Rodrigo Sánchez‐González
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Rodrigo Sánchez‐González has a total of 11 co-authors. Here are the top co-authors by number of shared publications:
- Andrés Díaz-Gómez
Interdisciplinary Group of Applied Nanotechnology (GINA), Hybrid Materials Laboratory (HML), Department of Materials Engineering (DIMAT), Faculty of Engineering, University of Concepcion, 270 Edmundo Larenas, Box 160-C, Concepcion 4070409, Chile
1 shared publication - Bárbara Valverde
Escuela de Ingeniería Mecánica, Pontificia Universidad Católica de Valparaíso, Valparaíso 2362807, Chile
1 shared publication - Constanza Suazo
Instituto de Química Pontificia Universidad Católica de Valparaíso Valparaíso Chile
1 shared publication - Elizabeth Imbarack
Facultad de Química y Biología, Departamento de Química de los Materiales, Universidad de Santiago de Chile (USACH), Av. Libertador B. O’Higgins 3363, Santiago 9170022, Chile
1 shared publication - Jesús Ramírez
Facultad de Ingeniería, Universidad San Sebastián, Campus Las Tres Pascualas, Lientur 1457, Concepción 4060000, Chile
1 shared publication - Juan Pablo Soto
Instituto de Química Pontificia Universidad Católica de Valparaíso Valparaíso Chile
1 shared publication
Latest Publications
- 23 February 2021
- Published by Wiley in Journal of Raman Spectroscopy
- Vol. 52 (5) , 959-970
Synthesis, characterization and surface enhanced Raman spectroscopy study of a new family of different substituted cruciform molecular systems deposited on gold nanoparticles
In this work, the adsorption and orientation on gold nanoparticles (AuNps) of a new family of cruciform systems consisting of thiophene rings and imino groups were studied. The structural modification and its influence on the adsorbate‐substrate interaction were evaluated by UV–Vis spectroscopy and Surface Enhanced Raman Spectroscopy (SERS). The absence of SERS spectrum for (N,N′‐bis(4‐(trifluoromethyl)benzylidene)‐2,5‐di (thiophene‐2‐yl)‐1,4‐diaminobenzene) CFF shows that the inclusion of a trifluoromethyl group (‐CF3) on the benzylidene fragment limits the interaction of the CFF system with the gold substrate, in contrast, to that obtained for (N, N′‐dibenzylidene‐2,5‐di (thiophene‐2‐yl) ‐1,4‐diaminobenzene) 2‐CF and (N, N′‐bis (4‐methoxybenzylidene) ‐2,5‐di (thiophene‐2yl) ‐1,4‐diaminobenzene) CMF, where the adsorption took place preferentially through the thiophene rings, resulting in partial quinoidization. On the other hand, the interaction for compound (N, N′‐bis (4‐methylenepyridinyl) ‐2,5‐di (thiophene‐2‐yl) ‐1,4‐diaminobenzene) CPy with the surface was conducted by means of the pyridinic fragments. The systematic modification of the bifunctional cruciform systems, with groups of different nature, makes it possible to rationalize the structural aspects that directly influence the adsorbate‐substrate interaction and molecular orientation on gold substrates. These structural parameters are the basis to the development of stable molecular assemblies, which can act as basic building blocks in the manufacture of molecular switches.
- 23 February 2021
- Published by Wiley in Journal of Raman Spectroscopy
- Vol. 52 (5) , 959-970
Synthesis, characterization and surface enhanced Raman spectroscopy study of a new family of different substituted cruciform molecular systems deposited on gold nanoparticles
In this work, the adsorption and orientation on gold nanoparticles (AuNps) of a new family of cruciform systems consisting of thiophene rings and imino groups were studied. The structural modification and its influence on the adsorbate‐substrate interaction were evaluated by UV–Vis spectroscopy and Surface Enhanced Raman Spectroscopy (SERS). The absence of SERS spectrum for (N,N′‐bis(4‐(trifluoromethyl)benzylidene)‐2,5‐di (thiophene‐2‐yl)‐1,4‐diaminobenzene) CFF shows that the inclusion of a trifluoromethyl group (‐CF3) on the benzylidene fragment limits the interaction of the CFF system with the gold substrate, in contrast, to that obtained for (N, N′‐dibenzylidene‐2,5‐di (thiophene‐2‐yl) ‐1,4‐diaminobenzene) 2‐CF and (N, N′‐bis (4‐methoxybenzylidene) ‐2,5‐di (thiophene‐2yl) ‐1,4‐diaminobenzene) CMF, where the adsorption took place preferentially through the thiophene rings, resulting in partial quinoidization. On the other hand, the interaction for compound (N, N′‐bis (4‐methylenepyridinyl) ‐2,5‐di (thiophene‐2‐yl) ‐1,4‐diaminobenzene) CPy with the surface was conducted by means of the pyridinic fragments. The systematic modification of the bifunctional cruciform systems, with groups of different nature, makes it possible to rationalize the structural aspects that directly influence the adsorbate‐substrate interaction and molecular orientation on gold substrates. These structural parameters are the basis to the development of stable molecular assemblies, which can act as basic building blocks in the manufacture of molecular switches.
- 14 January 2020
- Published by Wiley in Materials and Corrosion
- Vol. 71 (7) , 1125-1137
Effect of height on the corrosion of steel and galvanized steel in nontropical coastal marine environments
In this study, the behavior of carbon steel and galvanized steel in nontropical coastal marine environments was evaluated. Evaluation was carried out with specimens with dimensions of 10 cm × 10 cm × 0.3 cm. These specimens were exposed to four testing stations (Iquique, Mejillones, Los Vilos, and San Vicente), where racks were installed both at ground level (ground), as well as in the upper zone of electrical transmission towers (tower). In each station, 24 specimens of A36 carbon steel and galvanized steel were placed (12 each). The corrosivity of the environment was measured using the ISO 9223, 9225, and 9226 standards. The specimens were evaluated on‐site, monthly, through visual inspection and photographic record. Once withdrawn, the corrosion rate was determined and the corrosion products were analyzed through Raman and Fourier‐transform infrared. The results show that, in all cases, the corrosion rate is greater in the tower than on the ground. However, even though the Los Vilos station is located farther from the sea (3,500 vs. ≈500 m), the corrosion rate of steel in the tower is the highest. This is caused by the generation of HCl from the transformation of lepidocrocite into goethite, in the presence of low chloride content, which acidifies the steel/corrosion product interface. In the case of galvanized steel, the corrosion rate is a function of the chloride content in the atmosphere, obtaining an excellent correlation between both parameters.
- 14 January 2020
- Published by Wiley in Materials and Corrosion
- Vol. 71 (7) , 1125-1137
Effect of height on the corrosion of steel and galvanized steel in nontropical coastal marine environments
In this study, the behavior of carbon steel and galvanized steel in nontropical coastal marine environments was evaluated. Evaluation was carried out with specimens with dimensions of 10 cm × 10 cm × 0.3 cm. These specimens were exposed to four testing stations (Iquique, Mejillones, Los Vilos, and San Vicente), where racks were installed both at ground level (ground), as well as in the upper zone of electrical transmission towers (tower). In each station, 24 specimens of A36 carbon steel and galvanized steel were placed (12 each). The corrosivity of the environment was measured using the ISO 9223, 9225, and 9226 standards. The specimens were evaluated on‐site, monthly, through visual inspection and photographic record. Once withdrawn, the corrosion rate was determined and the corrosion products were analyzed through Raman and Fourier‐transform infrared. The results show that, in all cases, the corrosion rate is greater in the tower than on the ground. However, even though the Los Vilos station is located farther from the sea (3,500 vs. ≈500 m), the corrosion rate of steel in the tower is the highest. This is caused by the generation of HCl from the transformation of lepidocrocite into goethite, in the presence of low chloride content, which acidifies the steel/corrosion product interface. In the case of galvanized steel, the corrosion rate is a function of the chloride content in the atmosphere, obtaining an excellent correlation between both parameters.