Gaoming Mo
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Research Subjects
Gaoming Mo has a total of 36 co-authors. Here are the top co-authors by number of shared publications:
- Qing Huang
YongJiang Laboratory
7 shared publications Haijun Chen
Zhejiang Key Laboratory of Data‐Driven High‐Safety Energy Materials and Applications Ningbo Key Laboratory of Special Energy Materials and Chemistry Ningbo Institute of Materials Technology and Engineering, Chinese Academy of Sciences Ningbo China
3 shared publicationsQing Huang
3 shared publicationsFucheng Xie
Zhejiang Key Laboratory of Data‐Driven High‐Safety Energy Materials and Applications Ningbo Key Laboratory of Special Energy Materials and Chemistry Ningbo Institute of Materials Technology and Engineering, Chinese Academy of Sciences Ningbo China
2 shared publicationsJing Huang
Zhejiang Key Laboratory of Data‐Driven High‐Safety Energy Materials and Applications Ningbo Key Laboratory of Special Energy Materials and Chemistry Ningbo Institute of Materials Technology and Engineering Chinese Academy of Sciences Ningbo China
2 shared publicationsLiu He
Engineering Laboratory of Advanced Energy Materials, Ningbo Institute of Materials Technology and Engineering, Chinese Academy of Sciences, Ningbo, People’s Republic of China
2 shared publications
Latest Publications
- 4 February 2026
- Published by Wiley in Journal of the American Ceramic Society
- Vol. 109 (2)
Synthesis of Polyborocarbosilane With Low Carbon Content and Investigation of Its Pyrolysis Process
This study presents the synthesis of low‐carbon polyborocarbosilane (PBCS) through a high‐temperature and high‐pressure method using polysilacarbosilane (PSCS) and o‐carborane, addressing the issue of excess carbon and difficulty in introducing boron (B) in conventional polycarbosilane (PCS) precursors. The incorporation of o‐carborane significantly accelerates the reaction kinetics compared to conventional PCS synthesis, and structural characterization (FTIR, NMR) confirms the successful integration of boron into the polymer backbone. The PBCS precursor exhibits a reduced carbon content (C/Si molar ratio: 1.48) and enhanced branching degree. During pyrolysis, TG‐MS and FTIR analyses reveal accelerated polymer‐to‐ceramic conversion below 800°C, due to the crosslinking reactions among B─H, Si─H, and Si─CH 3 groups, which promote hydrocarbon release and yield near‐stoichiometric SiC ceramics (C/Si = 1.08 at 1800°C). Furthermore, ultrafine PBCS fibers are fabricated via electrospinning of PBCS, after direct thermal curing (without oxidative crosslinking) and pyrolysis, ultrafine near‐stoichiometric crystalline SiC ultrafine fibers with low oxygen content and dense structure are obtained. During the sintering process, the formation of B─C/B─Si bonds promotes densification of the SiC ultrafine fibers and suppresses abnormal grain growth, potentially through the formation of boron solid solutions.
- 4 February 2026
- Published by Wiley in Journal of the American Ceramic Society
- Vol. 109 (2)
Synthesis of Polyborocarbosilane With Low Carbon Content and Investigation of Its Pyrolysis Process
This study presents the synthesis of low‐carbon polyborocarbosilane (PBCS) through a high‐temperature and high‐pressure method using polysilacarbosilane (PSCS) and o‐carborane, addressing the issue of excess carbon and difficulty in introducing boron (B) in conventional polycarbosilane (PCS) precursors. The incorporation of o‐carborane significantly accelerates the reaction kinetics compared to conventional PCS synthesis, and structural characterization (FTIR, NMR) confirms the successful integration of boron into the polymer backbone. The PBCS precursor exhibits a reduced carbon content (C/Si molar ratio: 1.48) and enhanced branching degree. During pyrolysis, TG‐MS and FTIR analyses reveal accelerated polymer‐to‐ceramic conversion below 800°C, due to the crosslinking reactions among B─H, Si─H, and Si─CH 3 groups, which promote hydrocarbon release and yield near‐stoichiometric SiC ceramics (C/Si = 1.08 at 1800°C). Furthermore, ultrafine PBCS fibers are fabricated via electrospinning of PBCS, after direct thermal curing (without oxidative crosslinking) and pyrolysis, ultrafine near‐stoichiometric crystalline SiC ultrafine fibers with low oxygen content and dense structure are obtained. During the sintering process, the formation of B─C/B─Si bonds promotes densification of the SiC ultrafine fibers and suppresses abnormal grain growth, potentially through the formation of boron solid solutions.
- 31 July 2025
- Published by Wiley in Journal of the American Ceramic Society
- Vol. 108 (12)
Facilitating Si‐O bond transformation in Si‐Al‐C‐O fibers by fast Joule heating
The decomposition of the SiCxOy phase constitutes the critical pathway for the evolution of Si‐Al‐C‐O fibers into highly crystalline silicon carbide (SiC) fibers. However, the traditional pyrolysis process is limited by the slow heating rate and fails to realize the efficient transformation of high‐bond‐energy Si‐O bonds to Si‐C bonds. In this work, a fast Joule heating (JH) method was employed, and the transformation of Si‐O bonds to Si‐C bonds and the growth process of β‐SiC microcrystals of Si‐Al‐C‐O fibers under ultrafast high‐temperature treatment were investigated, contrasting with the traditional heating method. Two types of Si‐Al‐C‐O fibers, one retaining Si‐CHx‐Si moieties and the other fully inorganic, exhibit distinct transformation behaviors. In the Si‐Al‐C‐O fibers containing residual Si‐CHx‐Si groups, the dehydrogenation reaction and SiCxOy phase decomposition reaction were coupled under ultrafast high‐temperature treatment, which effectively reduced the transformation temperature of Si‐O bonds to Si‐C bonds and promoted the growth of β‐SiC microcrystals. The synergistic regulation strategy of fast JH and residual organic structures proposed in this study expands the paradigms for designing advanced precursor‐derived ceramic materials.
- 31 July 2025
- Published by Wiley in Journal of the American Ceramic Society
- Vol. 108 (12)
Facilitating Si‐O bond transformation in Si‐Al‐C‐O fibers by fast Joule heating
The decomposition of the SiCxOy phase constitutes the critical pathway for the evolution of Si‐Al‐C‐O fibers into highly crystalline silicon carbide (SiC) fibers. However, the traditional pyrolysis process is limited by the slow heating rate and fails to realize the efficient transformation of high‐bond‐energy Si‐O bonds to Si‐C bonds. In this work, a fast Joule heating (JH) method was employed, and the transformation of Si‐O bonds to Si‐C bonds and the growth process of β‐SiC microcrystals of Si‐Al‐C‐O fibers under ultrafast high‐temperature treatment were investigated, contrasting with the traditional heating method. Two types of Si‐Al‐C‐O fibers, one retaining Si‐CHx‐Si moieties and the other fully inorganic, exhibit distinct transformation behaviors. In the Si‐Al‐C‐O fibers containing residual Si‐CHx‐Si groups, the dehydrogenation reaction and SiCxOy phase decomposition reaction were coupled under ultrafast high‐temperature treatment, which effectively reduced the transformation temperature of Si‐O bonds to Si‐C bonds and promoted the growth of β‐SiC microcrystals. The synergistic regulation strategy of fast JH and residual organic structures proposed in this study expands the paradigms for designing advanced precursor‐derived ceramic materials.
- 6 May 2025
- Published by Wiley in Journal of the American Ceramic Society
- Vol. 108 (12)
Fabrication of SiAlCNO and SiAlC fibers from a photo‐sensitive polyvinylaluminocarbosilane precursor using the ultraviolet curing method
SiC fiber is a critical structural material for high‐temperature extreme environments and nuclear energy applications. Traditional methods for producing industrial SiC fibers include oxidation and electron irradiation. In this study, a photo‐sensitive nitrogenous polyvinylaluminocarbosilane (PVACNS) is synthesized by uniformly blending polyaluminocarbosilane (PACS) and triallyl isocyanurate (TAIC). This precursor can be melt‐spun into fibers and rapidly UV‐cured at room temperature. After thermal pyrolysis at 1200°C and sintering at 1800°C of the cured fiber, amorphous SiAlCNO fibers with an oxygen content of 9.25 wt%, nitrogen content of 4.42 wt%, and a C/Si ratio of 1.60, and crystalline SiAlC fibers with an oxygen content of 0.02 wt%, nitrogen content of 0.11 wt%, and a C/Si ratio of 1.18 are obtained. The main UV curing mechanism involves homopolymerization of C = C bonds, in addition to minor hydrosilylation reaction between Si–H and C = C bonds. Between 400°C and 600°C, oxygen, nitrogen, and carbon contents decrease significantly due to the decomposition of TAIC. At 1200°C, the amorphous SiAlCNO fiber consists of amorphous SiCxOy, SiCxNy phases, and free carbon, with formation of Al–C and Al–N bonds. β‐SiC begins to form at 1400°C. At higher temperatures above 1400°C, SiCxOy and SiCxNy phases decompose, leading to notable decrease in oxygen and nitrogen content at 1600°C and 1800°C. However, due to the presence of Al–C and Al–N bonds, the formation of voids and defects is inhibited and the coarsening of β‐SiC is suppressed, resulting in a relatively dense structure in the SiAlC fibers at 1600°C and 1800°C.
- 6 May 2025
- Published by Wiley in Journal of the American Ceramic Society
- Vol. 108 (12)
Fabrication of SiAlCNO and SiAlC fibers from a photo‐sensitive polyvinylaluminocarbosilane precursor using the ultraviolet curing method
SiC fiber is a critical structural material for high‐temperature extreme environments and nuclear energy applications. Traditional methods for producing industrial SiC fibers include oxidation and electron irradiation. In this study, a photo‐sensitive nitrogenous polyvinylaluminocarbosilane (PVACNS) is synthesized by uniformly blending polyaluminocarbosilane (PACS) and triallyl isocyanurate (TAIC). This precursor can be melt‐spun into fibers and rapidly UV‐cured at room temperature. After thermal pyrolysis at 1200°C and sintering at 1800°C of the cured fiber, amorphous SiAlCNO fibers with an oxygen content of 9.25 wt%, nitrogen content of 4.42 wt%, and a C/Si ratio of 1.60, and crystalline SiAlC fibers with an oxygen content of 0.02 wt%, nitrogen content of 0.11 wt%, and a C/Si ratio of 1.18 are obtained. The main UV curing mechanism involves homopolymerization of C = C bonds, in addition to minor hydrosilylation reaction between Si–H and C = C bonds. Between 400°C and 600°C, oxygen, nitrogen, and carbon contents decrease significantly due to the decomposition of TAIC. At 1200°C, the amorphous SiAlCNO fiber consists of amorphous SiCxOy, SiCxNy phases, and free carbon, with formation of Al–C and Al–N bonds. β‐SiC begins to form at 1400°C. At higher temperatures above 1400°C, SiCxOy and SiCxNy phases decompose, leading to notable decrease in oxygen and nitrogen content at 1600°C and 1800°C. However, due to the presence of Al–C and Al–N bonds, the formation of voids and defects is inhibited and the coarsening of β‐SiC is suppressed, resulting in a relatively dense structure in the SiAlC fibers at 1600°C and 1800°C.
- 28 April 2025
- Published by Wiley in Journal of the American Ceramic Society
- Vol. 108 (9)
Oxygen evolution in the organic–inorganic transformation of polycarbosilane fibers via temperature‐programmed analysis
During the process of preparing SiC fibers by oxidation curing method, the chemical bonding form of oxygen and its content undergo significant changes, and oxygen plays a crucial role in the process of organic–inorganic–polycrystalline structure transformation. Currently, there are certain difficulties in specifically studying the evolution of oxygen chemical structure and the variation regularity of its content during the process of organic–inorganic transformation of precursor fibers. In this work, a novel research strategy, temperature‐programmed oxygen–nitrogen analyzer, is proposed to study the evolution of oxygen chemical structure and its content during the organic–inorganic transformation of polycarbosilane (PCS) precursor fibers. Three oxygen partial peaks of different oxygen chemical structures are separated by this method, oxygen is identified as Si–OH, low‐oxygen silicon groups (SiOC₃ + SiO₂C₂), and high‐oxygen silicon groups (SiO₃C + SiO₄). Fourier transform infrared (FTIR) and solid‐state 29 Si magic angle spinning (MAS) nuclear magnetic resonance (NMR) validated these assignments, showing Si–OH depletion above 700°C and progressive conversion of low‐ to high‐oxygen groups with temperature. In addition, after 600°C, the number of high‐oxygen silicon groups in the system began to increase significantly. The oxygen content introduced in the low‐temperature preoxidation stage significantly affects the evolution of oxygen structure and the change of oxygen content after 700°C. Higher oxygen content (>6%) promotes the formation of more high‐oxygen silicon groups in the high‐temperature decomposition stage. The method demonstrated reliability for oxygen content below 20%, offering insights into structural evolution critical for optimizing SiC fiber properties.
- 28 April 2025
- Published by Wiley in Journal of the American Ceramic Society
- Vol. 108 (9)
Oxygen evolution in the organic–inorganic transformation of polycarbosilane fibers via temperature‐programmed analysis
During the process of preparing SiC fibers by oxidation curing method, the chemical bonding form of oxygen and its content undergo significant changes, and oxygen plays a crucial role in the process of organic–inorganic–polycrystalline structure transformation. Currently, there are certain difficulties in specifically studying the evolution of oxygen chemical structure and the variation regularity of its content during the process of organic–inorganic transformation of precursor fibers. In this work, a novel research strategy, temperature‐programmed oxygen–nitrogen analyzer, is proposed to study the evolution of oxygen chemical structure and its content during the organic–inorganic transformation of polycarbosilane (PCS) precursor fibers. Three oxygen partial peaks of different oxygen chemical structures are separated by this method, oxygen is identified as Si–OH, low‐oxygen silicon groups (SiOC₃ + SiO₂C₂), and high‐oxygen silicon groups (SiO₃C + SiO₄). Fourier transform infrared (FTIR) and solid‐state 29 Si magic angle spinning (MAS) nuclear magnetic resonance (NMR) validated these assignments, showing Si–OH depletion above 700°C and progressive conversion of low‐ to high‐oxygen groups with temperature. In addition, after 600°C, the number of high‐oxygen silicon groups in the system began to increase significantly. The oxygen content introduced in the low‐temperature preoxidation stage significantly affects the evolution of oxygen structure and the change of oxygen content after 700°C. Higher oxygen content (>6%) promotes the formation of more high‐oxygen silicon groups in the high‐temperature decomposition stage. The method demonstrated reliability for oxygen content below 20%, offering insights into structural evolution critical for optimizing SiC fiber properties.
- 7 February 2025
- Published by Springer Nature in Silicon
- Vol. 17 (4) , 799-808
Study of the Method for the Accurate Determination of Gel Content in Cured Polyaluminocarbosilane Fibers
- 7 February 2025
- Published by Springer Nature in Silicon
- Vol. 17 (4) , 799-808
Study of the Method for the Accurate Determination of Gel Content in Cured Polyaluminocarbosilane Fibers
- 30 January 2025
- Published by Elsevier in Journal of Alloys and Compounds
- Vol. 1015
Polycarbosilane-derived Ti3SiC2 and its reaction mechanism
- 30 January 2025
- Published by Elsevier in Journal of Alloys and Compounds
- Vol. 1015
Polycarbosilane-derived Ti3SiC2 and its reaction mechanism
- Open Access
Structural Evolution of Polyaluminocarbosilane during the Polymer–Ceramic Conversion Process
Polyaluminocarbosilane (PACS) is an important precursor for silicon carbide (SiC) fibers and ceramics. The structure of PACS and the oxidative curing, thermal pyrolysis, and sintering effect of Al have already been substantially studied. However, the structural evolution of polyaluminocarbosilane itself during the polymer–ceramic conversion process, especially the changes in the structure forms of Al, are still pending questions. In this study, PACS with a higher Al content is synthesized and the above questions are elaborately investigated by FTIR, NMR, Raman, XPS, XRD, and TEM analyses. It is found that up to 800–900 °C the amorphous SiOxCy, AlOxSiy, and free carbon phases are initially formed. With increasing temperature, the SiOxCy phase partially separates into SiO2 then reacts with free carbon. The AlOxSiy phase changes into Al3C4 and Al2O3 by reaction with free carbon at around 1100 °C. The complicated reactions between Al3C4, Al2O3, and free carbon occur, leading to the formation of the Al4O4C and Al2OC phases at around 1600 °C, which then react with the SiC and free carbon, resulting in the formation of the Al4SiC4 phase at 1800 °C. The amorphous carbon phase grows with the increasing temperature, which then turns into a crystalline graphitic structure at around 1600 °C. The growth of β-SiC is inhibited by the existence of the Al4O4C, Al2OC, and Al4SiC4 phases, which also favor the formation of α-SiC at 1600–1800 °C.
Open AccessStructural Evolution of Polyaluminocarbosilane during the Polymer–Ceramic Conversion Process
Polyaluminocarbosilane (PACS) is an important precursor for silicon carbide (SiC) fibers and ceramics. The structure of PACS and the oxidative curing, thermal pyrolysis, and sintering effect of Al have already been substantially studied. However, the structural evolution of polyaluminocarbosilane itself during the polymer–ceramic conversion process, especially the changes in the structure forms of Al, are still pending questions. In this study, PACS with a higher Al content is synthesized and the above questions are elaborately investigated by FTIR, NMR, Raman, XPS, XRD, and TEM analyses. It is found that up to 800–900 °C the amorphous SiOxCy, AlOxSiy, and free carbon phases are initially formed. With increasing temperature, the SiOxCy phase partially separates into SiO2 then reacts with free carbon. The AlOxSiy phase changes into Al3C4 and Al2O3 by reaction with free carbon at around 1100 °C. The complicated reactions between Al3C4, Al2O3, and free carbon occur, leading to the formation of the Al4O4C and Al2OC phases at around 1600 °C, which then react with the SiC and free carbon, resulting in the formation of the Al4SiC4 phase at 1800 °C. The amorphous carbon phase grows with the increasing temperature, which then turns into a crystalline graphitic structure at around 1600 °C. The growth of β-SiC is inhibited by the existence of the Al4O4C, Al2OC, and Al4SiC4 phases, which also favor the formation of α-SiC at 1600–1800 °C.
- 26 May 2023
- Published by Springer Nature in Silicon
- Vol. 15 (15) , 6421-6429
Fabrication of SiC ultrafine fiber with low oxygen content by electrospinning, thermal curing and pyrolysis of cyano-polycarbosilane
- 26 May 2023
- Published by Springer Nature in Silicon
- Vol. 15 (15) , 6421-6429
Fabrication of SiC ultrafine fiber with low oxygen content by electrospinning, thermal curing and pyrolysis of cyano-polycarbosilane
- 1 January 2019
- Published by Pleiades Publishing Ltd in Polymer Science, Series B
- Vol. 61 (1) , 77-85
Rheokinetics and Characteristics of Resulted Gels during Isothermal Gelation Process for Lower Concentrated PAN/DMSO/H2O Solutions
Isothermal gelation processes for relatively low concentration PAN/DMSO/H2O solutions are studied by rheology. Winter–Chambon criterion is unitedly used to investigate the rheological...
- 1 January 2019
- Published by Pleiades Publishing Ltd in Polymer Science, Series B
- Vol. 61 (1) , 77-85
Rheokinetics and Characteristics of Resulted Gels during Isothermal Gelation Process for Lower Concentrated PAN/DMSO/H2O Solutions
Isothermal gelation processes for relatively low concentration PAN/DMSO/H2O solutions are studied by rheology. Winter–Chambon criterion is unitedly used to investigate the rheological...
- 11 December 2018
- Published by Wiley in Applied Organometallic Chemistry
- Vol. 33 (2) , e4720
Synthesis of polyaluminocarbosilane with low branched molecular structure using liquid polysilacarbosilane and aluminum acetylacetonate by high‐pressure method
The synthesis of polyaluminocarbosilane (PACS) using liquid polysilacarbosilane (PSCS) and aluminum acetylacetonate [Al (acac)3] by a high‐pressure method is reported for the first time. The effects of reaction time, temperature and feed ratio on the structure of PACS are investigated in detail by gel permeation chromatography, Fourier transform‐infrared, 1H‐NMR, 29Si‐NMR and 27Al‐NMR methods. It was found that the molecular weight and its polydispersity, as well as the branching degree of the molecular structure of PACS, increase with reaction time and temperature. Increasing the weight percentage of Al (acac)3 has a similar effect as temperature. Combined with the gas chromatography–mass spectroscopy results, the reaction mechanism is proposed, which contains three main reactions: (i) cleavage and rearrangement reaction of PSCS; (ii) silicon‐free radicals react with Al (acac)3, leading to cleavage of O=C and/or O‐C bonds and formation of AlOx ligands; and (iii) conversion reaction of Al ligands from AlO6 into AlO5 and AlO4. It is also found that PACS prepared by high‐pressure method has a lower branched molecular structure in comparison to its analog prepared under ambient pressure conditions, and it is achieved to increase the molecular weight and ceramic yield of PACS, which is beneficial for the processing and overall quality of the final product.
- 11 December 2018
- Published by Wiley in Applied Organometallic Chemistry
- Vol. 33 (2) , e4720
Synthesis of polyaluminocarbosilane with low branched molecular structure using liquid polysilacarbosilane and aluminum acetylacetonate by high‐pressure method
The synthesis of polyaluminocarbosilane (PACS) using liquid polysilacarbosilane (PSCS) and aluminum acetylacetonate [Al (acac)3] by a high‐pressure method is reported for the first time. The effects of reaction time, temperature and feed ratio on the structure of PACS are investigated in detail by gel permeation chromatography, Fourier transform‐infrared, 1H‐NMR, 29Si‐NMR and 27Al‐NMR methods. It was found that the molecular weight and its polydispersity, as well as the branching degree of the molecular structure of PACS, increase with reaction time and temperature. Increasing the weight percentage of Al (acac)3 has a similar effect as temperature. Combined with the gas chromatography–mass spectroscopy results, the reaction mechanism is proposed, which contains three main reactions: (i) cleavage and rearrangement reaction of PSCS; (ii) silicon‐free radicals react with Al (acac)3, leading to cleavage of O=C and/or O‐C bonds and formation of AlOx ligands; and (iii) conversion reaction of Al ligands from AlO6 into AlO5 and AlO4. It is also found that PACS prepared by high‐pressure method has a lower branched molecular structure in comparison to its analog prepared under ambient pressure conditions, and it is achieved to increase the molecular weight and ceramic yield of PACS, which is beneficial for the processing and overall quality of the final product.