Vladimir N. Malyshev
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Research Subjects
Vladimir N. Malyshev has a total of 23 co-authors. Here are the top co-authors by number of shared publications:
G. M. Sorokin
Gubkin State Oil and Gas University
4 shared publicationsN.S. Poches
2 shared publicationsO.V. Denisov
2 shared publicationsA. A. Petrosyants
1 shared publicationA. M. Volkhin
Gubkin Russian State University of Oil and Gas, 65 Leninsky Prospect, Moscow 119991, Russia
1 shared publicationA.I. Rodionov
Novosibirsk State Technical University, Russia
1 shared publication
Latest Publications
- 1 August 2026
- Published by Allerton Press in Russian Engineering Research
- Vol. 46 (8) , 1037-1041
Improving the Effectiveness of a Friction Machine for Testing of Materials and Coatings for Resistance to Abrasive Wear
Based on operating experience of friction machines, recommendations are formulated for improving the quality of abrasive wear tests under simultaneous slid
- 1 August 2026
- Published by Allerton Press in Russian Engineering Research
- Vol. 46 (8) , 1037-1041
Improving the Effectiveness of a Friction Machine for Testing of Materials and Coatings for Resistance to Abrasive Wear
Based on operating experience of friction machines, recommendations are formulated for improving the quality of abrasive wear tests under simultaneous slid
- 1 January 2025
- Published by Science & Technology in Repair. Reconditioning. Modernization
- No. 12
EFFECT OF CARBON NANOTUBES ON CORROSION RESISTANCE MAO-COATINGS
Using the concept of a multifactorial experiment, the influence of factors determining the formation of coatings by microarc oxidation (MAO) on their corrosion resistance: the density of the anode current, the concentration of nanotube suspension in the base electrolyte solution and the substrate material of the sample have been studied. Corrosion resistance was studied in a 3.5% NaCl solution by a three-electrode scheme using a silver chloride reference electrode. Correlation-and-regression analysis with subsequent verification of the adequacy of the model by the Fisher criterion allowed us to reasonably obtain a combination of factors that increase the corrosion resistance of the coating formed on aluminum alloy B95 by five times relative to the coating formed in the base electrolyte.
- 1 January 2025
- Published by Science & Technology in Repair. Reconditioning. Modernization
- No. 12
EFFECT OF CARBON NANOTUBES ON CORROSION RESISTANCE MAO-COATINGS
Using the concept of a multifactorial experiment, the influence of factors determining the formation of coatings by microarc oxidation (MAO) on their corrosion resistance: the density of the anode current, the concentration of nanotube suspension in the base electrolyte solution and the substrate material of the sample have been studied. Corrosion resistance was studied in a 3.5% NaCl solution by a three-electrode scheme using a silver chloride reference electrode. Correlation-and-regression analysis with subsequent verification of the adequacy of the model by the Fisher criterion allowed us to reasonably obtain a combination of factors that increase the corrosion resistance of the coating formed on aluminum alloy B95 by five times relative to the coating formed in the base electrolyte.
- 1 January 2024
- Published by Innovative Mashinostroenie Publishing
Effect of laser hardening and gas-flame surfasing on hardness and wear resistance of logging telemetry devices protective coating
In this work, the effect of laser hardening on increasing the hardness and wear resistance of combined protective coatings obtained by gas-flame and/or laser surfacing is studied. The integral hardness of coatings obtained by the studied technologies with different proportions of WC-8Co and viscous matrix is calculated. It has been found that laser hardening has a positive effect on the hardness of the WC-8Co pins and on the hardness of the nickel-based matrix containing up to 55 % WC, but its effect on the gas-flame surfacing is negative. The increment of integral hardness reached 5.1 % for WC—8Co and 3.5 % for the matrix.
- 1 January 2024
- Published by Innovative Mashinostroenie Publishing
Effect of laser hardening and gas-flame surfasing on hardness and wear resistance of logging telemetry devices protective coating
In this work, the effect of laser hardening on increasing the hardness and wear resistance of combined protective coatings obtained by gas-flame and/or laser surfacing is studied. The integral hardness of coatings obtained by the studied technologies with different proportions of WC-8Co and viscous matrix is calculated. It has been found that laser hardening has a positive effect on the hardness of the WC-8Co pins and on the hardness of the nickel-based matrix containing up to 55 % WC, but its effect on the gas-flame surfacing is negative. The increment of integral hardness reached 5.1 % for WC—8Co and 3.5 % for the matrix.
- 1 January 2024
- Published by Innovative Mashinostroenie Publishing
Determination of optimal laser hardening mode of hard alloy pins for mining tools
In this work, the effect of laser hardening on increasing the hardness and wear resistance of teeth made of sintered hard alloy WC8-Co, used for reinforcing mining tools and submersible borehole equipment, was studied. The optimal laser quenching mode has been determined, which provides an increase in wear resistance. The quantitative increment of hardness in depth was 5.14 %, and the increase in surface hardness reached 15.78 %.
- 1 January 2024
- Published by Innovative Mashinostroenie Publishing
Determination of optimal laser hardening mode of hard alloy pins for mining tools
In this work, the effect of laser hardening on increasing the hardness and wear resistance of teeth made of sintered hard alloy WC8-Co, used for reinforcing mining tools and submersible borehole equipment, was studied. The optimal laser quenching mode has been determined, which provides an increase in wear resistance. The quantitative increment of hardness in depth was 5.14 %, and the increase in surface hardness reached 15.78 %.
- Open Access
Processing and Tribological Properties of PEO Coatings on AlZn5.5MgCu Aluminium Alloy with Incorporated Al-Cu-Fe Quasicrystals
The modification of ceramic PEO coatings developed for friction units is in trend of modern research aimed at the improvement of friction and wear. This study presents ceramic coatings formed on AlZn5.5MgCu aluminum alloy by microarc oxidation (PEO) in a one-stage technological process with inclusions of Al-Cu-Fe quasi-crystals. The technology of rubbing quasi-crystals into the surface of the coating during final polishing was also used. Friction and wear tests, followed by analysis of the surface and cross-sections by SEM microscopy, showed that quasicrystals affect the coating structure and frictional characteristics. The addition of a small amount of modifier to the electrolyte (0.5 percent), as well as rubbing-in technology, can reduce the coefficient of friction (up to 16 percent) and wear rate (up to 43 times) compared to pure ceramic coatings. More modifier provides a negative result.
Open AccessProcessing and Tribological Properties of PEO Coatings on AlZn5.5MgCu Aluminium Alloy with Incorporated Al-Cu-Fe Quasicrystals
The modification of ceramic PEO coatings developed for friction units is in trend of modern research aimed at the improvement of friction and wear. This study presents ceramic coatings formed on AlZn5.5MgCu aluminum alloy by microarc oxidation (PEO) in a one-stage technological process with inclusions of Al-Cu-Fe quasi-crystals. The technology of rubbing quasi-crystals into the surface of the coating during final polishing was also used. Friction and wear tests, followed by analysis of the surface and cross-sections by SEM microscopy, showed that quasicrystals affect the coating structure and frictional characteristics. The addition of a small amount of modifier to the electrolyte (0.5 percent), as well as rubbing-in technology, can reduce the coefficient of friction (up to 16 percent) and wear rate (up to 43 times) compared to pure ceramic coatings. More modifier provides a negative result.
- 1 January 2022
- Published by Innovative Mashinostroenie Publishing
Study of microarc oxidation coatings friction and wearing under base oils greasing conditions
The presented paper is considered the issues of coatings wear resistance formed by the microarc oxidation method (MAO-coatings) on aluminum alloys. To form coatings, the aluminum alloys D16 (2024) and V95 (7075) in base weakly alkaline electrolyte and its modification by the way introduction into it such components like sodium aluminate, suspension of fluoroplastic and their combination with carbon nanoparticles were used. Tribotests of the friction couple "MAO-coating — steel ShKh15" by the scheme "Ring—Ring" under greasing condition performed an improvement of MAO-coatings tribological characteristics in the electrolyte modified by the fluoroplastic suspension.
- 1 January 2022
- Published by Innovative Mashinostroenie Publishing
Study of microarc oxidation coatings friction and wearing under base oils greasing conditions
The presented paper is considered the issues of coatings wear resistance formed by the microarc oxidation method (MAO-coatings) on aluminum alloys. To form coatings, the aluminum alloys D16 (2024) and V95 (7075) in base weakly alkaline electrolyte and its modification by the way introduction into it such components like sodium aluminate, suspension of fluoroplastic and their combination with carbon nanoparticles were used. Tribotests of the friction couple "MAO-coating — steel ShKh15" by the scheme "Ring—Ring" under greasing condition performed an improvement of MAO-coatings tribological characteristics in the electrolyte modified by the fluoroplastic suspension.
- 1 January 2021
- Published by Vestnik RGUPS, Rostov State Transport University
STUDY OF MAO-COATINGS TRIBOTECHNICAL CHARACTERISTICS FORMED IN WEAKLY ALKALINE ELECTROLYTES WITH ADDITION OF VARIOUS COMPONENTS
Работа посвящена вопросам износостойкости покрытий, сформированных методом микродугового оксидирования (МДО-покрытий) на алюминиевых сплавах. Для формирования покрытий использовался слабощелочной электролит и его модификации путем введения алюмината натрия, суспензии фторопласта и ее сочетание с углеродными наночастицами. Испытания на трение и изнашивание пары трения «МДО-покрытие - Сталь» по схеме «Кольцо-Кольцо» в смазочном материале показали улучшение триботехнических характеристик МДО-покрытий при добавлении суспензии...
- 1 January 2021
- Published by Vestnik RGUPS, Rostov State Transport University
STUDY OF MAO-COATINGS TRIBOTECHNICAL CHARACTERISTICS FORMED IN WEAKLY ALKALINE ELECTROLYTES WITH ADDITION OF VARIOUS COMPONENTS
Работа посвящена вопросам износостойкости покрытий, сформированных методом микродугового оксидирования (МДО-покрытий) на алюминиевых сплавах. Для формирования покрытий использовался слабощелочной электролит и его модификации путем введения алюмината натрия, суспензии фторопласта и ее сочетание с углеродными наночастицами. Испытания на трение и изнашивание пары трения «МДО-покрытие - Сталь» по схеме «Кольцо-Кольцо» в смазочном материале показали улучшение триботехнических характеристик МДО-покрытий при добавлении суспензии...
- Open Access
- 1 May 2020
- Published by IOP Publishing in IOP Conference Series: Materials Science and Engineering
- Vol. 862 (2)
Tribological tests of micro-arc oxidation coatings in environmentally safe lubricants
This study is devoted to wearing resistance of MAO-coatings formed on aluminum alloys 2024 (Al-Cu-Mg) and 7075 (Al-Zn-Mg-Cu) at the friction in pair with steel 100Cr6 in environmentally safe lubricants and represents a generalization and analysis of tests’ results. Investigations were conducted using two methods: reciprocating sliding on the “ball-on-disk” friction scheme and unidirectional sliding on the “pin-on-disk” friction scheme. As environmentally lubricants were used some base oils like polyalphaolefin (PAO), polyethylene glycol (PEG), Silicon Oil, perfluorinated polyether (PFPE) and diisotridecyl adipate ether (DITA). Tests on the first friction scheme allowed us to determine the maximal value of load for investigated friction pairs and tests on the second friction scheme showed their antifriction properties in different lubricants and in the mode of the greasing starvation. There was revealed that MAO-coatings formed on alloy 7075 at high contact pressures demonstrate a friction coefficient lower than on alloy 2024. Some problems of the used “pin-on-disk” scheme is discussed also for improving the tests’ results data.
- 1 May 2020
- Published by IOP Publishing in IOP Conference Series: Materials Science and Engineering
- Vol. 862 (2)
Open AccessTribological tests of micro-arc oxidation coatings in environmentally safe lubricants
This study is devoted to wearing resistance of MAO-coatings formed on aluminum alloys 2024 (Al-Cu-Mg) and 7075 (Al-Zn-Mg-Cu) at the friction in pair with steel 100Cr6 in environmentally safe lubricants and represents a generalization and analysis of tests’ results. Investigations were conducted using two methods: reciprocating sliding on the “ball-on-disk” friction scheme and unidirectional sliding on the “pin-on-disk” friction scheme. As environmentally lubricants were used some base oils like polyalphaolefin (PAO), polyethylene glycol (PEG), Silicon Oil, perfluorinated polyether (PFPE) and diisotridecyl adipate ether (DITA). Tests on the first friction scheme allowed us to determine the maximal value of load for investigated friction pairs and tests on the second friction scheme showed their antifriction properties in different lubricants and in the mode of the greasing starvation. There was revealed that MAO-coatings formed on alloy 7075 at high contact pressures demonstrate a friction coefficient lower than on alloy 2024. Some problems of the used “pin-on-disk” scheme is discussed also for improving the tests’ results data.
- Open Access
- 1 January 2020
- Published by Euroasian Scientific and Industrial Chamber, Ltd. in Современные наукоемкие технологии (Modern High Technologies)
- No. №10 2020,p. 45-50
STRENGTHENING OF WORKING SURFACES BY FRICTION STIR PROCESSING
- 1 January 2020
- Published by Euroasian Scientific and Industrial Chamber, Ltd. in Современные наукоемкие технологии (Modern High Technologies)
- No. №10 2020,p. 45-50
Open AccessSTRENGTHENING OF WORKING SURFACES BY FRICTION STIR PROCESSING