Latest Publications
- Open Access
- 19 March 2026
- Published by Elsevier in SSRN Electronic Journal
Interplay between hydrogen uptake and microstructural transformation in Al-Si coated tailor rolled blanks under hot press forming conditions
The demand for lightweight automotive components has driven the development of Tailor Rolled Blanks (TRB) using ultra-high-strength boron steels. However, these materials exhibit high sensitivity to hydrogen embrittlement (HE), particularly during the hot press forming (HPF) process. This study investigates the correlation between the thickness reduction ratio of Al-Si coated TRB and the subsequent hydrogen transport behavior. During heat treatment, moisture in the furnace atmosphere reacts with the Al-Si coating to generate atomic hydrogen, which diffuses into the steel substrate. Upon cooling, the transformed coating becomes diffusion-tight, trapping diffusible hydrogen within the material. Our findings reveal that the hydrogen absorption behavior is significantly influenced by the differential rolling profiles of the TRB. Specifically, a distinct trend of increased hydrogen inflow was observed at higher rolling ratios and elevated dew points during hot stamping. By isolating variables such as substrate thickness and cold rolling, this research identifies Al-Si coating thickness as a dominant factor promoting hydrogen uptake during continuous heating. Microstructural analysis elucidates the interplay between the transverse microsection of the Al-Si coating and the base material's trapping sites as a function of plastic deformation. Furthermore, while specimens with a 50% rolling degree and a 15°C dew point remained stable under laser cutting, they were predicted to be susceptible to delayed fracture during cold trimming. This study provides comprehensive insights into microstructural deformation and hydrogen trapping, offering critical guidelines for managing hydrogen sensitivity in advanced automotive applications.
- 19 March 2026
- Published by Elsevier in SSRN Electronic Journal
Open AccessInterplay between hydrogen uptake and microstructural transformation in Al-Si coated tailor rolled blanks under hot press forming conditions
The demand for lightweight automotive components has driven the development of Tailor Rolled Blanks (TRB) using ultra-high-strength boron steels. However, these materials exhibit high sensitivity to hydrogen embrittlement (HE), particularly during the hot press forming (HPF) process. This study investigates the correlation between the thickness reduction ratio of Al-Si coated TRB and the subsequent hydrogen transport behavior. During heat treatment, moisture in the furnace atmosphere reacts with the Al-Si coating to generate atomic hydrogen, which diffuses into the steel substrate. Upon cooling, the transformed coating becomes diffusion-tight, trapping diffusible hydrogen within the material. Our findings reveal that the hydrogen absorption behavior is significantly influenced by the differential rolling profiles of the TRB. Specifically, a distinct trend of increased hydrogen inflow was observed at higher rolling ratios and elevated dew points during hot stamping. By isolating variables such as substrate thickness and cold rolling, this research identifies Al-Si coating thickness as a dominant factor promoting hydrogen uptake during continuous heating. Microstructural analysis elucidates the interplay between the transverse microsection of the Al-Si coating and the base material's trapping sites as a function of plastic deformation. Furthermore, while specimens with a 50% rolling degree and a 15°C dew point remained stable under laser cutting, they were predicted to be susceptible to delayed fracture during cold trimming. This study provides comprehensive insights into microstructural deformation and hydrogen trapping, offering critical guidelines for managing hydrogen sensitivity in advanced automotive applications.
- Open Access
Improving the Metal Inert Gas Welding Efficiency and Microstructural Stability in the Butt and Lap Joints of Aluminum Automotive Components Using Sc- and Zr-Enhanced Filler Wires
The grain growth in the fusion zone (FZ) and heat-affected zone (HAZ) of metal inert gas (MIG) welding processes negatively affect the mechanical properties of aluminum alloy MIG welds used in automotive components. Although the addition of Sc- and Zr-based filler wires can refine weld microstructures and enhance the mechanical properties, conditions resembling actual automotive component joints have not been sufficiently investigated. In this study, 5083-O aluminum alloy base material was welded into butt and lap joints using conventional 5000-series aluminum alloy filler wires (Al-5.0Mg) and wires containing Sc and Zr (Al-4.8Mg-0.7Sc-0.3Zr) under various heat input conditions. The mechanical properties of the welds were evaluated via tensile tests, and the microstructures in the FZ and HAZ were analyzed. In butt joints, Al-4.8Mg-0.7Sc-0.3Zr exhibited a finer and more uniform grain structure with increased tensile strength compared with those welded using Al-5.0Mg. The microstructure became coarser with the increased heat input, and the tensile strength tended to decrease. In lap joints, the tensile-shear strength of Al-4.8Mg-0.7Sc-0.3Zr was higher than that of Al-5.0Mg; it further increased with the increase in the amount of deposited metal. The coarsening of the microstructure with the increased heat input was disadvantageous for the tensile-shear strength, and the increased weld size offset the adverse effects of the coarse microstructure. These results indicate that the heat input and the amount of deposited metal must be optimized to ensure stiffness in various joints of automotive components.
Open AccessImproving the Metal Inert Gas Welding Efficiency and Microstructural Stability in the Butt and Lap Joints of Aluminum Automotive Components Using Sc- and Zr-Enhanced Filler Wires
The grain growth in the fusion zone (FZ) and heat-affected zone (HAZ) of metal inert gas (MIG) welding processes negatively affect the mechanical properties of aluminum alloy MIG welds used in automotive components. Although the addition of Sc- and Zr-based filler wires can refine weld microstructures and enhance the mechanical properties, conditions resembling actual automotive component joints have not been sufficiently investigated. In this study, 5083-O aluminum alloy base material was welded into butt and lap joints using conventional 5000-series aluminum alloy filler wires (Al-5.0Mg) and wires containing Sc and Zr (Al-4.8Mg-0.7Sc-0.3Zr) under various heat input conditions. The mechanical properties of the welds were evaluated via tensile tests, and the microstructures in the FZ and HAZ were analyzed. In butt joints, Al-4.8Mg-0.7Sc-0.3Zr exhibited a finer and more uniform grain structure with increased tensile strength compared with those welded using Al-5.0Mg. The microstructure became coarser with the increased heat input, and the tensile strength tended to decrease. In lap joints, the tensile-shear strength of Al-4.8Mg-0.7Sc-0.3Zr was higher than that of Al-5.0Mg; it further increased with the increase in the amount of deposited metal. The coarsening of the microstructure with the increased heat input was disadvantageous for the tensile-shear strength, and the increased weld size offset the adverse effects of the coarse microstructure. These results indicate that the heat input and the amount of deposited metal must be optimized to ensure stiffness in various joints of automotive components.
- 27 April 2024
- Published by Elsevier in Journal of Materials Science & Technology
- Vol. 206, 62-73
Correlation between pre-strain and hydrogen embrittlement behavior in medium-Mn steel
- 27 April 2024
- Published by Elsevier in Journal of Materials Science & Technology
- Vol. 206, 62-73
Correlation between pre-strain and hydrogen embrittlement behavior in medium-Mn steel
- Open Access
- 12 March 2024
- Published by Elsevier in Materials Science and Engineering: A
- Vol. 897
Hydrogen diffusion and hydrogen embrittlement of a 1500 MPa hot-stamped steel 22MnB5 in different austenitizing conditions
- 12 March 2024
- Published by Elsevier in Materials Science and Engineering: A
- Vol. 897
Open AccessHydrogen diffusion and hydrogen embrittlement of a 1500 MPa hot-stamped steel 22MnB5 in different austenitizing conditions
- 21 January 2024
- Published by Elsevier in International Journal of Plasticity
- Vol. 173
A continuum scale chemo-mechanical model for multi-trap hydrogen transport in deformed polycrystalline metals
- 21 January 2024
- Published by Elsevier in International Journal of Plasticity
- Vol. 173
A continuum scale chemo-mechanical model for multi-trap hydrogen transport in deformed polycrystalline metals
- 11 November 2023
- Published by Elsevier in Acta Materialia
- Vol. 263
Pre-strain and hydrogen charging effect on the plastic and fracture behavior of quenching and partitioning (Q&P) steel
- 11 November 2023
- Published by Elsevier in Acta Materialia
- Vol. 263
Pre-strain and hydrogen charging effect on the plastic and fracture behavior of quenching and partitioning (Q&P) steel