-Based Powder Electrocontact
The influence of various schemes of pressure treatment (pressing, rolling) and modes of heat treatment of powder mixtures on the service properties and adhesion strength of the working and current-carrying layers of electrical contacts with a conductivity of at least 75% of the copper conductivity was studied. The dependence of the permissible fraction of the working layer in the total contact thickness on its resistivity was established. It was calculated that, in the created contacts, the thickness of the working layer of two compositions 97% Cu + 1% CA + 2% PA (1) and 97.5% Cu + 1% CA + 0.5% PA + 1% Al2O3 (2), with the electrical resistivity of 3.20 and 3.28 μΩ cm, respectively, can be increased to the thickness of the copper layer (here, CA is activated carbon; PA is a (Fe–Cu) nanocrystalline pseudoalloy). Among the considered processes, we determined the optimum method to fabricate contacts that consists of combined rolling with a reduction of 50% of copper powder and the powder mixture for the working layer using the metering hoppers separated for the charge of each layer, reducing sintering at 600°C for 1 h, and re-compacting rolling with strain of 85% and sintering at 800°С for 1 h. This technique was used to obtain samples of contacts with working layers of two compositions with a relative density of 0.99 and 0.98, hardness HB of 990 and 830 MPa, and electrical resistivity of 2.57 and 2.61 μΩ cm, respectively. The adhesion strength of contact layers is more than 200 MPa (breaking stress for copper).
- 30 May 2022
- Published by Pleiades Publishing Ltd in Inorganic Materials: Applied Research
- Vol. 13 (3) , 818-822
Two-Layer Copper-Based Powder Electrocontact
The influence of various schemes of pressure treatment (pressing, rolling) and modes of heat treatment of powder mixtures on the service properties and adhesion strength of the working and current-carrying layers of electrical contacts with a conductivity of at least 75% of the copper conductivity was studied. The dependence of the permissible fraction of the working layer in the total contact thickness on its resistivity was established. It was calculated that, in the created contacts, the thickness of the working layer of two compositions 97% Cu + 1% CA + 2% PA (1) and 97.5% Cu + 1% CA + 0.5% PA + 1% Al2O3 (2), with the electrical resistivity of 3.20 and 3.28 μΩ cm, respectively, can be increased to the thickness of the copper layer (here, CA is activated carbon; PA is a (Fe–Cu) nanocrystalline pseudoalloy). Among the considered processes, we determined the optimum method to fabricate contacts that consists of combined rolling with a reduction of 50% of copper powder and the powder mixture for the working layer using the metering hoppers separated for the charge of each layer, reducing sintering at 600°C for 1 h, and re-compacting rolling with strain of 85% and sintering at 800°С for 1 h. This technique was used to obtain samples of contacts with working layers of two compositions with a relative density of 0.99 and 0.98, hardness HB of 990 and 830 MPa, and electrical resistivity of 2.57 and 2.61 μΩ cm, respectively. The adhesion strength of contact layers is more than 200 MPa (breaking stress for copper).
- 20 April 2022
- Published by Pleiades Publishing Ltd in Inorganic Materials: Applied Research
- Vol. 13 (2) , 560-568
Interaction of WC and Cr3C2 Carbides at Heat Treatment of WC–Cr3C2–Cu Alloys
We obtained WC–Cr3C2–Cu composite alloys by the copper melt infiltration into uncompacted WC and Cr3C2 powders (the reference alloys) and their mixtures with the weight ratio WC : Cr3C2 = 1 : 1. Impregnation of the uncompacted carbide powders with the copper melt was performed at low-frequency (~80 Hz) vertical vibration (LFV) of the crucible with the alloy components for 10 min in a resistance furnace under a flow-through argon atmosphere. We studied the influence of the heat treatment of the obtained model composites on interaction of the WС and Cr3С2 carbides under isothermal and dynamic temperature impact, as well as during high-speed cyclic heating of the alloy surface by an electric arc (120 A, 45 V, 2 Hz, 10 000 arc interruption cycles). We investigated the evolution of alloy structures by means of electron microscopy, X-ray spectral microanalysis, X-ray phase, and differential thermal analysis. We show that the impact on the sample surface by the temperature field created by the electric arc leads to intense interaction of the carbides. Here, the matrix copper transforms periodically into a melt and plays the role of a transfer medium (the diffusion medium). As a result of such heat treatment, in the upper layers of the alloys, finely dispersed compositions of complex carbide phases occurred with the sizes ≤1–2 μm, i.e., 1–2 orders of magnitude less than that of the initial carbides.
- 20 April 2022
- Published by Pleiades Publishing Ltd in Inorganic Materials: Applied Research
- Vol. 13 (2) , 560-568
Interaction of WC and Cr3C2 Carbides at Heat Treatment of WC–Cr3C2–Cu Alloys
We obtained WC–Cr3C2–Cu composite alloys by the copper melt infiltration into uncompacted WC and Cr3C2 powders (the reference alloys) and their mixtures with the weight ratio WC : Cr3C2 = 1 : 1. Impregnation of the uncompacted carbide powders with the copper melt was performed at low-frequency (~80 Hz) vertical vibration (LFV) of the crucible with the alloy components for 10 min in a resistance furnace under a flow-through argon atmosphere. We studied the influence of the heat treatment of the obtained model composites on interaction of the WС and Cr3С2 carbides under isothermal and dynamic temperature impact, as well as during high-speed cyclic heating of the alloy surface by an electric arc (120 A, 45 V, 2 Hz, 10 000 arc interruption cycles). We investigated the evolution of alloy structures by means of electron microscopy, X-ray spectral microanalysis, X-ray phase, and differential thermal analysis. We show that the impact on the sample surface by the temperature field created by the electric arc leads to intense interaction of the carbides. Here, the matrix copper transforms periodically into a melt and plays the role of a transfer medium (the diffusion medium). As a result of such heat treatment, in the upper layers of the alloys, finely dispersed compositions of complex carbide phases occurred with the sizes ≤1–2 μm, i.e., 1–2 orders of magnitude less than that of the initial carbides.
- 1 May 2020
- Published by Allerton Press in Russian Journal of Non-Ferrous Metals
- Vol. 61 (3) , 319-324
Effect of Temperature on the Formation of Stable and Metastable Aluminide Phases in Al‒Zr‒Nb Alloys
The conditions of the formation of stable and metastable aluminides Aln(Zr1 – xNbx) formed during the crystallization of superheated melts
- 1 May 2020
- Published by Allerton Press in Russian Journal of Non-Ferrous Metals
- Vol. 61 (3) , 319-324
Effect of Temperature on the Formation of Stable and Metastable Aluminide Phases in Al‒Zr‒Nb Alloys
The conditions of the formation of stable and metastable aluminides Aln(Zr1 – xNbx) formed during the crystallization of superheated melts
- 1 March 2020
- Published by Pleiades Publishing Ltd in Inorganic Materials: Applied Research
- Vol. 11 (2) , 495-502
Synthesis of Arc-Resistant W70Cu30 Composite Alloy with Frameless Placing of Thin-Dispersed Tungsten Phase
Prototypes of high-current electrical contacts W70Cu30 with a frameless packing of dispersed W particles were obtained using precrystallization low-frequency vibration of the compositions “copper melt–uncompacted powder W.” Samples were tested for arc resistance in air in a laboratory device that simulates the operation of an AC contactor. Analysis of the structure (before and after 10 000 arc discharge times) and functional properties (transitional contact resistance and hardness) of the obtained alloys in comparison with industrial contacts W70D30-MP was carried out. It is shown that the difference in the structures of the initial alloys is in the nature of the distribution and size of inclusions of the tungsten phase. In the industrial alloy, tungsten forms a continuous framework of large monolithic formations oriented parallel to the working surface. Their thickness is in the range of 10–100 μm, and length reaches 500 μm. In the experimental alloy, the tungsten phase is represented by dispersed particles with size of 1–3 μm, separated by copper. After repeated arc discharges, these microparticles do not cure and do not form a continuous frame even in the uppermost working layers of the contacts. In the industrial alloy, under the action of the arc, both the dispersion of the framework into individual large particles of tungsten (up to 60 μm) and their subsequent merger occur simultaneously, which leads to an increase in the relief of the working surface. The values of transitional contact resistance up to 6000 arc discharge times in both alloys have similar extents. After that, there is a tendency to a more intense increase in transition resistance in the industrial alloy. Despite the fact that the hardness of the frameless alloy is lower than that of industrial alloy, its undoubted advantages are in dispersion and dimensional stability of inclusions of the hardening tungsten phase under the action of high temperatures (in the arc plasma).
- 1 March 2020
- Published by Pleiades Publishing Ltd in Inorganic Materials: Applied Research
- Vol. 11 (2) , 495-502
Synthesis of Arc-Resistant W70Cu30 Composite Alloy with Frameless Placing of Thin-Dispersed Tungsten Phase
Prototypes of high-current electrical contacts W70Cu30 with a frameless packing of dispersed W particles were obtained using precrystallization low-frequency vibration of the compositions “copper melt–uncompacted powder W.” Samples were tested for arc resistance in air in a laboratory device that simulates the operation of an AC contactor. Analysis of the structure (before and after 10 000 arc discharge times) and functional properties (transitional contact resistance and hardness) of the obtained alloys in comparison with industrial contacts W70D30-MP was carried out. It is shown that the difference in the structures of the initial alloys is in the nature of the distribution and size of inclusions of the tungsten phase. In the industrial alloy, tungsten forms a continuous framework of large monolithic formations oriented parallel to the working surface. Their thickness is in the range of 10–100 μm, and length reaches 500 μm. In the experimental alloy, the tungsten phase is represented by dispersed particles with size of 1–3 μm, separated by copper. After repeated arc discharges, these microparticles do not cure and do not form a continuous frame even in the uppermost working layers of the contacts. In the industrial alloy, under the action of the arc, both the dispersion of the framework into individual large particles of tungsten (up to 60 μm) and their subsequent merger occur simultaneously, which leads to an increase in the relief of the working surface. The values of transitional contact resistance up to 6000 arc discharge times in both alloys have similar extents. After that, there is a tendency to a more intense increase in transition resistance in the industrial alloy. Despite the fact that the hardness of the frameless alloy is lower than that of industrial alloy, its undoubted advantages are in dispersion and dimensional stability of inclusions of the hardening tungsten phase under the action of high temperatures (in the arc plasma).
- 30 November 2017
- Published by Ore and Metals Publishing House in Tsvetnye Metally
- p. 65-70
Meta-stable aluminides formation in Al – Hf – Ti alloys
The aim of our investigation is producing of the new master alloys based on Al – Hf – Ti system including meta-stable aluminides with the cubic lattice of L12 structure type identical to the aluminum matrix. The preparing of ligature alloys was carried out in the carbon resistance furnace. Melts overheated on about 100–400 degrees higher than liquidus were cast into a bronze mold. The crystallization speed was about 103 oC/s. High speed of crystallization of Al-transition metal melts leads to the appearing of internal tensions and then to the formation of primary metastable aluminides which are thermodynamically non-stable phases. Under the studied conditions we can observe different aluminide growth forms: cuboid, petal, cross-like and dendritic. The internal structure of primary crystals shows gradually increasing of titanium and hafnium concentration from the edge of aluminide crystal to its center. The Ti and Hf content in the formed Aln(HfхTi1–х) meta-stable aluminides is proportional to their content in alloys in spite of the partial solubility of addition metals in the α-Al dendritic cells. The 2.3 times increasing of hafnium content in alloy leads to the similar increasing of Hf fraction x in the aluminides (about 2.1 times, from 0.31 to 0.66). At the same time the lattice parameter mismatch between the aluminide lattice and aluminum matrix lattice significantly decreases. The master alloy with such nucleating phase will provide a greater effect of grain refinement. In the crystallization of superheated melts of the Al – Hf – Ti system, the degree of supersaturation of the aluminum solid solution by hafnium is almost twice as high as that for the binary Al – Hf system and with less overheating. This indicates the possibility of obtaining a larger volume fraction of secondary Al3(HfхTi1–х) aluminides upon doping the dispersively hardened aluminum alloys with small additives of Hf + Ti.
- 30 November 2017
- Published by Ore and Metals Publishing House in Tsvetnye Metally
- p. 65-70
Meta-stable aluminides formation in Al – Hf – Ti alloys
The aim of our investigation is producing of the new master alloys based on Al – Hf – Ti system including meta-stable aluminides with the cubic lattice of L12 structure type identical to the aluminum matrix. The preparing of ligature alloys was carried out in the carbon resistance furnace. Melts overheated on about 100–400 degrees higher than liquidus were cast into a bronze mold. The crystallization speed was about 103 oC/s. High speed of crystallization of Al-transition metal melts leads to the appearing of internal tensions and then to the formation of primary metastable aluminides which are thermodynamically non-stable phases. Under the studied conditions we can observe different aluminide growth forms: cuboid, petal, cross-like and dendritic. The internal structure of primary crystals shows gradually increasing of titanium and hafnium concentration from the edge of aluminide crystal to its center. The Ti and Hf content in the formed Aln(HfхTi1–х) meta-stable aluminides is proportional to their content in alloys in spite of the partial solubility of addition metals in the α-Al dendritic cells. The 2.3 times increasing of hafnium content in alloy leads to the similar increasing of Hf fraction x in the aluminides (about 2.1 times, from 0.31 to 0.66). At the same time the lattice parameter mismatch between the aluminide lattice and aluminum matrix lattice significantly decreases. The master alloy with such nucleating phase will provide a greater effect of grain refinement. In the crystallization of superheated melts of the Al – Hf – Ti system, the degree of supersaturation of the aluminum solid solution by hafnium is almost twice as high as that for the binary Al – Hf system and with less overheating. This indicates the possibility of obtaining a larger volume fraction of secondary Al3(HfхTi1–х) aluminides upon doping the dispersively hardened aluminum alloys with small additives of Hf + Ti.
- Open Access
- 4 November 2017
- Published by National University of Science and Technology MISiS in Izvestiya Vuzov. Tsvetnaya Metallurgiya (Proceedings of Higher Schools. Nonferrous Metallurgy)
- No. 5,p. 69-74
STRUCTURE PECULIARITIES OF AL–HF–SC MASTER ALLOYS
С использованием методов оптической и электронной сканирующей микроскопии, рентгеноспектрального микроанализа изучены особенности микроструктуры новых лигатурных сплавов системы Al–Hf–Sc с метастабильными алюминидами, имеющими кубическую решетку, идентичную решетке матрицы алюминиевых сплавов. Выплавку бинарных и тройных сплавов проводили в печи угольного сопротивления в графитовых тиглях в атмосфере аргона. Сплавы Al–0,96ат.%Hf (5,98 мас.% Hf) и Al–0,59ат.%Hf (3,77 мас.% Hf) готовили при перегреве над температурой ликвидуса около 200 и 400 град соответственно. Расплавы заливали в бронзовую изложницу, скорость кристаллизации в которой составляла ~103 град/с. Только в сплаве, перегретом над температурой ликвидуса на 400 град, наряду со стабильными алюминидами с тетрагональной решеткой образовались метастабильные алюминиды Al3Hf с кубической решеткой. Перегрев тройных расплавов, в которых сформировались метастабильные алюминиды Aln(Hf1–xScx), составил 240, 270 и 370 град. В зависимости от соотношения Hf и Sc в сплаве доля гафния в алюминидах Aln(Hf1–xScx) изменяется от 0,46 до 0,71. Лигатурные сплавы (ат.%) Al–0,26Hf–0,29Sc и Al–0,11Hf–0,25Sc (мас.%: Al–1,70Hf–0,47Sc и Al–0,75Hf–0,42Sc) характеризуются тонкой структурой зерна и метастабильными алюминидами состава Aln(Hf0,58Sc0,42) и Aln(Hf0,46Sc0,54) соответственно. Размеры алюминидов не превышают 12 и 7 мкм. Несоответствие их решеток с решеткой матрицы алюминиевых сплавов меньше, чем таковое для Al3Sc. Это позволяет предположить проявление опытными лигатурами Al–Hf–Sc высокого модифицирующего эффекта при их дальнейшем использовании. Кроме того, замещение гафнием дорогостоящего скандия в лигатурных сплавах может значительно сократить расход последнего.
- 4 November 2017
- Published by National University of Science and Technology MISiS in Izvestiya Vuzov. Tsvetnaya Metallurgiya (Proceedings of Higher Schools. Nonferrous Metallurgy)
- No. 5,p. 69-74
Open AccessSTRUCTURE PECULIARITIES OF AL–HF–SC MASTER ALLOYS
С использованием методов оптической и электронной сканирующей микроскопии, рентгеноспектрального микроанализа изучены особенности микроструктуры новых лигатурных сплавов системы Al–Hf–Sc с метастабильными алюминидами, имеющими кубическую решетку, идентичную решетке матрицы алюминиевых сплавов. Выплавку бинарных и тройных сплавов проводили в печи угольного сопротивления в графитовых тиглях в атмосфере аргона. Сплавы Al–0,96ат.%Hf (5,98 мас.% Hf) и Al–0,59ат.%Hf (3,77 мас.% Hf) готовили при перегреве над температурой ликвидуса около 200 и 400 град соответственно. Расплавы заливали в бронзовую изложницу, скорость кристаллизации в которой составляла ~103 град/с. Только в сплаве, перегретом над температурой ликвидуса на 400 град, наряду со стабильными алюминидами с тетрагональной решеткой образовались метастабильные алюминиды Al3Hf с кубической решеткой. Перегрев тройных расплавов, в которых сформировались метастабильные алюминиды Aln(Hf1–xScx), составил 240, 270 и 370 град. В зависимости от соотношения Hf и Sc в сплаве доля гафния в алюминидах Aln(Hf1–xScx) изменяется от 0,46 до 0,71. Лигатурные сплавы (ат.%) Al–0,26Hf–0,29Sc и Al–0,11Hf–0,25Sc (мас.%: Al–1,70Hf–0,47Sc и Al–0,75Hf–0,42Sc) характеризуются тонкой структурой зерна и метастабильными алюминидами состава Aln(Hf0,58Sc0,42) и Aln(Hf0,46Sc0,54) соответственно. Размеры алюминидов не превышают 12 и 7 мкм. Несоответствие их решеток с решеткой матрицы алюминиевых сплавов меньше, чем таковое для Al3Sc. Это позволяет предположить проявление опытными лигатурами Al–Hf–Sc высокого модифицирующего эффекта при их дальнейшем использовании. Кроме того, замещение гафнием дорогостоящего скандия в лигатурных сплавах может значительно сократить расход последнего.
- 1 November 2017
- Published by Allerton Press in Russian Journal of Non-Ferrous Metals
- Vol. 58 (6) , 639-643
Structural Features of Al–Hf–Sc Master Alloys
Microstructural features of new master alloys of the Al–Hf–Sc system with metastable aluminides with a cubic lattice identical to the lattice of a matrix of aluminum alloys are investigated using...
- 1 November 2017
- Published by Allerton Press in Russian Journal of Non-Ferrous Metals
- Vol. 58 (6) , 639-643
Structural Features of Al–Hf–Sc Master Alloys
Microstructural features of new master alloys of the Al–Hf–Sc system with metastable aluminides with a cubic lattice identical to the lattice of a matrix of aluminum alloys are investigated using...