Keiko Matsuda
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Research Subjects
Research Interests
Keiko Matsuda has a total of 12 co-authors. Here are the top co-authors by number of shared publications:
- Masanobu Yoshikawa
Toray Research Center Inc., 3-3-7 Sonoyama, Otsu, Shiga 520-8567, Japan
2 shared publications - Atsushi Masuda
Niigata University
1 shared publication - Hideki Sako
Toray Research Center, Inc., Otsu, Japan
1 shared publication Hirohumi Seki
Toray Research Center Inc., Sonoyama 3-3-7, Otsu, Shiga 520-8567, Japan (M.Y., H.S., K.I., K.M., Y.T., H.S.)
1 shared publicationKeiko Inoue
Toray Research Center Inc., Sonoyama 3-3-7, Otsu, Shiga 520-8567, Japan (M.Y., H.S., K.I., K.M., Y.T., H.S.)
1 shared publication- Koichi Sakaguchi
Pacific Northwest National Laboratory (Richland, United States of America)
1 shared publication
Latest Publications
- 1 October 2012
- Published by IOP Publishing in Japanese Journal of Applied Physics
- Vol. 51 (10S) , 10NF07
Microscopic Degradation Mechanisms in Silicon Photovoltaic Module under Long-Term Environmental Exposure
We used several analytical methods to identify the mechanism underlying the performance degradation in a photovoltaic (PV) module subjected to long-term (10 years) field exposure. Cloudy visual defects in this module were caused by delamination between the poly(ethylene vinyl acetate) (EVA) and antireflection coating films on the Si substrate. The delamination was considered to be caused by the formation of a segregation layer and oxidative degradation of EVA. Furthermore, it was found that sodium ions diffused from the superstrate glass into the EVA film and Si cell. We confirm that diffusion of sodium ions caused the degradation of Si cells and the superstrate glass of this module.
- 1 October 2012
- Published by IOP Publishing in Japanese Journal of Applied Physics
- Vol. 51 (10S) , 10NF07
Microscopic Degradation Mechanisms in Silicon Photovoltaic Module under Long-Term Environmental Exposure
We used several analytical methods to identify the mechanism underlying the performance degradation in a photovoltaic (PV) module subjected to long-term (10 years) field exposure. Cloudy visual defects in this module were caused by delamination between the poly(ethylene vinyl acetate) (EVA) and antireflection coating films on the Si substrate. The delamination was considered to be caused by the formation of a segregation layer and oxidative degradation of EVA. Furthermore, it was found that sodium ions diffused from the superstrate glass into the EVA film and Si cell. We confirm that diffusion of sodium ions caused the degradation of Si cells and the superstrate glass of this module.
- 1 May 2011
- Published by SAGE Publications in Applied Spectroscopy
- Vol. 65 (5) , 543-548
Characterization of Silicon Dioxide Films on a 4H-SiC Si(0001) Face by Fourier Transform Infrared (FT-IR) Spectroscopy and Cathodoluminescence Spectroscopy
We used Fourier transform infrared (FT-IR) spectroscopy to characterize silicon dioxide (SiO(2)) films on a 4H-SiC(0001) Si face. We found that the peak frequency of the transverse optical (TO) phonon in SiO(2) films grown on a 4H-SiC substrate agrees well with that in SiO(2) films grown on a Si substrate, whereas the peak frequency of the longitudinal optical (LO) phonon in SiO(2) films on a 4H-SiC substrate is red-shifted by approximately 50 cm(-1) relative to that in SiO(2) films on a Si substrate. We concluded that this red-shift of the LO phonon is mainly caused by a change in inhomogeneity due to a decrease in density in the SiO(2) films. Furthermore, cathodoluminescence (CL) spectroscopy results indicated that the channel mobility of the SiC metal-oxide-semiconductor field-effect transistor (MOSFET) decreases roughly in proportion to the increase in the intensity of the CL peak at 460 and 490 nm, which is attributed to the increase in the number of oxygen vacancy centers (OVCs). FT-IR and CL spectroscopies provide us with a large amount of data on OVCs in the SiO(2) films on a 4H-SiC substrate.
- 1 May 2011
- Published by SAGE Publications in Applied Spectroscopy
- Vol. 65 (5) , 543-548
Characterization of Silicon Dioxide Films on a 4H-SiC Si(0001) Face by Fourier Transform Infrared (FT-IR) Spectroscopy and Cathodoluminescence Spectroscopy
We used Fourier transform infrared (FT-IR) spectroscopy to characterize silicon dioxide (SiO(2)) films on a 4H-SiC(0001) Si face. We found that the peak frequency of the transverse optical (TO) phonon in SiO(2) films grown on a 4H-SiC substrate agrees well with that in SiO(2) films grown on a Si substrate, whereas the peak frequency of the longitudinal optical (LO) phonon in SiO(2) films on a 4H-SiC substrate is red-shifted by approximately 50 cm(-1) relative to that in SiO(2) films on a Si substrate. We concluded that this red-shift of the LO phonon is mainly caused by a change in inhomogeneity due to a decrease in density in the SiO(2) films. Furthermore, cathodoluminescence (CL) spectroscopy results indicated that the channel mobility of the SiC metal-oxide-semiconductor field-effect transistor (MOSFET) decreases roughly in proportion to the increase in the intensity of the CL peak at 460 and 490 nm, which is attributed to the increase in the number of oxygen vacancy centers (OVCs). FT-IR and CL spectroscopies provide us with a large amount of data on OVCs in the SiO(2) films on a 4H-SiC substrate.