SBSandeep Bansal

Sandeep Bansal

*This is an algorithmically generated author record based on publicly available information.

Current Organizations / Institutes

The organizations/institutes from the scholar's latest article


Sandeep Bansal has a total of 30 co-authors. Here are the top co-authors by number of shared publications:


Latest Publications

  • Different Techniques Used for Characterizing Nanomaterials

    by Sandeep Bansal, Yudhveer Kumar Verma, Pushpinder Kumar, Mayank Choubey, Atul Raj

    This chapter explores the significance of nanomaterials and their unique properties that differentiate them from bulk materials. The chapter emphasizes their potential applications across diverse fields, including medicine, electronics, energy, and environmental science, thereby underscoring the necessity for precise characterization techniques. It discusses a range of advanced methods used for analyzing nanomaterials, such as microscopic techniques (scanning electron microscopy, transmission electron microscopy, and atomic force microscopy), spectroscopic techniques (X-ray diffraction, Raman spectroscopy, and Fourier-transform infrared spectroscopy), and surface characterization techniques (X-ray photoelectron spectroscopy and secondary ion mass spectrometry). The chapter discusses the challenges in characterization of nanomaterials such as resolution requirements, sample preparation problems, data interpretation difficulties, concerns of reproducibility, and environmental stability. It stresses the need for a combination of techniques to provide a comprehensive view of the structure, composition, and properties of nanomaterials. By describing these techniques and putting them into application, the chapter supplies insights for researchers and practitioners into the utilization of the extraordinary properties of nanomaterials to promote innovation in several fields.

  • Advancements in Nanomaterials and Nanofluids for Enhanced Tribological and Thermal Applications

    by Deepika Singh Singraur, Chayan Das, Asad Habeeb, Pushpinder Kumar, Sandeep Bansal


  • Green Synthesis Approaches for Nanomaterials

    by Mayank Choubey, Shweta Mishra, Ekta Verma, Sandeep Bansal, Sunny Misra, Prem Narayan Ahirwar

  • Nanoparticles – Synthesis Techniques of Nanomaterials

    by Shaman Gupta, Atul Raj, Pushpinder Kumar, Dinesh Deshwal, Sunny Misra, Sandeep Bansal

  • A sustainable approach for the development of Ni-based composite clads for enhancing cavitation erosion resistance

    by Sandeep Bansal, Khalid Bashir, Dheeraj Gupta

    Large revenue losses are being incurred by hydropower plants as a result of cavitation-related hydro turbine failure. One feasible way to solve this issue is to modify the exposed surface of the component. The use of microwaves to clad on metallic surfaces has grown in recent years. Hence, this work presents a development of NiCrSiC-x Al 2 O 3 (Where x = 5 and 15) composite clads that developed by using multimode home microwave applicator operating at 2.45 GHz frequency and maximum 900 W power. The clads were developed on AISI-316, an austenitic grade of stainless steel by microwave hybrid heating concept. The microstructure, crystal structure, porosity, microhardness of the as-deposited composite clad was investigated. The vibratory cavitation method was used to analyse cavitation erosion using Taguchi L9 orthogonal array. According to the results, the deposited NiCrSiC-x Al 2 O 3 composite clads possessed maximum of 1.20% and 1.33% porosity, 489.16 ± 47.95HV 0.3 and 744.12 ± 32 HV 0.3 microhardness, 625 ± 6 MPa and 854 ± 16 MPa of flexural strengths and cavitation resistance that was 4.13 and 8.18 times greater than AISI-316.

  • Microwave cladding of NiCrSiC-5Al 2 O 3 on austenitic stainless steel to improve cavitation erosion resistance

    by Sandeep Bansal, Jonty Mago, Dheeraj Gupta, Vivek Jain

    The current investigation aimed to study the cavitation erosion performance of the microwave synthesized NiCrSiC-5Al 2 O 3 composite clad with a 900 W power multimode domestic microwave applicator of 2.45 GHz frequency. The clads were deposited on the austenitic grade stainless steel, namely AISI-316. The as-deposited composite clad’s microstructure, crystal structure, porosity, microhardness, and flexural strength were examined. Cavitation erosion study was done using the vibratory cavitation method at varying standoff distance (SOD)-(0.5 mm, 1 mm, 1.5 mm) and vibration amplitude (AMP)-(40 μ m, 50 μ m, 60 μ m), keeping other parameters constant. The results had shown that the deposited NiCrSiC-5Al 2 O 3 composite clad exhibited 1.20% porosity, 489.16 ± 47.95 HV 0.3 microhardness, 264.91 ± 4.5 MPa flexural strength, and performed 3.5 times much better than the AISI-316 in terms of cavitation resistance. The least weight loss occurred at 1.5 mm SOD and 40 μ m AMP, where the highest weight loss was observed at 0.5 mm SOD and 60 μ m AMP. The erosion mechanism of the NiCrSiC-5Al 2 O 3 composite clad surface was observed as plastic deformation followed by surface fatigue; the clad surface was eroded in the form of pits, craters, impingement marks, secondary cracks, and plastically deformed lips.


  • Parametric optimization and analysis of cavitation erosion behavior of Ni-based + 10WC microwave processed composite clad using Taguchi approach

    by Sandeep Bansal, Jonty Mago, Dheeraj Gupta, Vivek Jain

    This study aims to develop cavitation erosion-resistant clads on stainless steel (SS-316) using the microwave cladding technique. Ni-based alloy powder (EWAC) was reinforced with tungsten carbide (10% by wt) powder to obtain composite clads. The cladding process was carried out in a domestic microwave applicator of 2.45 GHz frequency with 900 W power. The microstructure, crystal structure (phase identification and quantification), and microhardness of the developed clad were investigated with scanning electron microscopy (SEM), energy-dispersive x-ray spectroscopy (EDX), x-ray diffraction (XRD), and Vickers microhardness tester, respectively. It was found that the deposited clad has a uniform thickness of ∼520 μ m, and the microstructure mainly consists of equally dispersed and agglomerated carbides in cellular like Ni-Matrix. XRD analysis reveals that the composite clad was composed of various intermetallic, carbide, and oxide phases. The EWAC + 10WC clad (625 ± 81 HV 0.3 ) has a hardness ∼3.5 times higher than the stainless steel substrate (195 ± 15 HV 0.3 ). The cavitation erosion behavior of the SS-316 and EWAC + 10WC clad was examined by using a vibratory cavitation test apparatus. The parametric cavitation erosion testing was conducted according to the Taguchi L9 orthogonal array (OA) to study the effects of variations in amplitude (AMP), immersion depth (ID), and standoff distance (SOD) on mass loss in SS-316 and composite clad. The parametric study results show that SOD was the most influential test parameter, followed by AMP and ID. SOD contributes more than 50% in the mass loss of SS-316 and clad specimens, whereas AMP and ID contribution was around 32%–37% and 7%–11%, respectively. The developed EWAC + 10WC clad performed ∼6.7 times better than the SS-316. Nevertheless, the SS-316 and EWAC + 10WC clad specimens got severely damage in the form of pits, craters, plastic deformation, lip formation, impingement marks, and secondary cracks.


  • Analysis of susceptor temperature during microwave heating and characterization of Ni-30Cr3C2 clads

    by Sandeep Bansal, Dheeraj Gupta, Vivek Jain

    Hydropower plants are experiencing huge revenue losses due to the failure of hydro turbines caused by cavitation. Surface modification could be a feasible solution to tackle this problem. Microwave processing of metallic materials to coat/clad has gained popularity in recent years. In the current study, microwave exposure time by analyzing susceptor temperature is optimized to get sound clads. Nickel-based and Cr3C2-reinforced clad on SS-316 substrate is developed for cavitation erosion resistance. The clads have been developed in a domestic microwave oven of 2.45 GHz and 900 W. The Ni + 30% Cr3C2 developed clad has been characterized through various standard mechanical and metallurgical techniques like X-ray diffraction, scanning electron microscopy, energy-dispersive spectroscopy, Vicker’s micro-hardness, porosity measurement, and flexural study. The presence of various carbide and intermetallic phases Cr2Ni3, Cr7C3, CrSi, SiO2, and FeNi3 is confirmed from the X-ray diffraction pattern. The distribution of hard carbide phases into soft matrix is confirmed from the microstructural investigation. Vicker’s microhardness study confirms the enhanced average microhardness of the clad region by 2.5 times of the substrate. The analysis of porosity shows significantly less (0.98%) porosity. The flexural study of developed clads by using three-point bending test is evaluated and flexural strength and deformation index values of developed clads of 814 ± 11.5 MPa and 2.29 × 10−4 mm N−1 respectively are observed.