Tobias Weingärtner
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Research Subjects
Tobias Weingärtner has a total of 81 co-authors. Here are the top co-authors by number of shared publications:
Andreas Hoffmann
3 shared publicationsJan Hoffmann
3 shared publications- Michael Rieth
Institute for Applied Materials, Karlsruhe Institute of Technology, 76344 Karlsruhe, Germany
3 shared publications Anton Möslang
2 shared publications- Bernd Gludovatz
School of Mechanical and Manufacturing Engineering, UNSW Sydney, Sydney, Australia
2 shared publications Henri Greuner
2 shared publications
Latest Publications
- Open Access
- 31 January 2026
- Published by Springer Nature in Nature Communications
- Vol. 17 (1)
Printed origami thermoelectric generator achieves > 20 Wm−² from low-grade heat via material and process design
Printing facilitates low-cost thermoelectric generators to power battery-free internet-of-things devices, wearables, and Industry 4.0 systems. However, scaling up requires printable thermoelectric materials with good mechanical properties and high performance. Here, we report a high-performance Ag 2 (Se 1- x S x ) 1.05 -based n-type printed thermoelectric film through a combination of engineering non-stoichiometric defects and sulfur substitution. An optimal sulfur substitution of 2 at. % facilitates an excellent flexibility and a power factor of~16 µWcm −1 K −2 at 360 K, a 65 % increase compared to a pristine Ag 2 Se film. A fully printed origami-thermoelectric generator produces a maximum power output $${P}_{\max }$$ of 907 µW at a temperature difference of 80 K. A record-high power density p d of 21 W m −2 (corresponding to 800 µW g −1 as a weight-normalized power density) is achieved, twice that of previously reported origami-thermoelectric generators. These results highlight cost-effective manufacturing of thermoelectric generators with the capability to power next-generation autonomous electronic devices.- 31 January 2026
- Published by Springer Nature in Nature Communications
- Vol. 17 (1)
Open AccessPrinted origami thermoelectric generator achieves > 20 Wm−² from low-grade heat via material and process design
Printing facilitates low-cost thermoelectric generators to power battery-free internet-of-things devices, wearables, and Industry 4.0 systems. However, scaling up requires printable thermoelectric materials with good mechanical properties and high performance. Here, we report a high-performance Ag 2 (Se 1- x S x ) 1.05 -based n-type printed thermoelectric film through a combination of engineering non-stoichiometric defects and sulfur substitution. An optimal sulfur substitution of 2 at. % facilitates an excellent flexibility and a power factor of~16 µWcm −1 K −2 at 360 K, a 65 % increase compared to a pristine Ag 2 Se film. A fully printed origami-thermoelectric generator produces a maximum power output $${P}_{\max }$$ of 907 µW at a temperature difference of 80 K. A record-high power density p d of 21 W m −2 (corresponding to 800 µW g −1 as a weight-normalized power density) is achieved, twice that of previously reported origami-thermoelectric generators. These results highlight cost-effective manufacturing of thermoelectric generators with the capability to power next-generation autonomous electronic devices. - 18 September 2019
- Published by Institute of Electrical and Electronics Engineers (IEEE) in IEEE Journal of Photovoltaics
- Vol. 9 (6) , 1532-1540
Microcharacterization of Interface Oxide Layer on Laser-Structured Silicon Surfaces of Plated Ni–Cu Solar Cells
Light-induced plating on laser-structured passivation layer openings is an alternative method to silver screen printing for fabrication of the front-side metal grid on silicon solar cells. Fundamental contact properties, such as adhesion and contact resistance, are determined at the highly inhomogeneous interface of laser-structured silicon and plated nickel. Usage of laser structuring and plating holds the risk that an interfacial oxide layer is incorporated to the contact stack. It is shown within this article that both native and laser-induced oxide formation influence contact properties. Although, a native oxide layer does not impede metal deposition during plating, the dynamics of the layer formation is shown to be changed. It is known that interface oxides harm the contact resistance, and it is reported that postplating annealing decreases the contact resistance. In this article, the microstructural basis of the temperature-induced changes is examined. By transmission electron microscopy and energy dispersive X-ray spectroscopy, no temperature-induced modification of the interface microstructure, such as silicide formation or metal-induced crystallization of the amorphous surface, is observed. Results suggest that the decrease is attributed to a temperature-induced change of the electrical properties of the interface oxide. Considering reports that partially closed interface oxide layers are an inherent feature of laser-structured plated contacts, the results presented motivate reconsidering the objective of postplating annealing. The results indicate that the beneficial impact of silicide formation is overrated for the case of laser-structured plated contacts, whereas the temperature-induced modifications on residual interface oxide layers are neglected in the scientific discussions on the given contact stack.
- 18 September 2019
- Published by Institute of Electrical and Electronics Engineers (IEEE) in IEEE Journal of Photovoltaics
- Vol. 9 (6) , 1532-1540
Microcharacterization of Interface Oxide Layer on Laser-Structured Silicon Surfaces of Plated Ni–Cu Solar Cells
Light-induced plating on laser-structured passivation layer openings is an alternative method to silver screen printing for fabrication of the front-side metal grid on silicon solar cells. Fundamental contact properties, such as adhesion and contact resistance, are determined at the highly inhomogeneous interface of laser-structured silicon and plated nickel. Usage of laser structuring and plating holds the risk that an interfacial oxide layer is incorporated to the contact stack. It is shown within this article that both native and laser-induced oxide formation influence contact properties. Although, a native oxide layer does not impede metal deposition during plating, the dynamics of the layer formation is shown to be changed. It is known that interface oxides harm the contact resistance, and it is reported that postplating annealing decreases the contact resistance. In this article, the microstructural basis of the temperature-induced changes is examined. By transmission electron microscopy and energy dispersive X-ray spectroscopy, no temperature-induced modification of the interface microstructure, such as silicide formation or metal-induced crystallization of the amorphous surface, is observed. Results suggest that the decrease is attributed to a temperature-induced change of the electrical properties of the interface oxide. Considering reports that partially closed interface oxide layers are an inherent feature of laser-structured plated contacts, the results presented motivate reconsidering the objective of postplating annealing. The results indicate that the beneficial impact of silicide formation is overrated for the case of laser-structured plated contacts, whereas the temperature-induced modifications on residual interface oxide layers are neglected in the scientific discussions on the given contact stack.
- Open Access
- 1 December 2017
- Published by Elsevier in International Journal of Refractory Metals and Hard Materials
- Vol. 69, 66-109
Ductilisation of tungsten (W): Tungsten laminated composites
- 1 December 2017
- Published by Elsevier in International Journal of Refractory Metals and Hard Materials
- Vol. 69, 66-109
Open AccessDuctilisation of tungsten (W): Tungsten laminated composites
- 1 July 2015
- Published by Elsevier in International Journal of Refractory Metals and Hard Materials
- Vol. 51, 264-274
Tungsten laminates made of ultrafine-grained (UFG) tungsten foil — Ageing of tungsten–titanium (W–Ti) laminates
- 1 July 2015
- Published by Elsevier in International Journal of Refractory Metals and Hard Materials
- Vol. 51, 264-274
Tungsten laminates made of ultrafine-grained (UFG) tungsten foil — Ageing of tungsten–titanium (W–Ti) laminates
- 7 July 2014
- Published by Wiley in Advanced Engineering Materials
- Vol. 17 (4) , 491-501
Tungsten (W) Laminate Pipes for Innovative High Temperature Energy Conversion Systems
The aim of this paper is to present the mechanical properties of tungsten laminate pipes made of tungsten foil and to discuss their use in innovative high temperature energy conversion systems. Tungsten is the metal with the highest melting point of all metals and would therefore be an excellent fit for high temperature applications. But tungsten has one major drawback which is its low fracture toughness at room temperature (RT) or its high brittle‐to‐ductile transition temperature (BDTT). However, one of the extraordinary properties of tungsten is that by cold working the BDTT can be shifted to lower temperatures. At the extreme, these results in a tungsten foil with a BDTT below −120 °C combined with an RT fracture toughness of 70 MPa m1/2. By rolling up and joining a tungsten foil, tungsten laminate pipes can be synthesized that can dissipate at least 20 J in a Charpy impact test at RT and survive a burst test at RT at 1000 bar without any residual damage. The technical maturity of these W laminate pipes is approved by high heat flux tests performed at the Plataforma Solar de Almería, Spain, as well as at the Max Planck Institute of Plasma Physics, Garching, Germany.
- 7 July 2014
- Published by Wiley in Advanced Engineering Materials
- Vol. 17 (4) , 491-501
Tungsten (W) Laminate Pipes for Innovative High Temperature Energy Conversion Systems
The aim of this paper is to present the mechanical properties of tungsten laminate pipes made of tungsten foil and to discuss their use in innovative high temperature energy conversion systems. Tungsten is the metal with the highest melting point of all metals and would therefore be an excellent fit for high temperature applications. But tungsten has one major drawback which is its low fracture toughness at room temperature (RT) or its high brittle‐to‐ductile transition temperature (BDTT). However, one of the extraordinary properties of tungsten is that by cold working the BDTT can be shifted to lower temperatures. At the extreme, these results in a tungsten foil with a BDTT below −120 °C combined with an RT fracture toughness of 70 MPa m1/2. By rolling up and joining a tungsten foil, tungsten laminate pipes can be synthesized that can dissipate at least 20 J in a Charpy impact test at RT and survive a burst test at RT at 1000 bar without any residual damage. The technical maturity of these W laminate pipes is approved by high heat flux tests performed at the Plataforma Solar de Almería, Spain, as well as at the Max Planck Institute of Plasma Physics, Garching, Germany.
- 18 June 2013
- Published by Oxford University Press (OUP) in Microscopy and Microanalysis
- Vol. 19 (5) , 1308-1316
Phases in the Al-Corner of the Al–Mn–Be System
This work studied the phases in the Al corner of the Al–Mn–Be phase diagram in the as-cast state and heat-treated conditions. Metallographic investigations, X-ray diffraction, scanning electron microscopy, and energy-dispersive spectroscopy were used for identifying the phases. The Be contents in the identified phases were precisely determined using Auger electron spectroscopy. The results indicated that Al6Mn does not dissolve Be, whilst λ-Al4Mn dissolves up to 7 at.% Be. The average composition of the T phase, which is normally designated as Al15Mn3Be2, was 72 at.% Al, 19 at.% Mn, and 9 at.% Be. The phase with the nominal composition Be4AlMn contained more Al than Mn. The atomic ratio Al:Mn was between 1.3:1 and 2:1. The hexagonal Be-rich phase did not dissolve any Al and Mn. The icosahedral quasicrystalline (IQC) phase contained up to 45 at.% Be. The compositions of T phase, λ–Al4Mn, IQC, and Be4AlMn may vary, however, the ratio (Al + Be):Mn remained constant, and was close either to four or six indicating substitution of Al atoms with Be atoms in these phases.
- 18 June 2013
- Published by Oxford University Press (OUP) in Microscopy and Microanalysis
- Vol. 19 (5) , 1308-1316
Phases in the Al-Corner of the Al–Mn–Be System
This work studied the phases in the Al corner of the Al–Mn–Be phase diagram in the as-cast state and heat-treated conditions. Metallographic investigations, X-ray diffraction, scanning electron microscopy, and energy-dispersive spectroscopy were used for identifying the phases. The Be contents in the identified phases were precisely determined using Auger electron spectroscopy. The results indicated that Al6Mn does not dissolve Be, whilst λ-Al4Mn dissolves up to 7 at.% Be. The average composition of the T phase, which is normally designated as Al15Mn3Be2, was 72 at.% Al, 19 at.% Mn, and 9 at.% Be. The phase with the nominal composition Be4AlMn contained more Al than Mn. The atomic ratio Al:Mn was between 1.3:1 and 2:1. The hexagonal Be-rich phase did not dissolve any Al and Mn. The icosahedral quasicrystalline (IQC) phase contained up to 45 at.% Be. The compositions of T phase, λ–Al4Mn, IQC, and Be4AlMn may vary, however, the ratio (Al + Be):Mn remained constant, and was close either to four or six indicating substitution of Al atoms with Be atoms in these phases.
- 9 August 2012
- Published by American Chemical Society (ACS) in Langmuir
- Vol. 28 (33) , 12060-12066
Interface of Nanoparticle-Coated Electropolished Stents
Nanostructures entail a high potential for improving implant surfaces, for instance, in stent applications. The electrophoretic deposition of laser-generated colloidal nanoparticles is an appropriate tool for creating large-area nanostructures on surfaces. Until now, the bonding and characteristics of the interface between deposited nanoparticles and the substrate surface has not been known. It is investigated using X-ray photoelectron spectroscopy, Auger electron spectroscopy, and transmission electron microscopy to characterize an electropolished NiTi stent surface coated by laser-generated Au and Ti nanoparticles. The deposition of elemental Au and Ti nanoparticles is observed on the total 3D surface. Ti-coated samples are composed of Ti oxide and Ti carbide because of nanoparticle fabrication and the coating process carried out in 2-propanol. The interface between nanoparticles and the electropolished surface consists of a smooth, monotone elemental depth profile. The interface depth is higher for the Ti nanoparticle coating than for the Au nanoparticle coating. This smooth depth gradient of Ti across the coating–substrate intersection and the thicker interface layer indicate the hard bonding of Ti-based nanoparticles on the surface. Accordingly, electron microscopy reveals nanoparticles adsorbed on the surface without any sorption-blocking intermediate layer. The physicomechanical stability of the bond may benefit from such smooth depth gradients and direct, ligand-free contact. This would potentially increase the coating stability during stent application.
- 9 August 2012
- Published by American Chemical Society (ACS) in Langmuir
- Vol. 28 (33) , 12060-12066
Interface of Nanoparticle-Coated Electropolished Stents
Nanostructures entail a high potential for improving implant surfaces, for instance, in stent applications. The electrophoretic deposition of laser-generated colloidal nanoparticles is an appropriate tool for creating large-area nanostructures on surfaces. Until now, the bonding and characteristics of the interface between deposited nanoparticles and the substrate surface has not been known. It is investigated using X-ray photoelectron spectroscopy, Auger electron spectroscopy, and transmission electron microscopy to characterize an electropolished NiTi stent surface coated by laser-generated Au and Ti nanoparticles. The deposition of elemental Au and Ti nanoparticles is observed on the total 3D surface. Ti-coated samples are composed of Ti oxide and Ti carbide because of nanoparticle fabrication and the coating process carried out in 2-propanol. The interface between nanoparticles and the electropolished surface consists of a smooth, monotone elemental depth profile. The interface depth is higher for the Ti nanoparticle coating than for the Au nanoparticle coating. This smooth depth gradient of Ti across the coating–substrate intersection and the thicker interface layer indicate the hard bonding of Ti-based nanoparticles on the surface. Accordingly, electron microscopy reveals nanoparticles adsorbed on the surface without any sorption-blocking intermediate layer. The physicomechanical stability of the bond may benefit from such smooth depth gradients and direct, ligand-free contact. This would potentially increase the coating stability during stent application.
- 1 August 2012
- Published by Taylor & Francis in Fusion Science and Technology
- Vol. 62 (1) , 110-115
Two-Component Tungsten Powder Injection Molding for Mass Production of He-Cooled DEMO Divertor Parts
Fusion technology as a possible and promising alternative energy source for the future is intensively investigated at Karlsruhe Institute of Technology (KIT). The KIT divertor design for the future DEMO fusion power plant is based on a modular concept of He-cooling finger units. More than 250,000 single parts are needed for the whole divertor system, where the most promising divertor material, tungsten, must withstand steady-state heat loads of up to 10 MW/m2. Powder injection molding (PIM) as a mass-oriented manufacturing method of parts with high near-net-shape precision has been adapted and developed at KIT for producing tungsten parts, which provides a cost-saving alternative compared to conventional machining. While manufactured tungsten parts are normally composed of only one material, two-component PIM applied in this work allows the joining of two different materials, e.g., tungsten with a tungsten alloy, without brazing. The complete technological process of two-component tungsten PIM of samples, including the subsequent heat-treatment process, is outlined. Characterization results of the finished samples, e.g., microstructure, hardness, density, and joining zone quality, are discussed.
- 1 August 2012
- Published by Taylor & Francis in Fusion Science and Technology
- Vol. 62 (1) , 110-115
Two-Component Tungsten Powder Injection Molding for Mass Production of He-Cooled DEMO Divertor Parts
Fusion technology as a possible and promising alternative energy source for the future is intensively investigated at Karlsruhe Institute of Technology (KIT). The KIT divertor design for the future DEMO fusion power plant is based on a modular concept of He-cooling finger units. More than 250,000 single parts are needed for the whole divertor system, where the most promising divertor material, tungsten, must withstand steady-state heat loads of up to 10 MW/m2. Powder injection molding (PIM) as a mass-oriented manufacturing method of parts with high near-net-shape precision has been adapted and developed at KIT for producing tungsten parts, which provides a cost-saving alternative compared to conventional machining. While manufactured tungsten parts are normally composed of only one material, two-component PIM applied in this work allows the joining of two different materials, e.g., tungsten with a tungsten alloy, without brazing. The complete technological process of two-component tungsten PIM of samples, including the subsequent heat-treatment process, is outlined. Characterization results of the finished samples, e.g., microstructure, hardness, density, and joining zone quality, are discussed.
- 1 January 2012
- Published by Elsevier in Intermetallics
- Vol. 20 (1) , 141-154
On the fracture toughness of fine-grained Mo-3Si-1B (wt.%) alloys at ambient to elevated (1300 °C) temperatures
- 1 January 2012
- Published by Elsevier in Intermetallics
- Vol. 20 (1) , 141-154
On the fracture toughness of fine-grained Mo-3Si-1B (wt.%) alloys at ambient to elevated (1300 °C) temperatures