Sureurg Khongtong
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Sureurg Khongtong has a total of 4 co-authors. Here are the top co-authors by number of shared publications:
Benjama Meethaworn
Materials Science and Engineering Programs, School of Engineering and Technology, Walailak University, Thasala, Nakhon Si Thammarat, Thailand
1 shared publication- Kamon Thinsurat
School of Engineering and Technology, Walailak University, Nakhon Si Thammarat 80160, Thailand
1 shared publication - Pravat Kumar Ray
Department of Electrical Engineering, National Institute of Technology, Rourkela, India
1 shared publication - Suratsavadee Koonlaboon Korkua
School of Engineering and Technology, Walailak University, Nakhon Si Thammarat 80160, Thailand
1 shared publication
Latest Publications
- Open Access
Cleaner Potential for Natural Rubber Drying Process Using Microwave Technology Powered by Solar Energy
To reduce carbon dioxide emissions from traditional drying methods, this research investigated the use of microwave technology for drying Standard Thai Rubber (STR) in Thailand. Commercial microwave ovens were modified and integrated with the microwave emitting power control system to maintain the appropriate temperature levels to evaporate the moisture from rubber. Throughout the drying process, the temperature of the rubber was measured both internally and outside. The results revealed that STR5L and STR20 could be dried satisfactorily and met the requirements for standard Thai rubber properties by utilizing 500 W for 140 and 120 min, respectively. By keeping the temperatures less than 150 °C, rubbers’ molecular structure is not destroyed from internal heat stress. Although utilizing less power for a longer period of time is possible, more energy was used, which is unfavorable. Compared to traditional hot air drying technologies, which take approximately 4–6 h for the drying process, microwave technology potentially reduces the drying time by half or more. If solar energy is used to supply electrical energy, 300,000 tons of Carbon dioxide can potentially be eliminated annually in the STR drying industry in Thailand by promoting approximately 1115 MW of Photovoltaic technology installations with the solar resources in southern Thailand.
Open AccessCleaner Potential for Natural Rubber Drying Process Using Microwave Technology Powered by Solar Energy
To reduce carbon dioxide emissions from traditional drying methods, this research investigated the use of microwave technology for drying Standard Thai Rubber (STR) in Thailand. Commercial microwave ovens were modified and integrated with the microwave emitting power control system to maintain the appropriate temperature levels to evaporate the moisture from rubber. Throughout the drying process, the temperature of the rubber was measured both internally and outside. The results revealed that STR5L and STR20 could be dried satisfactorily and met the requirements for standard Thai rubber properties by utilizing 500 W for 140 and 120 min, respectively. By keeping the temperatures less than 150 °C, rubbers’ molecular structure is not destroyed from internal heat stress. Although utilizing less power for a longer period of time is possible, more energy was used, which is unfavorable. Compared to traditional hot air drying technologies, which take approximately 4–6 h for the drying process, microwave technology potentially reduces the drying time by half or more. If solar energy is used to supply electrical energy, 300,000 tons of Carbon dioxide can potentially be eliminated annually in the STR drying industry in Thailand by promoting approximately 1115 MW of Photovoltaic technology installations with the solar resources in southern Thailand.
- 10 June 2020
- Published by Taylor & Francis in Wood Material Science & Engineering
- Vol. 16 (6) , 397-406
The tuneable rubberwood: roles of impregnated polymer level
This study exhibits the tuneable rubberwood with the actively controlled properties. Various amounts of polymethyl methacrylate (PMMA) were introduced into rubberwood tissues under the allowed environment. The embedded PMMA resulted to weight gaining up to about 60% and caused an increase in the density from 650 (for untreated rubberwood) to 1060 kg/m3 (for fully impregnated one). Additionally, scanning electron microscopic images revealed the evidence of the raising of PMMA amounts in the microstructure of treated rubberwood corresponding to the degrees of polymer impregnation. The embedded PMMA, from 0% to about 60% in wood tissues, enhanced water-resistant properties, i.e. the increasing in the surface contact angles for about 20 degrees, the improvement of water absorption for four times and the development of anti-swelling efficiency (ASE) for almost 20%, to the treated rubberwood. Mechanical properties, including shear, compressive and flexural strength of treated rubberwood were also gradually improved when higher levels of PMMA were incorporated into rubberwood. Moreover, the logarithm values of water absorption, ASE, shear strength and compressive strength revealed the linear tendency when the degree of impregnation was raised. This would provide an opportunity of treating rubberwood as a tuneable wood-polymer composite material for the designated applications.
- 10 June 2020
- Published by Taylor & Francis in Wood Material Science & Engineering
- Vol. 16 (6) , 397-406
The tuneable rubberwood: roles of impregnated polymer level
This study exhibits the tuneable rubberwood with the actively controlled properties. Various amounts of polymethyl methacrylate (PMMA) were introduced into rubberwood tissues under the allowed environment. The embedded PMMA resulted to weight gaining up to about 60% and caused an increase in the density from 650 (for untreated rubberwood) to 1060 kg/m3 (for fully impregnated one). Additionally, scanning electron microscopic images revealed the evidence of the raising of PMMA amounts in the microstructure of treated rubberwood corresponding to the degrees of polymer impregnation. The embedded PMMA, from 0% to about 60% in wood tissues, enhanced water-resistant properties, i.e. the increasing in the surface contact angles for about 20 degrees, the improvement of water absorption for four times and the development of anti-swelling efficiency (ASE) for almost 20%, to the treated rubberwood. Mechanical properties, including shear, compressive and flexural strength of treated rubberwood were also gradually improved when higher levels of PMMA were incorporated into rubberwood. Moreover, the logarithm values of water absorption, ASE, shear strength and compressive strength revealed the linear tendency when the degree of impregnation was raised. This would provide an opportunity of treating rubberwood as a tuneable wood-polymer composite material for the designated applications.