  • Effect of PBAT-g-MA as a compatibilizer towards PBAT/palm frond/palm stearin blend composite via compression molding

    by Nur Azrini Ramlee, Yoichi Tominaga, Mohd Fadzrul Ikhwan Mohd Noordin, Rahimi Mohd Shariff, Istikamah Subuki

  • Open Access

    Synthetization and Characterization of Yttria Stabilized Zirconia Powder from Amang Zircon Sand

    by Nur Fatinhanani Fatimah Norsham, Istikamah Subuki

    Zirconia is widely used in industry as it exhibits high strength and amazing properties. However, pure zirconia powder is often unstable to be used in high temperature applications due to phase transformation that will lead to fracture and crack. Hence, zirconia is doped with yttrium oxide in order to enhance zirconium content and stability as it helps to hinder the phase transformation of zirconia. Locally available Amang zircon sand from tin tailing industry in Malaysia can be an economical alternative to synthesize zirconia due to the high zirconium content. Sadly, the study on utilizing Amang zircon sand is scarce despite decomposition of zircon sand to zirconia has been intensely done by other countries. Therefore, a study on Amang zircon sand was done with alkali sodium hydroxide fusion to obtain zirconium oxychloride. Zirconium oxychloride precursor was then stabilized with yttrium oxide in varied concentration using coprecipitation method with ammonia solution. Amang yttria stabilized zirconia powder was then characterized in order to study the effect of yttrium oxide concentration on Amang yttria stabilized zirconia powder. X-ray florescence analysis confirmed the high zirconium content of 71.01 wt.% after increasing the yttrium oxide concentration to 5 wt.% with lesser silicon impurity of 2.94 wt.%. The diffraction patterns satisfied monoclinic yttria stabilized zirconia with minor tetragonal and cubic phase. The peaks became sharper as concentration increased due to the stabilization of zirconia powder. Tetragonal and cubic phase increased along with the concentration, but the concentration of yttrium oxide was insufficient to fully stabilized the synthesized zirconia powder. Morphology analysis showed yttria stabilized zirconia powder was angular and pyramidal with large grain size in which led to high tendency of monoclinic phase.

  • Open Access

    Application of Mixture Design for Optimization of Smoke Signal Formulation: A Comparative Study of KClO3 and KNO3 as Oxidizers

    by Noor Farahana Abdul Rahman, Istikamah Subuki, Zuraidah Salleh, Ahmad Hussein Abdul Hamid, Nurnadia Andenan, Azmi Minal, Mohammed Abdillah Ahmad Faid

    Smoke signals are traditionally used in military contexts, but in recent times, they have gained popularity among civilians. The M18 smoke grenade was designed with a highly reactive oxidizer, KClO3, and substituting it with a safer oxidizer, notably KNO3, is one way that helps provide a safer choice for civilian use. However, providing optimal formulations for both formulations helps in deciding whether KNO3 can be substituted for the traditional KClO3 oxidizer. One of the techniques for enhancing smoke formulation is the Design of Experiments (DOE). Many researchers these days are focusing on substituting the smoke chemicals for a safer option using a trial-and-error process. However, from the standpoint of environmental contamination, numerical testing to identify the most significant output causes air pollution and chemical waste, which is not only costly but also endangers sea life if not properly disposed of. Therefore, it is crucial to optimize the smoke formulation in order to decrease waste and air pollution as well as enable future mass production of the product for both military and civilian use. The purpose of this paper is to implement the mixture design tool of the DOE approach to determine the optimal formulation of smoke signals using KClO3-based formulations, as well as to provide a comparative analysis of substituting KNO3 to optimize KClO3-based formulations in terms of time and smoke emission. From the KClO3-based formulation (28.68 wt.% KClO3, 23.47 wt.% C12H22O11, 34.39 wt.% dye, and 13.46 wt.% MgCO3) with an average time of 73.43 seconds, an acceptable formulation with a data means of 73.43, substituting with KNO3 oxidizer gave an average of 80.18 seconds, in which the smoke emission was slightly thinner compared to KClO3. As a result, KNO3 can be used as an alternative oxidizer to KClO3, and the KClO3-optimized formulation can be considered a baseline for smoke formulation for future research.


  • Effect of Temperature on Zirconia Powder Synthesized from Amang Zirconium Oxychloride Precursor

    by Istikamah Subuki

    Silica (SiO2) is widely used in numerous applications, including ceramic membranes, and can be extracted from rice husks, which is an agricultural waste containing high amounts of silica. In fact, it is essential to reduce the vast amounts of discarded rice husks as open burning of the rice husk can have detrimental effects on the environment due to the release of hazardous pollutants. For the rice husk to be used, a suitable sintering temperature should be obtained to ensure the membrane synthesized has the desired porous structure. A high sintering temperature can affect the melting condition of the membrane’s porous structure. While a low sintering temperature may not give the required porosity. Therefore, this study aims to evaluate the effect of sintering temperature on the pore size of the membrane fabricated from kaolin, polyvinyl alcohol, and rice husk ash. The rice husk was initially treated with hydrochloric acid (HCl) and heated at 900 ℃ to produce rice husk ash. The membranes fabricated were then sintered at 1000 ℃ to 1400 ℃. X-ray fluorescence (XRF) results show that 71.36% of silica was successfully extracted from the rice husk. According to the XRD results, only two membranes sintered at 1300 °C and 1400 °C have crystallinity forms. Because the ceramic membrane contains a crystalline phase, it was determined that 1300 °C is an appropriate temperature for sintering. It also has a low absorption percentage (88.89%) and the desired porosity (69.93%).

  • Open Access

    Effect of Temperature on Zirconia Powder Synthesized from Amang Zirconium Oxychloride Precursor

    by Nur Fatinhanani Fatimah Norsham, Istikamah Subuki

    Polymorphic zirconia is economically attractive in various applications due to its low reactivity, high strength, and stability. Zirconia can be synthesized from locally available Amang zircon sand as an inexpensive green alternative as it has a high zirconium content as reported by previous report. Unfortunately, the study was only focused on the formation of zirconium oxychloride despite of high zirconium content from the improved alkali fusion method proposed. Therefore, a further study on zirconia powder calcined in varied temperatures from Amang zirconium oxychloride precursor was done. Amang zirconia powder was then characterized in order to study the effect of temperature on Amang zirconia powder. Elemental analysis showed that zirconium composition was affected by temperature and increased as the temperature increased with the highest zirconium content of 81.28 wt.% with low impurities after calcined at 800 °C for 4 hours. The phase analysis satisfied monoclinic zirconia with minor tetragonal and cubic phase with sharper peaks as calcined temperature increased. Increased tetragonal and cubic phase was observed as the temperature was increased. Morphology analysis showed zirconia powder was angular and pyramidal with large crystal size which led to high tendency of monoclinic phase. Calcination temperature of 800 °C was determined to be the most suitable temperature to calcine high purity zirconia powder using Amang zirconium oxychloride precursor.


  • Synthesis of smoke signal with potassium nitrate (KNO3) as the oxidizer

    by Istikamah Subuki, Zuraidah Salleh, Mecktin Molinka, Ahmad Hussein Abdul Hamid, Noor Farahana Abdul Rahman

    Pyrotechnic smoke is very commonly used in the military as a weapon and in photography as a background effect. The smoke signal can be sabotage, deceive, and pa


  • Open Access

    The Effect of Palm Stearin in Poly (Butylene Adipate-Co-Terephthalate) (PBAT)/ Poly (Lactic Acid) (PLA) Biodegradable Feedstock

    by Nur Azrini Ramlee, Ahmad Rafizan Mohamad Daud, Muhammad Hussain Ismail, Siti Fatimah Mohd Ariff, Istikamah Subuki

    Because of environmental concerns, the need to minimize reliance on fossil-based polymers and achieve sustainable growth is important today. In this study, poly (butylene adipate-co-terephthalate) (PBAT) and poly (lactic acid) (PLA) blend at 50/50 wt.% ratio were mixed with palm stearin (PS) ranging from 5 to 20 wt.%. The characterizations of the tri-component PBAT/PLA/PS polymer blend were done based on torque analysis, rheology, thermal properties, and mechanical properties. Results showed the PS induced the compatibilization to PBAT/PLA blend, with the evidence of both Tg PLA and PBAT shifter closer to each other. Moreover, the addition of the PS in the PBAT/PLA matrix decreased the torque value from 4 Nm to 2 Nm of the PBAT/PLA blends and reduce fluidity and showed good thermal stability properties, suggesting that the PS is an alternative material to compatibilized the PBAT/PLA blend. Evidently addition of 15 wt.% PS has also improved the PBAT/PLA blends properties such the elongation at break to approximately 200%.

  • Open Access

    Study of the Synthesis of Zirconia Powder from Zircon Sand obtained from Zircon Minerals Malaysia by Caustic Fusion Method

    by Istikamah Subuki, Mimi Fazzlinda Mohsin, Muhammad Hussain Ismail, Fazira Suriani Mohamed Fadzil

    The zircon powder from Zircon Minerals Malaysia is a pure premium grade zircon sand milled 1.5 µm that contain ZrSiO4, ZrO2, HfO2, SiO2, Al2O3, TiO2, and Fe2O3. The monoclinic zirconia powders were synthesized from the zircon sand of Zircon Minerals Malaysia, by caustic fusion method at calcination temperatures between 500 °C to 800 °C. The as-synthesized zirconia was characterized through X-Ray diffraction (XRD), scanning electron microscopy (SEM), thermogravimetric and differential thermal analysis (TG-DTA), and X-Ray fluorescence (XRF) techniques. The XRD results show two monoclinic phases of microcrystalline zirconia. Zirconia that was calcined at 600 °C obtained the highest value of ZrO2, which was 54.48%; followed by zirconia calcined at 700 °C, 800 °C, and 500 °C, which obtained the ZrO2 values of 53.58%, 52.41%, and 51.53%, respectively, based on the XRF analysis. As-synthesized zirconia showed monoclinic phases where the surface areas were 0.0635 m2/g, 0.135 m2/g, 0.0268 m2/g, and 0.0288 m2/g, for zirconia calcined at temperatures of 500 °C, 600 °C, 700 °C, and 800 °C, respectively. The surface structure of the powder that had been calcined at 600 C showed similarities with the commercial zirconia. The similarities of the synthesized zirconia and commercial zirconia showed that the zirconia powder could be synthesized using zircon sand by caustic fusion method, even though the content of zirconia was lower compared to that of the commercial zirconia powder.