Babette Tonn
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Babette Tonn has a total of 25 co-authors. Here are the top co-authors by number of shared publications:
- Felix Stieler
Institute of Metallurgy, Clausthal Technical University, Clausthal, Germany
2 shared publications A. Esderts
Institute for Plant Engineering and Fatigue Analysis, Clausthal University of Technology, Clausthal-Zellerfeld, Germany
1 shared publication- Bernadette Domengès
Normandie Univ, UNICAEN, ENSICAEN, CNRS, CRISMAT, Caen, France
1 shared publication Daniel Funk
Georg Funk Eisengießerei GmbH & Co. KG, Aalen, Germany
1 shared publicationE. Stolz
Institute for Plant Engineering and Fatigue Analysis, Clausthal University of Technology, Clausthal-Zellerfeld, Germany
1 shared publication- Felix Mori
Department of Foundry Technology, Institute for Metallurgy, Clausthal University of Technology, Clausthal-Zellerfeld, Germany
1 shared publication
Latest Publications
- Open Access
- 23 July 2025
- Published by Springer Nature in International Journal of Metalcasting
- Vol. 20 (3) , 1922-1935
Objective Description of Graphite Morphology in Ductile Cast Iron by Numerical Geometric Parameters
As an innovative evolution of conventional cast iron, solid solution-strengthened ductile iron (SSDI) with its excellent ductility and strength stands out from compared to commonly used standard grades. The spheroidal graphite precipitates in the present metal matrix are produced by a magnesium treatment of the cast iron melt and are decisive for the excellent mechanical properties of the cast material. Deviations of the graphite particles from the spheroidal form, up to degenerations such as chunky graphite, lead to a deterioration of the mechanical properties. The current standards ISO 945-2 and 4 mention nodularity and roundness as important quantities to describe different graphite morphologies. Furthermore, analysis software for graphite description uses probability formulas containing the two-dimensional geometric parameters compactness, convexity, and roundness to distinguish between the different graphite forms I to VI. However, there is no objective description of degenerated graphite, like chunky graphite or exploded graphite. To avoid different interpretations of the same graphite morphology and to provide a more objective analysis, a logistic regression/data-driven approach is suggested. Different two-dimensional geometric parameters are measured to describe each graphite precipitate in a microsection, namely, roundness, convexity, Feret-ratio, nearest-neighbor distance, compactness, graphite particle area A real , and sphericity. The individual geometric parameters are evaluated using a logistic regression model on the basis of their empirical distribution (e.g., mean value, first and third quantile, etc.). The present results show that an objective quantification of the change in graphite morphology toward degeneration is possible using this statistical approach.
- 23 July 2025
- Published by Springer Nature in International Journal of Metalcasting
- Vol. 20 (3) , 1922-1935
Open AccessObjective Description of Graphite Morphology in Ductile Cast Iron by Numerical Geometric Parameters
As an innovative evolution of conventional cast iron, solid solution-strengthened ductile iron (SSDI) with its excellent ductility and strength stands out from compared to commonly used standard grades. The spheroidal graphite precipitates in the present metal matrix are produced by a magnesium treatment of the cast iron melt and are decisive for the excellent mechanical properties of the cast material. Deviations of the graphite particles from the spheroidal form, up to degenerations such as chunky graphite, lead to a deterioration of the mechanical properties. The current standards ISO 945-2 and 4 mention nodularity and roundness as important quantities to describe different graphite morphologies. Furthermore, analysis software for graphite description uses probability formulas containing the two-dimensional geometric parameters compactness, convexity, and roundness to distinguish between the different graphite forms I to VI. However, there is no objective description of degenerated graphite, like chunky graphite or exploded graphite. To avoid different interpretations of the same graphite morphology and to provide a more objective analysis, a logistic regression/data-driven approach is suggested. Different two-dimensional geometric parameters are measured to describe each graphite precipitate in a microsection, namely, roundness, convexity, Feret-ratio, nearest-neighbor distance, compactness, graphite particle area A real , and sphericity. The individual geometric parameters are evaluated using a logistic regression model on the basis of their empirical distribution (e.g., mean value, first and third quantile, etc.). The present results show that an objective quantification of the change in graphite morphology toward degeneration is possible using this statistical approach.
- Open Access
- 29 January 2024
- Published by Springer Nature in International Journal of Metalcasting
- Vol. 18 (3) , 1982-1993
Prediction of Cross-Section-Dependent ADI Microstructures by Experimental Heat Treatment Simulation
Heavy section Austempered Ductile Iron (ADI) components may contain pearlitic or a mixed microstructure (mixture of pearlite and ausferrite) in their centres besides ausferrite. As a result, mechanical properties are not homogeneously distributed across the thicknesses of the components. The oversizing of the components therefore leads to unnecessary material expenses in foundries. In order to avoid the complex manufacturing process of heavy section ADI components and subsequent investigations, preliminary tests were performed with smaller test samples. Here, temperature-time curves were detected during heat treatment at different depths. Material samples of the customised composition were heat treated in a dilatometer under the same heat treatment conditions according to different sections of the cast component. A variation of the quenching rates was conducted to investigate the influence on the mixed microstructure formation and ratio of pearlitic and ausferritic microstructures. A comparison of the conventionally heat-treated and dilatometer produced microstructures proved the successful application for heavy section parts and enables microstructure predictions with small samples only. In this way, there is no requirement of expensive tests with high-mass components.
- 29 January 2024
- Published by Springer Nature in International Journal of Metalcasting
- Vol. 18 (3) , 1982-1993
Open AccessPrediction of Cross-Section-Dependent ADI Microstructures by Experimental Heat Treatment Simulation
Heavy section Austempered Ductile Iron (ADI) components may contain pearlitic or a mixed microstructure (mixture of pearlite and ausferrite) in their centres besides ausferrite. As a result, mechanical properties are not homogeneously distributed across the thicknesses of the components. The oversizing of the components therefore leads to unnecessary material expenses in foundries. In order to avoid the complex manufacturing process of heavy section ADI components and subsequent investigations, preliminary tests were performed with smaller test samples. Here, temperature-time curves were detected during heat treatment at different depths. Material samples of the customised composition were heat treated in a dilatometer under the same heat treatment conditions according to different sections of the cast component. A variation of the quenching rates was conducted to investigate the influence on the mixed microstructure formation and ratio of pearlitic and ausferritic microstructures. A comparison of the conventionally heat-treated and dilatometer produced microstructures proved the successful application for heavy section parts and enables microstructure predictions with small samples only. In this way, there is no requirement of expensive tests with high-mass components.
- Open Access
- 27 December 2023
- Published by Springer Nature in International Journal of Metalcasting
- Vol. 18 (3) , 1926-1934
XRD-Analysis of the Relation of Stacking Fault Formation and the TRIP-Effect in ADI
The mechanical properties of ausferritic ductile iron are strongly influenced by the ability of the austenite to undergo martensite formation. Strain-induced martensite formation occurring under the right circumstances results in transformation induced plasticity (TRIP) that improves ductility and strength. TRIP has been shown to depend on the austenite’s stacking fault energy (SFE), which describes the crystals micromechanical behaviour. In austenitic FeMnAlSi-TRIP steels, TRIP as a reaction to mechanical load only occurs for SFE 2. For carbon-stabilised austenite as in ADI, the relationship between stacking faults, mechanical properties and martensitic transformation has not yet been established. To investigate the TRIP-effect in ADI, unalloyed ADI with 3.43 wt% C, 2.52 wt% Si and 0.21 wt% Mn was ausferritised and subjected to tensile tests at temperatures between −180 °C and 200 °C. The amount of martensite produced by thermal and mechanical activation, crystalline microstrain and stacking fault density were measured on deformed and undeformed regions of the specimen by XRD and the resulting SFE calculated. Between −70 and 20 °C, the elongation at fracture exceeded 10 % compared to below 2 % in the temperature range of −130 to −180 °C. At temperatures above 80 °C, elongation at fracture gradually decreased to 4.5 % at 200 °C. High sample ductility was associated with lower SFEs as low as 35 mJ/m2, indicating a correlation of stacking fault formation and strain-induced martensite formation in ADI.
- 27 December 2023
- Published by Springer Nature in International Journal of Metalcasting
- Vol. 18 (3) , 1926-1934
Open AccessXRD-Analysis of the Relation of Stacking Fault Formation and the TRIP-Effect in ADI
The mechanical properties of ausferritic ductile iron are strongly influenced by the ability of the austenite to undergo martensite formation. Strain-induced martensite formation occurring under the right circumstances results in transformation induced plasticity (TRIP) that improves ductility and strength. TRIP has been shown to depend on the austenite’s stacking fault energy (SFE), which describes the crystals micromechanical behaviour. In austenitic FeMnAlSi-TRIP steels, TRIP as a reaction to mechanical load only occurs for SFE 2. For carbon-stabilised austenite as in ADI, the relationship between stacking faults, mechanical properties and martensitic transformation has not yet been established. To investigate the TRIP-effect in ADI, unalloyed ADI with 3.43 wt% C, 2.52 wt% Si and 0.21 wt% Mn was ausferritised and subjected to tensile tests at temperatures between −180 °C and 200 °C. The amount of martensite produced by thermal and mechanical activation, crystalline microstrain and stacking fault density were measured on deformed and undeformed regions of the specimen by XRD and the resulting SFE calculated. Between −70 and 20 °C, the elongation at fracture exceeded 10 % compared to below 2 % in the temperature range of −130 to −180 °C. At temperatures above 80 °C, elongation at fracture gradually decreased to 4.5 % at 200 °C. High sample ductility was associated with lower SFEs as low as 35 mJ/m2, indicating a correlation of stacking fault formation and strain-induced martensite formation in ADI.
- Open Access
- 9 October 2023
- Published by Elsevier in Results in Materials
- Vol. 20
Fast reactive interdiffusion between solid brass and liquid aluminium
- 9 October 2023
- Published by Elsevier in Results in Materials
- Vol. 20
Open AccessFast reactive interdiffusion between solid brass and liquid aluminium
- Open Access
- 4 September 2022
- Published by Springer Nature in International Journal of Metalcasting
- Vol. 17 (2) , 1315-1325
Alteration of the Graphite Morphology in Solid Solution-Strengthened Ductile Iron Due to High Contents of Cerium and Bismuth
The impact of combined addition of high levels of bismuth up to 120 wt ppm and cerium up to 2000 wt ppm on the graphite morphology in GJS 450-18 with 3.2 wt% carbon and 3.2 wt% silicon was studied. Experiments were conducted with insulated keel blocks with a solidification time of 40 min. Samples from the thermal centre of the castings were analysed by optical microscopy, and the forms and sizes of graphite particles were characterised. Bismuth addition, even at 25 wt ppm, resulted in an altered graphite form in the last-to-freeze regions resembling intercellular lamellar graphite (ILG). Additions of 45 wt ppm or more Ce to these Bi-containing melts prevented the formation of ILG and produced chunky graphite (CHG) instead. ILG did not appear for ratios Bi/Ce > 1.5, while CHG could not be found for ratios Bi/Ce < 0.7. Only one type of graphite degeneration (either ILG or CHG) was present in each sample, thus rendering their formation mutually exclusive. Larger amounts of Ce between 300 and 500 wt ppm resulted in the formation of predominantly graphite form V, while no degenerations could be observed. The addition of Ce to a Bi-contaminated cast iron melt to avoid ILG formation and achieve a regular graphite structure with mainly form VI graphite is not possible. Instead, form V replaces form VI as the predominantly formed morphology. Ce levels higher than 1000 wt ppm resulted in the formation of large areas of undercooled graphite in the last-to-freeze regions regardless of the Bi content in the cast iron melt.
- 4 September 2022
- Published by Springer Nature in International Journal of Metalcasting
- Vol. 17 (2) , 1315-1325
Open AccessAlteration of the Graphite Morphology in Solid Solution-Strengthened Ductile Iron Due to High Contents of Cerium and Bismuth
The impact of combined addition of high levels of bismuth up to 120 wt ppm and cerium up to 2000 wt ppm on the graphite morphology in GJS 450-18 with 3.2 wt% carbon and 3.2 wt% silicon was studied. Experiments were conducted with insulated keel blocks with a solidification time of 40 min. Samples from the thermal centre of the castings were analysed by optical microscopy, and the forms and sizes of graphite particles were characterised. Bismuth addition, even at 25 wt ppm, resulted in an altered graphite form in the last-to-freeze regions resembling intercellular lamellar graphite (ILG). Additions of 45 wt ppm or more Ce to these Bi-containing melts prevented the formation of ILG and produced chunky graphite (CHG) instead. ILG did not appear for ratios Bi/Ce > 1.5, while CHG could not be found for ratios Bi/Ce < 0.7. Only one type of graphite degeneration (either ILG or CHG) was present in each sample, thus rendering their formation mutually exclusive. Larger amounts of Ce between 300 and 500 wt ppm resulted in the formation of predominantly graphite form V, while no degenerations could be observed. The addition of Ce to a Bi-contaminated cast iron melt to avoid ILG formation and achieve a regular graphite structure with mainly form VI graphite is not possible. Instead, form V replaces form VI as the predominantly formed morphology. Ce levels higher than 1000 wt ppm resulted in the formation of large areas of undercooled graphite in the last-to-freeze regions regardless of the Bi content in the cast iron melt.
- Open Access
- 25 February 2020
- Published by Springer Nature in International Journal of Metalcasting
- Vol. 14 (3) , 827-835
Effect of Antimony on Graphite Growth in Ductile Iron
Antimony is used in ductile cast iron melts to avoid graphite degenerations like exploded graphite and chunky graphite. However, the effect of Sb in the melt on the crystallization of ductile cast iron is still unknown, therefore the aim of our investigations. The current study presents thermodynamic calculations showing that at the beginning of the eutectic solidification, Mg3Sb2 is formed. Furthermore, the amount of Sb increases in the austenite and decreases in the remaining melt during solidification. An experiment was conducted, in which a higher amount of Sb than usual was added to a ductile iron melt. In the microstructure of the Sb-containing sample, a higher graphite precipitate count was measured than in the reference sample without Sb. The graphite spheroids of the Sb-containing sample show an almost perfect roundness and a very smooth surface. However, lamellar outgrowths from the graphite spheroids were also observed. Using scanning electron microscopy with energy-dispersive X-ray spectroscopy, it could be shown that Sb-containing phases have been formed, which are located in the pearlitic matrix and also in graphite spheroids. As a result of spectroscopic investigations, it can be assumed that Sb-containing phases act as nucleant for graphite nucleation. Further investigations by Auger electron spectroscopy showed that a thin layer of Sb at the interface between graphite and matrix has been formed. It seems that this layer constricts the diffusion of carbon to the spheroidal graphite and acts as a surfactant favoring a layer-by-layer growth of the graphite spheroids.
- 25 February 2020
- Published by Springer Nature in International Journal of Metalcasting
- Vol. 14 (3) , 827-835
Open AccessEffect of Antimony on Graphite Growth in Ductile Iron
Antimony is used in ductile cast iron melts to avoid graphite degenerations like exploded graphite and chunky graphite. However, the effect of Sb in the melt on the crystallization of ductile cast iron is still unknown, therefore the aim of our investigations. The current study presents thermodynamic calculations showing that at the beginning of the eutectic solidification, Mg3Sb2 is formed. Furthermore, the amount of Sb increases in the austenite and decreases in the remaining melt during solidification. An experiment was conducted, in which a higher amount of Sb than usual was added to a ductile iron melt. In the microstructure of the Sb-containing sample, a higher graphite precipitate count was measured than in the reference sample without Sb. The graphite spheroids of the Sb-containing sample show an almost perfect roundness and a very smooth surface. However, lamellar outgrowths from the graphite spheroids were also observed. Using scanning electron microscopy with energy-dispersive X-ray spectroscopy, it could be shown that Sb-containing phases have been formed, which are located in the pearlitic matrix and also in graphite spheroids. As a result of spectroscopic investigations, it can be assumed that Sb-containing phases act as nucleant for graphite nucleation. Further investigations by Auger electron spectroscopy showed that a thin layer of Sb at the interface between graphite and matrix has been formed. It seems that this layer constricts the diffusion of carbon to the spheroidal graphite and acts as a surfactant favoring a layer-by-layer growth of the graphite spheroids.
- Open Access
- 1 June 2018
- Published by Trans Tech Publications, Ltd. in Materials Science Forum
- Vol. 925, 62-69
Degenerated Graphite Growth in Ductile Iron
As part of a study devoted to the effect of trace elements on graphite degeneracy, near-eutectic ductile iron melts were prepared to which minute amounts of lead and of both lead and cerium were added. The melts were cast into an insulated Y4 mould, giving a solidification time of about 1 hour and a cooling time to room temperature of about 15 hours. In the thermal centre of the Pb containing sample graphite spheroids as well as intergranular lamellar graphite have been found. At the same location of the casting containing both Pb and Ce, exploded as well as chunky graphite could be observed, while the formation of intergranular lamellar graphite has been suppressed. Deep etching of the samples allowed reaching the following conclusions: i) intergranular graphite in the SG-Pb sample often, if not always, originates on graphite nodules and extends towards the last to freeze areas; ii) in one location of the SG-PbCe sample, chunky graphite strings were observed to originate on an exploded nodule, thus confirming the close relationship between these two forms of graphite. Because of the over-treatment in cerium of the SG-PbCe sample, other unusual degenerate graphite was observed which appears as coarse aggregates of "porous" graphite after deep etching.
- 1 June 2018
- Published by Trans Tech Publications, Ltd. in Materials Science Forum
- Vol. 925, 62-69
Open AccessDegenerated Graphite Growth in Ductile Iron
As part of a study devoted to the effect of trace elements on graphite degeneracy, near-eutectic ductile iron melts were prepared to which minute amounts of lead and of both lead and cerium were added. The melts were cast into an insulated Y4 mould, giving a solidification time of about 1 hour and a cooling time to room temperature of about 15 hours. In the thermal centre of the Pb containing sample graphite spheroids as well as intergranular lamellar graphite have been found. At the same location of the casting containing both Pb and Ce, exploded as well as chunky graphite could be observed, while the formation of intergranular lamellar graphite has been suppressed. Deep etching of the samples allowed reaching the following conclusions: i) intergranular graphite in the SG-Pb sample often, if not always, originates on graphite nodules and extends towards the last to freeze areas; ii) in one location of the SG-PbCe sample, chunky graphite strings were observed to originate on an exploded nodule, thus confirming the close relationship between these two forms of graphite. Because of the over-treatment in cerium of the SG-PbCe sample, other unusual degenerate graphite was observed which appears as coarse aggregates of "porous" graphite after deep etching.
- 10 February 2016
- Published by Maney Publishing in International Journal of Cast Metals Research
- Vol. 29 (1-2) , 85-91
Occurrence and behaviour of Mo containing precipitates in nodular cast iron at high temperatures
In nodular cast iron, molybdenum is alloyed in the range of 0.5 to 1.5 wt.-% to increase the mechanical properties for high temperature application, especially for thick walled castings like housings of gas or steam turbines. The behaviour of Mo precipitates in the as cast state as well as under long exposure to heat was the object of this investigation. In the as cast state, Mo forms metastable carbidic grain boundary precipitates with iron, silicon and carbon. These transform into stable MoC precipitates during sustained temperature influence. Furthermore, there are finely dispersed Mo containing precipitates found in the matrix. These increase the high temperature strength of Mo alloyed cast iron due to the Orowan mechanism and the occurrence of additional grain boundaries. However, it has been shown that these Mo containing precipitates underlie Ostwald ripening under continuous heat exposure, and a precipitate free area occurs along the ferritic grain boundary.
- 10 February 2016
- Published by Maney Publishing in International Journal of Cast Metals Research
- Vol. 29 (1-2) , 85-91
Occurrence and behaviour of Mo containing precipitates in nodular cast iron at high temperatures
In nodular cast iron, molybdenum is alloyed in the range of 0.5 to 1.5 wt.-% to increase the mechanical properties for high temperature application, especially for thick walled castings like housings of gas or steam turbines. The behaviour of Mo precipitates in the as cast state as well as under long exposure to heat was the object of this investigation. In the as cast state, Mo forms metastable carbidic grain boundary precipitates with iron, silicon and carbon. These transform into stable MoC precipitates during sustained temperature influence. Furthermore, there are finely dispersed Mo containing precipitates found in the matrix. These increase the high temperature strength of Mo alloyed cast iron due to the Orowan mechanism and the occurrence of additional grain boundaries. However, it has been shown that these Mo containing precipitates underlie Ostwald ripening under continuous heat exposure, and a precipitate free area occurs along the ferritic grain boundary.