Yuri Yurievich Kaplanskii
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Previous Organizations / Institutes
The organizations / institutes from the scholar's other articles in the past ten years
Research Subjects
Yuri Yurievich Kaplanskii has a total of 52 co-authors. Here are the top co-authors by number of shared publications:
E.A. Levashov
6 shared publications- Alexander A. Zaitsev
National University of Science and Technology “MISIS
5 shared publications - Evgeny Alexandrovich Levashov
National University of Science and Technology “MISIS
5 shared publications P.A. Loginov
5 shared publications- Yury S. Pogozhev
National University of Science and Technology “MISiS”, Moscow, Russia
4 shared publications Zh.A. Sentyurina
4 shared publications
Latest Publications
- Open Access
- 6 June 2023
- Published by National University of Science and Technology MISiS in Izvestiya. Ferrous Metallurgy
- Vol. 66 (2) , 184-190
Influence of laser spot size on structure and properties of high-temperature CompoNIAL-M5-3 alloy produced by selective laser melting
The CompoNiAl-M5-3 high-temperature alloy based on nickel monoaluminide was obtained by selective laser melting (SLM) of a spheroidized powder with particle size in the range of 20 – 45 μm. The powder was manufactured using an integral technology including self-propagating high-temperature synthesis (SHS), briquette grinding, sieve and air classification followed with spheroidization of powder particles in a thermal plasma flow and ultrasonic purification of spheroidized particles from nanofraction. Using parametric studies, the SLM modes were tested on SLM 280H and TruPrint 1000 machines. Mechanical tests of the samples were carried out using the uniaxial compression scheme with the strain rate dε/dt = 10–4 s–1 in the temperature range 1023 – 1273 K. Scanning and transmission electron microscopy methods were used to study the influence of laser spot size on the evolution of microstructure and thermomechanical properties of the SLM-consolidated material in comparison with that obtained by hot isostatic pressing (HIP). The authors established the effect of HIP + HT (aging in vacuum) post-treatment on the structure and mechanical properties of the material. The yield strength at 1073 K of the alloy built on the additive machine with a laser spot diameter of 38 μm after SLM + HIP + HT was 500 MPa, which exceeded the yield strength of the HIP-samples by 220 MPa.
- 6 June 2023
- Published by National University of Science and Technology MISiS in Izvestiya. Ferrous Metallurgy
- Vol. 66 (2) , 184-190
Open AccessInfluence of laser spot size on structure and properties of high-temperature CompoNIAL-M5-3 alloy produced by selective laser melting
The CompoNiAl-M5-3 high-temperature alloy based on nickel monoaluminide was obtained by selective laser melting (SLM) of a spheroidized powder with particle size in the range of 20 – 45 μm. The powder was manufactured using an integral technology including self-propagating high-temperature synthesis (SHS), briquette grinding, sieve and air classification followed with spheroidization of powder particles in a thermal plasma flow and ultrasonic purification of spheroidized particles from nanofraction. Using parametric studies, the SLM modes were tested on SLM 280H and TruPrint 1000 machines. Mechanical tests of the samples were carried out using the uniaxial compression scheme with the strain rate dε/dt = 10–4 s–1 in the temperature range 1023 – 1273 K. Scanning and transmission electron microscopy methods were used to study the influence of laser spot size on the evolution of microstructure and thermomechanical properties of the SLM-consolidated material in comparison with that obtained by hot isostatic pressing (HIP). The authors established the effect of HIP + HT (aging in vacuum) post-treatment on the structure and mechanical properties of the material. The yield strength at 1073 K of the alloy built on the additive machine with a laser spot diameter of 38 μm after SLM + HIP + HT was 500 MPa, which exceeded the yield strength of the HIP-samples by 220 MPa.
- Open Access
Structure Formation and Tribological Properties of Mo-Si-B-Hf Electrospark Coatings Based on Mo2Ni3Si Laves Phase
Coatings were produced on the EP741NP nickel alloy substrates by electrospark deposition (ESD) in argon using an MoSi2-MoB-HfB2 electrode. In situ high-resolution transmission electron microscopy and X-ray diffraction analysis studies have identified the temperature above which the strengthening Mo2Ni3Si Laves phase is formed in the coatings. At 25 °C, the coatings with a predominant content of the Laves phase are characterized by enhanced wear resistance, as well as a lower coefficient of friction compared to the non-annealed coatings containing binary silicides. At 700 °C, the EP741NP substrate was characterized by the lowest friction coefficient (Ktr = 0.35), and its wear was approximately at the same level as the wear of both coatings.
Open AccessStructure Formation and Tribological Properties of Mo-Si-B-Hf Electrospark Coatings Based on Mo2Ni3Si Laves Phase
Coatings were produced on the EP741NP nickel alloy substrates by electrospark deposition (ESD) in argon using an MoSi2-MoB-HfB2 electrode. In situ high-resolution transmission electron microscopy and X-ray diffraction analysis studies have identified the temperature above which the strengthening Mo2Ni3Si Laves phase is formed in the coatings. At 25 °C, the coatings with a predominant content of the Laves phase are characterized by enhanced wear resistance, as well as a lower coefficient of friction compared to the non-annealed coatings containing binary silicides. At 700 °C, the EP741NP substrate was characterized by the lowest friction coefficient (Ktr = 0.35), and its wear was approximately at the same level as the wear of both coatings.
- Open Access
- 29 January 2022
- Published by Southwest State University in Proceedings of the Southwest State University
- Vol. 25 (3) , 8-26
Investigation of Molding Process and Consolidation of Preforms from Mechanically Synthesized Powders of Europium and Cerium Hafnates
Purpose of research. To study the process of molding and consolidation of preforms from mechanically synthesized powders of europium and cerium hafnates.Methods. Complex compounds of europium hafnateEu2HfO5 and cerium hafnate Ce2HfO5 have been synthesized from europium, hafnate and cerium oxides using mechanochemical synthesis in a planetary centrifugal mill. The rotational speed of the disk was 600 - 900 rpm and the rotational speed of the drums is 1000 - 1800 rpm, with the ratio of grinding bodies to the mass of the powder charge (35 - 45): 1, in an argon atmosphere. Synthesis lasts 5 - 120 minutes.Results. An X-ray phase analysis has been performed showing the formation of Eu2HfO5 and Ce2HfO5; as well as the study of the morphology of particles of the obtained powders, their technological properties, granulometric composition, formability and compaction, as well as the process of their consolidation.Conclusion. On the basis of the experimental studies aimed at studying the molding process and consolidation of preforms from mechanically synthesized powders of europium and cerium hafnates, it has been revealed the optimal mode of synthesis of cerium and europium hafnates. We have obtained a cerium hafnate powder with a particle size of 30-100 nm and a europium hafnate powder with a particle size of 40-70 nm by the method of mechanical activation. Using X-ray phase analysis, TEM and SEM methods, the mixed structure of lanthanide hafnates powders obtained by mechanosynthesis have been studied. The technological properties of mechanically synthesized powders of cerium and europium hafnate, as well as, their compaction and formability after pressing and sintering have been determined and studied. Samples from europium hafnate powder have a relative density higher than samples from cerium hafnate powder after consolidation at temperatures of 900-1200 ° C and isothermal holding time from 30 to 120 min. A study of the microhardness of lanthanide hafnate samples after sintering has shown that europium hafnate samples have greater hardness than cerium hafnate samples .
- 29 January 2022
- Published by Southwest State University in Proceedings of the Southwest State University
- Vol. 25 (3) , 8-26
Open AccessInvestigation of Molding Process and Consolidation of Preforms from Mechanically Synthesized Powders of Europium and Cerium Hafnates
Purpose of research. To study the process of molding and consolidation of preforms from mechanically synthesized powders of europium and cerium hafnates.Methods. Complex compounds of europium hafnateEu2HfO5 and cerium hafnate Ce2HfO5 have been synthesized from europium, hafnate and cerium oxides using mechanochemical synthesis in a planetary centrifugal mill. The rotational speed of the disk was 600 - 900 rpm and the rotational speed of the drums is 1000 - 1800 rpm, with the ratio of grinding bodies to the mass of the powder charge (35 - 45): 1, in an argon atmosphere. Synthesis lasts 5 - 120 minutes.Results. An X-ray phase analysis has been performed showing the formation of Eu2HfO5 and Ce2HfO5; as well as the study of the morphology of particles of the obtained powders, their technological properties, granulometric composition, formability and compaction, as well as the process of their consolidation.Conclusion. On the basis of the experimental studies aimed at studying the molding process and consolidation of preforms from mechanically synthesized powders of europium and cerium hafnates, it has been revealed the optimal mode of synthesis of cerium and europium hafnates. We have obtained a cerium hafnate powder with a particle size of 30-100 nm and a europium hafnate powder with a particle size of 40-70 nm by the method of mechanical activation. Using X-ray phase analysis, TEM and SEM methods, the mixed structure of lanthanide hafnates powders obtained by mechanosynthesis have been studied. The technological properties of mechanically synthesized powders of cerium and europium hafnate, as well as, their compaction and formability after pressing and sintering have been determined and studied. Samples from europium hafnate powder have a relative density higher than samples from cerium hafnate powder after consolidation at temperatures of 900-1200 ° C and isothermal holding time from 30 to 120 min. A study of the microhardness of lanthanide hafnate samples after sintering has shown that europium hafnate samples have greater hardness than cerium hafnate samples .
- 1 November 2021
- Published by Allerton Press in Russian Journal of Non-Ferrous Metals
- Vol. 62 (6) , 740-755
Influence of Molybdenum and Rhenium Dopants on the Structure and Properties of NiAl–Cr–Co Cast Alloy
Centrifugal SHS casting has been used for the production of NiAl–Cr–Co–X alloys, where X = 2.5–15.0 wt % Mo and up to 1.5 wt % Re.
- 1 November 2021
- Published by Allerton Press in Russian Journal of Non-Ferrous Metals
- Vol. 62 (6) , 740-755
Influence of Molybdenum and Rhenium Dopants on the Structure and Properties of NiAl–Cr–Co Cast Alloy
Centrifugal SHS casting has been used for the production of NiAl–Cr–Co–X alloys, where X = 2.5–15.0 wt % Mo and up to 1.5 wt % Re.
- Open Access
Structure, Corrosion Resistance, Mechanical and Tribological Properties of ZrB2 and Zr-B-N Coatings
The coatings ZrB2 and Zr-B-N were deposited by magnetron sputtering of ZrB2 target in Ar and Ar–15%N2 atmospheres. The structure and properties of the coatings were investigated via scanning and transmission electron microscopy, energy dispersion analysis, optical profilometry, glowing discharge optical emission spectroscopy and X-ray diffraction analysis. Mechanical and tribological properties of the coatings were investigated using nanoindentation, “pin-on-disc” tribological testing and “ball-on-plate” impact testing. Free corrosion potential and corrosion current density were measured by electrochemical testing in 1 N H2SO4 and 3.5%NaCl solutions. The oxidation resistance of the coatings was investigated in the 600–800 °C temperature interval. The coatings deposited in Ar contained 4–11 nm grains of the h-ZrB2 phase along with free boron. Nitrogen-containing coatings consisted of finer crystals (1–4 nm) of h-ZrB2, separated by interlayers of amorphous a-BN. Both types of coatings featured hardness of 22–23 GPa; however, the introduction of nitrogen decreased the coating’s elastic modulus from 342 to 266 GPa and increased the elastic recovery from 62 to 72%, which enhanced the wear resistance of the coatings. N-doped coatings demonstrated a relatively low friction coefficient of 0.4 and a specific wear rate of ~1.3 × 10−6 mm3N−1m−1. Electrochemical investigations revealed that the introduction of nitrogen into the coatings resulted in the decrease of corrosion current density in 3.5% NaCl and 1 N H2SO4 solution up to 3.5 and 5 times, correspondingly. The superior corrosion resistance of Zr-B-N coatings was related to the finer grains size and increased volume of the BN phase. The samples ZrB2 and Zr-B-N resisted oxidation at 600 °C. N-free coatings resisted oxidation (up to 800 °C) and the diffusion of metallic elements from the substrate better. In contrast, Zr-B-N coatings experienced total oxidation and formed loose oxide layers, which could be easily removed from the substrate.
Open AccessStructure, Corrosion Resistance, Mechanical and Tribological Properties of ZrB2 and Zr-B-N Coatings
The coatings ZrB2 and Zr-B-N were deposited by magnetron sputtering of ZrB2 target in Ar and Ar–15%N2 atmospheres. The structure and properties of the coatings were investigated via scanning and transmission electron microscopy, energy dispersion analysis, optical profilometry, glowing discharge optical emission spectroscopy and X-ray diffraction analysis. Mechanical and tribological properties of the coatings were investigated using nanoindentation, “pin-on-disc” tribological testing and “ball-on-plate” impact testing. Free corrosion potential and corrosion current density were measured by electrochemical testing in 1 N H2SO4 and 3.5%NaCl solutions. The oxidation resistance of the coatings was investigated in the 600–800 °C temperature interval. The coatings deposited in Ar contained 4–11 nm grains of the h-ZrB2 phase along with free boron. Nitrogen-containing coatings consisted of finer crystals (1–4 nm) of h-ZrB2, separated by interlayers of amorphous a-BN. Both types of coatings featured hardness of 22–23 GPa; however, the introduction of nitrogen decreased the coating’s elastic modulus from 342 to 266 GPa and increased the elastic recovery from 62 to 72%, which enhanced the wear resistance of the coatings. N-doped coatings demonstrated a relatively low friction coefficient of 0.4 and a specific wear rate of ~1.3 × 10−6 mm3N−1m−1. Electrochemical investigations revealed that the introduction of nitrogen into the coatings resulted in the decrease of corrosion current density in 3.5% NaCl and 1 N H2SO4 solution up to 3.5 and 5 times, correspondingly. The superior corrosion resistance of Zr-B-N coatings was related to the finer grains size and increased volume of the BN phase. The samples ZrB2 and Zr-B-N resisted oxidation at 600 °C. N-free coatings resisted oxidation (up to 800 °C) and the diffusion of metallic elements from the substrate better. In contrast, Zr-B-N coatings experienced total oxidation and formed loose oxide layers, which could be easily removed from the substrate.
- 1 January 2019
- Published by Elsevier in Materials Science and Engineering: A
- Vol. 743, 567-580
Microstructure and mechanical properties of the (Fe,Ni)Al-based alloy produced by SLM and HIP of spherical composite powder
- 1 January 2019
- Published by Elsevier in Materials Science and Engineering: A
- Vol. 743, 567-580
Microstructure and mechanical properties of the (Fe,Ni)Al-based alloy produced by SLM and HIP of spherical composite powder
- 1 December 2018
- Published by Pleiades Publishing Ltd in Doklady Chemistry
- Vol. 483 (2) , 312-317
Plasma Spheroidization of Micropowders of a Heat-Resistant Alloy Based on Nickel Monoaluminide
Spheroidization of micropowders of a heat-resistant alloy based on nickel aluminide with a particle size of 20 to 45 μm was studied. The alloy was produced by calcium hydride reduction (CHR)...
- 1 December 2018
- Published by Pleiades Publishing Ltd in Doklady Chemistry
- Vol. 483 (2) , 312-317
Plasma Spheroidization of Micropowders of a Heat-Resistant Alloy Based on Nickel Monoaluminide
Spheroidization of micropowders of a heat-resistant alloy based on nickel aluminide with a particle size of 20 to 45 μm was studied. The alloy was produced by calcium hydride reduction (CHR)...
- 1 October 2018
- Published by Allerton Press in International Journal of Self-Propagating High-Temperature Synthesis
- Vol. 27 (4) , 236-244
Fabrication of Narrow-Fraction Micropowders of NiAl-Based Refractory Alloy CompoNiAl-M5-3
Powders of new CompoNiAl M5-3 heat-resistant alloy were prepared by mechanoactivated SHS from (Ni–Al–Cr–Co–Hf)–NaCl mixtures. Ni dissolution in Al melt was found to be the motive force of combustion....
- 1 October 2018
- Published by Allerton Press in International Journal of Self-Propagating High-Temperature Synthesis
- Vol. 27 (4) , 236-244
Fabrication of Narrow-Fraction Micropowders of NiAl-Based Refractory Alloy CompoNiAl-M5-3
Powders of new CompoNiAl M5-3 heat-resistant alloy were prepared by mechanoactivated SHS from (Ni–Al–Cr–Co–Hf)–NaCl mixtures. Ni dissolution in Al melt was found to be the motive force of combustion....