Rositza Yakimova
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Research Subjects
Rositza Yakimova has a total of 62 co-authors. Here are the top co-authors by number of shared publications:
- Gholam Reza Yazdi
Department of Physics, Chemistry and Biology, Linköping University, SE-58183 Linköping, Sweden
4 shared publications M. Syväjärvi
IFM, Linköping University, SE-58183 Linköping, Sweden
3 shared publications- Volodymyr Khranovskyy
Department of Physics, Chemistry and Biology, Linköping University, SE-58183, Linköping, Sweden
3 shared publications - Alexei A. Zakharov
MAX-lab, Lund University, Lund S-22100, Sweden
2 shared publications - Chao Xia
Applied Nano Surfaces AB, Knivstagatan 12, SE 753 23 Uppsala, Sweden
2 shared publications - Chariya Virojanadara
Department of Physics and Measurement Technology, Linköping University, S-581 83 Linköping, Sweden
2 shared publications
Latest Publications
- Open Access
Thermal Stability of Epitaxial Graphene Electrodes for Conductive Polymer Nanofiber Devices
We used large area, monolayer graphene epitaxially grown on SiC (0001) as contact electrodes for polymer nanofiber devices. Our fabrication process, which avoids polymer resist residues on the graphene surface, results in graphene-polyaniline nanofiber devices with Ohmic contacts and electrical conductivity comparable to that of Au-nanofiber devices. We further checked the thermal stability of the graphene contacts to polyaniline devices by annealing up to T = 800 °C, the temperature at which polyaniline nanofibers are carbonized but the graphene electrode remains intact. The thermal stability and Ohmic contact of polymer nanofibers are demonstrated here, which together with the chemical stability and atomic flatness of graphene, make epitaxial graphene on SiC an attractive contact material for future all-carbon electronic devices.
Open AccessThermal Stability of Epitaxial Graphene Electrodes for Conductive Polymer Nanofiber Devices
We used large area, monolayer graphene epitaxially grown on SiC (0001) as contact electrodes for polymer nanofiber devices. Our fabrication process, which avoids polymer resist residues on the graphene surface, results in graphene-polyaniline nanofiber devices with Ohmic contacts and electrical conductivity comparable to that of Au-nanofiber devices. We further checked the thermal stability of the graphene contacts to polyaniline devices by annealing up to T = 800 °C, the temperature at which polyaniline nanofibers are carbonized but the graphene electrode remains intact. The thermal stability and Ohmic contact of polymer nanofibers are demonstrated here, which together with the chemical stability and atomic flatness of graphene, make epitaxial graphene on SiC an attractive contact material for future all-carbon electronic devices.
- Open Access
Role of the Potential Barrier in the Electrical Performance of the Graphene/SiC Interface
In spite of the great expectations for epitaxial graphene (EG) on silicon carbide (SiC) to be used as a next-generation high-performance component in high-power nano- and micro-electronics, there are still many technological challenges and fundamental problems that hinder the full potential of EG/SiC structures and that must be overcome. Among the existing problems, the quality of the graphene/SiC interface is one of the most critical factors that determines the electroactive behavior of this heterostructure. This paper reviews the relevant studies on the carrier transport through the graphene/SiC, discusses qualitatively the possibility of controllable tuning the potential barrier height at the heterointerface and analyses how the buffer layer formation affects the electronic properties of the combined EG/SiC system. The correlation between the sp2/sp3 hybridization ratio at the interface and the barrier height is discussed. We expect that the barrier height modulation will allow realizing a monolithic electronic platform comprising different graphene interfaces including ohmic contact, Schottky contact, gate dielectric, the electrically-active counterpart in p-n junctions and quantum wells.
Open AccessRole of the Potential Barrier in the Electrical Performance of the Graphene/SiC Interface
In spite of the great expectations for epitaxial graphene (EG) on silicon carbide (SiC) to be used as a next-generation high-performance component in high-power nano- and micro-electronics, there are still many technological challenges and fundamental problems that hinder the full potential of EG/SiC structures and that must be overcome. Among the existing problems, the quality of the graphene/SiC interface is one of the most critical factors that determines the electroactive behavior of this heterostructure. This paper reviews the relevant studies on the carrier transport through the graphene/SiC, discusses qualitatively the possibility of controllable tuning the potential barrier height at the heterointerface and analyses how the buffer layer formation affects the electronic properties of the combined EG/SiC system. The correlation between the sp2/sp3 hybridization ratio at the interface and the barrier height is discussed. We expect that the barrier height modulation will allow realizing a monolithic electronic platform comprising different graphene interfaces including ohmic contact, Schottky contact, gate dielectric, the electrically-active counterpart in p-n junctions and quantum wells.
- Open Access
Application of 2D Non-Graphene Materials and 2D Oxide Nanostructures for Biosensing Technology
The discovery of graphene and its unique properties has inspired researchers to try to invent other two-dimensional (2D) materials. After considerable research effort, a distinct “beyond graphene” domain has been established, comprising the library of non-graphene 2D materials. It is significant that some 2D non-graphene materials possess solid advantages over their predecessor, such as having a direct band gap, and therefore are highly promising for a number of applications. These applications are not limited to nano- and opto-electronics, but have a strong potential in biosensing technologies, as one example. However, since most of the 2D non-graphene materials have been newly discovered, most of the research efforts are concentrated on material synthesis and the investigation of the properties of the material. Applications of 2D non-graphene materials are still at the embryonic stage, and the integration of 2D non-graphene materials into devices is scarcely reported. However, in recent years, numerous reports have blossomed about 2D material-based biosensors, evidencing the growing potential of 2D non-graphene materials for biosensing applications. This review highlights the recent progress in research on the potential of using 2D non-graphene materials and similar oxide nanostructures for different types of biosensors (optical and electrochemical). A wide range of biological targets, such as glucose, dopamine, cortisol, DNA, IgG, bisphenol, ascorbic acid, cytochrome and estradiol, has been reported to be successfully detected by biosensors with transducers made of 2D non-graphene materials.
Open AccessApplication of 2D Non-Graphene Materials and 2D Oxide Nanostructures for Biosensing Technology
The discovery of graphene and its unique properties has inspired researchers to try to invent other two-dimensional (2D) materials. After considerable research effort, a distinct “beyond graphene” domain has been established, comprising the library of non-graphene 2D materials. It is significant that some 2D non-graphene materials possess solid advantages over their predecessor, such as having a direct band gap, and therefore are highly promising for a number of applications. These applications are not limited to nano- and opto-electronics, but have a strong potential in biosensing technologies, as one example. However, since most of the 2D non-graphene materials have been newly discovered, most of the research efforts are concentrated on material synthesis and the investigation of the properties of the material. Applications of 2D non-graphene materials are still at the embryonic stage, and the integration of 2D non-graphene materials into devices is scarcely reported. However, in recent years, numerous reports have blossomed about 2D material-based biosensors, evidencing the growing potential of 2D non-graphene materials for biosensing applications. This review highlights the recent progress in research on the potential of using 2D non-graphene materials and similar oxide nanostructures for different types of biosensors (optical and electrochemical). A wide range of biological targets, such as glucose, dopamine, cortisol, DNA, IgG, bisphenol, ascorbic acid, cytochrome and estradiol, has been reported to be successfully detected by biosensors with transducers made of 2D non-graphene materials.
- Open Access
Soft X-ray Exposure Promotes Na Intercalation in Graphene Grown on Si-Face SiC
An investigation of how electron/photon beam exposures affect the intercalation rate of Na deposited on graphene prepared on Si-face SiC is presented. Focused radiation from a storage ring is used for soft X-ray exposures while the electron beam in a low energy electron microscope is utilized for electron exposures. The microscopy and core level spectroscopy data presented clearly show that the effect of soft X-ray exposure is significantly greater than of electron exposure, i.e., it produces a greater increase in the intercalation rate of Na. Heat transfer from the photoelectrons generated during soft X-ray exposure and by the electrons penetrating the sample during electron beam exposure is suggested to increase the local surface temperature and thus the intercalation rate. The estimated electron flux density is 50 times greater for soft X-ray exposure compared to electron exposure, which explains the larger increase in the intercalation rate from soft X-ray exposure. Effects occurring with time only at room temperature are found to be fairly slow, but detectable. The graphene quality, i.e., domain/grain size and homogeneity, was also observed to be an important factor since exposure-induced effects occurred more rapidly on a graphene sample prepared in situ compared to on a furnace grown sample.
Open AccessSoft X-ray Exposure Promotes Na Intercalation in Graphene Grown on Si-Face SiC
An investigation of how electron/photon beam exposures affect the intercalation rate of Na deposited on graphene prepared on Si-face SiC is presented. Focused radiation from a storage ring is used for soft X-ray exposures while the electron beam in a low energy electron microscope is utilized for electron exposures. The microscopy and core level spectroscopy data presented clearly show that the effect of soft X-ray exposure is significantly greater than of electron exposure, i.e., it produces a greater increase in the intercalation rate of Na. Heat transfer from the photoelectrons generated during soft X-ray exposure and by the electrons penetrating the sample during electron beam exposure is suggested to increase the local surface temperature and thus the intercalation rate. The estimated electron flux density is 50 times greater for soft X-ray exposure compared to electron exposure, which explains the larger increase in the intercalation rate from soft X-ray exposure. Effects occurring with time only at room temperature are found to be fairly slow, but detectable. The graphene quality, i.e., domain/grain size and homogeneity, was also observed to be an important factor since exposure-induced effects occurred more rapidly on a graphene sample prepared in situ compared to on a furnace grown sample.
- Open Access
- 1 January 2014
- Published by Frontiers Media SA in Frontiers in Physics
- Vol. 2
Local electric field screening in bi-layer graphene devices
We present experimental studies of both local and macroscopic electrical effects in uniform single- (1LG) and bi-layer graphene (2LG) devices as well as in devices with non-uniform graphene coverage, under ambient conditions. DC transport measurements on sub-micron scale Hall bar devices were used to show a linear rise in carrier density with increasing amounts of 2LG coverage. Electrical scanning gate microscopy was used to locally top gate uniform and non-uniform devices in order to observe the effect of local electrical gating. We experimentally show a significant level of electric field screening by 2LG. We demonstrate that SGM technique is an extremely useful research tool for studies of local screening effects, which provides a complementary view on phenomena that are usually considered only within a macroscopic experimental scheme.
- 1 January 2014
- Published by Frontiers Media SA in Frontiers in Physics
- Vol. 2
Open AccessLocal electric field screening in bi-layer graphene devices
We present experimental studies of both local and macroscopic electrical effects in uniform single- (1LG) and bi-layer graphene (2LG) devices as well as in devices with non-uniform graphene coverage, under ambient conditions. DC transport measurements on sub-micron scale Hall bar devices were used to show a linear rise in carrier density with increasing amounts of 2LG coverage. Electrical scanning gate microscopy was used to locally top gate uniform and non-uniform devices in order to observe the effect of local electrical gating. We experimentally show a significant level of electric field screening by 2LG. We demonstrate that SGM technique is an extremely useful research tool for studies of local screening effects, which provides a complementary view on phenomena that are usually considered only within a macroscopic experimental scheme.
- Open Access
Is the Registry Between Adjacent Graphene Layers Grown on C-Face SiC Different Compared to That on Si-Face SiC
Graphene grown on C-face SiC substrates using two procedures, high and low growth temperature and different ambients, was investigated using Low Energy Electron Microscopy (LEEM), X-ray Photo Electron Electron Microscopy (XPEEM), selected area Low Energy Electron Diffraction (μ-LEED) and selected area Photo Electron Spectroscopy (μ-PES). Both types of samples showed formation of μm-sized grains of graphene. The sharp (1 × 1) μ-LEED pattern and six Dirac cones observed in constant energy photoelectron angular distribution patterns from a grain showed that adjacent layers are not rotated relative to each other, but that adjacent grains in general have different azimuthal orientations. Diffraction spots from the SiC substrate appeared in μ-LEED patterns collected at higher energies, showing that the rotation angle between graphene and SiC varied. C 1s spectra collected did not show any hint of a carbon interface layer. A hydrogen treatment applied was found to have a detrimental effect on the graphene quality for both types of samples, since the graphene domain/grain size was drastically reduced. From hydrogen treated samples, μ-LEED showed at first a clear (1 × 1) pattern, but within minutes, a pattern containing strong superstructure spots, indicating the presence of twisted graphene layers. The LEED electron beam was found to induce local desorption of hydrogen. Heating a hydrogenated C-face graphene sample did not restore the quality of the original as-grown sample.
Open AccessIs the Registry Between Adjacent Graphene Layers Grown on C-Face SiC Different Compared to That on Si-Face SiC
Graphene grown on C-face SiC substrates using two procedures, high and low growth temperature and different ambients, was investigated using Low Energy Electron Microscopy (LEEM), X-ray Photo Electron Electron Microscopy (XPEEM), selected area Low Energy Electron Diffraction (μ-LEED) and selected area Photo Electron Spectroscopy (μ-PES). Both types of samples showed formation of μm-sized grains of graphene. The sharp (1 × 1) μ-LEED pattern and six Dirac cones observed in constant energy photoelectron angular distribution patterns from a grain showed that adjacent layers are not rotated relative to each other, but that adjacent grains in general have different azimuthal orientations. Diffraction spots from the SiC substrate appeared in μ-LEED patterns collected at higher energies, showing that the rotation angle between graphene and SiC varied. C 1s spectra collected did not show any hint of a carbon interface layer. A hydrogen treatment applied was found to have a detrimental effect on the graphene quality for both types of samples, since the graphene domain/grain size was drastically reduced. From hydrogen treated samples, μ-LEED showed at first a clear (1 × 1) pattern, but within minutes, a pattern containing strong superstructure spots, indicating the presence of twisted graphene layers. The LEED electron beam was found to induce local desorption of hydrogen. Heating a hydrogenated C-face graphene sample did not restore the quality of the original as-grown sample.
- 1 January 2012
- Published by IMR Press in Frontiers in Bioscience-Elite
- Vol. E4 (1) , 254-78
ZnO materials and surface tailoring for biosensing
ZnO nanostructured materials, such as films and nanoparticles, could provide a suitable platform for development of high performance biosensors due to their unique fundamental material properties. This paper reviews different preparation techniques of ZnO nanocrystals and material issues like wettability, biocompatibility and toxicity, which have an important relevance to biosensor functionality. Efforts are made to summarize and analyze existing results regarding surface modification and molecular attachments for successful biofunctionalization and understanding of the mechanisms involved. A section is devoted to implementations of tailored surfaces in biosensors. We end with conclusions on the feasibility of using ZnO nanocrystals for biosensing
- 1 January 2012
- Published by IMR Press in Frontiers in Bioscience-Elite
- Vol. E4 (1) , 254-78
ZnO materials and surface tailoring for biosensing
ZnO nanostructured materials, such as films and nanoparticles, could provide a suitable platform for development of high performance biosensors due to their unique fundamental material properties. This paper reviews different preparation techniques of ZnO nanocrystals and material issues like wettability, biocompatibility and toxicity, which have an important relevance to biosensor functionality. Efforts are made to summarize and analyze existing results regarding surface modification and molecular attachments for successful biofunctionalization and understanding of the mechanisms involved. A section is devoted to implementations of tailored surfaces in biosensors. We end with conclusions on the feasibility of using ZnO nanocrystals for biosensing
- Open Access
- 29 March 2011
- Published by Springer Nature in Discover Nano
- Vol. 6 (1) , 269
Nanoscale structural characterization of epitaxial graphene grown on off-axis 4H-SiC (0001)
In this work, we present a nanometer resolution structural characterization of epitaxial graphene (EG) layers grown on 4H-SiC (0001) 8° off-axis, by annealing in inert gas ambient (Ar) in a wide temperature range (Tgr from 1600 to 2000°C). For all the considered growth temperatures, few layers of graphene (FLG) conformally covering the 100 to 200-nm wide terraces of the SiC surface have been observed by high-resolution cross-sectional transmission electron microscopy (HR-XTEM). Tapping mode atomic force microscopy (t-AFM) showed the formation of wrinkles with approx. 1 to 2 nm height and 10 to 20 nm width in the FLG film, as a result of the release of the compressive strain, which builds up in FLG during the sample cooling due to the thermal expansion coefficients mismatch between graphene and SiC. While for EG grown on on-axis 4H-SiC an isotropic mesh-like network of wrinkles interconnected into nodes is commonly reported, in the present case of a vicinal SiC surface, wrinkles are preferentially oriented in the direction perpendicular to the step edges of the SiC terraces. For each Tgr, the number of graphene layers was determined on very small sample areas by HR-XTEM and, with high statistics and on several sample positions, by measuring the depth of selectively etched trenches in FLG by t-AFM. Both the density of wrinkles and the number of graphene layers are found to increase almost linearly as a function of the growth temperature in the considered temperature range.
- 29 March 2011
- Published by Springer Nature in Discover Nano
- Vol. 6 (1) , 269
Open AccessNanoscale structural characterization of epitaxial graphene grown on off-axis 4H-SiC (0001)
In this work, we present a nanometer resolution structural characterization of epitaxial graphene (EG) layers grown on 4H-SiC (0001) 8° off-axis, by annealing in inert gas ambient (Ar) in a wide temperature range (Tgr from 1600 to 2000°C). For all the considered growth temperatures, few layers of graphene (FLG) conformally covering the 100 to 200-nm wide terraces of the SiC surface have been observed by high-resolution cross-sectional transmission electron microscopy (HR-XTEM). Tapping mode atomic force microscopy (t-AFM) showed the formation of wrinkles with approx. 1 to 2 nm height and 10 to 20 nm width in the FLG film, as a result of the release of the compressive strain, which builds up in FLG during the sample cooling due to the thermal expansion coefficients mismatch between graphene and SiC. While for EG grown on on-axis 4H-SiC an isotropic mesh-like network of wrinkles interconnected into nodes is commonly reported, in the present case of a vicinal SiC surface, wrinkles are preferentially oriented in the direction perpendicular to the step edges of the SiC terraces. For each Tgr, the number of graphene layers was determined on very small sample areas by HR-XTEM and, with high statistics and on several sample positions, by measuring the depth of selectively etched trenches in FLG by t-AFM. Both the density of wrinkles and the number of graphene layers are found to increase almost linearly as a function of the growth temperature in the considered temperature range.
- 5 April 2009
- Published by Elsevier in Journal of Crystal Growth
- Vol. 311 (11) , 3147-3151
ScAlN nanowires: A cathodoluminescence study
- 5 April 2009
- Published by Elsevier in Journal of Crystal Growth
- Vol. 311 (11) , 3147-3151
ScAlN nanowires: A cathodoluminescence study