Deepan Bharathi Kannan Thangaraju
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Previous Organizations / Institutes
The organizations / institutes from the scholar's other articles in the past ten years
Deepan Bharathi Kannan Thangaraju has a total of 30 co-authors. Here are the top co-authors by number of shared publications:
Rudra Mahadev
College of Engineering Guindy, Anna University
3 shared publicationsKaviamudhan Venkateshkumar
College of Engineering Guindy, Anna University
2 shared publicationsR. Manoj Samson
SRM Institute of Science and Technology
2 shared publicationsRahul Manoj Nellanickal
College of Engineering Guindy, Anna University
2 shared publicationsSrinath Selvaperumal
Department of Mechanical Engineering SRM Institute of Science and Technology Kattankulathur Chengalpattu District Tamilnadu 603203 India
2 shared publicationsAjay Amirtharaj P
Department of Mechanical Engineering, College of Engineering Guindy, Anna University, Chennai, India
1 shared publication
Latest Publications
- 16 December 2025
- Published by Springer Nature in Journal of Materials Engineering and Performance
- Vol. 35 (19) , 19390-19411
Comparative Study of Metal Inert Gas Welding Modes on 15CDV6 Steel for Aerospace Structural Applications
- 16 December 2025
- Published by Springer Nature in Journal of Materials Engineering and Performance
- Vol. 35 (19) , 19390-19411
Comparative Study of Metal Inert Gas Welding Modes on 15CDV6 Steel for Aerospace Structural Applications
- 2 December 2025
- Published by Wiley in Steel Research International
- Vol. 97 (6) , 3040-3061
The Effect of Novel Double Pulse Metal Inert Gas Welding on Microstructure and Mechanical Properties of P91 Steel
This study investigates the joining of P91 steel plates using conventional metal inert gas (MIG) and double pulse (DP)‐MIG welding, focusing on the effect of pulse frequency on weld quality by measuring bead geometry, hardness, tensile, and impact strength. The conventional MIG weldment exhibits inferior mechanical properties, with an ultimate tensile strength (UTS) of 270 MPa (44% of base metal strength). Microstructural analysis reveals a coarse columnar structure with large prior austenite grains (PAGs), extensive δ‐ferrite, and severe precipitate coarsening. Energy dispersive spectroscopy confirms significant elemental segregation, resulting in a high peak hardness of ≈480 HV. Electron backscatter diffraction (EBSD) analysis quantifies its poor integrity, showing elevated residual strain and a low fraction of crack‐resistant high‐angle grain boundaries. In contrast, the optimized 8 Hz DP‐MIG process produced a vastly superior weldment with an UTS of 535 MPa (85% of base metal strength), a controlled peak hardness of ≈450 HV, and the highest impact toughness of 20 J. This performance is attributed to exceptional microstructural refinement with fine, equiaxed PAGs and suppressed δ‐ferrite. EBSD analysis validates this superiority, showing minimal residual strain and high HAGB density of 77.6%, which enhances crack propagation resistance.
- 2 December 2025
- Published by Wiley in Steel Research International
- Vol. 97 (6) , 3040-3061
The Effect of Novel Double Pulse Metal Inert Gas Welding on Microstructure and Mechanical Properties of P91 Steel
This study investigates the joining of P91 steel plates using conventional metal inert gas (MIG) and double pulse (DP)‐MIG welding, focusing on the effect of pulse frequency on weld quality by measuring bead geometry, hardness, tensile, and impact strength. The conventional MIG weldment exhibits inferior mechanical properties, with an ultimate tensile strength (UTS) of 270 MPa (44% of base metal strength). Microstructural analysis reveals a coarse columnar structure with large prior austenite grains (PAGs), extensive δ‐ferrite, and severe precipitate coarsening. Energy dispersive spectroscopy confirms significant elemental segregation, resulting in a high peak hardness of ≈480 HV. Electron backscatter diffraction (EBSD) analysis quantifies its poor integrity, showing elevated residual strain and a low fraction of crack‐resistant high‐angle grain boundaries. In contrast, the optimized 8 Hz DP‐MIG process produced a vastly superior weldment with an UTS of 535 MPa (85% of base metal strength), a controlled peak hardness of ≈450 HV, and the highest impact toughness of 20 J. This performance is attributed to exceptional microstructural refinement with fine, equiaxed PAGs and suppressed δ‐ferrite. EBSD analysis validates this superiority, showing minimal residual strain and high HAGB density of 77.6%, which enhances crack propagation resistance.
- 9 June 2025
- Published by SAGE Publications in Proceedings of the Institution of Mechanical Engineers, Part E: Journal of Process Mechanical Engineering
- Vol. 240 (6) , 6650-6656
Optimization and metallurgical characterization of double-pulse metal inert gas welded P91 steel
The principal aim of this research was to optimize the welding parameters in the double-pulse metal inert gas welding of P91 alloy steel. Welding was carried out using a P91 filler wire of 1.2 mm diameter. The plates were welded in butt joint configuration and all trials were conducted in accordance with the L9 Taguchi array. Welding parameters such as wire feed speed, frequency, and amplitude were considered for controlling weld quality. Bead geometry, tensile strength, impact strength, and hardness were the factors considered for studying the weld characteristics. The technique for order preference by similarity to an ideal solution multi-objective function was used to identify the best welding parameter combination. Electron backscatter diffraction analysis was also done on the weld and it was observed that the optimized weld (sample 6) had a higher percentage (22.8%) of high-angle grain boundaries: > 15° than the weld (sample 7) that had the least favorable properties (16.8%). A greater percentage of high-angle grain boundaries imparts higher strength and hardness as they act as barriers to dislocation motion. On comparing the mechanical characteristics (which were heavily influenced by the microstructure) of samples 6 and 7, it was found that sample 6 had a much higher toughness value of 48 J as opposed to 8 J for sample 7. The bead width of sample 6 was also lower by a factor of 42.5%. Although both the hardness and tensile strength were reported to be lower for sample 6 (by 3.86% and 20.34%, respectively), the overall characteristics of weld sample 6 were more closely aligned with boiler application requirements.
- 9 June 2025
- Published by SAGE Publications in Proceedings of the Institution of Mechanical Engineers, Part E: Journal of Process Mechanical Engineering
- Vol. 240 (6) , 6650-6656
Optimization and metallurgical characterization of double-pulse metal inert gas welded P91 steel
The principal aim of this research was to optimize the welding parameters in the double-pulse metal inert gas welding of P91 alloy steel. Welding was carried out using a P91 filler wire of 1.2 mm diameter. The plates were welded in butt joint configuration and all trials were conducted in accordance with the L9 Taguchi array. Welding parameters such as wire feed speed, frequency, and amplitude were considered for controlling weld quality. Bead geometry, tensile strength, impact strength, and hardness were the factors considered for studying the weld characteristics. The technique for order preference by similarity to an ideal solution multi-objective function was used to identify the best welding parameter combination. Electron backscatter diffraction analysis was also done on the weld and it was observed that the optimized weld (sample 6) had a higher percentage (22.8%) of high-angle grain boundaries: > 15° than the weld (sample 7) that had the least favorable properties (16.8%). A greater percentage of high-angle grain boundaries imparts higher strength and hardness as they act as barriers to dislocation motion. On comparing the mechanical characteristics (which were heavily influenced by the microstructure) of samples 6 and 7, it was found that sample 6 had a much higher toughness value of 48 J as opposed to 8 J for sample 7. The bead width of sample 6 was also lower by a factor of 42.5%. Although both the hardness and tensile strength were reported to be lower for sample 6 (by 3.86% and 20.34%, respectively), the overall characteristics of weld sample 6 were more closely aligned with boiler application requirements.
- 23 April 2025
- Published by Wiley in Steel Research International
- Vol. 96 (11) , 243-255
Effect of Different Shielding Gases on the Metallurgical and Mechanical Properties of Double‐Pulse Metal Inert Gas‐Welded SS 304H
This study seeks to analyze the impact of various shielding gas compositions on the mechanical properties of stainless steel 304 H plates joined using the double pulse metal inert gas process. The investigation focuses on three shielding gases—100% CO 2 , 100% argon, and a mixture of 80% argon with 20% CO 2 —and their influence on the overall weld quality. Depth of penetration, bead width, tensile strength (TS), and impact toughness, are used to assess weld quality. Microstructural analysis is done using electron backscatter diffraction (EBSD), scanning electron microscopy, and energy dispersive spectroscopy. The study reveals that using 100% CO 2 as the shielding gas results in a significant increase in TS, ≈21% higher than the base material. The microstructures at the weld centers and interfaces exhibit a combination of columnar dendrites and equiaxed grains. EBSD analysis indicates a high percentage of high‐angle grain boundaries in the weld center, interface, and heat‐affected zone. It is also noted that, irrespective of the shielding gases used, the ferrite fractions in the welds are restricted to below 5%.
- 23 April 2025
- Published by Wiley in Steel Research International
- Vol. 96 (11) , 243-255
Effect of Different Shielding Gases on the Metallurgical and Mechanical Properties of Double‐Pulse Metal Inert Gas‐Welded SS 304H
This study seeks to analyze the impact of various shielding gas compositions on the mechanical properties of stainless steel 304 H plates joined using the double pulse metal inert gas process. The investigation focuses on three shielding gases—100% CO 2 , 100% argon, and a mixture of 80% argon with 20% CO 2 —and their influence on the overall weld quality. Depth of penetration, bead width, tensile strength (TS), and impact toughness, are used to assess weld quality. Microstructural analysis is done using electron backscatter diffraction (EBSD), scanning electron microscopy, and energy dispersive spectroscopy. The study reveals that using 100% CO 2 as the shielding gas results in a significant increase in TS, ≈21% higher than the base material. The microstructures at the weld centers and interfaces exhibit a combination of columnar dendrites and equiaxed grains. EBSD analysis indicates a high percentage of high‐angle grain boundaries in the weld center, interface, and heat‐affected zone. It is also noted that, irrespective of the shielding gases used, the ferrite fractions in the welds are restricted to below 5%.
- 27 December 2024
- Published by Wiley in Steel Research International
- Vol. 96 (7)
Optimization of Welding Parameters in Double‐Pulse Metal Inert Gas Welding of 15CDV6 High‐Strength Low‐Alloy Steel for Fabrication of Critical Rocket Components
In this work, an attempt is made to find out the optimized weld parameters in double‐pulse metal inert gas‐welded 15CDV6 high‐strength low‐alloy steel. Three parameters namely wire feed speed, pulse frequency, and amplitude were varied and the weld quality was assessed based on bead width, depth of penetration, and tensile strength. Best and worst weld parameter combinations were identified using Technique for Order of Preference by similarity to ideal solution optimisation technique. Weld obtained through optimised parameter combination had a tensile strength of 867.28 MPa and the weld obtained through worst weld parameter combination had a tensile strength of 212.21 MPa. Compared to the base metal, the best weld had 21% higher tensile strength, and the worst weld had 65% lower tensile strength. A higher percentage of martensite in the microstructure of the best weld played a major role in achieving a high value of tensile strength. The best weld also had lower percentage of ferrite in both the heat‐affected zone and the weld zone compared to the worst weld. Best weld also had a lower percentage of high strain regions than the worst weld as indicated by electron backscatter diffraction results.
- 27 December 2024
- Published by Wiley in Steel Research International
- Vol. 96 (7)
Optimization of Welding Parameters in Double‐Pulse Metal Inert Gas Welding of 15CDV6 High‐Strength Low‐Alloy Steel for Fabrication of Critical Rocket Components
In this work, an attempt is made to find out the optimized weld parameters in double‐pulse metal inert gas‐welded 15CDV6 high‐strength low‐alloy steel. Three parameters namely wire feed speed, pulse frequency, and amplitude were varied and the weld quality was assessed based on bead width, depth of penetration, and tensile strength. Best and worst weld parameter combinations were identified using Technique for Order of Preference by similarity to ideal solution optimisation technique. Weld obtained through optimised parameter combination had a tensile strength of 867.28 MPa and the weld obtained through worst weld parameter combination had a tensile strength of 212.21 MPa. Compared to the base metal, the best weld had 21% higher tensile strength, and the worst weld had 65% lower tensile strength. A higher percentage of martensite in the microstructure of the best weld played a major role in achieving a high value of tensile strength. The best weld also had lower percentage of ferrite in both the heat‐affected zone and the weld zone compared to the worst weld. Best weld also had a lower percentage of high strain regions than the worst weld as indicated by electron backscatter diffraction results.
- 25 July 2024
- Published by SAGE Publications in Proceedings of the Institution of Mechanical Engineers, Part E: Journal of Process Mechanical Engineering
- Vol. 239 (6) , 3708-3716
Effect of heat input on the mechanical and metallurgical aspects of double-pulse MIG welded IN 617
In this article, an attempt is made to analyze the influence of heat input in double-pulse metal inert gas (DP MIG) welding of Inconel 617 (IN 617). IN 617 plates were joined in the butt joint configuration with 1.2 mm diameter IN 617 filler wire. Three welding trials were conducted at different heat input, viz. 31.3, 37.1, and 41.5 J/mm. Weld quality was assessed using bead geometry, tensile strength, toughness, and hardness. The changes in mechanical properties were discussed using the optical microscope, scanning electron microscope with energy dispersion spectroscopy, and backscattered energy diffraction. Substantial changes were observed in the weld tensile strength for a small variation in heat input. Molybdenum segregation was observed in all the weld samples. At lower heat input, the tensile test was reduced by 31.62% compared with base metal. Similarly, for the medium and high heat input, the tensile strength was reduced by 25.13% and 49.59%, respectively. Weld had lower toughness compared with the base metal and no significant variation was observed in toughness to changes in heat input. Hardness of the weld at all three heat inputs was almost similar to base metal. Liquation cracks were seen in the partially melted zone. At higher heat input, the lack of sidewall fusion was observed along with liquation crack.
- 25 July 2024
- Published by SAGE Publications in Proceedings of the Institution of Mechanical Engineers, Part E: Journal of Process Mechanical Engineering
- Vol. 239 (6) , 3708-3716
Effect of heat input on the mechanical and metallurgical aspects of double-pulse MIG welded IN 617
In this article, an attempt is made to analyze the influence of heat input in double-pulse metal inert gas (DP MIG) welding of Inconel 617 (IN 617). IN 617 plates were joined in the butt joint configuration with 1.2 mm diameter IN 617 filler wire. Three welding trials were conducted at different heat input, viz. 31.3, 37.1, and 41.5 J/mm. Weld quality was assessed using bead geometry, tensile strength, toughness, and hardness. The changes in mechanical properties were discussed using the optical microscope, scanning electron microscope with energy dispersion spectroscopy, and backscattered energy diffraction. Substantial changes were observed in the weld tensile strength for a small variation in heat input. Molybdenum segregation was observed in all the weld samples. At lower heat input, the tensile test was reduced by 31.62% compared with base metal. Similarly, for the medium and high heat input, the tensile strength was reduced by 25.13% and 49.59%, respectively. Weld had lower toughness compared with the base metal and no significant variation was observed in toughness to changes in heat input. Hardness of the weld at all three heat inputs was almost similar to base metal. Liquation cracks were seen in the partially melted zone. At higher heat input, the lack of sidewall fusion was observed along with liquation crack.
- 7 February 2024
- Published by SAGE Publications in Proceedings of the Institution of Mechanical Engineers, Part E: Journal of Process Mechanical Engineering
- Vol. 238 (3) , 1449-1461
The effect of heat input on weld-bead geometry, mechanical, phase transformation temperature, and corrosion properties of autogenous double pulse TIG welded nitinol sheets
This research aims to analyze the welding of 1 mm thick NiTinol sheets using an autogenous double pulse tungsten inert gas (DPTIG) welding process. The effect of heat input (HI) on bead geometry, microstructure, hardness, tensile strength, phase transformation temperature (PTT), and corrosion behavior was studied. The lower (111.25 J/mm), and higher (120.14 J/mm) HI produced an average grain size of 26 μm and 36 μm, respectively. The microstructure of the fusion zone (FZ) had coarser columnar grains with intermetallic phases such as Ni 3 Ti, and TiO 2 . The grain size in the FZ increased with the increase in HI. Sample P (111.25 J/mm) showed a higher hardness of 280.54 HV and tensile strength of 566 MPa due to a higher proportion of austenite phase (99.4%), the smaller grain size of 26 µm, a larger fraction of high angle grain boundary (HAGB) of 75.8%, and higher kernel average misorientation (KAM) value of 4.93. Compared to base metal (BM), sample P (111.25 J/mm), and sample S (120.14 J/mm) exhibited a reduction in tensile strength of 19.14% and 32.29%, respectively. The decline in hardness and tensile strength was attributed to the formation of intermetallic phases, a decrease in the Ti/Ni ratio, coarser grain formation, and a decrease in HAGB fraction and KAM values. The fractured tensile samples showed a mixed mode of fracture with dimples and cleavage facets. Compared to BM, Sample Q (118.05 J/mm) exhibited lesser variation in temperature hysteresis values for austenite and martensite temperatures, with a deviation of 0.4°C and 3.1°C, respectively. All the welded samples had better corrosion behavior than the BM due to a higher Ti/Ni ratio.
- 7 February 2024
- Published by SAGE Publications in Proceedings of the Institution of Mechanical Engineers, Part E: Journal of Process Mechanical Engineering
- Vol. 238 (3) , 1449-1461
The effect of heat input on weld-bead geometry, mechanical, phase transformation temperature, and corrosion properties of autogenous double pulse TIG welded nitinol sheets
This research aims to analyze the welding of 1 mm thick NiTinol sheets using an autogenous double pulse tungsten inert gas (DPTIG) welding process. The effect of heat input (HI) on bead geometry, microstructure, hardness, tensile strength, phase transformation temperature (PTT), and corrosion behavior was studied. The lower (111.25 J/mm), and higher (120.14 J/mm) HI produced an average grain size of 26 μm and 36 μm, respectively. The microstructure of the fusion zone (FZ) had coarser columnar grains with intermetallic phases such as Ni 3 Ti, and TiO 2 . The grain size in the FZ increased with the increase in HI. Sample P (111.25 J/mm) showed a higher hardness of 280.54 HV and tensile strength of 566 MPa due to a higher proportion of austenite phase (99.4%), the smaller grain size of 26 µm, a larger fraction of high angle grain boundary (HAGB) of 75.8%, and higher kernel average misorientation (KAM) value of 4.93. Compared to base metal (BM), sample P (111.25 J/mm), and sample S (120.14 J/mm) exhibited a reduction in tensile strength of 19.14% and 32.29%, respectively. The decline in hardness and tensile strength was attributed to the formation of intermetallic phases, a decrease in the Ti/Ni ratio, coarser grain formation, and a decrease in HAGB fraction and KAM values. The fractured tensile samples showed a mixed mode of fracture with dimples and cleavage facets. Compared to BM, Sample Q (118.05 J/mm) exhibited lesser variation in temperature hysteresis values for austenite and martensite temperatures, with a deviation of 0.4°C and 3.1°C, respectively. All the welded samples had better corrosion behavior than the BM due to a higher Ti/Ni ratio.
- 16 August 2023
- Published by Springer Nature in Transactions of the Indian Institute of Metals
- Vol. 77 (1) , 105-117
Experimental Investigation on Single Pulse MIG Welding of Inconel 617
- 16 August 2023
- Published by Springer Nature in Transactions of the Indian Institute of Metals
- Vol. 77 (1) , 105-117
Experimental Investigation on Single Pulse MIG Welding of Inconel 617
- 7 March 2023
- Published by Taylor & Francis in Advances in Materials and Processing Technologies
- Vol. 10 (2) , 1182-1206
MECHANICAL AND METALLURGICAL CHARACTERISATION OF DOUBLE PULSE MIG WELDED IN 617- SS 304 H
This work attempts to study the mechanical and metallurgical properties of dissimilar welded IN (Inconel) 617-SS (Stainless steel) 304 H plates. Welding was carried out using the Double Pulse MIG Welding Process (DP-MIG) with two different heat inputs, namely 412 J/mm and 452 J/mm. The presence of chromium-rich carbides Cr23C6 helped in strengthening the weld. The tensile strength of the weld made at 452 J/mm was 22% more than that of the weld made at 412 J/mm. Similarly, the weld hardness at 452 J/mm was 8% greater than the weld strength at 412 J/mm. The impact strength did not change significantly with respect to the heat input. Weld made at lower heat input (412 J/mm) had a lack of sidewall fusion. Lower frequency and amplitude contributed to poor heat distribution, leading to a lack of sidewall fusion.
- 7 March 2023
- Published by Taylor & Francis in Advances in Materials and Processing Technologies
- Vol. 10 (2) , 1182-1206
MECHANICAL AND METALLURGICAL CHARACTERISATION OF DOUBLE PULSE MIG WELDED IN 617- SS 304 H
This work attempts to study the mechanical and metallurgical properties of dissimilar welded IN (Inconel) 617-SS (Stainless steel) 304 H plates. Welding was carried out using the Double Pulse MIG Welding Process (DP-MIG) with two different heat inputs, namely 412 J/mm and 452 J/mm. The presence of chromium-rich carbides Cr23C6 helped in strengthening the weld. The tensile strength of the weld made at 452 J/mm was 22% more than that of the weld made at 412 J/mm. Similarly, the weld hardness at 452 J/mm was 8% greater than the weld strength at 412 J/mm. The impact strength did not change significantly with respect to the heat input. Weld made at lower heat input (412 J/mm) had a lack of sidewall fusion. Lower frequency and amplitude contributed to poor heat distribution, leading to a lack of sidewall fusion.
- 17 November 2022
- Published by SAGE Publications in Proceedings of the Institution of Mechanical Engineers, Part E: Journal of Process Mechanical Engineering
- Vol. 238 (1) , 171-179
Experimental studies and optimization of process parameters in laser welding of stainless steel 304 H
The prime objective of this work is to find the best combination of parameters in laser welding of stainless-steel 304 H plates. CO 2 laser welding was used to join 5 mm thick stainless-steel 304 H plates. Laser power, welding speed, and focal position were used as input parameters, and experiments were conducted on the basis of the Taguchi L27 matrix. The quality of the weld was analysed by measuring depth of penetration, bead width and hardness. The best parameter combination was found using artificial neural network and genetic algorithm. The Levenberg–Marquardt algorithm predicted output responses more accurately. A confirmatory test was carried out for the optimized parameters identified by the genetic algorithm. The percentage error between the experimental and predicted genetic algorithm values was below 6%. In comparison to the base metal, the optimized weld hardness was increased by 8%. The electron backscatter diffraction analysis of the optimized weld revealed the presence of a higher percentage of high-angle grain boundary than low-angle grain boundary.
- 17 November 2022
- Published by SAGE Publications in Proceedings of the Institution of Mechanical Engineers, Part E: Journal of Process Mechanical Engineering
- Vol. 238 (1) , 171-179
Experimental studies and optimization of process parameters in laser welding of stainless steel 304 H
The prime objective of this work is to find the best combination of parameters in laser welding of stainless-steel 304 H plates. CO 2 laser welding was used to join 5 mm thick stainless-steel 304 H plates. Laser power, welding speed, and focal position were used as input parameters, and experiments were conducted on the basis of the Taguchi L27 matrix. The quality of the weld was analysed by measuring depth of penetration, bead width and hardness. The best parameter combination was found using artificial neural network and genetic algorithm. The Levenberg–Marquardt algorithm predicted output responses more accurately. A confirmatory test was carried out for the optimized parameters identified by the genetic algorithm. The percentage error between the experimental and predicted genetic algorithm values was below 6%. In comparison to the base metal, the optimized weld hardness was increased by 8%. The electron backscatter diffraction analysis of the optimized weld revealed the presence of a higher percentage of high-angle grain boundary than low-angle grain boundary.