Vladimir E. Strel’nitskij
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Research Subjects
Research Interests
Vladimir E. Strel’nitskij has a total of 22 co-authors. Here are the top co-authors by number of shared publications:
- Alexander I. Kalinichenko
National Science Centre “Kharkiv Institute of Physics and Technology
2 shared publications A.O. Chumak
V. Bakul Institute for Superhard Materials
1 shared publicationA.O. Lyamtseva
V. Bakul Institute for Superhard Materials
1 shared publicationA.о. Omarov
National Science Center "Kharkov Institute of Physics and Technology", Kharkiv, Ukraine
1 shared publication- Anton Baranovskiy
Institute of Strength Physics and Materials Science, Siberian Branch, Russian Academy of Sciences, Tomsk, Russia
1 shared publication City Clinical Hospital No16
1 shared publication
Latest Publications
- 14 April 2026
- Published by Problems of Atomic Science and Technology in Problems of Atomic Science and Technology
USE OF GLOW DISCHARGE PLASMA FOR DEPOSITION WEAR RESISTANT CVD DIAMOND COATINGS TO CUTTING TOOLS WITH PCD
To improve the wear resistance of cutting tools equipped with inserts sintered from synthetic diamond powder, processes have been developed for synthesizing polycrystalline diamond coatings on their surface using the CVD method from H2/CH4 gas mixture in a glow discharge stabilized by a transverse magnetic field. Homogeneous coatings with a thickness of 17…56 μm and a clearly formed microcrystalline structure were obtained. A comparison was made between the DC and pulsed modes of operation of the discharge power source during the preparatory treatment of the cutting inserts surface and directly during the deposition of the coating. The advantages of the pulsed mode (frequency 50 kHz, duty cycle 1.1) at the preparatory treatment stage were revealed, which ensures rapid cleaning and heating of the cutting inserts surface to a synthesis temperature of 1070…1150 °C without the glow discharge transitioning to an arc discharge. It has been found that the deposition rate and surface morphology of coatings synthesized in pulsed and DC modes do not differ significantly. As the coating thickness increases, the average size of diamond crystals increases. It has been shown that the deposition of diamond coating increases the wear resistance of cutting tools when machining difficult-to-machine materials (ceramics, hard alloy) by more than 1.5 times. A coating with a thickness of 56 μm, deposited by DC mode, provided the tool with the greatest wear resistance when turning the VK8 hard alloy, however, the increase in diamond crystal size led to a deterioration in the quality of the machined surface due to an increase in its roughness. The feasibility of optimizing the size of diamond grains to improve the performance characteristics of the tool is discussed.
- 14 April 2026
- Published by Problems of Atomic Science and Technology in Problems of Atomic Science and Technology
USE OF GLOW DISCHARGE PLASMA FOR DEPOSITION WEAR RESISTANT CVD DIAMOND COATINGS TO CUTTING TOOLS WITH PCD
To improve the wear resistance of cutting tools equipped with inserts sintered from synthetic diamond powder, processes have been developed for synthesizing polycrystalline diamond coatings on their surface using the CVD method from H2/CH4 gas mixture in a glow discharge stabilized by a transverse magnetic field. Homogeneous coatings with a thickness of 17…56 μm and a clearly formed microcrystalline structure were obtained. A comparison was made between the DC and pulsed modes of operation of the discharge power source during the preparatory treatment of the cutting inserts surface and directly during the deposition of the coating. The advantages of the pulsed mode (frequency 50 kHz, duty cycle 1.1) at the preparatory treatment stage were revealed, which ensures rapid cleaning and heating of the cutting inserts surface to a synthesis temperature of 1070…1150 °C without the glow discharge transitioning to an arc discharge. It has been found that the deposition rate and surface morphology of coatings synthesized in pulsed and DC modes do not differ significantly. As the coating thickness increases, the average size of diamond crystals increases. It has been shown that the deposition of diamond coating increases the wear resistance of cutting tools when machining difficult-to-machine materials (ceramics, hard alloy) by more than 1.5 times. A coating with a thickness of 56 μm, deposited by DC mode, provided the tool with the greatest wear resistance when turning the VK8 hard alloy, however, the increase in diamond crystal size led to a deterioration in the quality of the machined surface due to an increase in its roughness. The feasibility of optimizing the size of diamond grains to improve the performance characteristics of the tool is discussed.
- Open Access
- 2 June 2022
- Published by V. N. Karazin Kharkiv National University in East European Journal of Physics
- No. 2,p. 6-11
Influence of the Inert Gas Pressure on Intrinsic Stress in Diamond-Like Coating Deposited From Vacuum Arc Carbon Plasma
Within the framework of the model of the nonlocal thermoelastic peak of low-energy ion, the formation of intrinsic stress in a carbon coating deposited from the vacuum arc plasma in the argon atmosphere is theoretically studied. It is shown that the flow of particles bombarding the deposited coating contains, along with C+ ions, also Ar+ ions involved in the formation of intrinsic stress in the coating. The flux density of Ar+ ions resulting from ionization losses of C+ ions passing through the argon atmosphere is proportional to both the flux density of C+ ions and the density (pressure) of argon. Expressions are obtained for the intrinsic stress in the deposited carbon coating depending on the bias potential on the substrate and the argon pressure for the cases of both constant and pulsed potentials. The analysis of the obtained expressions shows that the intrinsic stress in the carbon coating decrease with increasing argon pressure.
- 2 June 2022
- Published by V. N. Karazin Kharkiv National University in East European Journal of Physics
- No. 2,p. 6-11
Open AccessInfluence of the Inert Gas Pressure on Intrinsic Stress in Diamond-Like Coating Deposited From Vacuum Arc Carbon Plasma
Within the framework of the model of the nonlocal thermoelastic peak of low-energy ion, the formation of intrinsic stress in a carbon coating deposited from the vacuum arc plasma in the argon atmosphere is theoretically studied. It is shown that the flow of particles bombarding the deposited coating contains, along with C+ ions, also Ar+ ions involved in the formation of intrinsic stress in the coating. The flux density of Ar+ ions resulting from ionization losses of C+ ions passing through the argon atmosphere is proportional to both the flux density of C+ ions and the density (pressure) of argon. Expressions are obtained for the intrinsic stress in the deposited carbon coating depending on the bias potential on the substrate and the argon pressure for the cases of both constant and pulsed potentials. The analysis of the obtained expressions shows that the intrinsic stress in the carbon coating decrease with increasing argon pressure.
- Open Access
- 7 April 2021
- Published by Problems of Atomic Science and Technology in Problems of Atomic Science and Technology
- No. 2,p. 109-112
GROWTH RATE OF DIAMOND-LIKE COATINGS SYNTHESIZED IN RF DISCHARGE AT VARIOUS RATIOS OF THE CONCENTRATIONS OF Ar AND C6H6
Diamond-like coatings (DLC) synthesized by plasma-chemical deposition from a vapor mixture of C6H6 and Ar have been investigated. The growth rate of the coating was measured, which showed a nonlinear dependence on the partial pressure of Ar. The mathematical model of the deposition has been developed, which qualitatively and quantitatively describes the dependence of the ion flux density and deposition rate on the partial pressure of argon.
- 7 April 2021
- Published by Problems of Atomic Science and Technology in Problems of Atomic Science and Technology
- No. 2,p. 109-112
Open AccessGROWTH RATE OF DIAMOND-LIKE COATINGS SYNTHESIZED IN RF DISCHARGE AT VARIOUS RATIOS OF THE CONCENTRATIONS OF Ar AND C6H6
Diamond-like coatings (DLC) synthesized by plasma-chemical deposition from a vapor mixture of C6H6 and Ar have been investigated. The growth rate of the coating was measured, which showed a nonlinear dependence on the partial pressure of Ar. The mathematical model of the deposition has been developed, which qualitatively and quantitatively describes the dependence of the ion flux density and deposition rate on the partial pressure of argon.
- 24 December 2020
- Published by Vitebsk State Medical University in Novosti Khirurgii
- Vol. 28 (6) , 617-624
Osseointegration of Implants with A Diamond-Like Carbon Coating in the Experiment
Цель. Изучить в эксперименте на крысах интеграцию с костью металлических имплантатов из нержавеющей стали с алмазоподобным углеродным (DLC) покрытием. Материал и методы. Эксперимент проведен на 48 белых крысах-самцах в возрасте 6 месяцев. Животным имплантировали в метафизарные дефекты бедренной кости (диаметр 2 мм и глубина 3 мм) имплантаты из стали и стальные имплантаты с DLC-покрытием (по 24 крысы в контрольной и опытной группах). На поверхность стального имплантата наносили DLC-покрытие из отфильтрованных потоков вакуумно-дуговой плазмы. Материал покрытия не содержал примесей металлов и водорода. Нанотвердость нанесенного на образец покрытия составляла от 30 до 40 ГПа. Толщина DLC-покрытия составляла не менее 1 мкм. Эвтаназию крыс проводили через 7, 14, 30 и 90 дней после операции путем введения летальной дозы тиопентала натрия (90 мг/кг внутримышечно). Ремоделирование кости вокруг имплантатов исследовали гистологическими методами с морфометрической оценкой остеоинтеграции (контакт костной ткани с имплантатом в процентах). Результаты. Алмазоподобное углеродное покрытие на стальных имплантатах обладает высокими адгезионными качествами, о чем свидетельствует прикрепление клеток к поверхности в течение 7 дней после имплантации и формирование вокруг них костной ткани через 14 дней. Вокруг стальных имплантатов зафиксировано образование прослойки из соединительной ткани с участками костной ткани. Выявлено, что за весь период исследования вокруг имплантатов из стали с DLC-покрытием процент остеоинтеграции был выше по сравнению с имплантатами без покрытия: на 14-й день – в 2,6 раза, на 30-й день – в 2,1 раза, на 90-й день – в 1,5 раза. Заключение. Алмазоподобные углеродные покрытия на стальных имплантатах являются перспективным материалом для использования в ортопедии и травматологии благодаря биосовместимости, остеоинтеграции и отсутствию негативного ремоделирования прилегающей костной ткани. Научная новизна статьи Впервые в эксперименте изучена перестройка кости вокруг имплантатов с разработанным алмазоподобным углеродным покрытием. Установлено, что использованное покрытие обладает биосовместимостью и высокими показателями остеоинтеграции.
- 24 December 2020
- Published by Vitebsk State Medical University in Novosti Khirurgii
- Vol. 28 (6) , 617-624
Osseointegration of Implants with A Diamond-Like Carbon Coating in the Experiment
Цель. Изучить в эксперименте на крысах интеграцию с костью металлических имплантатов из нержавеющей стали с алмазоподобным углеродным (DLC) покрытием. Материал и методы. Эксперимент проведен на 48 белых крысах-самцах в возрасте 6 месяцев. Животным имплантировали в метафизарные дефекты бедренной кости (диаметр 2 мм и глубина 3 мм) имплантаты из стали и стальные имплантаты с DLC-покрытием (по 24 крысы в контрольной и опытной группах). На поверхность стального имплантата наносили DLC-покрытие из отфильтрованных потоков вакуумно-дуговой плазмы. Материал покрытия не содержал примесей металлов и водорода. Нанотвердость нанесенного на образец покрытия составляла от 30 до 40 ГПа. Толщина DLC-покрытия составляла не менее 1 мкм. Эвтаназию крыс проводили через 7, 14, 30 и 90 дней после операции путем введения летальной дозы тиопентала натрия (90 мг/кг внутримышечно). Ремоделирование кости вокруг имплантатов исследовали гистологическими методами с морфометрической оценкой остеоинтеграции (контакт костной ткани с имплантатом в процентах). Результаты. Алмазоподобное углеродное покрытие на стальных имплантатах обладает высокими адгезионными качествами, о чем свидетельствует прикрепление клеток к поверхности в течение 7 дней после имплантации и формирование вокруг них костной ткани через 14 дней. Вокруг стальных имплантатов зафиксировано образование прослойки из соединительной ткани с участками костной ткани. Выявлено, что за весь период исследования вокруг имплантатов из стали с DLC-покрытием процент остеоинтеграции был выше по сравнению с имплантатами без покрытия: на 14-й день – в 2,6 раза, на 30-й день – в 2,1 раза, на 90-й день – в 1,5 раза. Заключение. Алмазоподобные углеродные покрытия на стальных имплантатах являются перспективным материалом для использования в ортопедии и травматологии благодаря биосовместимости, остеоинтеграции и отсутствию негативного ремоделирования прилегающей костной ткани. Научная новизна статьи Впервые в эксперименте изучена перестройка кости вокруг имплантатов с разработанным алмазоподобным углеродным покрытием. Установлено, что использованное покрытие обладает биосовместимостью и высокими показателями остеоинтеграции.
- 1 September 2016
- Published by Trans Tech Publications, Ltd. in Key Engineering Materials
- Vol. 712, 195-199
Fabrication of «TiC-HSS Steel Binder» Composite Powders by Self-Propagating High Temperature Synthesis
The phase composition, microstructure and morphology of composite powders «TiC-HSS steel binder» obtained by the SHS method in layerwise combustion mode have been studied. Titanium powder, carbon (carbon black) in a ratio corresponding to equiatomic titanium carbide and high speed steel as a thermally inert binder was used as a reaction mixture. It was found that the mass transfer of reaction mixture components between the carbide and metal binder was taking place during synthesis, as a result of which the final phase and elemental composition of the synthesis products was formed. It is shown that the volume content of thermally inert binder significantly affects the dispersion of the formed carbide phase.
- 1 September 2016
- Published by Trans Tech Publications, Ltd. in Key Engineering Materials
- Vol. 712, 195-199
Fabrication of «TiC-HSS Steel Binder» Composite Powders by Self-Propagating High Temperature Synthesis
The phase composition, microstructure and morphology of composite powders «TiC-HSS steel binder» obtained by the SHS method in layerwise combustion mode have been studied. Titanium powder, carbon (carbon black) in a ratio corresponding to equiatomic titanium carbide and high speed steel as a thermally inert binder was used as a reaction mixture. It was found that the mass transfer of reaction mixture components between the carbide and metal binder was taking place during synthesis, as a result of which the final phase and elemental composition of the synthesis products was formed. It is shown that the volume content of thermally inert binder significantly affects the dispersion of the formed carbide phase.