Yang Peng
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Research Subjects
Yang Peng has a total of 11 co-authors. Here are the top co-authors by number of shared publications:
- Wei Ding
School of Resources and Environmental Engineering, Wuhan University of Technology, Wuhan 430070, China
7 shared publications - Junhui Xiao
School of Environment and Resource, Southwest University of Science and Technology, Mianyang, China
6 shared publications - Kai Zou
Institute of Multipurpose Utilization of Mineral Resource, Chinese Academy of Geological Sciences, Chengdu 610041, China
5 shared publications - Tao Chen
Sichuan Provincial Engineering Lab of NonMetallic Mineral Powder Modification and High-Value Utilization, Southwest University of Science and Technology, Mianyang 621010, China
5 shared publications - Zhen Wang
Key Laboratory of Solid Waste Treatment and Resource Recycle Ministry of Education, Southwest University of Science and Technology, Mianyang 621010, China
3 shared publications - Chao Chen
Sichuan Provincial Engineering Lab of Non-Metallic Mineral Powder Modification and High-Value Utilization, Southwest University of Science and Technology, Mianyang 621010, China
1 shared publication
Latest Publications
- Open Access
- 28 July 2020
- Published by MDPI AG in Applied Sciences
- Vol. 10 (15) , 5174
Preparing High-Purity Anhydrous ScCl3 Molten Salt Using One-Step Rapid Heating Process
In this study, a one-step rapid heating novel process was used to prepare high-purity anhydrous scandium chloride molten salt with low-purity scandium oxide. High-purity anhydrous ScCl3 molten salt was used as the Sc-bearing raw material for preparing the Sc-bearing master alloy. Inert gas was used to enhance the purity of anhydrous scandium chloride and reduce the hydrolysis rate of scandium. The results show that high-purity scandium chloride (purity, 99.69%) with the scandium content of 29.61%, was obtained, and the hydrolysis rate of scandium was 1.19% under the conditions used: removing ammonium chloride; residual crystal water temperature of 400 °C; m(Sc2O3):m(NH4Cl) = 1:2.5; holding-time of 90 min; heating-rate of 12 °C/min; and argon flow of 7.5 L/min. XRD, SEM, and EPMA analyses further verified that anhydrous scandium chloride crystallization condition was relatively good and the purity of high-purity anhydrous scandium chloride approached the theory purity of anhydrous scandium chloride.
- 28 July 2020
- Published by MDPI AG in Applied Sciences
- Vol. 10 (15) , 5174
Open AccessPreparing High-Purity Anhydrous ScCl3 Molten Salt Using One-Step Rapid Heating Process
In this study, a one-step rapid heating novel process was used to prepare high-purity anhydrous scandium chloride molten salt with low-purity scandium oxide. High-purity anhydrous ScCl3 molten salt was used as the Sc-bearing raw material for preparing the Sc-bearing master alloy. Inert gas was used to enhance the purity of anhydrous scandium chloride and reduce the hydrolysis rate of scandium. The results show that high-purity scandium chloride (purity, 99.69%) with the scandium content of 29.61%, was obtained, and the hydrolysis rate of scandium was 1.19% under the conditions used: removing ammonium chloride; residual crystal water temperature of 400 °C; m(Sc2O3):m(NH4Cl) = 1:2.5; holding-time of 90 min; heating-rate of 12 °C/min; and argon flow of 7.5 L/min. XRD, SEM, and EPMA analyses further verified that anhydrous scandium chloride crystallization condition was relatively good and the purity of high-purity anhydrous scandium chloride approached the theory purity of anhydrous scandium chloride.
- Open Access
Extraction of Phosphorous from a Phosphorous-Containing Vanadium Titano-Magnetite Tailings by Direct Flotation
In this study, there is 1.42% P2O5 in the P-containing V-Ti magnetite tailings in Miyi Region of China, with the valuable minerals mainly including apatite, and aluminosilicate minerals as the main gangue components. The direction flotation process was used to recover phosphorous from the low-grade phosphorous-bearing V-Ti magnetite tailings. The results showed that an optimized phosphorous concentrate with a P2O5 grade of 31.35% and P2O5 recovery of 88.02% was obtained by flotation process of one roughing, three scavengings, and three cleanings under roughing conditions, which employed pulp pH of 9, grinding fineness of <0.039 mm occupying 90%, flotation concentration of 25%, and dosages of carboxymethylcellulose, oxidized paraffin wax soap, and pine oil of 400 g/t, 300 g/t, and 20 g/t, respectively. Optimized one scavenging, two scavenging, and three scavenging conditions used a pulp pH of 9, and dosages of carboxymethylcellulose, oxidized paraffin wax soap, and pine oil of 200 g/t, 150 g/t, 10 g/t; 100 g/t, 75 g/t, and 5 g/t; and 100 g/t, 75 g/t, and 5 g/t, respectively. Optimized one cleaning, two cleaning, and three cleaning condition dosages of carboxymethylcellulose of 100 g/t, 50 g/t, and 25 g/t, respectively. Study of analysis and characterization of phosphorous concentrate by X-ray diffraction (XRD), scanning electron microscopy (SEM), and energy dispersive spectroscopy (EDS) show that most gangue minerals enter the flotation tailings, the main minerals in phosphorous concentrate are apatite, olivine, and feldspar.
Open AccessExtraction of Phosphorous from a Phosphorous-Containing Vanadium Titano-Magnetite Tailings by Direct Flotation
In this study, there is 1.42% P2O5 in the P-containing V-Ti magnetite tailings in Miyi Region of China, with the valuable minerals mainly including apatite, and aluminosilicate minerals as the main gangue components. The direction flotation process was used to recover phosphorous from the low-grade phosphorous-bearing V-Ti magnetite tailings. The results showed that an optimized phosphorous concentrate with a P2O5 grade of 31.35% and P2O5 recovery of 88.02% was obtained by flotation process of one roughing, three scavengings, and three cleanings under roughing conditions, which employed pulp pH of 9, grinding fineness of <0.039 mm occupying 90%, flotation concentration of 25%, and dosages of carboxymethylcellulose, oxidized paraffin wax soap, and pine oil of 400 g/t, 300 g/t, and 20 g/t, respectively. Optimized one scavenging, two scavenging, and three scavenging conditions used a pulp pH of 9, and dosages of carboxymethylcellulose, oxidized paraffin wax soap, and pine oil of 200 g/t, 150 g/t, 10 g/t; 100 g/t, 75 g/t, and 5 g/t; and 100 g/t, 75 g/t, and 5 g/t, respectively. Optimized one cleaning, two cleaning, and three cleaning condition dosages of carboxymethylcellulose of 100 g/t, 50 g/t, and 25 g/t, respectively. Study of analysis and characterization of phosphorous concentrate by X-ray diffraction (XRD), scanning electron microscopy (SEM), and energy dispersive spectroscopy (EDS) show that most gangue minerals enter the flotation tailings, the main minerals in phosphorous concentrate are apatite, olivine, and feldspar.
- Open Access
Preparing Sc-Bearing Master Alloy Using Aluminum–Magnesium Thermoreduction Method
In this study, preparation of Al–Mg–Sc master alloy tests were carried out by Al–Mg thermoreduction method. Stirring by blowing argon and pressing with molten salt jar were adopted to reduce scandium segregation and upgrading scandium recovery of scandium-bearing master alloy. The results show that the Al–Mg–Sc master alloy ingot contained 2.90% Sc, 5.73% Mg, 0.0058% Cu, 0.29%, 0.029% Ti, 0.13% Fe, 0.075% Zn, 0.025% Na, and 96.72% recovered scandium obtained under the comprehensive conditions used: m(Al): m(Mg): m(ScCl3) = 10:1:1.5, stirring speed of eight rpm, reduction temperature of 1223 K, reduction time of 40 min. The experimental results are in agreement with the thermodynamic predictions, and Al–Mg–Sc master alloy indicator was ideal.
Open AccessPreparing Sc-Bearing Master Alloy Using Aluminum–Magnesium Thermoreduction Method
In this study, preparation of Al–Mg–Sc master alloy tests were carried out by Al–Mg thermoreduction method. Stirring by blowing argon and pressing with molten salt jar were adopted to reduce scandium segregation and upgrading scandium recovery of scandium-bearing master alloy. The results show that the Al–Mg–Sc master alloy ingot contained 2.90% Sc, 5.73% Mg, 0.0058% Cu, 0.29%, 0.029% Ti, 0.13% Fe, 0.075% Zn, 0.025% Na, and 96.72% recovered scandium obtained under the comprehensive conditions used: m(Al): m(Mg): m(ScCl3) = 10:1:1.5, stirring speed of eight rpm, reduction temperature of 1223 K, reduction time of 40 min. The experimental results are in agreement with the thermodynamic predictions, and Al–Mg–Sc master alloy indicator was ideal.
- Open Access
Extraction of Nickel from Garnierite Laterite Ore Using Roasting and Magnetic Separation with Calcium Chloride and Iron Concentrate
In this study, segregation roasting and magnetic separation are used to extract nickel from a garnierite laterite ore. The garnierite laterite ore containing 0.72% Ni, 0.029% Co, 8.65% Fe, 29.66% MgO, and 37.86% SiO2 was collected in the Mojiang area of China. Garnierite was the Ni-bearing mineral; the other main minerals were potash feldspar, forsterite, tremolite, halloysite, quartz, and kaolinite in the garnierite laterite ore. The iron phase transformations show that nickel is transformed from (Ni,Mg)O·SiO2·nH2O to a new nickel mineral phase dominated by [Ni]Fe solid solution; and iron changed from Fe2O3 and FeOOH to a new iron mineral phase dominated by metal Fe and Fe3O4 after segregation roasting. Ferronickel concentrate with Ni of 16.16%, Fe of 73.67%, and nickel recovery of 90.33% was obtained under the comprehensive conditions used: A roasting temperature of 1100 °C, a roasting time of 90 min, a calcium chloride dosage of 15%, an iron concentrate dosage of 30%, a coke dosage of 15%, a coke size of −1 + 0.5 mm, a magnetic separation grinding fineness of H = 0.10 T. The main minerals in ferronickel concentrate are Fe, [Ni]Fe, Fe3O4, and a small amount of gangue minerals, such as CaO·SiO2 and CaO·Al2O3·SiO2.
Open AccessExtraction of Nickel from Garnierite Laterite Ore Using Roasting and Magnetic Separation with Calcium Chloride and Iron Concentrate
In this study, segregation roasting and magnetic separation are used to extract nickel from a garnierite laterite ore. The garnierite laterite ore containing 0.72% Ni, 0.029% Co, 8.65% Fe, 29.66% MgO, and 37.86% SiO2 was collected in the Mojiang area of China. Garnierite was the Ni-bearing mineral; the other main minerals were potash feldspar, forsterite, tremolite, halloysite, quartz, and kaolinite in the garnierite laterite ore. The iron phase transformations show that nickel is transformed from (Ni,Mg)O·SiO2·nH2O to a new nickel mineral phase dominated by [Ni]Fe solid solution; and iron changed from Fe2O3 and FeOOH to a new iron mineral phase dominated by metal Fe and Fe3O4 after segregation roasting. Ferronickel concentrate with Ni of 16.16%, Fe of 73.67%, and nickel recovery of 90.33% was obtained under the comprehensive conditions used: A roasting temperature of 1100 °C, a roasting time of 90 min, a calcium chloride dosage of 15%, an iron concentrate dosage of 30%, a coke dosage of 15%, a coke size of −1 + 0.5 mm, a magnetic separation grinding fineness of H = 0.10 T. The main minerals in ferronickel concentrate are Fe, [Ni]Fe, Fe3O4, and a small amount of gangue minerals, such as CaO·SiO2 and CaO·Al2O3·SiO2.
- Open Access
Extraction of Lead and Zinc from a Rotary Kiln Oxidizing Roasting Cinder
In this study, sulfuric acid leaching and gravity shaking-table separation by shaking a table are used to extract lead and zinc from a Pb-Zn oxidizing roasting cinder. The oxidizing roasting cinder—containing 16.9% Pb, 30.5% Zn, 10.3% Fe and 25.1% S—was obtained from a Pb-Zn sulfide ore in the Hanyuan area of China by a flotation-rotary kiln oxidizing roasting process. Anglesite and lead oxide were the main Pb-bearing minerals, while zinc sulfate, zinc oxide and zinc ferrite were the main Zn-bearing minerals. The results show that a part of lead contained in lead oxide is transformed to anglesite, and a 3PbO·PbSO4·H2O-dominated new lead mineral phase after acid leaching. A zinc leaching efficiency of 96.7% was obtained under the leaching conditions used: a leaching temperature of 55 °C; a leaching time of 90 min; a sulfuric acid dosage of 20%; a sulfurous acid dosage of 4%; a cinder particle size of R = 1:4. After the gravity shaking-table separation, a lead concentrate with 50.2% Pb, 2.33% Zn and lead recovery of 86.0% was produced. The main chemical compounds in leaching residue are anglesite, 3PbO·PbSO4·H2O, SiO2 and ZnFe2O4, while the main chemical compounds in lead concentrate are anglesite, 3PbO·PbSO4·H2O and SiO2.
Open AccessExtraction of Lead and Zinc from a Rotary Kiln Oxidizing Roasting Cinder
In this study, sulfuric acid leaching and gravity shaking-table separation by shaking a table are used to extract lead and zinc from a Pb-Zn oxidizing roasting cinder. The oxidizing roasting cinder—containing 16.9% Pb, 30.5% Zn, 10.3% Fe and 25.1% S—was obtained from a Pb-Zn sulfide ore in the Hanyuan area of China by a flotation-rotary kiln oxidizing roasting process. Anglesite and lead oxide were the main Pb-bearing minerals, while zinc sulfate, zinc oxide and zinc ferrite were the main Zn-bearing minerals. The results show that a part of lead contained in lead oxide is transformed to anglesite, and a 3PbO·PbSO4·H2O-dominated new lead mineral phase after acid leaching. A zinc leaching efficiency of 96.7% was obtained under the leaching conditions used: a leaching temperature of 55 °C; a leaching time of 90 min; a sulfuric acid dosage of 20%; a sulfurous acid dosage of 4%; a cinder particle size of R = 1:4. After the gravity shaking-table separation, a lead concentrate with 50.2% Pb, 2.33% Zn and lead recovery of 86.0% was produced. The main chemical compounds in leaching residue are anglesite, 3PbO·PbSO4·H2O, SiO2 and ZnFe2O4, while the main chemical compounds in lead concentrate are anglesite, 3PbO·PbSO4·H2O and SiO2.
- Open Access
New Combined Depressant/Collectors System for the Separation of Powellite from Dolomite and the Interaction Mechanism
The flotation beneficiation of powellite from dolomite was achieved with a new reagent system that consists of a mixed collector of sodium oleate (NaOl) and benzohydroxamic acid (BHA) and a depressant sodium hexametaphosphate (SHMP). The interaction mechanism of the reagent regime with minerals was studied using zeta potential and X-ray photoelectron spectroscopy (XPS) detection together with crystal chemistry and interaction energy analysis. The matching features of O–O distance in BHA with that in saline minerals and active site density/activity were used as methods to explain the reagent/mineral interaction. The results of microflotation finally established the new reagent regime at pH 8–12: 2.5 × 10−4 M SHMP, 2 × 10−4 M mixed collector containing 1.5 × 10−4 M NaOl and 0.5 × 10−4 M BHA. SHMP selectively depresses the adsorption of NaOl and BHA onto dolomite but minimally affects the adsorption of NaOl and BHA on the powellite surface.
Open AccessNew Combined Depressant/Collectors System for the Separation of Powellite from Dolomite and the Interaction Mechanism
The flotation beneficiation of powellite from dolomite was achieved with a new reagent system that consists of a mixed collector of sodium oleate (NaOl) and benzohydroxamic acid (BHA) and a depressant sodium hexametaphosphate (SHMP). The interaction mechanism of the reagent regime with minerals was studied using zeta potential and X-ray photoelectron spectroscopy (XPS) detection together with crystal chemistry and interaction energy analysis. The matching features of O–O distance in BHA with that in saline minerals and active site density/activity were used as methods to explain the reagent/mineral interaction. The results of microflotation finally established the new reagent regime at pH 8–12: 2.5 × 10−4 M SHMP, 2 × 10−4 M mixed collector containing 1.5 × 10−4 M NaOl and 0.5 × 10−4 M BHA. SHMP selectively depresses the adsorption of NaOl and BHA onto dolomite but minimally affects the adsorption of NaOl and BHA on the powellite surface.
- Open Access
Recovering Scandium from Scandium Rough Concentrate Using Roasting-Hydrolysis-Leaching Process
In this study, a roasting-hydrolysis-acid leaching process is used to extract scandium from the scandium rough concentrate. The scandium rough concentrate containing Sc2O3 of 76.98 g/t was obtained by magnetic separation, gravity separation, and electric separation from Sc-bearing Vi-Ti magnetite tailings in the Panxi area of China. The majority of scandium in scandium rough concentrate mainly occurs in diopside, titanopyroxene, montmorillonite, chlorite, talc, aluminosilicate minerals, and isomorphism. Sodium salt and scandium coarse concentrate are added into the roasting furnace for roasting, which makes the fusion reaction of silicon, aluminum and sodium salt to produce soluble salts such as sodium silicate and sodium metaaluminate. Scandium is further recovered from the hydrolysis residue by acid leaching. Test results show scandium leaching recovery of 95.12% and the acid leaching residue with Sc2O3 content of 8.12 g/t are obtained, while the extraction of scandium is obvious. There is no obvious peak value of Scandium spectrum in hydrochloric acid leach residue. Most of scandium in hydrolytic residue is dissolved into Sc3+ and enters into the liquid phase. The main minerals in leach residue are perovskite, ferric silicate, and olivine.
Open AccessRecovering Scandium from Scandium Rough Concentrate Using Roasting-Hydrolysis-Leaching Process
In this study, a roasting-hydrolysis-acid leaching process is used to extract scandium from the scandium rough concentrate. The scandium rough concentrate containing Sc2O3 of 76.98 g/t was obtained by magnetic separation, gravity separation, and electric separation from Sc-bearing Vi-Ti magnetite tailings in the Panxi area of China. The majority of scandium in scandium rough concentrate mainly occurs in diopside, titanopyroxene, montmorillonite, chlorite, talc, aluminosilicate minerals, and isomorphism. Sodium salt and scandium coarse concentrate are added into the roasting furnace for roasting, which makes the fusion reaction of silicon, aluminum and sodium salt to produce soluble salts such as sodium silicate and sodium metaaluminate. Scandium is further recovered from the hydrolysis residue by acid leaching. Test results show scandium leaching recovery of 95.12% and the acid leaching residue with Sc2O3 content of 8.12 g/t are obtained, while the extraction of scandium is obvious. There is no obvious peak value of Scandium spectrum in hydrochloric acid leach residue. Most of scandium in hydrolytic residue is dissolved into Sc3+ and enters into the liquid phase. The main minerals in leach residue are perovskite, ferric silicate, and olivine.