Minglong Ma
Research Subjects
Minglong Ma has a total of 71 co-authors. Here are the top co-authors by number of shared publications:
Kui Zhang
11 shared publications- Kui Zhang
State Key Laboratory of Nonferrous Metals and Process, GRINM Group Co., Ltd., Beijing 100088, China
8 shared publications Yongjun Li
8 shared publicationsGuoliang Shi
6 shared publicationsJiawei Yuan
6 shared publicationsXinggang Li
6 shared publications
Latest Publications
- Open Access
- 3 August 2024
- Published by Elsevier in Next Materials
- Vol. 7
Effects of Sn on the electrochemistry and discharge performances of as-extruded Mg-1.2Ga as an anode for Mg-air batteries
- 3 August 2024
- Published by Elsevier in Next Materials
- Vol. 7
Open AccessEffects of Sn on the electrochemistry and discharge performances of as-extruded Mg-1.2Ga as an anode for Mg-air batteries
- 6 March 2024
- Published by Elsevier in Materials Chemistry and Physics
- Vol. 317
Study on hot processing map with ANN modification and DRX behaviors of a novel Mg-Ga-Sn anode for an air battery
- 6 March 2024
- Published by Elsevier in Materials Chemistry and Physics
- Vol. 317
Study on hot processing map with ANN modification and DRX behaviors of a novel Mg-Ga-Sn anode for an air battery
- Open Access
Effects of Bulk LPSO Phases on Mechanical Properties and Fracture Behavior of As-Extruded Mg-Gd-Y-Zn-Zr Alloys
Despite the consensus on the constructive effect of LPSO (long-period stacking-ordered) phases, the true effect of bulk LPSO phases on strengthening and toughening in deformed magnesium alloys is still controversial. This article, which introduces the alloys Mg-8Gd-4Y-0.6Zn-0.5Zr, without bulk LPSO phases, and Mg-8Gd-4Y-1.6Zn-0.5Zr, containing bulk LPSO phases, details a systematically comparative analysis conducted to clarify the true contribution of bulk LPSO phases to the properties of as-extruded alloys. The results indicate that bulk LPSO phases significantly improve strength by refining grain sizes remarkably. But contrary to expectations, bulk LPSO phases themselves only provide a small strengthening effect and deteriorate plasticity, ascribed to the poor compatible plastic deformation of bulk LPSO phases. More importantly, this work may offer new insights into the strengthening and toughening of LPSO phases for further research and engineering applications of this series of alloys. Additionally, an example of a design strategy for Mg-Gd-Y-Zn alloys with superior strength and excellent plasticity is proposed at the end of this article.
Open AccessEffects of Bulk LPSO Phases on Mechanical Properties and Fracture Behavior of As-Extruded Mg-Gd-Y-Zn-Zr Alloys
Despite the consensus on the constructive effect of LPSO (long-period stacking-ordered) phases, the true effect of bulk LPSO phases on strengthening and toughening in deformed magnesium alloys is still controversial. This article, which introduces the alloys Mg-8Gd-4Y-0.6Zn-0.5Zr, without bulk LPSO phases, and Mg-8Gd-4Y-1.6Zn-0.5Zr, containing bulk LPSO phases, details a systematically comparative analysis conducted to clarify the true contribution of bulk LPSO phases to the properties of as-extruded alloys. The results indicate that bulk LPSO phases significantly improve strength by refining grain sizes remarkably. But contrary to expectations, bulk LPSO phases themselves only provide a small strengthening effect and deteriorate plasticity, ascribed to the poor compatible plastic deformation of bulk LPSO phases. More importantly, this work may offer new insights into the strengthening and toughening of LPSO phases for further research and engineering applications of this series of alloys. Additionally, an example of a design strategy for Mg-Gd-Y-Zn alloys with superior strength and excellent plasticity is proposed at the end of this article.
- Open Access
Study on the Microstructure of Mg-4Zn-4Sn-1Mn-xAl As-Cast Alloys
In this study, the microstructure of the Mg-4Zn-4Sn-1Mn-xAl (x = 0, 0.3 wt.%, denoted as ZTM441 and ZTM441-0.3Al) as-cast alloys was investigated using scanning electron microscopy (SEM), focused-ion/electron-beam (FIB) micromachining, transmission electron microscopy (TEM), and high-angle annular dark-field scanning transmission electron microscopy (HAADF-STEM). The analysis results revealed that the microstructure of the ZTM441 and ZTM441-0.3Al as-cast alloys both mainly consist of the α-Mg matrix, skeleton-shaped MgZn2 eutectic texture, block-shaped Mg2Sn, and Zn/Sn-rich nanoscale precipitate bands along the grain boundary and the interdendrite. Nanoscale α-Mn dispersoids formed in the grain in the ZTM441 alloy, while no α-Mn formed in the ZTM441-0.3Al alloy instead of nanoscale Al3Mn2 particles. In the ZTM441 as-cast alloy, part of the Zn element is dissolved into the α-Mn phase, and part of the Mn element is dissolved into the MgZn2 phase, but in the ZTM441-0.3Al alloy, there are no such characteristics of mutual solubility. Zn and Mn elements are easy to combine in ZTM441 as-cast alloy, while Al and Mn are easy to combine in ZTM441-0.3Al as-cast alloy. The Mg-Zn phases have not only MgZn2-type crystal structure but also Mg4Zn7- and Mg149Zn-type crystal structure in the ZTM441-0.3Al as-cast alloy. The addition of Al changes the combination of Mn and Zn, promotes the formation of Al3Mn2, and the growth of the grain.
Open AccessStudy on the Microstructure of Mg-4Zn-4Sn-1Mn-xAl As-Cast Alloys
In this study, the microstructure of the Mg-4Zn-4Sn-1Mn-xAl (x = 0, 0.3 wt.%, denoted as ZTM441 and ZTM441-0.3Al) as-cast alloys was investigated using scanning electron microscopy (SEM), focused-ion/electron-beam (FIB) micromachining, transmission electron microscopy (TEM), and high-angle annular dark-field scanning transmission electron microscopy (HAADF-STEM). The analysis results revealed that the microstructure of the ZTM441 and ZTM441-0.3Al as-cast alloys both mainly consist of the α-Mg matrix, skeleton-shaped MgZn2 eutectic texture, block-shaped Mg2Sn, and Zn/Sn-rich nanoscale precipitate bands along the grain boundary and the interdendrite. Nanoscale α-Mn dispersoids formed in the grain in the ZTM441 alloy, while no α-Mn formed in the ZTM441-0.3Al alloy instead of nanoscale Al3Mn2 particles. In the ZTM441 as-cast alloy, part of the Zn element is dissolved into the α-Mn phase, and part of the Mn element is dissolved into the MgZn2 phase, but in the ZTM441-0.3Al alloy, there are no such characteristics of mutual solubility. Zn and Mn elements are easy to combine in ZTM441 as-cast alloy, while Al and Mn are easy to combine in ZTM441-0.3Al as-cast alloy. The Mg-Zn phases have not only MgZn2-type crystal structure but also Mg4Zn7- and Mg149Zn-type crystal structure in the ZTM441-0.3Al as-cast alloy. The addition of Al changes the combination of Mn and Zn, promotes the formation of Al3Mn2, and the growth of the grain.
- 13 February 2023
- Published by Elsevier in Materials Chemistry and Physics
- Vol. 300, 127500
The discharge and corrosion performances of as-cast Mg-Ga-Sn anodes for the primary magnesium-air battery
- 13 February 2023
- Published by Elsevier in Materials Chemistry and Physics
- Vol. 300, 127500
The discharge and corrosion performances of as-cast Mg-Ga-Sn anodes for the primary magnesium-air battery
- Open Access
- 15 November 2022
- Published by Oxford University Press (OUP) in Regenerative Biomaterials
- Vol. 10, rbac093
Plain metallic biomaterials: opportunities and challenges
The ‘plainification of materials’ has been conceptualized to promote the sustainable development of materials. This perspective, for the first time in the field of biomaterials, proposes and defines ‘plain metallic biomaterials (PMBs)’ with demonstrated research and application case studies of pure titanium with high strength and toughness, and biodegradable, fine-grained and high-purity magnesium. Then, after discussing the features, benefits and opportunities of PMBs, the challenges are analyzed from both technical and regulatory aspects. Regulatory perspectives on PMB-based medical devices are also provided for the benefit of future research, development and commercialization.
- 15 November 2022
- Published by Oxford University Press (OUP) in Regenerative Biomaterials
- Vol. 10, rbac093
Open AccessPlain metallic biomaterials: opportunities and challenges
The ‘plainification of materials’ has been conceptualized to promote the sustainable development of materials. This perspective, for the first time in the field of biomaterials, proposes and defines ‘plain metallic biomaterials (PMBs)’ with demonstrated research and application case studies of pure titanium with high strength and toughness, and biodegradable, fine-grained and high-purity magnesium. Then, after discussing the features, benefits and opportunities of PMBs, the challenges are analyzed from both technical and regulatory aspects. Regulatory perspectives on PMB-based medical devices are also provided for the benefit of future research, development and commercialization.
- Open Access
- 3 November 2021
- Published by Frontiers Media SA in Frontiers in Materials
- Vol. 8
Research on Microstructure, Mechanical Properties and Electromagnetic Shielding Properties of Mg-6Zn-3Sn-0.5Cu Alloy
In this paper, the microstructure, electromagnetic shielding properties and mechanical properties of Mg-6Zn-3Sn-0.5Cu alloys are studied. As indicated from the results, the phases in the as-cast alloy comprise α-Mg, MgZnCu, Mg2Sn and Mg2Zn3 phases. After homogenization, Mg2Sn and Mg2Zn3 phases are decomposed, but the MgZnCu phase remains. During extrusion, complete dynamic recrystallization (DRX) occurs, and the spherical Mg2Sn phase precipitates dynamically. Due to considerable rod-like β′1 phases precipitate by complying with the [0001] Mg direction, the mechanical properties of aged alloys are remarkably enhanced. The peak-aged alloy achieves the tensile strength of 366 MPa, the yield strength of 358 MPa and the elongation of 7%. With the increase in the size of the β′1 phase, the mechanical properties of the over-aged alloy are reduced. Since the phases precipitate, the electrical conductivity of the alloy is enhanced, and the internal reflective interface increases, so the aged alloys exhibit improved electromagnetic shielding performance. The electromagnetic shielding efficiency of the peak-aged alloy exceeds 105 dB in the range of 30–1500 MHz, showing the best match between mechanical and electromagnetic shielding properties.
- 3 November 2021
- Published by Frontiers Media SA in Frontiers in Materials
- Vol. 8
Open AccessResearch on Microstructure, Mechanical Properties and Electromagnetic Shielding Properties of Mg-6Zn-3Sn-0.5Cu Alloy
In this paper, the microstructure, electromagnetic shielding properties and mechanical properties of Mg-6Zn-3Sn-0.5Cu alloys are studied. As indicated from the results, the phases in the as-cast alloy comprise α-Mg, MgZnCu, Mg2Sn and Mg2Zn3 phases. After homogenization, Mg2Sn and Mg2Zn3 phases are decomposed, but the MgZnCu phase remains. During extrusion, complete dynamic recrystallization (DRX) occurs, and the spherical Mg2Sn phase precipitates dynamically. Due to considerable rod-like β′1 phases precipitate by complying with the [0001] Mg direction, the mechanical properties of aged alloys are remarkably enhanced. The peak-aged alloy achieves the tensile strength of 366 MPa, the yield strength of 358 MPa and the elongation of 7%. With the increase in the size of the β′1 phase, the mechanical properties of the over-aged alloy are reduced. Since the phases precipitate, the electrical conductivity of the alloy is enhanced, and the internal reflective interface increases, so the aged alloys exhibit improved electromagnetic shielding performance. The electromagnetic shielding efficiency of the peak-aged alloy exceeds 105 dB in the range of 30–1500 MHz, showing the best match between mechanical and electromagnetic shielding properties.
- Open Access
Microstructure and Hot Deformation Behavior of the Mg–8 wt.% Sn–1.5 wt.% Al Alloy
Mg–Sn–Al alloy is a new type of heat-resistant magnesium alloy with great potential and the hot deformation process of this alloy is of great significance for its application. The microstructure, hot deformation behavior, textural evolution, and processing map of a Mg–8 wt.% Sn–1.5 wt.% Al alloy were studied. A Gleeble 1500 D thermo-mechanical simulator was used. The temperature of deformation was 653 to 773 K, the strain rate was 0.001–1 s−1, and the maximum deformation degree was 60%. The obtained results show that the rheological stress of the alloy decreases with an increase in deformation temperature and increases with an increase in the strain rate. The alloy is completely dynamically recrystallized at 653 K, and the entire structure is formed of homogeneous crystals/grains, with small secondary phase particles distributed at the crystal boundary. The mean apparent activation energy of hot compression deformation is 153.5 kJ/mol. The Mg–8 wt.% Sn–1.5 wt.% Al alloy exhibits excellent plastic deformation properties, an expansive thermal processing interval, and a narrow instability zone under the test temperature and deformation rate. The optimal process parameters of the alloy comprise deformation temperatures between 603 and 633 K and strain rates of 0.03 to 0.005 s−1.
Open AccessMicrostructure and Hot Deformation Behavior of the Mg–8 wt.% Sn–1.5 wt.% Al Alloy
Mg–Sn–Al alloy is a new type of heat-resistant magnesium alloy with great potential and the hot deformation process of this alloy is of great significance for its application. The microstructure, hot deformation behavior, textural evolution, and processing map of a Mg–8 wt.% Sn–1.5 wt.% Al alloy were studied. A Gleeble 1500 D thermo-mechanical simulator was used. The temperature of deformation was 653 to 773 K, the strain rate was 0.001–1 s−1, and the maximum deformation degree was 60%. The obtained results show that the rheological stress of the alloy decreases with an increase in deformation temperature and increases with an increase in the strain rate. The alloy is completely dynamically recrystallized at 653 K, and the entire structure is formed of homogeneous crystals/grains, with small secondary phase particles distributed at the crystal boundary. The mean apparent activation energy of hot compression deformation is 153.5 kJ/mol. The Mg–8 wt.% Sn–1.5 wt.% Al alloy exhibits excellent plastic deformation properties, an expansive thermal processing interval, and a narrow instability zone under the test temperature and deformation rate. The optimal process parameters of the alloy comprise deformation temperatures between 603 and 633 K and strain rates of 0.03 to 0.005 s−1.
- Open Access
Microstructure, Hot Deformation Behavior, and Recrystallization Behavior of Zn-1Fe-1Mg Alloy under Isothermal Compression
Nowadays, wrought zinc-based biodegradable alloys are favored by researchers, due to their excellent mechanical properties and suitable degradation rates. However, there are few research studies on their thermal deformation behavior at present. This study took Zn-1Fe-1Mg and explored its microstructural change, deformation, recrystallization behavior and processing map by means of the thermal simulation experiment, at temperatures ranging from 235 °C to 340 °C and strain rates ranging from 10−2 s−1 to 10 s−1. The constitutive model was constructed using the Arrhenius formula. The results indicated that the evolution of microstructure included the dynamic recrystallization (DRX) of the Zn matrix, the spheroidization of the Mg2Zn11 phase, and breaking of the FeZn13 phase. The subgrains observed within the deformed grain resulted mainly from continuous dynamic recrystallization (CDRX). The precipitated FeZn13 grains overlapped with the precipitated MgZn2 from the matrix, thus forming a spine-like structure at the phase interface. After compression, the alloy possessed a strong basal texture. Affected by the change of Zn twins, textural strength decreased at first and then increased as the deformation temperature rose. There was only a small unstable region in the processing map, indicating that the alloy exhibited good machinability.
Open AccessMicrostructure, Hot Deformation Behavior, and Recrystallization Behavior of Zn-1Fe-1Mg Alloy under Isothermal Compression
Nowadays, wrought zinc-based biodegradable alloys are favored by researchers, due to their excellent mechanical properties and suitable degradation rates. However, there are few research studies on their thermal deformation behavior at present. This study took Zn-1Fe-1Mg and explored its microstructural change, deformation, recrystallization behavior and processing map by means of the thermal simulation experiment, at temperatures ranging from 235 °C to 340 °C and strain rates ranging from 10−2 s−1 to 10 s−1. The constitutive model was constructed using the Arrhenius formula. The results indicated that the evolution of microstructure included the dynamic recrystallization (DRX) of the Zn matrix, the spheroidization of the Mg2Zn11 phase, and breaking of the FeZn13 phase. The subgrains observed within the deformed grain resulted mainly from continuous dynamic recrystallization (CDRX). The precipitated FeZn13 grains overlapped with the precipitated MgZn2 from the matrix, thus forming a spine-like structure at the phase interface. After compression, the alloy possessed a strong basal texture. Affected by the change of Zn twins, textural strength decreased at first and then increased as the deformation temperature rose. There was only a small unstable region in the processing map, indicating that the alloy exhibited good machinability.
- Open Access
Precipitation Behavior of Mg-7Gd-3Y-2Zn-0.5Zr Alloy during Isothermal Aging
Precipitate phases in an Mg–7Gd–3Y–2Zn–0.5Zr alloy aged isothermally at 240 °C were examined using high-resolution transmission electron microscopy (TEM) and high-angle annular dark-field scanning TEM. The two types of precipitation sequence that involve Mg–Gd and long period stacking ordered (LPSO) type were found. The LPSO type sequence consisted of the precipitation of γ′′, γ′, 14H-LPSO/18R-LPSO. The Mg–Gd type precipitation sequence involved the formation of β′(b.c.o.) and β1(f.c.c.). The sequence, morphology, distribution, and crystal structure of these precipitates formed during isothermal aging were investigated. The results indicated that the priority precipitation of Mg–Gd and LPSO type sequences during aging can be affected by Nd, which has a higher diffusion coefficient than Gd and Y. The dislocation structures and strengthening mechanism were also discussed.
Open AccessPrecipitation Behavior of Mg-7Gd-3Y-2Zn-0.5Zr Alloy during Isothermal Aging
Precipitate phases in an Mg–7Gd–3Y–2Zn–0.5Zr alloy aged isothermally at 240 °C were examined using high-resolution transmission electron microscopy (TEM) and high-angle annular dark-field scanning TEM. The two types of precipitation sequence that involve Mg–Gd and long period stacking ordered (LPSO) type were found. The LPSO type sequence consisted of the precipitation of γ′′, γ′, 14H-LPSO/18R-LPSO. The Mg–Gd type precipitation sequence involved the formation of β′(b.c.o.) and β1(f.c.c.). The sequence, morphology, distribution, and crystal structure of these precipitates formed during isothermal aging were investigated. The results indicated that the priority precipitation of Mg–Gd and LPSO type sequences during aging can be affected by Nd, which has a higher diffusion coefficient than Gd and Y. The dislocation structures and strengthening mechanism were also discussed.