Irina Nikolaevna Sevostyanova
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Previous Organizations / Institutes
The organizations / institutes from the scholar's other articles in the past ten years
Irina Nikolaevna Sevostyanova has a total of 66 co-authors. Here are the top co-authors by number of shared publications:
- Nikolai L. Savchenko
Institute of Strength Physics and Materials Science, Siberian Branch, Russian Academy of Science, Tomsk, Russia
13 shared publications - Tatiana Yu. Sablina
Institute of Strength Physics and Materials Science of the Siberian Branch of the Russian Academy of Sciences, Tomsk, Russia
12 shared publications - Sergei N. Kulkov
Institute of Strength Physics and Materials Science, Siberian Branch, Russian Academy of Sciences, Tomsk, Russia
8 shared publications T. Yu. Sablina
Institute of Strength Physics and Materials Science, Siberian Branch, Russian Academy of Sciences, Tomsk, Russia
6 shared publications- Svetlana Petrovna Buyakova
Institute of Strength Physics and Materials Science, Siberian Branch of the Russian Academy of Sciences
5 shared publications S. N. Kulkov
Institute of Strength Physics and Materials Science, Siberian Branch, Russian Academy of Sciences, Tomsk, Russia
4 shared publications
Latest Publications
- Open Access
- 2 May 2026
- Published by Elsevier in SSRN Electronic Journal
Comparative Analysis of Self-Healing and Hetero-Healing of Macro-Cracks in WC–Co cemented carbide
The study comparatively analyzes self-healing and hetero-healing mechanisms for macro-cracks repair in WC–8 wt.% Co alloy. Self-healing was evaluated via stepwise isothermal treatments near the sintering temperature, while hetero-healing employed a developed eutectic infiltrant (30 wt.% WC–Co). Results indicate that intrinsic self-healing achieved only a 30% reduction in crack length, limited to defects ≤50 µm wide, and led to detrimental η-phase formation due to carbon depletion. Conversely, hetero-healing facilitated complete closure of macro-crack in a single treatment cycle. The healed region exhibited a narrow Co-enriched zone (~50 µm) without brittle phases, maintaining microstructural homogeneity with the bulk. The developed eutectic infiltrant protocol offers a superior strategy for restoring structural integrity in hardmetals, overcoming the kinetic and compositional constraints of self-healing.
- 2 May 2026
- Published by Elsevier in SSRN Electronic Journal
Open AccessComparative Analysis of Self-Healing and Hetero-Healing of Macro-Cracks in WC–Co cemented carbide
The study comparatively analyzes self-healing and hetero-healing mechanisms for macro-cracks repair in WC–8 wt.% Co alloy. Self-healing was evaluated via stepwise isothermal treatments near the sintering temperature, while hetero-healing employed a developed eutectic infiltrant (30 wt.% WC–Co). Results indicate that intrinsic self-healing achieved only a 30% reduction in crack length, limited to defects ≤50 µm wide, and led to detrimental η-phase formation due to carbon depletion. Conversely, hetero-healing facilitated complete closure of macro-crack in a single treatment cycle. The healed region exhibited a narrow Co-enriched zone (~50 µm) without brittle phases, maintaining microstructural homogeneity with the bulk. The developed eutectic infiltrant protocol offers a superior strategy for restoring structural integrity in hardmetals, overcoming the kinetic and compositional constraints of self-healing.
- 3 July 2024
- Published by Springer Nature in Russian Physics Journal
- Vol. 67 (7) , 879-887
Effect of Pore Size on the Mechanical Properties and Deformation Behavior of Porous ZrO2(Y2O3) Ceramics Under Axial Compression
- 3 July 2024
- Published by Springer Nature in Russian Physics Journal
- Vol. 67 (7) , 879-887
Effect of Pore Size on the Mechanical Properties and Deformation Behavior of Porous ZrO2(Y2O3) Ceramics Under Axial Compression
- Open Access
- 30 August 2023
- Published by MDPI AG in Lubricants
- Vol. 11 (9) , 365
Towards Self-Lubricating Effect of In Situ Iron Tungstate in Rubbing WC/Mn13 Steel Cermet against a HSS Steel
We study the mechanism of formation of the multilayer structure of the subsurface regions of WC/Mn13 steel cermets after sliding on a steel disk at speeds from 10 to 37 m/s and contact pressure of 5 MPa in order to elucidate the fundamental role of the processes of tribooxidation on a worn surface in the formation of the tribomechanical properties of a large family of similar W/Fe-containing materials. It was shown that the maximum antifriction effect of WC/Mn13 steel cermets under conditions of high-speed sliding was due to in-situ generated FeWO4 that provided friction coefficient drop from ~0.17 to ~0.07 when sliding at 10 and 37 m/s, respectively. The sliding speed had its effect on the subsurface structure and tribolayer thickness, so micron-sized, mechanically mixed 3–4 μm-thick layers (MML) were generated in sliding at 10 and 20 m/s, whose wear occurred mainly by subsurface fracture and delamination of tile-shaped wear particles. Continuous tribolayers with 10–15 μm thickness were generated at 30–37 m/s with underlying zones containing fragmented and deformed WC grains. Such a structure provided plasticizing effect during sliding so that wear was mainly by flow of so plasticized subsurface layers.
- 30 August 2023
- Published by MDPI AG in Lubricants
- Vol. 11 (9) , 365
Open AccessTowards Self-Lubricating Effect of In Situ Iron Tungstate in Rubbing WC/Mn13 Steel Cermet against a HSS Steel
We study the mechanism of formation of the multilayer structure of the subsurface regions of WC/Mn13 steel cermets after sliding on a steel disk at speeds from 10 to 37 m/s and contact pressure of 5 MPa in order to elucidate the fundamental role of the processes of tribooxidation on a worn surface in the formation of the tribomechanical properties of a large family of similar W/Fe-containing materials. It was shown that the maximum antifriction effect of WC/Mn13 steel cermets under conditions of high-speed sliding was due to in-situ generated FeWO4 that provided friction coefficient drop from ~0.17 to ~0.07 when sliding at 10 and 37 m/s, respectively. The sliding speed had its effect on the subsurface structure and tribolayer thickness, so micron-sized, mechanically mixed 3–4 μm-thick layers (MML) were generated in sliding at 10 and 20 m/s, whose wear occurred mainly by subsurface fracture and delamination of tile-shaped wear particles. Continuous tribolayers with 10–15 μm thickness were generated at 30–37 m/s with underlying zones containing fragmented and deformed WC grains. Such a structure provided plasticizing effect during sliding so that wear was mainly by flow of so plasticized subsurface layers.
- Open Access
Evidence of Tribological Adaptation Controlled by Tribosynthesis of FeWO4 on an WC-Reinforced Electron Beam M2 Steel Coating Rubbed against a HSS Disk in a Range of Sliding Speeds
In the present work, the tribological experiments on sliding the electron beam composite M2+WC coating have been carried out with characterization of the sample microstructures and phases both before and after the testing using metallography, SEM, EDS, and XRD. The sliding in the speed range 0.8–3.6 m/s resulted in simultaneous reduction in both wear rate and coefficient of friction with the sliding speed. Investigations showed that such a tribological adaptation was due to the tribochemical generation of lubricative FeWO4 and Fe2WO6 mixed oxides and the generation of a mechanically mixed composite layer on the worn surfaces that consisted of carbide fragments, an oxidized metal matrix, and was lubricated by in-situ formed mixed iron-tungsten oxides.
Open AccessEvidence of Tribological Adaptation Controlled by Tribosynthesis of FeWO4 on an WC-Reinforced Electron Beam M2 Steel Coating Rubbed against a HSS Disk in a Range of Sliding Speeds
In the present work, the tribological experiments on sliding the electron beam composite M2+WC coating have been carried out with characterization of the sample microstructures and phases both before and after the testing using metallography, SEM, EDS, and XRD. The sliding in the speed range 0.8–3.6 m/s resulted in simultaneous reduction in both wear rate and coefficient of friction with the sliding speed. Investigations showed that such a tribological adaptation was due to the tribochemical generation of lubricative FeWO4 and Fe2WO6 mixed oxides and the generation of a mechanically mixed composite layer on the worn surfaces that consisted of carbide fragments, an oxidized metal matrix, and was lubricated by in-situ formed mixed iron-tungsten oxides.
- 1 November 2022
- Published by Springer Nature in Russian Physics Journal
- Vol. 65 (7) , 1116-1122
Deformation and Fracture of ZrO2 (Y2O3) Porous Ceramics During Axial Compression Measured by Digital Image Correlation
- 1 November 2022
- Published by Springer Nature in Russian Physics Journal
- Vol. 65 (7) , 1116-1122
Deformation and Fracture of ZrO2 (Y2O3) Porous Ceramics During Axial Compression Measured by Digital Image Correlation
- 1 August 2022
- Published by Springer Nature in Russian Physics Journal
- Vol. 65 (4) , 635-642
Influence of the Grain Size of ZrO2(Y2O3) Ceramics on the Hardness, Fracture Toughness and Formation of a Transformation-Deformation Relief in the Indentation Zone
- 1 August 2022
- Published by Springer Nature in Russian Physics Journal
- Vol. 65 (4) , 635-642
Influence of the Grain Size of ZrO2(Y2O3) Ceramics on the Hardness, Fracture Toughness and Formation of a Transformation-Deformation Relief in the Indentation Zone
- Open Access
- 4 July 2022
- Published by MDPI AG in Lubricants
- Vol. 10 (7) , 140
Self-Lubricating Effect of WC/Y–TZP–Al2O3 Hybrid Ceramic–Matrix Composites with Dispersed Hadfield Steel Particles during High-Speed Sliding against an HSS Disk
WC/Y–TZP–Al2O3 hybrid ceramic–matrix composites (CMCs) with dispersed Hadfield steel particles were sintered and then tested at sliding speeds in the range of 7–37 m/s and contact pressure 5 MPa. Fast and low-temperature sinter-forging allowed obtaining micron-sized WC grains, submicron-sized alumina-reinforced yttria partially stabilized polycrystalline tetragonal zirconia (Y–TZP–Al2O3), and evenly distributed Hadfield steel grains. Such a microstructure provided new hybrid characteristics combining high hardness with high fracture toughness and tribological adaptation. The CMCs demonstrated low friction and high wear resistance that were better than those demonstrated by other composite materials such as, for example, MAX-phase composites, zirconia-base ceramics, ZrB2-SiC ceramics, and metal matrix WC–(Fe–Mn–C) composites. These good tribological characteristics were obtained due to the in situ mechanochemical formation of iron tungstates FeWO4 and Fe2WO6 on the worn surfaces of composite samples. These mixed oxides were included in multilayer subsurface structures that provided the self-lubricating and self-healing effects in high-speed sliding because of their easy shear and quasi-viscous behavior.
- 4 July 2022
- Published by MDPI AG in Lubricants
- Vol. 10 (7) , 140
Open AccessSelf-Lubricating Effect of WC/Y–TZP–Al2O3 Hybrid Ceramic–Matrix Composites with Dispersed Hadfield Steel Particles during High-Speed Sliding against an HSS Disk
WC/Y–TZP–Al2O3 hybrid ceramic–matrix composites (CMCs) with dispersed Hadfield steel particles were sintered and then tested at sliding speeds in the range of 7–37 m/s and contact pressure 5 MPa. Fast and low-temperature sinter-forging allowed obtaining micron-sized WC grains, submicron-sized alumina-reinforced yttria partially stabilized polycrystalline tetragonal zirconia (Y–TZP–Al2O3), and evenly distributed Hadfield steel grains. Such a microstructure provided new hybrid characteristics combining high hardness with high fracture toughness and tribological adaptation. The CMCs demonstrated low friction and high wear resistance that were better than those demonstrated by other composite materials such as, for example, MAX-phase composites, zirconia-base ceramics, ZrB2-SiC ceramics, and metal matrix WC–(Fe–Mn–C) composites. These good tribological characteristics were obtained due to the in situ mechanochemical formation of iron tungstates FeWO4 and Fe2WO6 on the worn surfaces of composite samples. These mixed oxides were included in multilayer subsurface structures that provided the self-lubricating and self-healing effects in high-speed sliding because of their easy shear and quasi-viscous behavior.
- Open Access
- 4 May 2022
- Published by MDPI AG in Lubricants
- Vol. 10 (5) , 86
Self-Lubricating Effect of FeWO4 Tribologically Synthesized from WC-(Fe-Mn-C) Composite during High-Speed Sliding against a HSS Disk
WC-(Fe-Mn-C) composites with γ-iron and γ + α’ matrices were sintered and then tested at sliding speeds in the range 7–37 m/s. The coefficient of friction was exponentially reduced as a function of sliding speed reaching its minimum at 37 m/s. This behavior was provided by the mechanochemical formation of iron tungstate FeWO4 on the worn surfaces of composite samples. The lubricating effect of iron tungstate did not, however, allow for a reduction in wear. The worn surface was represented by a 3–10 μm-thickness tribological layer composed of fine WC and iron particles cemented by FeWO4. This layer provided the self-lubricating effect in high-speed (high-temperature) sliding because of its easy shear and quasi-viscous behavior. The underlying 25–65 μm of thickness layer was composed of only heat-affected WC and recrystallized iron grains.
- 4 May 2022
- Published by MDPI AG in Lubricants
- Vol. 10 (5) , 86
Open AccessSelf-Lubricating Effect of FeWO4 Tribologically Synthesized from WC-(Fe-Mn-C) Composite during High-Speed Sliding against a HSS Disk
WC-(Fe-Mn-C) composites with γ-iron and γ + α’ matrices were sintered and then tested at sliding speeds in the range 7–37 m/s. The coefficient of friction was exponentially reduced as a function of sliding speed reaching its minimum at 37 m/s. This behavior was provided by the mechanochemical formation of iron tungstate FeWO4 on the worn surfaces of composite samples. The lubricating effect of iron tungstate did not, however, allow for a reduction in wear. The worn surface was represented by a 3–10 μm-thickness tribological layer composed of fine WC and iron particles cemented by FeWO4. This layer provided the self-lubricating effect in high-speed (high-temperature) sliding because of its easy shear and quasi-viscous behavior. The underlying 25–65 μm of thickness layer was composed of only heat-affected WC and recrystallized iron grains.
- 1 March 2022
- Published by Pleiades Publishing Ltd in Physical Mesomechanics
- Vol. 25 (2) , 142-148
Deformation and Fracture Mechanics of WC-(Fe-Mn-C) Composite in Axial Compression
The paper analyzes the surface relief of a tungsten carbide–ferromanganese steel composite (WC–(Fe–Mn–C)) under axial compression, including its structure on the microscale (variation in coherent scattering region sizes and mode II stresses) and on the macroscale (accumulation of deformed WC grains and interface cracks, evolution of ordered shear bands). The analysis shows that compressing the composite decreases the average size of plastically deformed WC grains, increases the density of interface microcracks, and decreases the average shear band spacing. The composite reveals a stage character of deformation and prefracture correlating with its stress–strain curve. In the first strain hardening stage, the material is deformed in its matrix and WC grains without continuity loss. In the second stage, numerous shear macrobands oriented in two directions at ~45° to the loading axis appear on its free surfaces. The macrobands are rich in deformed grains and cracks. Their intersection gives rise to macrocracks of length 40–150 µm as precursors of catastrophic failure. Also presented are X-ray diffraction data on the fine crystal structure of the carbide and binder phases of WC–(Fe–Mn–C) at different loading stages. The data suggests that increasing the strain decreases the size of coherent scattering regions and increases the lattice microstress in both phases. The binder starts to deform earlier than the tungsten carbide. Most of the change in the fine crystal structure of the tungsten carbide falls on the stage of shear band formation.
- 1 March 2022
- Published by Pleiades Publishing Ltd in Physical Mesomechanics
- Vol. 25 (2) , 142-148
Deformation and Fracture Mechanics of WC-(Fe-Mn-C) Composite in Axial Compression
The paper analyzes the surface relief of a tungsten carbide–ferromanganese steel composite (WC–(Fe–Mn–C)) under axial compression, including its structure on the microscale (variation in coherent scattering region sizes and mode II stresses) and on the macroscale (accumulation of deformed WC grains and interface cracks, evolution of ordered shear bands). The analysis shows that compressing the composite decreases the average size of plastically deformed WC grains, increases the density of interface microcracks, and decreases the average shear band spacing. The composite reveals a stage character of deformation and prefracture correlating with its stress–strain curve. In the first strain hardening stage, the material is deformed in its matrix and WC grains without continuity loss. In the second stage, numerous shear macrobands oriented in two directions at ~45° to the loading axis appear on its free surfaces. The macrobands are rich in deformed grains and cracks. Their intersection gives rise to macrocracks of length 40–150 µm as precursors of catastrophic failure. Also presented are X-ray diffraction data on the fine crystal structure of the carbide and binder phases of WC–(Fe–Mn–C) at different loading stages. The data suggests that increasing the strain decreases the size of coherent scattering regions and increases the lattice microstress in both phases. The binder starts to deform earlier than the tungsten carbide. Most of the change in the fine crystal structure of the tungsten carbide falls on the stage of shear band formation.