Afanasij Mikhailovich Ivanov
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Previous Organizations / Institutes
The organizations / institutes from the scholar's other articles in the past ten years
Research Subjects
Research Interests
Afanasij Mikhailovich Ivanov has a total of 12 co-authors. Here are the top co-authors by number of shared publications:
- Al'BErt Viktorovich Grigor'EV
Институт физико-технических проблем Севера им. В.П. Ларионова Сибирского отделения Российской академии наук – обособленное подразделение Федерального исследовательского центра «Якутский научный центр Сибирского отделения Российской академии наук
1 shared publication - Anastassia Anatolievna Ivanova1 shared publication
Anton Borisovich Loginov
1 shared publication- Boris Albertovich Loginov
National Research University of Electronic Technology MIET
1 shared publication Institute of Physics and Technologies of the M.K. Ammosov North-East Federal University
1 shared publicationLubov Gavrilievna Anempodistova
1 shared publication
Latest Publications
- 1 January 2020
- Published by Allerton Press in Russian Engineering Research
- Vol. 40 (1) , 33-37
Low-Temperature Fracture of Low-Alloy Steel after Severe Plastic Deformation
For the example of 09G2S steel Charpy samples, the impact strength and failure mechanism of low-alloy steel is considered in impact flexure at 213–29
- 1 January 2020
- Published by Allerton Press in Russian Engineering Research
- Vol. 40 (1) , 33-37
Low-Temperature Fracture of Low-Alloy Steel after Severe Plastic Deformation
For the example of 09G2S steel Charpy samples, the impact strength and failure mechanism of low-alloy steel is considered in impact flexure at 213–29
- Open Access
- 1 November 2019
- Published by IOP Publishing in IOP Conference Series: Materials Science and Engineering
- Vol. 672 (1) , 012029
Combining methods of severe plastic deformation as an effective way to increase the strength of metallic materials
The article reviews the combined methods of severe plastic deformation (SPD) for hardening metallic materials. The combined deformation processing, extrusion with the equal-channel angular pressing (ECAP) is presented. The comparison is made of the mechanical characteristics and the fracture mode of the Fe360 low carbon steel strengthened by the combined methods of extrusion with ECAP and ECAP with extrusion.
- 1 November 2019
- Published by IOP Publishing in IOP Conference Series: Materials Science and Engineering
- Vol. 672 (1) , 012029
Open AccessCombining methods of severe plastic deformation as an effective way to increase the strength of metallic materials
The article reviews the combined methods of severe plastic deformation (SPD) for hardening metallic materials. The combined deformation processing, extrusion with the equal-channel angular pressing (ECAP) is presented. The comparison is made of the mechanical characteristics and the fracture mode of the Fe360 low carbon steel strengthened by the combined methods of extrusion with ECAP and ECAP with extrusion.
- 1 July 2018
- Published by Pleiades Publishing Ltd in Inorganic Materials: Applied Research
- Vol. 9 (4) , 741-745
Strength and Destruction Mechanism of Low-Alloy Steel Subjected to a Combined Deformation Treatment
The strength and mechanism of destruction are studied for low-alloy steel 09G2S subjected to a combined treatment using an extrusion and screw pressing (ESP) of bulk billets at room temperature and...
- 1 July 2018
- Published by Pleiades Publishing Ltd in Inorganic Materials: Applied Research
- Vol. 9 (4) , 741-745
Strength and Destruction Mechanism of Low-Alloy Steel Subjected to a Combined Deformation Treatment
The strength and mechanism of destruction are studied for low-alloy steel 09G2S subjected to a combined treatment using an extrusion and screw pressing (ESP) of bulk billets at room temperature and...
- 1 July 2017
- Published by Allerton Press in Russian Journal of Non-Ferrous Metals
- Vol. 58 (4) , 383-388
Pressing prismatic and screw profiles from copper M4
Pressing methods of prismatic and screw metallic profiles are considered. An example of cold pressing of a billet from copper M4 with the formation of a solid square-cross-section profile is presented. Conventional pressing (extrusion) and extrusion followed by torsion pressing (extrusion and screw pressing (ESP)) are compared by mechanical characteristics, energy intensity, and the destruction character of copper samples. Herewith, the ESP of the billet was performed in one facility during the united production process. Pressing prismatic and screw profiles for one pass at room temperature was performed for copper billets Ø11.7 × 60 mm. The billet was loaded with a puncheon with the help of a hydraulic press. After the deformation treatment, solid prismatic and screw copper profiles with a square cross section of 8 × 8 mm were formed. The results on mechanical properties, deformation regularities, and destruction mechanism during the uniaxial tension of the samples made of technical copper M4 in the delivery state and after hardening are presented. Mechanical tests for uniaxial tension of the samples with a working size of Ø3 × 15 mm were performed using an UTS-20k testing machine at a constant loading speed of 3.33 × 10–5 m s–1. A certain increase in the strength of copper subjected to extrusion for one pass at room temperature is established. Screw pressing after extrusion provides higher plasticity compared with the initial state and extrusion. A fractographic research of sample ruptures is performed using a Hitachi TM 3030 scanning electron microscope in the secondary electron mode. It is shown that the destruction mechanism of copper samples in the delivery state, as well as after extrusion and ESP, is qualitatively identical. The destruction of the samples of copper M4 both in the initial state and after the deformation treatment according to the specified modes occurred according to the viscous fracture mechanism. It is revealed that ESP-subjected copper possesses larger energy intensity in connection with an increase in plasticity. The rupture in a fibrous zone for the ESP-subjected sample differs by the tier arrangement of pit blocks. Large pits and micropits in all states of copper are present both in the fibrous zone and in the peripheral cut zone.
- 1 July 2017
- Published by Allerton Press in Russian Journal of Non-Ferrous Metals
- Vol. 58 (4) , 383-388
Pressing prismatic and screw profiles from copper M4
Pressing methods of prismatic and screw metallic profiles are considered. An example of cold pressing of a billet from copper M4 with the formation of a solid square-cross-section profile is presented. Conventional pressing (extrusion) and extrusion followed by torsion pressing (extrusion and screw pressing (ESP)) are compared by mechanical characteristics, energy intensity, and the destruction character of copper samples. Herewith, the ESP of the billet was performed in one facility during the united production process. Pressing prismatic and screw profiles for one pass at room temperature was performed for copper billets Ø11.7 × 60 mm. The billet was loaded with a puncheon with the help of a hydraulic press. After the deformation treatment, solid prismatic and screw copper profiles with a square cross section of 8 × 8 mm were formed. The results on mechanical properties, deformation regularities, and destruction mechanism during the uniaxial tension of the samples made of technical copper M4 in the delivery state and after hardening are presented. Mechanical tests for uniaxial tension of the samples with a working size of Ø3 × 15 mm were performed using an UTS-20k testing machine at a constant loading speed of 3.33 × 10–5 m s–1. A certain increase in the strength of copper subjected to extrusion for one pass at room temperature is established. Screw pressing after extrusion provides higher plasticity compared with the initial state and extrusion. A fractographic research of sample ruptures is performed using a Hitachi TM 3030 scanning electron microscope in the secondary electron mode. It is shown that the destruction mechanism of copper samples in the delivery state, as well as after extrusion and ESP, is qualitatively identical. The destruction of the samples of copper M4 both in the initial state and after the deformation treatment according to the specified modes occurred according to the viscous fracture mechanism. It is revealed that ESP-subjected copper possesses larger energy intensity in connection with an increase in plasticity. The rupture in a fibrous zone for the ESP-subjected sample differs by the tier arrangement of pit blocks. Large pits and micropits in all states of copper are present both in the fibrous zone and in the peripheral cut zone.
- 1 May 2017
- Published by Allerton Press in Russian Engineering Research
- Vol. 37 (5) , 420-423
Strengthening of low-alloy steel by extrusion, helical pressing, and equal-channel angular pressing
Metals may be strengthened by a combination of extrusion, helical pressing, and equal-channel angular pressing. The mechanical properties of 09G2S low-alloy steel with and without such strengthening are presented. The steel is subjected to failure tests under uniaxial tension.
- 1 May 2017
- Published by Allerton Press in Russian Engineering Research
- Vol. 37 (5) , 420-423
Strengthening of low-alloy steel by extrusion, helical pressing, and equal-channel angular pressing
Metals may be strengthened by a combination of extrusion, helical pressing, and equal-channel angular pressing. The mechanical properties of 09G2S low-alloy steel with and without such strengthening are presented. The steel is subjected to failure tests under uniaxial tension.
- 1 January 2016
- Published by Tambov State University - G.R. Derzhavin in Tambov University Reports. Series: Natural and Technical Sciences
- Vol. 21 (3) , 1016-1019
FRACTURE MECHANISM OF LOW-ALLOY STEEL SUBJECTED COMBINED SEVERE PLASTIC DEFORMATION AND ANNEALING
- 1 January 2016
- Published by Tambov State University - G.R. Derzhavin in Tambov University Reports. Series: Natural and Technical Sciences
- Vol. 21 (3) , 1016-1019
FRACTURE MECHANISM OF LOW-ALLOY STEEL SUBJECTED COMBINED SEVERE PLASTIC DEFORMATION AND ANNEALING