Fajar Nurjaman
Research Subjects
Research Interests
Fajar Nurjaman has a total of 50 co-authors. Here are the top co-authors by number of shared publications:
- Fathan Bahfie
Research Center for Mineral Technology, National Research and Innovation Agency, Tanjung Bintang, Lampung Selatan 35361, Indonesia
6 shared publications Bambang Suharno
Universitas Indonesia
5 shared publications- Deni Ferdian
Universitas Indonesia
5 shared publications A Shofi
Research Unit for Mineral Technology, Indonesian Institute of Sciences, Jl. Ir. Sutami Km. 15 Tanjung Bintang, South Lampung, Lampung, Indonesia
4 shared publicationsAchmad Shofi
Research Unit for Mineral Technology, Indonesian Institute of Sciences
3 shared publications- Azwar Manaf
Universitas Indonesia
3 shared publications
Latest Publications
- 22 June 2025
- Published by SAGE Publications in Ironmaking & Steelmaking: Processes, Products and Applications
- Vol. 53 (9) , 1887-1900
Effect of boric acid–sodium sulfate mixture on the selective reduction process of saprolitic nickel laterite
In selective reduction of nickel laterite process, sulphur-bearing materials as the sole additive have been studied to improve the nickel grade by inhibiting the metallisation of iron. However, the sulphidation reaction lowers the recovery of nickel. Therefore, the selection of proper additives carried out. Combining boric acid and sodium sulphate as additives, in selective reduction of saprolitic nickel ore has been investigated clearly in this work. Nickel saprolite, additives and coal were mixed and pelletised into 10–15 mm of diameter. The pellets were heated in a muffle furnace and before the wet magnetic separation process. The selective reduction process of saprolite with the mixture of boric acid and sodium sulphate at 20 wt% dosages (with 75–25 ratio), reductant amount of 0.4 stoichiometry of carbon, and temperature reduction of 1250°C has produced ferronickel contains nickel grade and recovery of 18.29% and 74.87%, respectively.
- 22 June 2025
- Published by SAGE Publications in Ironmaking & Steelmaking: Processes, Products and Applications
- Vol. 53 (9) , 1887-1900
Effect of boric acid–sodium sulfate mixture on the selective reduction process of saprolitic nickel laterite
In selective reduction of nickel laterite process, sulphur-bearing materials as the sole additive have been studied to improve the nickel grade by inhibiting the metallisation of iron. However, the sulphidation reaction lowers the recovery of nickel. Therefore, the selection of proper additives carried out. Combining boric acid and sodium sulphate as additives, in selective reduction of saprolitic nickel ore has been investigated clearly in this work. Nickel saprolite, additives and coal were mixed and pelletised into 10–15 mm of diameter. The pellets were heated in a muffle furnace and before the wet magnetic separation process. The selective reduction process of saprolite with the mixture of boric acid and sodium sulphate at 20 wt% dosages (with 75–25 ratio), reductant amount of 0.4 stoichiometry of carbon, and temperature reduction of 1250°C has produced ferronickel contains nickel grade and recovery of 18.29% and 74.87%, respectively.
- 1 May 2023
- Published by Springer Nature in Metal Science and Heat Treatment
- Vol. 65 (1-2) , 101-103
Effect of Direction of Additional Rolling on Anisotropy of Microstructure, Mechanical and Electrical Properties of Sheet Aluminum Alloy AA7075
- 1 May 2023
- Published by Springer Nature in Metal Science and Heat Treatment
- Vol. 65 (1-2) , 101-103
Effect of Direction of Additional Rolling on Anisotropy of Microstructure, Mechanical and Electrical Properties of Sheet Aluminum Alloy AA7075
- Open Access
- 1 March 2023
- Published by National University of Science and Technology MISiS in Izvestiya. Ferrous Metallurgy
- Vol. 66 (1) , 127-132
Composition of tailings after selective reduction of laterite
The selective reduction process generates products in the form of concentrates and tailing/by-products. There is high percentage of iron and other elements in the tailings that are not extracted in selective reduction process. Properties of by-products of selective reduction were investigated using X-ray diffraction (XRD), inductively coupled plasma optical emission spectroscopy (ICP–OES), ultraviolet-visible (UV–VIS), and scanning electron microscopy energy dispersion spectroscopy (SEM–EDS). Based on the results of this study, the properties of iron-sulfur, iron-magnesium-aluminium, and silica phases in the tailings can be interpreted experimentally. For future research, it can be the reference for such processes as acid and base leaching. Pure iron extracted from tailings can be used for metal fuel in the future. The tailings composition data will help future researchers to find optimal processes for the tailings.
- 1 March 2023
- Published by National University of Science and Technology MISiS in Izvestiya. Ferrous Metallurgy
- Vol. 66 (1) , 127-132
Open AccessComposition of tailings after selective reduction of laterite
The selective reduction process generates products in the form of concentrates and tailing/by-products. There is high percentage of iron and other elements in the tailings that are not extracted in selective reduction process. Properties of by-products of selective reduction were investigated using X-ray diffraction (XRD), inductively coupled plasma optical emission spectroscopy (ICP–OES), ultraviolet-visible (UV–VIS), and scanning electron microscopy energy dispersion spectroscopy (SEM–EDS). Based on the results of this study, the properties of iron-sulfur, iron-magnesium-aluminium, and silica phases in the tailings can be interpreted experimentally. For future research, it can be the reference for such processes as acid and base leaching. Pure iron extracted from tailings can be used for metal fuel in the future. The tailings composition data will help future researchers to find optimal processes for the tailings.
- Open Access
- 1 January 2023
- Published by AIP Publishing in AIP Conference Proceedings
- Vol. 2538 (1)
Effect of quaternary basicity (CaO+MgO/Al2O3+SiO2) in selective reduction of limonitic nickel ore
In this study, the quaternary basicity (CaO+MgO/Al2O3+SiO2) with modified MgO and CaO content in the selective reduction of limonitic nickel ore was investigated clearly. Limonitic nickel ore used in the process contains 1.38% Ni and 38.2% Fe. The anthracite coal and 10 wt% of Na2SO4 were used as reductants and additives, respectively. The reduction process conducted at 1150°C for an hour continued with the magnetic separation process to separate concentrate/ferronickel and tailing/impurities. The higher basicity with modified MgO resulted in lower nickel grade due to the formation of more magnesium silicate/forsterite, which could inhibit metal oxide reduction. The 0.3 of basicities with modified CaO addition showed the optimum condition due to its ability to break the silicate structure.
- 1 January 2023
- Published by AIP Publishing in AIP Conference Proceedings
- Vol. 2538 (1)
Open AccessEffect of quaternary basicity (CaO+MgO/Al2O3+SiO2) in selective reduction of limonitic nickel ore
In this study, the quaternary basicity (CaO+MgO/Al2O3+SiO2) with modified MgO and CaO content in the selective reduction of limonitic nickel ore was investigated clearly. Limonitic nickel ore used in the process contains 1.38% Ni and 38.2% Fe. The anthracite coal and 10 wt% of Na2SO4 were used as reductants and additives, respectively. The reduction process conducted at 1150°C for an hour continued with the magnetic separation process to separate concentrate/ferronickel and tailing/impurities. The higher basicity with modified MgO resulted in lower nickel grade due to the formation of more magnesium silicate/forsterite, which could inhibit metal oxide reduction. The 0.3 of basicities with modified CaO addition showed the optimum condition due to its ability to break the silicate structure.
- Open Access
- 27 July 2022
- Published by National University of Science and Technology MISiS in Izvestiya. Ferrous Metallurgy
- Vol. 65 (7) , 471-478
Thermal upgrading of nickel from limonite by means of selective reduction
X-ray diffraction (XRD), X-ray fluorescence (XRF), scanning electron microscopy energy dispersion spectroscopy (SEM–EDS), and differential thermal analysis (DTA) measurements were used to investigate the mineralogical characteristics and distribution of data set in limonite soil from Indonesia. The findings point to a complicated inner core in laterite ore. Ni, Fe, Mg, Al, and Si levels in limonite are 1.4, 50.5, 1.81, 4.86 and 16.5 wt %, respectively. The iron oxide/oxyhydroxide content of limonite is 94.4 and 5.6 % silicate. DTA shows that limonite has a phase transition in the low temperature (200 – 300 °C) with the goethite transformation to hematite. This phase is good optimalization for nickel diffusion in the iron. Moreover, for this limonite, the thermal upgrading was used as a good method.
- 27 July 2022
- Published by National University of Science and Technology MISiS in Izvestiya. Ferrous Metallurgy
- Vol. 65 (7) , 471-478
Open AccessThermal upgrading of nickel from limonite by means of selective reduction
X-ray diffraction (XRD), X-ray fluorescence (XRF), scanning electron microscopy energy dispersion spectroscopy (SEM–EDS), and differential thermal analysis (DTA) measurements were used to investigate the mineralogical characteristics and distribution of data set in limonite soil from Indonesia. The findings point to a complicated inner core in laterite ore. Ni, Fe, Mg, Al, and Si levels in limonite are 1.4, 50.5, 1.81, 4.86 and 16.5 wt %, respectively. The iron oxide/oxyhydroxide content of limonite is 94.4 and 5.6 % silicate. DTA shows that limonite has a phase transition in the low temperature (200 – 300 °C) with the goethite transformation to hematite. This phase is good optimalization for nickel diffusion in the iron. Moreover, for this limonite, the thermal upgrading was used as a good method.
- 5 September 2021
- Published by Springer Nature in Transactions of the Indian Institute of Metals
- Vol. 74 (12) , 3249-3263
Study of Binary, Ternary, and Quaternary Basicity in Reduction of Saprolitic Nickel Ore
- 5 September 2021
- Published by Springer Nature in Transactions of the Indian Institute of Metals
- Vol. 74 (12) , 3249-3263
Study of Binary, Ternary, and Quaternary Basicity in Reduction of Saprolitic Nickel Ore
- Open Access
- 1 January 2021
- Published by AIP Publishing in AIP Conference Proceedings
- Vol. 2382 (1) , 050007
Study effect of Na2SO4 dosage and graphite on the selective reduction of saprolite from nickel grade, recovery, and iron-nickel grain size
The selective reduction of nickel and adequate growth of ferronickel grains is imperative for efficient preparation of ferronickel from nickeliferous laterite ore via the process of direct reduction followed by magnetic separation. The reduction behaviours of a saprolite laterite ore in the presence of sodium sulphate were investigated, with an emphasis on thermodynamic analysis, selective reduction ratios and kinetics. To separate the interactions between Ni and Fe, chemical titration analysis was adopted to determine the contents of various Ni and Fe species in the roasted pellets and a modified equation to assay metallic iron content. This process uses the addition of sodium sulphate as the additive and graphite as the reductant. The additive and reductant are the optimal n the separation process to limit the form of iron oxide. The Na2SO4 dosage plays an important role in the process that causes its behaviour to reduce the growth of iron oxide. In this experiment, the study effect of Na2SO4 dosage with graphite as a reductant on the nickel grade, recovery and grain size of iron-nickel has been investigated in the variation of Na2SO4 dosage of 5, 10, and 15 % with reduction temperature 1150 °C for 60 minutes and the reductant stoichiometry is 0.125 from equilibrium condition is equal 0.63 gram. The mineralogical composition of the raw and reduced samples was analysed by XRD, AAS, and XRF. The grain size was measured with an optical microscope. The optimum Na2SO4 dosage is 15 %, which produces a concentrate with nickel grade, and the recoveries are 5.65 wt.% and 30.33 % when the grain size is greater than the high level of dosage because the liquid phase provides access for the transfer of metal ions and then prompts the growth of ferronickel grains.
- 1 January 2021
- Published by AIP Publishing in AIP Conference Proceedings
- Vol. 2382 (1) , 050007
Open AccessStudy effect of Na2SO4 dosage and graphite on the selective reduction of saprolite from nickel grade, recovery, and iron-nickel grain size
The selective reduction of nickel and adequate growth of ferronickel grains is imperative for efficient preparation of ferronickel from nickeliferous laterite ore via the process of direct reduction followed by magnetic separation. The reduction behaviours of a saprolite laterite ore in the presence of sodium sulphate were investigated, with an emphasis on thermodynamic analysis, selective reduction ratios and kinetics. To separate the interactions between Ni and Fe, chemical titration analysis was adopted to determine the contents of various Ni and Fe species in the roasted pellets and a modified equation to assay metallic iron content. This process uses the addition of sodium sulphate as the additive and graphite as the reductant. The additive and reductant are the optimal n the separation process to limit the form of iron oxide. The Na2SO4 dosage plays an important role in the process that causes its behaviour to reduce the growth of iron oxide. In this experiment, the study effect of Na2SO4 dosage with graphite as a reductant on the nickel grade, recovery and grain size of iron-nickel has been investigated in the variation of Na2SO4 dosage of 5, 10, and 15 % with reduction temperature 1150 °C for 60 minutes and the reductant stoichiometry is 0.125 from equilibrium condition is equal 0.63 gram. The mineralogical composition of the raw and reduced samples was analysed by XRD, AAS, and XRF. The grain size was measured with an optical microscope. The optimum Na2SO4 dosage is 15 %, which produces a concentrate with nickel grade, and the recoveries are 5.65 wt.% and 30.33 % when the grain size is greater than the high level of dosage because the liquid phase provides access for the transfer of metal ions and then prompts the growth of ferronickel grains.
- Open Access
- 1 December 2019
- Published by Chemical Engineering Department, Syiah Kuala University in Jurnal Rekayasa Kimia & Lingkungan
- Vol. 14 (2) , 130-138
Selective Reduction of High Alumina-Lateritic Nickel Ore (0.5 Ni-44Fe-16Al2O3)
In this present study, the effect of reductant dosage, temperature and holding time on selective reduction process of high alumina-lateritic nickel ore have been investigated clearly. The lateritic nickel ore was reduced with 5 until 15 wt. % anthracite and 10 wt. % sodium sulfate at reduction temperature of 950ºC, 1050ºC and 1150°C for 60, 90, and 120 minutes. Magnetic separation process was then conducted to separate the concentrate and tailing. The analysis of reduced nickel ore is performed by the Atomic Absorption Spectroscopy, X-Ray Diffraction, and Secondary Electron Microscopy. The optimal process resulted from the reduction of nickel ore with 10 wt. % anthracite at the temperature of 1050°C for 120 minutes which resulted in 0.84% nickel in concentrate. The troilite was not found in reduced ore. The iron grade increased along the increased of reduction temperature. The longer of holding time in selective reduction process increased the nickel grade but it decreased the iron grade.
- 1 December 2019
- Published by Chemical Engineering Department, Syiah Kuala University in Jurnal Rekayasa Kimia & Lingkungan
- Vol. 14 (2) , 130-138
Open AccessSelective Reduction of High Alumina-Lateritic Nickel Ore (0.5 Ni-44Fe-16Al2O3)
In this present study, the effect of reductant dosage, temperature and holding time on selective reduction process of high alumina-lateritic nickel ore have been investigated clearly. The lateritic nickel ore was reduced with 5 until 15 wt. % anthracite and 10 wt. % sodium sulfate at reduction temperature of 950ºC, 1050ºC and 1150°C for 60, 90, and 120 minutes. Magnetic separation process was then conducted to separate the concentrate and tailing. The analysis of reduced nickel ore is performed by the Atomic Absorption Spectroscopy, X-Ray Diffraction, and Secondary Electron Microscopy. The optimal process resulted from the reduction of nickel ore with 10 wt. % anthracite at the temperature of 1050°C for 120 minutes which resulted in 0.84% nickel in concentrate. The troilite was not found in reduced ore. The iron grade increased along the increased of reduction temperature. The longer of holding time in selective reduction process increased the nickel grade but it decreased the iron grade.
- Open Access
- 1 June 2019
- Published by IOP Publishing in IOP Conference Series: Materials Science and Engineering
- Vol. 541 (1) , 012002
Effect of reduction temperature and sodium-based additives on nickel upgrading process of laterites ores
In this present work, the selective reduction of nickel laterite was conducted by using 10 wt. % of sodium carbonate, sodium chloride and sodium sulphate as additives. The 5 wt. % of palm shell charcoal was used as the reductant. The selective reduction process for nickel laterite was carried out from 950ºC to 1150ºC for 60 minutes followed by wet magnetic separation using 500 Gausses permanent magnet. The characterization of reduced ore was performed by X-Ray Diffraction, optical microscope and Scanning Electron Microscope with Energy Dispersive X-Ray Spectroscopy, while the chemical composition of concentrate or ferronickel was identified by X-Ray Fluorescence. The results showed that the nickel grade was increased with the increasing of reduction temperature for nickel ore with sodium sulfate additive. Nevertheless, it was relatively constant for sodium carbonate and sodium chloride additive. Nickel recoveries found increased with the increasing of reduction temperatures of nickel ore with sodium-based additives. The ferronickel particle was agglomerated and growth with the increasing of reduction temperature, thus it provided favourable conditions for the separation of ferronickel from impurities in the magnetic separation process.
- 1 June 2019
- Published by IOP Publishing in IOP Conference Series: Materials Science and Engineering
- Vol. 541 (1) , 012002
Open AccessEffect of reduction temperature and sodium-based additives on nickel upgrading process of laterites ores
In this present work, the selective reduction of nickel laterite was conducted by using 10 wt. % of sodium carbonate, sodium chloride and sodium sulphate as additives. The 5 wt. % of palm shell charcoal was used as the reductant. The selective reduction process for nickel laterite was carried out from 950ºC to 1150ºC for 60 minutes followed by wet magnetic separation using 500 Gausses permanent magnet. The characterization of reduced ore was performed by X-Ray Diffraction, optical microscope and Scanning Electron Microscope with Energy Dispersive X-Ray Spectroscopy, while the chemical composition of concentrate or ferronickel was identified by X-Ray Fluorescence. The results showed that the nickel grade was increased with the increasing of reduction temperature for nickel ore with sodium sulfate additive. Nevertheless, it was relatively constant for sodium carbonate and sodium chloride additive. Nickel recoveries found increased with the increasing of reduction temperatures of nickel ore with sodium-based additives. The ferronickel particle was agglomerated and growth with the increasing of reduction temperature, thus it provided favourable conditions for the separation of ferronickel from impurities in the magnetic separation process.
- Open Access
- 1 May 2019
- Published by IOP Publishing in IOP Conference Series: Materials Science and Engineering
- Vol. 523 (1) , 012068
Optimal conditions for selective reduction process of Nickel Laterite Ore
A low-grade nickel laterite ore from Indonesia was selected to investigate the effect of temperature and time of reduction upon the extraction of nickel through the selective reduction-magnetic separation process to produce the ferronickel. The nickel ore was mixed with5 wt.% of anthracite coal and 10 wt.% of sodium sulfate additive. The mixed ore was pelletized into 10-15 mm of diameter. A series of selective reduction processes were carried out into the pellet ores at various temperatures of 950-1150 °C for 60-120 minutes. The optimal selective reduction parameters of nickel laterite ore were observed clearly. The experimental results indicated that the reduction reactions proceed more completely at a higher temperature and longer reduction time. The optimum of nickel grade and recovery in the ferronickel concentrate was obtained at the reduction temperature of 1150 °C for 120 minutes, which was 8.45% and 72.1%, respectively. The increasing of temperatures and times of reduction process resulted in higher of troilite phase formation which suppressed the iron metallization and also increased the ferronickel particle size.
- 1 May 2019
- Published by IOP Publishing in IOP Conference Series: Materials Science and Engineering
- Vol. 523 (1) , 012068
Open AccessOptimal conditions for selective reduction process of Nickel Laterite Ore
A low-grade nickel laterite ore from Indonesia was selected to investigate the effect of temperature and time of reduction upon the extraction of nickel through the selective reduction-magnetic separation process to produce the ferronickel. The nickel ore was mixed with5 wt.% of anthracite coal and 10 wt.% of sodium sulfate additive. The mixed ore was pelletized into 10-15 mm of diameter. A series of selective reduction processes were carried out into the pellet ores at various temperatures of 950-1150 °C for 60-120 minutes. The optimal selective reduction parameters of nickel laterite ore were observed clearly. The experimental results indicated that the reduction reactions proceed more completely at a higher temperature and longer reduction time. The optimum of nickel grade and recovery in the ferronickel concentrate was obtained at the reduction temperature of 1150 °C for 120 minutes, which was 8.45% and 72.1%, respectively. The increasing of temperatures and times of reduction process resulted in higher of troilite phase formation which suppressed the iron metallization and also increased the ferronickel particle size.