Elif Nur Durmaz
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Research Subjects
Elif Nur Durmaz has a total of 9 co-authors. Here are the top co-authors by number of shared publications:
- Wiebe Matthijs de Vos
Department of Membrane Science and Technology, University of Twente, Enschede, Netherlands
3 shared publications - Ettore Virga
Membrane Science and Technology, University of Twente, Drienerlolaan 5, 7522 NB Enschede, the Netherlands; Wetsus, European Centre of Excellence for Sustainable Water Technology, Oostergoweg 9, 8911 MA Leeuwarden, the Netherlands
1 shared publication Joshua D. Willott
Membrane Science and Technology, MESA+ Institute for Nanotechnology, University of Twente, Faculty of Science and Technology, P.O. Box 217, 7500 AE Enschede, The Netherlands
1 shared publication- Joshua D. Willott
University of Newcastle
1 shared publication - Louis C. P. M. de Smet
Laboratory of Organic Chemistry Wageningen University Wageningen The Netherlands
1 shared publication - Mizanul Haque Mizan
Department of Mechanical Engineering, 10-367 Donadeo Innovation Center for Engineering, Advanced Water Research Lab (AWRL), University of Alberta, Edmonton, Alberta T6G 1H9, Canada
1 shared publication
Latest Publications
- Open Access
- 30 September 2021
- Published by Royal Society of Chemistry (RSC) in Soft Matter
- Vol. 17 (41) , 9420-9427
Tuning the charge of polyelectrolyte complex membranes preparedviaaqueous phase separation
In this work, polyelectrolyte mixing ratio is studied as a tuning parameter to control the charge, and thus the separation properties of polyelectrolyte complex (PEC) membranes prepared via Aqueous Phase Separation (APS). In this approach, various ratios of poly(sodium 4-styrenesulfonate) (PSS) and poly(diallyldimethylammonium chloride) (PDADMAC) are mixed at high salinity and the PEC-based membranes are then precipitated using low salinity coagulation baths. The monomeric ratio of PSS to PDADMAC is varied from 1.0 : 0.8 through to 1.0 : 1.2. Obtained membranes have an asymmetric structure and function as nanofiltration membranes with on average 1 L m−2 h−1 bar−1 pure water permeance and 20 L m−2 h−1 bar−1) with a similarly low MWCO. For the first time, we report the formation of both negatively and positively charged PSS–PDADMAC based APS membranes, as determined by both streaming potential and salt retention measurements. We hypothesize that the salt type used in the APS process plays a key role in the observed change in membrane charge. The point where the membrane charge transitions from negative to positive is found to be between the 1.0 : 0.9 and 1.0 : 1.0 PSS : PDADMAC ratios. The polyelectrolyte ratio not only affects membrane charge, but also their mechanical properties. The 1.0 : 0.9 and 1.0 : 1.0 membranes perform the best amongst the membranes prepared in this study since they have high salt retentions (up to 90% Na2SO4 and 75% MgCl2, respectively) and better mechanical stability. The higher permeance of the more charged, and thus more swollen, 1.0 : 0.8 and 1.0 : 1.2 membranes provide a relevant new direction for the development of APS-based PEC membranes.
- 30 September 2021
- Published by Royal Society of Chemistry (RSC) in Soft Matter
- Vol. 17 (41) , 9420-9427
Open AccessTuning the charge of polyelectrolyte complex membranes preparedviaaqueous phase separation
In this work, polyelectrolyte mixing ratio is studied as a tuning parameter to control the charge, and thus the separation properties of polyelectrolyte complex (PEC) membranes prepared via Aqueous Phase Separation (APS). In this approach, various ratios of poly(sodium 4-styrenesulfonate) (PSS) and poly(diallyldimethylammonium chloride) (PDADMAC) are mixed at high salinity and the PEC-based membranes are then precipitated using low salinity coagulation baths. The monomeric ratio of PSS to PDADMAC is varied from 1.0 : 0.8 through to 1.0 : 1.2. Obtained membranes have an asymmetric structure and function as nanofiltration membranes with on average 1 L m−2 h−1 bar−1 pure water permeance and 20 L m−2 h−1 bar−1) with a similarly low MWCO. For the first time, we report the formation of both negatively and positively charged PSS–PDADMAC based APS membranes, as determined by both streaming potential and salt retention measurements. We hypothesize that the salt type used in the APS process plays a key role in the observed change in membrane charge. The point where the membrane charge transitions from negative to positive is found to be between the 1.0 : 0.9 and 1.0 : 1.0 PSS : PDADMAC ratios. The polyelectrolyte ratio not only affects membrane charge, but also their mechanical properties. The 1.0 : 0.9 and 1.0 : 1.0 membranes perform the best amongst the membranes prepared in this study since they have high salt retentions (up to 90% Na2SO4 and 75% MgCl2, respectively) and better mechanical stability. The higher permeance of the more charged, and thus more swollen, 1.0 : 0.8 and 1.0 : 1.2 membranes provide a relevant new direction for the development of APS-based PEC membranes.
- Open Access
- 26 August 2021
- Published by American Chemical Society (ACS) in ACS Applied Polymer Materials
- Vol. 3 (9) , 4347-4374
Polyelectrolytes as Building Blocks for Next-Generation Membranes with Advanced Functionalities
- 26 August 2021
- Published by American Chemical Society (ACS) in ACS Applied Polymer Materials
- Vol. 3 (9) , 4347-4374
Open AccessPolyelectrolytes as Building Blocks for Next-Generation Membranes with Advanced Functionalities
- Open Access
- 1 June 2020
- Published by American Chemical Society (ACS) in ACS Applied Polymer Materials
- Vol. 2 (7) , 2612-2621
Polyelectrolyte Complex Membranes via Salinity Change Induced Aqueous Phase Separation
Polymeric membranes are used on very large scales for drinking water production and kidney dialysis, but they are nearly always prepared using large quantities of unsustainable and toxic aprotic solvents. In this study, a water-based, sustainable and simple way of making polymeric membranes is presented without the need for harmful solvents or extreme pH conditions. Membranes were prepared from water-insoluble polyelectrolyte complexes (PECs) via aqueous phase separation (APS). Strong PEs, poly(sodium 4-styrenesulfonate) (PSS) and poly(diallyldimethylammonium chloride) (PDADMAC) were mixed in the presence of excess of salt, thereby preventing complexation. Immersing a thin film of this mixture into a low salinity bath induces complexation and consequently the precipitation of a solid PEC-based membrane. This approach leads to asymmetric nanofiltration membranes, with thin dense top layers and porous, macrovoid-free, support layers. While the PSS molecular weight and the total polymer concentrations of the casting mixture did not significantly affect the membrane structure, they did affect the film formation process, the resulting mechanical stability of the films and the membrane separation properties. The salt concentration of the coagulation bath has a large effect on membrane structure and allows for control over the thickness of the separation layer. The nanofiltration membranes prepared by APS have a low molecular weight cut-off (<300 Da), a high MgSO4 retention (~80%) and good stability even at high pressures (10 bar). PE complexation induced APS is simple and sustainable way to prepare membranes where membrane structure and performance can be tuned with molecular weight, polymer concentration and ionic strength.
- 1 June 2020
- Published by American Chemical Society (ACS) in ACS Applied Polymer Materials
- Vol. 2 (7) , 2612-2621
Open AccessPolyelectrolyte Complex Membranes via Salinity Change Induced Aqueous Phase Separation
Polymeric membranes are used on very large scales for drinking water production and kidney dialysis, but they are nearly always prepared using large quantities of unsustainable and toxic aprotic solvents. In this study, a water-based, sustainable and simple way of making polymeric membranes is presented without the need for harmful solvents or extreme pH conditions. Membranes were prepared from water-insoluble polyelectrolyte complexes (PECs) via aqueous phase separation (APS). Strong PEs, poly(sodium 4-styrenesulfonate) (PSS) and poly(diallyldimethylammonium chloride) (PDADMAC) were mixed in the presence of excess of salt, thereby preventing complexation. Immersing a thin film of this mixture into a low salinity bath induces complexation and consequently the precipitation of a solid PEC-based membrane. This approach leads to asymmetric nanofiltration membranes, with thin dense top layers and porous, macrovoid-free, support layers. While the PSS molecular weight and the total polymer concentrations of the casting mixture did not significantly affect the membrane structure, they did affect the film formation process, the resulting mechanical stability of the films and the membrane separation properties. The salt concentration of the coagulation bath has a large effect on membrane structure and allows for control over the thickness of the separation layer. The nanofiltration membranes prepared by APS have a low molecular weight cut-off (<300 Da), a high MgSO4 retention (~80%) and good stability even at high pressures (10 bar). PE complexation induced APS is simple and sustainable way to prepare membranes where membrane structure and performance can be tuned with molecular weight, polymer concentration and ionic strength.