Yong Chen has a total of 33 co-authors. Here are the top co-authors by number of shared publications:
Chenfu Fang
Provincial Key Lab of Advanced Welding Technology, College of Materials Science and Engineering, Jiangsu University of Science and Technology, Zhenjiang, China
4 shared publicationsTao Zhang
Industrial Perception and Intelligent Manufacturing Equipment Engineering Research Center of Jiangsu Province, Nanjing University of Industry Technology, Nanjing, China
4 shared publicationsQintao Li
2 shared publications- Wangwang Yu
School of Mechanical Engineering, Nanjing Vocational University of Industry Technology, Nanjing 210023, China
2 shared publications Xianrui Zhao
College of Marine and Intelligent Manufacturing, Jiangsu Maritime Institute, Nanjing, China
2 shared publications- Bo Cheng
State Key Laboratory of Precision Welding & Joining of Materials and Structures, Harbin Institute of Technology, Harbin 150001, China
1 shared publication
Latest Publications
- Open Access
Microstructural Modification and Strengthening Mechanisms in a ZM6 Magnesium Alloy Joint Processed by Ultrasonic-Assisted TIG Welding with Pre-Weld Heat Treatment
In the context of global industrial green transformation and the demand for light-weighting, magnesium alloys, as the most promising lightweight engineering materials, still face limitations due to inherent poor ductility, low strength, and insufficient corrosion resistance. ZM6 (Mg-Nd-Zr) magnesium alloy has attracted significant attention for its notable age-strengthening response; however, the quality of its welded repairs remains a critical bottleneck hindering its engineering application. Results demonstrate that ultrasonic-assisted welding significantly refines weld grain size (average 10–15 μm) and reduces porosity via acoustic streaming and cavitation effects. Pre-weld heat treatment effectively activates precipitation strengthening, promoting the uniform and dispersed precipitation of strengthening phases such as Nd-enriched secondary phases. Consequently, the mechanical properties of the repaired joint are remarkably restored, achieving an ultimate tensile strength of 267 MPa, a yield strength of 210 MPa, and an elongation of 6.8%. The microhardness of the repaired zone recovered to 72 HV, approaching the base metal value (83 HV). Fractography revealed a ductile–brittle mixed-fracture mode. This research confirms that the combination of ultrasonically assisted TIG welding and pre-weld heat treatment is a viable strategy for effectively enhancing the repair quality of ZM6 magnesium alloy, enabling the synergistic recovery of strength and ductility, thereby providing important theoretical and practical significance for promoting the reliable application of magnesium alloys in high-end equipment manufacturing.
Open AccessMicrostructural Modification and Strengthening Mechanisms in a ZM6 Magnesium Alloy Joint Processed by Ultrasonic-Assisted TIG Welding with Pre-Weld Heat Treatment
In the context of global industrial green transformation and the demand for light-weighting, magnesium alloys, as the most promising lightweight engineering materials, still face limitations due to inherent poor ductility, low strength, and insufficient corrosion resistance. ZM6 (Mg-Nd-Zr) magnesium alloy has attracted significant attention for its notable age-strengthening response; however, the quality of its welded repairs remains a critical bottleneck hindering its engineering application. Results demonstrate that ultrasonic-assisted welding significantly refines weld grain size (average 10–15 μm) and reduces porosity via acoustic streaming and cavitation effects. Pre-weld heat treatment effectively activates precipitation strengthening, promoting the uniform and dispersed precipitation of strengthening phases such as Nd-enriched secondary phases. Consequently, the mechanical properties of the repaired joint are remarkably restored, achieving an ultimate tensile strength of 267 MPa, a yield strength of 210 MPa, and an elongation of 6.8%. The microhardness of the repaired zone recovered to 72 HV, approaching the base metal value (83 HV). Fractography revealed a ductile–brittle mixed-fracture mode. This research confirms that the combination of ultrasonically assisted TIG welding and pre-weld heat treatment is a viable strategy for effectively enhancing the repair quality of ZM6 magnesium alloy, enabling the synergistic recovery of strength and ductility, thereby providing important theoretical and practical significance for promoting the reliable application of magnesium alloys in high-end equipment manufacturing.
- Open Access
- 22 June 2026
- Published by Polish Academy of Sciences Chancellery in Archives of Metallurgy and Materials
- Vol. 71 (2) , 667-675
Comparative Study on Welding Efficiency, Macrostructural/Microstructural Characteristics, and Mechanical Properties for Seven-wire Rotating Arc Electrogas Welding and Single-wire Electrogas Welding
- 22 June 2026
- Published by Polish Academy of Sciences Chancellery in Archives of Metallurgy and Materials
- Vol. 71 (2) , 667-675
Open AccessComparative Study on Welding Efficiency, Macrostructural/Microstructural Characteristics, and Mechanical Properties for Seven-wire Rotating Arc Electrogas Welding and Single-wire Electrogas Welding
- 24 February 2026
- Published by Springer Nature in Metallography, Microstructure, and Analysis
- Vol. 15 (2) , 519-534
Influence of Different Shielded Gases on Welding Performance in SRA EGW
- 24 February 2026
- Published by Springer Nature in Metallography, Microstructure, and Analysis
- Vol. 15 (2) , 519-534
Influence of Different Shielded Gases on Welding Performance in SRA EGW
- Open Access
Microstructure and Mechanical Properties of Toughened Seven-Wire Electrogas Welding
Based on the flexible adjustment of the seven-wire, this study will assemble a new toughened seven-wire which is combined with a common single welding wire and the existing welding wire containing ductile alloy element (Ni element), and the microstructure properties, mechanical properties and toughening mechanism of the welding seams were studied. The results show that the microstructure of the four combinatorial seven-wire welding seams is mainly composed of coarse proeutectoid ferrite (PF) and fine acicular ferrite (AF). Among them, the core of inclusions that induce AF nucleation and growth are mainly composed of Al, Ti, Si, and Mn-based oxides, and the edge of inclusions is mainly composed of Mn and Cu sulfides (MnS, CuS). The addition of Ti compounds further promotes AF nucleation. This is also a reason why the impact toughness of the combinatorial seven-wire W2/W3 welding seams is higher than that of other combinatorial seven-wire welding seams, but the impact toughness of the rich Ni seven-wire can meet the standard requirements of the China Classification Society (CCS). Among the four combinatorial seven-wire welding seams, the proportions of large angle grain boundaries (grain orientation difference ≥ 15°) that improve the ability of materials to prevent brittle fracture are 65.9%, 68.8%, 66.0%, 61.7%, respectively, that is, the larger proportion of large angle grain boundaries in combinatorial seven-wire W2 welding seams (Ni content is 0.0897%) is one of the reasons for the higher impact toughness of the welding seams. With the increase of Ni content in the welding seam, the AF content first increased and then decreased, the yield strength and tensile strength increased, and the elongation and section shrinkage first increased and then decreased. When the combinatorial seven-wire W2/W3 was used, the welding seam plasticity was the best.
Open AccessMicrostructure and Mechanical Properties of Toughened Seven-Wire Electrogas Welding
Based on the flexible adjustment of the seven-wire, this study will assemble a new toughened seven-wire which is combined with a common single welding wire and the existing welding wire containing ductile alloy element (Ni element), and the microstructure properties, mechanical properties and toughening mechanism of the welding seams were studied. The results show that the microstructure of the four combinatorial seven-wire welding seams is mainly composed of coarse proeutectoid ferrite (PF) and fine acicular ferrite (AF). Among them, the core of inclusions that induce AF nucleation and growth are mainly composed of Al, Ti, Si, and Mn-based oxides, and the edge of inclusions is mainly composed of Mn and Cu sulfides (MnS, CuS). The addition of Ti compounds further promotes AF nucleation. This is also a reason why the impact toughness of the combinatorial seven-wire W2/W3 welding seams is higher than that of other combinatorial seven-wire welding seams, but the impact toughness of the rich Ni seven-wire can meet the standard requirements of the China Classification Society (CCS). Among the four combinatorial seven-wire welding seams, the proportions of large angle grain boundaries (grain orientation difference ≥ 15°) that improve the ability of materials to prevent brittle fracture are 65.9%, 68.8%, 66.0%, 61.7%, respectively, that is, the larger proportion of large angle grain boundaries in combinatorial seven-wire W2 welding seams (Ni content is 0.0897%) is one of the reasons for the higher impact toughness of the welding seams. With the increase of Ni content in the welding seam, the AF content first increased and then decreased, the yield strength and tensile strength increased, and the elongation and section shrinkage first increased and then decreased. When the combinatorial seven-wire W2/W3 was used, the welding seam plasticity was the best.
- 1 December 2023
- Published by Pleiades Publishing Ltd in Physics of Metals and Metallography
- Vol. 124 (14) , 1826-1836
Arc Heat Distribution in Cable-Type Welding Wire Submerged Arc Surfacing
The cable-type welding wire (CWW) submerged arc surfacing (SAS) is an innovative welding process with the advantages of high efficiency, energy saving, and good welding quality. At present, this welding process has been applied to repair the large structure. This study investigate the arc heat efficiency and arc heat distribution of CWW SAS using the mathematical calculation method. The deposition rate and the surfacing layer area of CWW SAS increases with the increasing welding current. The deposition rate and the surfacing layer area of CWW SAS are larger than those in single-wire SAS. The ratio of the surfacing layer area between CWW SAS and single-wire SAS is similar to the ratio of the surfacing deposition rates between CWW SAS and single-wire SAS. The efficiency of the arc heat on melting wire in CWW SAS is larger than that in single-wire SAS. The arc heat working on base metal in CWW SAS is lower than that in single-wire SAS, leading to a smaller molten base metal area. The arc heat working on droplet transfer in CWW SAS is greater than that in single-wire SAS, leading to a larger surfacing area.
- 1 December 2023
- Published by Pleiades Publishing Ltd in Physics of Metals and Metallography
- Vol. 124 (14) , 1826-1836
Arc Heat Distribution in Cable-Type Welding Wire Submerged Arc Surfacing
The cable-type welding wire (CWW) submerged arc surfacing (SAS) is an innovative welding process with the advantages of high efficiency, energy saving, and good welding quality. At present, this welding process has been applied to repair the large structure. This study investigate the arc heat efficiency and arc heat distribution of CWW SAS using the mathematical calculation method. The deposition rate and the surfacing layer area of CWW SAS increases with the increasing welding current. The deposition rate and the surfacing layer area of CWW SAS are larger than those in single-wire SAS. The ratio of the surfacing layer area between CWW SAS and single-wire SAS is similar to the ratio of the surfacing deposition rates between CWW SAS and single-wire SAS. The efficiency of the arc heat on melting wire in CWW SAS is larger than that in single-wire SAS. The arc heat working on base metal in CWW SAS is lower than that in single-wire SAS, leading to a smaller molten base metal area. The arc heat working on droplet transfer in CWW SAS is greater than that in single-wire SAS, leading to a larger surfacing area.
- Open Access
A Study of the Laser Removal Process of Al-Si Coating from 22MnB5 Steel
22MnB5 hot forming steel is widely used in the automotive industry due to the increasing demand for lightweight vehicles. As surface oxidation and decarburization occur during hot stamping processes, an Al-Si coating is often precoated on surfaces. The coating tends to melt into the melt pool during the laser welding of the matrix and reduce the strength of the welded joint; therefore, it should be removed. The decoating process by sub-nanosecond and picosecond lasers and process parameter optimization were conducted in this paper. The corresponding analysis of the different decoating processes, the mechanical properties and the elemental distribution was carried out after laser welding and heat treatment. It was found that the Al element has an influence on the strength and elongation of the welded joint. The high-power picosecond laser has a better removal effect than the lower power sub-nanosecond laser. The best mechanical properties of the welded joint were obtained under the process conditions of 1064 nm center wavelength, 15 kW power, 100 kHz frequency, and 0.1 m/s speed. In addition, the content of the coating metal elements (mainly Al) melted into the welded joint is reduced with increasing coating removal width, which significantly improves the mechanical properties of the welded joints. Al in the coating rarely melts into the welding pool when the coating removal width is not less than 0.4 mm, and its mechanical properties can meet the automotive stamping requirements for the welded plate.
Open AccessA Study of the Laser Removal Process of Al-Si Coating from 22MnB5 Steel
22MnB5 hot forming steel is widely used in the automotive industry due to the increasing demand for lightweight vehicles. As surface oxidation and decarburization occur during hot stamping processes, an Al-Si coating is often precoated on surfaces. The coating tends to melt into the melt pool during the laser welding of the matrix and reduce the strength of the welded joint; therefore, it should be removed. The decoating process by sub-nanosecond and picosecond lasers and process parameter optimization were conducted in this paper. The corresponding analysis of the different decoating processes, the mechanical properties and the elemental distribution was carried out after laser welding and heat treatment. It was found that the Al element has an influence on the strength and elongation of the welded joint. The high-power picosecond laser has a better removal effect than the lower power sub-nanosecond laser. The best mechanical properties of the welded joint were obtained under the process conditions of 1064 nm center wavelength, 15 kW power, 100 kHz frequency, and 0.1 m/s speed. In addition, the content of the coating metal elements (mainly Al) melted into the welded joint is reduced with increasing coating removal width, which significantly improves the mechanical properties of the welded joints. Al in the coating rarely melts into the welding pool when the coating removal width is not less than 0.4 mm, and its mechanical properties can meet the automotive stamping requirements for the welded plate.
- 1 July 2020
- Published by Elsevier in Journal of Manufacturing Processes
- Vol. 55, 96-102
The decoupling behavior of arc coupling and rotating in seven-wire rotating arc EGW
- 1 July 2020
- Published by Elsevier in Journal of Manufacturing Processes
- Vol. 55, 96-102
The decoupling behavior of arc coupling and rotating in seven-wire rotating arc EGW
- 15 April 2020
- Published by Springer Nature in The International Journal of Advanced Manufacturing Technology
- Vol. 107 (7-8) , 3363-3369
Droplet formation and motion characteristics in seven-wire rotating arc electrogas welding
- 15 April 2020
- Published by Springer Nature in The International Journal of Advanced Manufacturing Technology
- Vol. 107 (7-8) , 3363-3369
Droplet formation and motion characteristics in seven-wire rotating arc electrogas welding
- 31 August 2009
- Published by Trans Tech Publications, Ltd. in Advanced Materials Research
- Vol. 79-82, 291-294
A New Type of Rubber Sandwich Coated Onto Ship for the Use of Underwater Explosion Shock Mitigating
How to moderate ship the damages caused by the underwater explosion (UNDEX) is of great interest to the modern ship designers. A new type of rubber sandwich with periodic honeycomb core was developed to mitigate the ship shock due to UNDEX. A ship with or without the rubber coat was tested under “near combat conditions” by igniting a 8 kg charge of TNT underwater at varying standoff distances from the ship. The effects of the shocks to ship systems were observed and the responses of the ship were monitored and recorded for each shot. The pressures in the water around the ship were also recorded to explore the fluid-structure interaction and UNDEX shock wave reflection with different targets. Acceleration and strain records indicate that the rubber coat is capable of moderating the high-frequency response excited by shock wave efficiently. Pressure records show that the core crushing and water cavitation promote superior energy absorption that yields an increased resistance to UNDEX.
- 31 August 2009
- Published by Trans Tech Publications, Ltd. in Advanced Materials Research
- Vol. 79-82, 291-294
A New Type of Rubber Sandwich Coated Onto Ship for the Use of Underwater Explosion Shock Mitigating
How to moderate ship the damages caused by the underwater explosion (UNDEX) is of great interest to the modern ship designers. A new type of rubber sandwich with periodic honeycomb core was developed to mitigate the ship shock due to UNDEX. A ship with or without the rubber coat was tested under “near combat conditions” by igniting a 8 kg charge of TNT underwater at varying standoff distances from the ship. The effects of the shocks to ship systems were observed and the responses of the ship were monitored and recorded for each shot. The pressures in the water around the ship were also recorded to explore the fluid-structure interaction and UNDEX shock wave reflection with different targets. Acceleration and strain records indicate that the rubber coat is capable of moderating the high-frequency response excited by shock wave efficiently. Pressure records show that the core crushing and water cavitation promote superior energy absorption that yields an increased resistance to UNDEX.