Ruiping Wang
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Previous Organizations / Institutes
The organizations / institutes from the scholar's other articles in the past ten years
Research Subjects
Ruiping Wang has a total of 139 co-authors. Here are the top co-authors by number of shared publications:
Mitsuru Itoh
Materials and Structures Laboratory, Tokyo Institute of Technology, Yokohama 226-8503, Japan
26 shared publicationsM. Itoh
Materials and Structures Laboratory, Tokyo Institute of Technology, 4259 Nagatsuta, Midori-ku, Yokohama, Japan
11 shared publicationsHiroshi Bando
National Institute of Advanced Industrial Science and Technology, Tsukuba, Ibaraki 305-8568, Japan
10 shared publications- Hiroshi Takashima
National Institute of Advanced Industrial Science and Technology, 1-1-1 Umezono, Tsukuba, Ibaraki 305-8560, Japan
10 shared publications - Mitsuru Itoh
Materials and Structures Laboratory, Tokyo Institute of Technology, 4259 Nagatsuta, Midori, Yokohama 226-8503, Japan
8 shared publications Tadashi Sekiya
National Institute of Advanced Industrial Science and Technology, Tsukuba, Ibaraki 305-8568
8 shared publications
Latest Publications
- 10 August 2018
- Published by Springer Nature in MRS Bulletin
- Vol. 43 (8) , 612-616
Applications of lead-free piezoelectric materials
- 10 August 2018
- Published by Springer Nature in MRS Bulletin
- Vol. 43 (8) , 612-616
Applications of lead-free piezoelectric materials
- 1 May 2018
- Published by Elsevier in Journal of Fluorine Chemistry
- Vol. 209, 65-72
Phase transitions and dielectric properties of perovskite-type oxyfluorides (1-x)KNbO3-xKMgF3
- 1 May 2018
- Published by Elsevier in Journal of Fluorine Chemistry
- Vol. 209, 65-72
Phase transitions and dielectric properties of perovskite-type oxyfluorides (1-x)KNbO3-xKMgF3
- Open Access
- 1 June 2016
- Published by World Scientific Pub Co Pte Ltd in Journal of Advanced Dielectrics
- Vol. 06 (02) , 1650014
Phase diagram of (Na0.5K0.5)NbO3-(Bi0.5Na0.5)ZrO3 solid solution
Phase diagram of [ ]Na[ ]K[ ]NbO3–x(Bi[ ]Na[ ]ZrO3 solid solution has been established from dielectric constant measurements and structure analyses. It is found that with increasing x, the C–T phase transition temperature [ ] and the T–O phase transition temperature [ ] decrease, while the [ ] phase transition temperature [ ] increases. [ ] of NKN–xBNZ is much different from that of NKN–xBZ solid solution. The result could be mainly elucidated by the hybridization between the A-site ion and oxygen.
- 1 June 2016
- Published by World Scientific Pub Co Pte Ltd in Journal of Advanced Dielectrics
- Vol. 06 (02) , 1650014
Open AccessPhase diagram of (Na0.5K0.5)NbO3-(Bi0.5Na0.5)ZrO3 solid solution
Phase diagram of [ ]Na[ ]K[ ]NbO3–x(Bi[ ]Na[ ]ZrO3 solid solution has been established from dielectric constant measurements and structure analyses. It is found that with increasing x, the C–T phase transition temperature [ ] and the T–O phase transition temperature [ ] decrease, while the [ ] phase transition temperature [ ] increases. [ ] of NKN–xBNZ is much different from that of NKN–xBZ solid solution. The result could be mainly elucidated by the hybridization between the A-site ion and oxygen.
- 1 January 2016
- Published by Elsevier in Journal of Alloys and Compounds
- Vol. 655, 290-295
Full set of material constants of (Na0.5K0.5)NbO3–BaZrO3–(Bi0.5Li0.5)TiO3 lead-free piezoelectric ceramics at the morphotropic phase boundary
- 1 January 2016
- Published by Elsevier in Journal of Alloys and Compounds
- Vol. 655, 290-295
Full set of material constants of (Na0.5K0.5)NbO3–BaZrO3–(Bi0.5Li0.5)TiO3 lead-free piezoelectric ceramics at the morphotropic phase boundary
- 23 April 2015
- Published by Wiley in Journal of the American Ceramic Society
- Vol. 98 (7) , 2177-2182
Temperature Stability of Lead‐Free Niobate Piezoceramics with Engineered Morphotropic Phase Boundary
The temperature dependence of piezoelectric properties (direct piezoelectric coefficient d 33 , converse piezoelectric coefficient d 33 ( E = 0), strain S and electromechanical coupling coefficient k p ) for two niobate‐based lead‐free piezoceramics have been contrasted. 0.92(Na 0.5 K 0.5 )NbO 3 –0.02(Bi 1/2 Li 1/2 )TiO 3 –0.06BaZrO 3 (6 BZ /2 BLT /92 NKN ) has a morphotropic phase boundary ( MPB ) between rhombohedral and tetragonal at room temperature and 0.92(Na 0.5 K 0.5 )NbO 3 –0.03(Bi 1/2 Li 1/2 )TiO 3 –0.05BaZrO 3 (5 BZ /3 BLT /92 NKN ) features an MPB engineered to be located below room temperature. At 30°C, d 33 , d 33 ( E = 0), S (at 2 kV/mm), and k p are 252 pC/N, 230 pm/V, 0.069%, 0.51 for 5 BZ /3 BLT /92 NKN ; and 348 pC/N, 380 pm/V, 0.106%, 0.57 for 6 BZ /2 BLT /92 NKN , respectively. With increasing temperature, the piezoelectric properties decrease. At 200°C, d 33 , d 33 ( E = 0), S (at 2 kV/mm), and k p are 170 pC/N, 160 pm/V, 0.059%, 0.36 for 5 BZ /3 BLT /92 NKN ; and 181 pC/N, 190 pm/V, 0.061%, 0.39 for 6 BZ /2 BLT /92 NKN . It is found that the electromechanical coupling coefficient has a better temperature stability than the piezoelectric coefficient in the studied system due to a large temperature‐dependent compliance change. The results demonstrate that engineering an MPB is highly effective in tailoring temperature stability of piezoceramics.
- 23 April 2015
- Published by Wiley in Journal of the American Ceramic Society
- Vol. 98 (7) , 2177-2182
Temperature Stability of Lead‐Free Niobate Piezoceramics with Engineered Morphotropic Phase Boundary
The temperature dependence of piezoelectric properties (direct piezoelectric coefficient d 33 , converse piezoelectric coefficient d 33 ( E = 0), strain S and electromechanical coupling coefficient k p ) for two niobate‐based lead‐free piezoceramics have been contrasted. 0.92(Na 0.5 K 0.5 )NbO 3 –0.02(Bi 1/2 Li 1/2 )TiO 3 –0.06BaZrO 3 (6 BZ /2 BLT /92 NKN ) has a morphotropic phase boundary ( MPB ) between rhombohedral and tetragonal at room temperature and 0.92(Na 0.5 K 0.5 )NbO 3 –0.03(Bi 1/2 Li 1/2 )TiO 3 –0.05BaZrO 3 (5 BZ /3 BLT /92 NKN ) features an MPB engineered to be located below room temperature. At 30°C, d 33 , d 33 ( E = 0), S (at 2 kV/mm), and k p are 252 pC/N, 230 pm/V, 0.069%, 0.51 for 5 BZ /3 BLT /92 NKN ; and 348 pC/N, 380 pm/V, 0.106%, 0.57 for 6 BZ /2 BLT /92 NKN , respectively. With increasing temperature, the piezoelectric properties decrease. At 200°C, d 33 , d 33 ( E = 0), S (at 2 kV/mm), and k p are 170 pC/N, 160 pm/V, 0.059%, 0.36 for 5 BZ /3 BLT /92 NKN ; and 181 pC/N, 190 pm/V, 0.061%, 0.39 for 6 BZ /2 BLT /92 NKN . It is found that the electromechanical coupling coefficient has a better temperature stability than the piezoelectric coefficient in the studied system due to a large temperature‐dependent compliance change. The results demonstrate that engineering an MPB is highly effective in tailoring temperature stability of piezoceramics.
- 21 October 2013
- Published by American Chemical Society (ACS) in Inorganic Chemistry
- Vol. 52 (21) , 12806-12810
Oxygen Diffusion and Nonstoichiometry in BiFeO3
Leakage current is a serious problem for the use of ferroelectricity in room-temperature multiferroics BiFeO3, and oxygen nonstoichiometry is considered as one of its principal origins. In order to establish a method to control oxygen content in the compound, we investigated the annealing process of stoichiometric BiFeO3 grains in air and revealed that oxygen diffusion occurs in two steps: (1) the weight of the sample decreases in a short time, which originates from the generation of oxygen deficiency near the surface of the grains; and then (2) it increases gradually and slowly, which originates from oxygen diffusion toward equilibrium in the inner part of the grains, introducing excess oxygen there. Step 1 causes the leakage current, and step 2 tends to cause inhomogeneity of oxygen content as well as the leakage current. Steps 1 and 2 are related to oxygen deficiency and excess oxygen often observed in thin films and bulk crystals, respectively. For the synthesis of homogeneous and highly insulating bulk sample, it is important to avoid these annealing processes, and it is a good way to grow a crystal with stoichiometric oxygen content by the control of atmospheric oxygen partial pressure and taking out its inner part.
- 21 October 2013
- Published by American Chemical Society (ACS) in Inorganic Chemistry
- Vol. 52 (21) , 12806-12810
Oxygen Diffusion and Nonstoichiometry in BiFeO3
Leakage current is a serious problem for the use of ferroelectricity in room-temperature multiferroics BiFeO3, and oxygen nonstoichiometry is considered as one of its principal origins. In order to establish a method to control oxygen content in the compound, we investigated the annealing process of stoichiometric BiFeO3 grains in air and revealed that oxygen diffusion occurs in two steps: (1) the weight of the sample decreases in a short time, which originates from the generation of oxygen deficiency near the surface of the grains; and then (2) it increases gradually and slowly, which originates from oxygen diffusion toward equilibrium in the inner part of the grains, introducing excess oxygen there. Step 1 causes the leakage current, and step 2 tends to cause inhomogeneity of oxygen content as well as the leakage current. Steps 1 and 2 are related to oxygen deficiency and excess oxygen often observed in thin films and bulk crystals, respectively. For the synthesis of homogeneous and highly insulating bulk sample, it is important to avoid these annealing processes, and it is a good way to grow a crystal with stoichiometric oxygen content by the control of atmospheric oxygen partial pressure and taking out its inner part.
- 20 June 2013
- Published by IOP Publishing in Japanese Journal of Applied Physics
- Vol. 52 (7S) , 07HB02
Formation of Morphotropic Phase Boundary in (Na0.5K0.5)NbO3–BaZrO3–(Bi0.5Li0.5)TiO3 Lead-Free Piezoelectric Ceramics
For the development of lead-free piezoelectric ceramics, which have a tetragonal–rhombohedral morphotropic phase boundary (MPB), 0.90(Na0.5K0.5)NbO3–xBaZrO3–(0.10 - x)(Bi0.5Li0.5)TiO3 ceramics have been synthesized by the conventional solid state reaction method. A phase diagram was summarized from the X-ray diffraction pattern and the dielectric measurements. It is found that 0.90(Na0.5K0.5)NbO3–xBaZrO3–(0.10 - x)(Bi0.5Li0.5)TiO3 ceramics have an MPB between x = 0.07 and 0.08. In the vicinity of the MPB, it was observed that the dielectric and piezoelectric properties were enhanced.
- 20 June 2013
- Published by IOP Publishing in Japanese Journal of Applied Physics
- Vol. 52 (7S) , 07HB02
Formation of Morphotropic Phase Boundary in (Na0.5K0.5)NbO3–BaZrO3–(Bi0.5Li0.5)TiO3 Lead-Free Piezoelectric Ceramics
For the development of lead-free piezoelectric ceramics, which have a tetragonal–rhombohedral morphotropic phase boundary (MPB), 0.90(Na0.5K0.5)NbO3–xBaZrO3–(0.10 - x)(Bi0.5Li0.5)TiO3 ceramics have been synthesized by the conventional solid state reaction method. A phase diagram was summarized from the X-ray diffraction pattern and the dielectric measurements. It is found that 0.90(Na0.5K0.5)NbO3–xBaZrO3–(0.10 - x)(Bi0.5Li0.5)TiO3 ceramics have an MPB between x = 0.07 and 0.08. In the vicinity of the MPB, it was observed that the dielectric and piezoelectric properties were enhanced.
- 1 July 2012
- Published by IOP Publishing in Japanese Journal of Applied Physics
- Vol. 51 (7S) , 07GC01
Effects of Mn Additive on Dielectric and Piezoelectric Properties of (Na0.5K0.5)NbO3–BaZrO3–(Bi0.5K0.5)TiO3Ternary System
- 1 July 2012
- Published by IOP Publishing in Japanese Journal of Applied Physics
- Vol. 51 (7S) , 07GC01
Effects of Mn Additive on Dielectric and Piezoelectric Properties of (Na0.5K0.5)NbO3–BaZrO3–(Bi0.5K0.5)TiO3Ternary System
- 1 September 2011
- Published by IOP Publishing in Japanese Journal of Applied Physics
- Vol. 50 (9S2) , 09ND10
Effects of A-Site Ions on the Phase Transition Temperatures and Dielectric Properties of (1-x)(Na0.5K0.5)NbO3–xAZrO3Solid Solutions
- 1 September 2011
- Published by IOP Publishing in Japanese Journal of Applied Physics
- Vol. 50 (9S2) , 09ND10
Effects of A-Site Ions on the Phase Transition Temperatures and Dielectric Properties of (1-x)(Na0.5K0.5)NbO3–xAZrO3Solid Solutions
- 29 October 2010
- Published by Taylor & Francis in Ferroelectrics
- Vol. 401 (1) , 51-55
Ferroelectricity in NaNbO 3 : Revisited
P-E hysteresis loop was measured for stoichiometric and non-stoichiometric NaNbO3. The untypical applied-field dependence of the hysteresis can be interpreted by the strong pinning effect on the domain reversal. The non-stoichiometry of the sample was found to enhance the pinning effect. It is finally concluded that NaNbO3 is intrinsically ferroelectric.
- 29 October 2010
- Published by Taylor & Francis in Ferroelectrics
- Vol. 401 (1) , 51-55
Ferroelectricity in NaNbO 3 : Revisited
P-E hysteresis loop was measured for stoichiometric and non-stoichiometric NaNbO3. The untypical applied-field dependence of the hysteresis can be interpreted by the strong pinning effect on the domain reversal. The non-stoichiometry of the sample was found to enhance the pinning effect. It is finally concluded that NaNbO3 is intrinsically ferroelectric.