Alexander N. Taldenkov
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Research Subjects
Research Interests
Alexander N. Taldenkov has a total of 46 co-authors. Here are the top co-authors by number of shared publications:
- Alexander V. Inyushkin
National Research Center Kurchatov Institute 1 , Moscow 123182, Russia
7 shared publications - Andrey A. Khomich
V. A. Kotelnikov Radio-Engineering and Electronics Institute of the Russian Academy of Sciences, Fryazino, Russia
4 shared publications - Dmitry V. Averyanov4 shared publications
- Ivan S. Sokolov
National Research Center “Kurchatov Institute”, Kurchatov Sq. 1, Moscow 123182, Russia
4 shared publications Oleg E. Parfenov
4 shared publications- Victor G. Ralchenko
Department of Light-Induced Surface Phenomena, Prokhorov General Physics Institute of the Russian Academy of Sciences, Vavilov Str. 38, 119991 Moscow, Russia
4 shared publications
Latest Publications
- 1 August 2026
- Published by Pleiades Publishing Ltd in JETP Letters
- Vol. 124 (4) , 281-290
Radiation-Induced Defects in Electron-Irradiated Pure and Nitrogen-Doped High-Pressure High-Temperature Diamond: Decrease in the Thermal Conductivity
The effect of 3-MeV electron irradiation at a fluence of 5 × 1018 cm–2 on the thermal conductivity κ(T) of type IIa and type Ib high-pressure high-temperature diamond single crystals with nitrogen concentrations of less than 1 ppm and approximately 70 ppm, respectively, has been studied. Irradiation reduces the thermal conductivity κ(T) over the entire studied temperature range 5 K < T < 410 K. For pure diamond, the strongest decrease in κ(T) by a factor of 350 is observed at 25–30 K, but the thermal conductivity κ(T) at room temperature T = 300 K decreases by a factor of only 1.56. Compared to pure diamond, the thermal conductivity of irradiated doped diamond decreases much less strongly at low temperatures, but more strongly at T > 140 K. After irradiation, the difference in the reduction of the thermal conductivity between the two types of diamond is so large that κ(T) for doped diamond is larger than that for pure diamond at T < 50 K and is an order of magnitude larger at 5 K. Experimental data allow the assumption that the rate of phonon scattering by neutral radiation defects—vacancies, their aggregates, and Frenkel pairs (pairs of interacting interstitial atoms and vacancies)—in pure diamond is much higher than that by such negatively charged defects in nitrogen-doped diamond at low temperatures. However, the ratio of scattering rates becomes inverse at high temperatures.
- 1 August 2026
- Published by Pleiades Publishing Ltd in JETP Letters
- Vol. 124 (4) , 281-290
Radiation-Induced Defects in Electron-Irradiated Pure and Nitrogen-Doped High-Pressure High-Temperature Diamond: Decrease in the Thermal Conductivity
The effect of 3-MeV electron irradiation at a fluence of 5 × 1018 cm–2 on the thermal conductivity κ(T) of type IIa and type Ib high-pressure high-temperature diamond single crystals with nitrogen concentrations of less than 1 ppm and approximately 70 ppm, respectively, has been studied. Irradiation reduces the thermal conductivity κ(T) over the entire studied temperature range 5 K < T < 410 K. For pure diamond, the strongest decrease in κ(T) by a factor of 350 is observed at 25–30 K, but the thermal conductivity κ(T) at room temperature T = 300 K decreases by a factor of only 1.56. Compared to pure diamond, the thermal conductivity of irradiated doped diamond decreases much less strongly at low temperatures, but more strongly at T > 140 K. After irradiation, the difference in the reduction of the thermal conductivity between the two types of diamond is so large that κ(T) for doped diamond is larger than that for pure diamond at T < 50 K and is an order of magnitude larger at 5 K. Experimental data allow the assumption that the rate of phonon scattering by neutral radiation defects—vacancies, their aggregates, and Frenkel pairs (pairs of interacting interstitial atoms and vacancies)—in pure diamond is much higher than that by such negatively charged defects in nitrogen-doped diamond at low temperatures. However, the ratio of scattering rates becomes inverse at high temperatures.
- 26 March 2025
- Published by AIP Publishing in Journal of Applied Physics
- Vol. 137 (12)
Thermal conductivity of chemical vapor deposition diamond enriched with 13C isotope
Thermal conductivity κ(T) of single-crystal CVD diamond enriched with 13C isotope to 98.16% was measured by the method of steady-state longitudinal heat flow in the temperature range from 6 to 410 K. This crystal with low nitrogen impurity content (<50 ppb) showed thermal conductivity 2010±50 W m−1 K−1 at 300 K (with a maximum of 12 100 W m−1 K−1 at 83 K), which is significantly lower than that of diamond with natural isotopic composition: κ(300K)=2360±50 W m−1 K−1. The measured data were analyzed using first-principles theory and the Callaway model, taking into account phonon scattering in three-phonon processes, scattering at sample boundaries and at isotopes. The first-principles calculations overestimate the thermal conductivity compared to the measured one near and to the right of the κ(T) peak, indicating the presence of significant additional phonon scattering by lattice defects in the studied chemically pure diamond samples. The results of both theoretical approaches for thermal conductivity at 300 K are in good agreement with our measured data and other published experimental data for isotopically modified diamonds. First-principles calculations yield a thermal conductivity ratio of κ12(T)/κ13(T)=1.072 for monoisotopic defect-free 12C and 13C crystals at 300 K. This ratio decreases at high temperatures to a value of 1.041 according to the Leibfried–Schlömann theory and to a value of 0.921 at very low temperatures.
- 26 March 2025
- Published by AIP Publishing in Journal of Applied Physics
- Vol. 137 (12)
Thermal conductivity of chemical vapor deposition diamond enriched with 13C isotope
Thermal conductivity κ(T) of single-crystal CVD diamond enriched with 13C isotope to 98.16% was measured by the method of steady-state longitudinal heat flow in the temperature range from 6 to 410 K. This crystal with low nitrogen impurity content (<50 ppb) showed thermal conductivity 2010±50 W m−1 K−1 at 300 K (with a maximum of 12 100 W m−1 K−1 at 83 K), which is significantly lower than that of diamond with natural isotopic composition: κ(300K)=2360±50 W m−1 K−1. The measured data were analyzed using first-principles theory and the Callaway model, taking into account phonon scattering in three-phonon processes, scattering at sample boundaries and at isotopes. The first-principles calculations overestimate the thermal conductivity compared to the measured one near and to the right of the κ(T) peak, indicating the presence of significant additional phonon scattering by lattice defects in the studied chemically pure diamond samples. The results of both theoretical approaches for thermal conductivity at 300 K are in good agreement with our measured data and other published experimental data for isotopically modified diamonds. First-principles calculations yield a thermal conductivity ratio of κ12(T)/κ13(T)=1.072 for monoisotopic defect-free 12C and 13C crystals at 300 K. This ratio decreases at high temperatures to a value of 1.041 according to the Leibfried–Schlömann theory and to a value of 0.921 at very low temperatures.
- 17 January 2024
- Published by Elsevier in Surfaces and Interfaces
- Vol. 45
Breakdown of rotational invariance in cube-on-cube epitaxy of rock-salt oxides on Si and Ge
- 17 January 2024
- Published by Elsevier in Surfaces and Interfaces
- Vol. 45
Breakdown of rotational invariance in cube-on-cube epitaxy of rock-salt oxides on Si and Ge
- 21 August 2023
- Published by Elsevier in Diamond and Related Materials
- Vol. 139
Thermal conductivity of type-Ib HPHT synthetic diamond irradiated with electrons
- 21 August 2023
- Published by Elsevier in Diamond and Related Materials
- Vol. 139
Thermal conductivity of type-Ib HPHT synthetic diamond irradiated with electrons
- 10 January 2023
- Published by AIP Publishing in Journal of Applied Physics
- Vol. 133 (2) , 025102
Thermal conductivity of pink CVD diamond: Influence of nitrogen-related centers
Thermal conductivity of single-crystal CVD diamond lightly doped (about 3 ppm) with nitrogen has been measured at temperatures from 5.7 to 410 K. The sample was carefully characterized by optical absorption and photoluminescence spectroscopy for the presence of impurities. Nine different optically active defects related with nitrogen, hydrogen, and silicon impurities have been identified and quantified. This pink-tint crystal showed a high thermal conductivity of W cm K at room temperature, which is very close to the highest value ever measured at about 25 W cm K for diamonds of natural isotopic composition. At the same time, the of the crystal showed strong suppression % at temperatures K with a maximum decrease of 2.7 times at K compared to high purity diamonds. This behavior of the conductivity is attributed to a phonon scattering by charge carriers bound to nitrogen-related impurity centers, which is ineffective, however, at room and higher temperatures. The has been calculated within the model based on the Callaway theory taking into account the elastic phonon scattering off charge carriers (holes and electrons) in the ground states of doping centers, and a very good agreement between the measured and theoretical data has been achieved. The model also gives a good approximation to the experimental data for given in the literature for synthetic and natural single-crystal diamonds.- 10 January 2023
- Published by AIP Publishing in Journal of Applied Physics
- Vol. 133 (2) , 025102
Thermal conductivity of pink CVD diamond: Influence of nitrogen-related centers
Thermal conductivity of single-crystal CVD diamond lightly doped (about 3 ppm) with nitrogen has been measured at temperatures from 5.7 to 410 K. The sample was carefully characterized by optical absorption and photoluminescence spectroscopy for the presence of impurities. Nine different optically active defects related with nitrogen, hydrogen, and silicon impurities have been identified and quantified. This pink-tint crystal showed a high thermal conductivity of W cm K at room temperature, which is very close to the highest value ever measured at about 25 W cm K for diamonds of natural isotopic composition. At the same time, the of the crystal showed strong suppression % at temperatures K with a maximum decrease of 2.7 times at K compared to high purity diamonds. This behavior of the conductivity is attributed to a phonon scattering by charge carriers bound to nitrogen-related impurity centers, which is ineffective, however, at room and higher temperatures. The has been calculated within the model based on the Callaway theory taking into account the elastic phonon scattering off charge carriers (holes and electrons) in the ground states of doping centers, and a very good agreement between the measured and theoretical data has been achieved. The model also gives a good approximation to the experimental data for given in the literature for synthetic and natural single-crystal diamonds.- 1 November 2021
- Published by Pleiades Publishing Ltd in Physics of the Solid State
- Vol. 63 (11) , 1638-1642
Influence of Substrate Crystal Structure on the Magnetic Anisotropy of MnxSi1 – x (x ≈ 0.5) Films
Thin films of MnxSi1 – x (x ≈ 0.5) alloy were synthesized by pulsed laser deposition in a droplet-free mode on sapphire substrates with different crystallographic cut-off plane orientations (c-Al2O3 and r-Al2O3) at various laser energy densities E at the polycrystalline target MnSi. X-ray structure properties, as well as static and resonance magnetic characteristics of the films depending on the value of E and substrate orientation were investigated. The presence of a ferromagnetic phase with an unusually high Curie temperature TC ~ 300 K which is untypical of MnSi single crystals (TC ~ 30 K) was revealed in films deposited using high laser energy densities E > 6 J/cm2 at the target. The magnetic moment of the films on c-Al2O3 substrates is somewhat larger than in the case of r-Al2O3 substrates. Moreover, the films deposited on c-Al2O3 substrates show significantly higher values of the effective magnetic anisotropy field 4πMeff, measured by ferromagnetic resonance. Obtained data show that the structure of the substrate has a remarkable influence on the formation process and magnetic properties of the high-temperature ferromagnetic phase in the MnxSi1 – x films.
- 1 November 2021
- Published by Pleiades Publishing Ltd in Physics of the Solid State
- Vol. 63 (11) , 1638-1642
Influence of Substrate Crystal Structure on the Magnetic Anisotropy of MnxSi1 – x (x ≈ 0.5) Films
Thin films of MnxSi1 – x (x ≈ 0.5) alloy were synthesized by pulsed laser deposition in a droplet-free mode on sapphire substrates with different crystallographic cut-off plane orientations (c-Al2O3 and r-Al2O3) at various laser energy densities E at the polycrystalline target MnSi. X-ray structure properties, as well as static and resonance magnetic characteristics of the films depending on the value of E and substrate orientation were investigated. The presence of a ferromagnetic phase with an unusually high Curie temperature TC ~ 300 K which is untypical of MnSi single crystals (TC ~ 30 K) was revealed in films deposited using high laser energy densities E > 6 J/cm2 at the target. The magnetic moment of the films on c-Al2O3 substrates is somewhat larger than in the case of r-Al2O3 substrates. Moreover, the films deposited on c-Al2O3 substrates show significantly higher values of the effective magnetic anisotropy field 4πMeff, measured by ferromagnetic resonance. Obtained data show that the structure of the substrate has a remarkable influence on the formation process and magnetic properties of the high-temperature ferromagnetic phase in the MnxSi1 – x films.
- Open Access
Isotope Effect in Thermal Conductivity of Polycrystalline CVD-Diamond: Experiment and Theory
We measured the thermal conductivity of polycrystalline diamond with natural (C) and isotopically enriched (C content up to 99.96 at.%) compositions over a broad temperature T range, from 5 to 410 K. The high quality polycrystalline diamond wafers were produced by microwave plasma chemical vapor deposition in CH-H mixtures. The thermal conductivity of C diamond along the wafer, as precisely determined using a steady-state longitudinal heat flow method, exceeds much that of the C sample at K. The enriched sample demonstrates the value of W cm K that is higher than the ever reported conductivity of natural and synthetic single crystalline diamonds with natural isotopic composition. A phenomenological theoretical model based on the full version of Callaway theory of thermal conductivity is developed which provides a good approximation of the experimental data. The role of different resistive scattering processes, including due to minor isotope C atoms, defects, and grain boundaries, is estimated from the data analysis. The model predicts about a 37% increase of thermal conductivity for impurity and dislocation free polycrystalline chemical vapor deposition (CVD)-diamond with the C-enriched isotopic composition at room temperature.Open AccessIsotope Effect in Thermal Conductivity of Polycrystalline CVD-Diamond: Experiment and Theory
We measured the thermal conductivity of polycrystalline diamond with natural (C) and isotopically enriched (C content up to 99.96 at.%) compositions over a broad temperature T range, from 5 to 410 K. The high quality polycrystalline diamond wafers were produced by microwave plasma chemical vapor deposition in CH-H mixtures. The thermal conductivity of C diamond along the wafer, as precisely determined using a steady-state longitudinal heat flow method, exceeds much that of the C sample at K. The enriched sample demonstrates the value of W cm K that is higher than the ever reported conductivity of natural and synthetic single crystalline diamonds with natural isotopic composition. A phenomenological theoretical model based on the full version of Callaway theory of thermal conductivity is developed which provides a good approximation of the experimental data. The role of different resistive scattering processes, including due to minor isotope C atoms, defects, and grain boundaries, is estimated from the data analysis. The model predicts about a 37% increase of thermal conductivity for impurity and dislocation free polycrystalline chemical vapor deposition (CVD)-diamond with the C-enriched isotopic composition at room temperature.