AGAndrea Gommeringer

Andrea Gommeringer

*This is an algorithmically generated author record based on publicly available information.

Current Organizations / Institutes

The organizations/institutes from the scholar's latest article


Andrea Gommeringer has a total of 4 co-authors. Here are the top co-authors by number of shared publications:

  • Frank Kern

    Institute for Ceramic Materials and Technologies (IKMT), University of Stuttgart, Allmandring 7B, 70569 Stuttgart, Germany

    5 shared publications
  • Rainer Gadow

    Institute for Manufacturing Technologies of Ceramic Components and Composites, University Stuttgart, Allmandring 7b, D-70569 Stuttgart, Germany

    2 shared publications
  • Lennart Nölle

    Institute for Manufacturing Technologies of Ceramic Components and Composites (IFKB), University of Stuttgart, Allmandring 7b, D-70569 Stuttgart, Germany

    1 shared publication
  • Maximilian Rapp

    Institute for Manufacturing Technologies of Ceramic Components and Composites, Faculty 7—Engineering Design, Production Engineering and Automotive Engineering, University of Stuttgart, Allmandring 7b, 70569 Stuttgart, Germany

    1 shared publication

Latest Publications

  • Open Access

    Electrical Discharge Machinable Ytterbia Samaria Co-Stabilized Zirconia Tungsten Carbide Composites

    by Maximilian Rapp, Andrea Gommeringer, Frank Kern

    Composite ceramics of stabilizer oxide coated ytterbia-samaria costabilized zirconia (1.5Yb1.5Sm-TZP) and 24–32 vol% of tungsten carbide as an electrically conductive dispersion were manufactured by hot pressing at 1300–1400 °C for 2 h at 60 MPa pressure. The materials were characterized with respect to microstructure, phase composition, mechanical properties and electrical discharge machinability by die sinking. Materials with a nanocomposite microstructure and a strength of up to 1700 MPa were obtained. An attractive toughness of 6–6.5 MPa√m is achieved as 40–50% of the zirconia transformed upon fracture. The materials show fair material removal rates of 1 mm³/min in die sinking. Smooth surfaces indicate a material removal mechanism dominated by melting.


  • Open Access

    Mechanical Properties of 2Y-TZP Fabricated from Detonation Synthesized Powder

    by Frank Kern, Andrea Gommeringer

    Yttria stabilized zirconia (Y-TZP) is frequently used in dental and engineering applications due to its high strength and fracture resistance. In this study, 2Y-TZP samples were manufactured from commercially available powder produced by detonation synthesis. Tests of the mechanical properties exhibited an unusual combination of both very high strength and toughness. The materials show a very weak correlation between toughness and grain size. The transformability, measurable by XRD, cannot explain the high toughness. Fractographic analysis revealed a broad transformation affected zone with secondary cracks and shear bands on the tensile side of bending bars which can be made responsible for the high toughness and non-linear stress–strain curves.


  • Open Access

    Mechanical Properties and Electrical Discharge Machinability of Alumina-10 vol% Zirconia-28 vol% Titanium Nitride Composites

    by Andrea Gommeringer, Frank Kern

    Electrical discharge machinable ceramics provide an alternative machining route independent on the material hardness which enables manufacturing of customized ceramic components. In this study a composite material based on an alumina/zirconia matrix and an electrically conductive titanium nitride dispersion was manufactured by hot pressing and characterized with respect to microstructure, mechanical properties and ED-machinability by die sinking. The composites show a combination of high strength of 700 MPa, hardness of 17–18 GPa and moderate fracture resistance of 4.5–5 MPa√m. With 40 kS/m the electrical conductivity is sufficiently high to ensure ED-machinability.


  • Open Access

    Yttria Ceria Co-Stabilized Zirconia Reinforced with Alumina and Strontium Hexaaluminate

    by Andrea Gommeringer, Lennart Nölle, Frank Kern, Rainer Gadow

    Zirconia materials are frequently used in dental applications due to their excellent strength and their tooth-like aspect. Standard yttria stabilized zirconia (Y-TZP) ceramics suffer, however, from moderate toughness and vulnerability to low-temperature degradation. In this study, 1Y6Ce-TZP materials reinforced with different amounts of alumina and/or strontium hexaaluminate were manufactured by slip casting and pressureless sintering at different temperatures to assess their mechanical properties, microstructure, phase composition, and low-temperature degradation stability. Results show that these materials exhibit a high fracture resistance of 10–12 MPa√m, a bending strength between 700–950 MPa, and a Vickers hardness of 1100–1200 HV10. Strontium hexaaluminate (SA6) precipitates were formed in situ by reaction of alumina and strontium zirconate. Although crack deflection at SA6 platelets was clearly visible, a net toughening was not observed. Accelerated ageing tests at 134 °C/3 bar water vapor pressure showed best results for mixed alumina/SA6 reinforcements and a sintering temperature of 1500 °C. Mehl-Avrami-Johnson plots used to describe the ageing kinetics showed clear indications of different ageing mechanisms due to the introduction of the SA6 phase.


  • Open Access

    Enhanced Mechanical Properties in ED-Machinable Zirconia-Tungsten Carbide Composites with Yttria-Neodymia Co-Stabilized Zirconia Matrix

    by Andrea Gommeringer, Frank Kern, Rainer Gadow

    The electrical discharge machining-process (EDM) is a smart solution to optimize the manufacturing chain of customized and complex shaped ceramic components. To comply with the high requirements for the machine and mold design, it is necessary to improve the mechanical properties of ED-machinable ceramics. In this study, ceramic composites with a tetragonal zirconia matrix and tungsten carbide as electrically conductive dispersion were investigated. To improve the toughness of this high strength material, co-stabilized zirconia coated with yttria and neodymia as dopants were used in the compositions with 1.5/1.5 and 1.75/1.25 mol %. These recipes were compared to commercial 3Y-TZP as a reference matrix material combined with the same WC raw powder. The electrically conductive phase content was varied from 20 to 28 vol %. For all compositions, the ceramic blanks were hot pressed at identical dwell and pressure, but with various sintering temperatures (1300 °C to 1450 °C) and then tested with respect to the mechanical and electrical properties. By variation of the stabilizer system, a significantly higher toughness of up to 11.3 MPa√m compared to 5.3 MPa√m for 3Y-TZP-20WC is achieved while the bending strength stays at a comparable high level of >1500 MPa.