Chenchen Jiang
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Research Subjects
Chenchen Jiang has a total of 15 co-authors. Here are the top co-authors by number of shared publications:
- Aiyue Zhang
Zhengzhou Light Alloy Institute Co., Ltd., Zhengzhou 450041, China
1 shared publication - Chujie Liu
State Key Laboratory of Digital Steel, Northeastern University, Shenyang 110819, China
1 shared publication - Di Mei
Zhengzhou University
1 shared publication - Hailian Zhang
Daotian High Technology Co., Ltd., Qinhuangdao, China
1 shared publication - Haitao Xie
Henan Province Key Laboratory of Advanced Light Alloys, School of Materials Science and Engineering, Zhengzhou University, Zhengzhou 450001, China
1 shared publication - Huijun Li
University of Wollongong
1 shared publication
Latest Publications
- Open Access
Hot Deformation Behavior and Microstructural Evolution of a High-Strength Mg-Gd-Y-Zr Alloy
Mg-Gd-Y-Zr alloys, with strong age-hardening and thermal stability, are ideal for lightweight load-bearing components, yet forming large complex parts is limited by high sensitivity to hot deformation parameters. This work investigates the hot deformation behavior and microstructure evolution of a Mg-9Gd-4Y-0.5Zr (wt.%) alloy via hot compression at 400 to 510 °C and strain rates of 0.001 to 10 s−1. An Arrhenius constitutive equation with an activation energy Q of 158.63 kJ/mol was established, and a hot processing map was constructed. EBSD characterization revealed the dynamic recrystallization, grain size evolution, and texture transition. The results show that flow stress depends strongly on temperature and strain rate. At strain rates of 0.001~1 s−1, a dynamic balance between work hardening and dynamic softening is achieved, and the post-peak flow stress gradually stabilizes. At a high strain rate of 10 s−1, the flow stress continues to decrease because the competition between softening from dynamic recrystallization and work hardening is disrupted by deformation-induced heating. Low strain rates (≤0.01 s−1) and high temperatures (≥470 °C) promote dynamic recrystallization and significant grain refinement. Two optimal processing windows were determined: 400 to 430 °C at 0.001 to 0.01 s−1, giving fully recrystallized fine equiaxed grains, and 440 to 460 °C at 0.01 to 0.1 s−1 with a power dissipation efficiency η of 0.43 to 0.51, balancing processing efficiency and microstructural uniformity. This work provides systematic theoretical and data support for optimizing hot forming parameters of large Mg-Gd-Y-Zr load-bearing components and offers guidance for applying high-strength magnesium alloys in high-end equipment.
Open AccessHot Deformation Behavior and Microstructural Evolution of a High-Strength Mg-Gd-Y-Zr Alloy
Mg-Gd-Y-Zr alloys, with strong age-hardening and thermal stability, are ideal for lightweight load-bearing components, yet forming large complex parts is limited by high sensitivity to hot deformation parameters. This work investigates the hot deformation behavior and microstructure evolution of a Mg-9Gd-4Y-0.5Zr (wt.%) alloy via hot compression at 400 to 510 °C and strain rates of 0.001 to 10 s−1. An Arrhenius constitutive equation with an activation energy Q of 158.63 kJ/mol was established, and a hot processing map was constructed. EBSD characterization revealed the dynamic recrystallization, grain size evolution, and texture transition. The results show that flow stress depends strongly on temperature and strain rate. At strain rates of 0.001~1 s−1, a dynamic balance between work hardening and dynamic softening is achieved, and the post-peak flow stress gradually stabilizes. At a high strain rate of 10 s−1, the flow stress continues to decrease because the competition between softening from dynamic recrystallization and work hardening is disrupted by deformation-induced heating. Low strain rates (≤0.01 s−1) and high temperatures (≥470 °C) promote dynamic recrystallization and significant grain refinement. Two optimal processing windows were determined: 400 to 430 °C at 0.001 to 0.01 s−1, giving fully recrystallized fine equiaxed grains, and 440 to 460 °C at 0.01 to 0.1 s−1 with a power dissipation efficiency η of 0.43 to 0.51, balancing processing efficiency and microstructural uniformity. This work provides systematic theoretical and data support for optimizing hot forming parameters of large Mg-Gd-Y-Zr load-bearing components and offers guidance for applying high-strength magnesium alloys in high-end equipment.
- Open Access
Microstructure and Mechanical Properties of 4Al Alumina-Forming Austenitic Steel after Cold-Rolling Deformation and Annealing
Microstructural evolutions of the 4Al alumina-forming austenitic steel after cold rolling with different reductions from 5% to 30% and then annealing were investigated using electron backscattering diffraction (EBSD), X-ray diffraction (XRD) and transmission electron microscopy (TEM). Tensile properties and hardness were also measured. The results show that the average grain size gradually decreases with an increase in the cold-rolling reduction. The low angle grain boundaries (LAGBs) are dominant in the cold-rolled samples, but high angle grain boundaries (HAGBs) form in the annealed samples, indicating that the grains are refined under the action of dislocations. During cold rolling, high-density dislocations are initially introduced in the samples, which contributes to a large number of dislocations remaining after annealing. With the sustaining increase in cold-rolled deformation, the samples exhibit more excellent tensile strength and hardness due to the decrease in grain size and increase in dislocation density, especially for the samples subjected to 30% cold-rolling reduction. The contribution of dislocations on yield strength is more than 60%.
Open AccessMicrostructure and Mechanical Properties of 4Al Alumina-Forming Austenitic Steel after Cold-Rolling Deformation and Annealing
Microstructural evolutions of the 4Al alumina-forming austenitic steel after cold rolling with different reductions from 5% to 30% and then annealing were investigated using electron backscattering diffraction (EBSD), X-ray diffraction (XRD) and transmission electron microscopy (TEM). Tensile properties and hardness were also measured. The results show that the average grain size gradually decreases with an increase in the cold-rolling reduction. The low angle grain boundaries (LAGBs) are dominant in the cold-rolled samples, but high angle grain boundaries (HAGBs) form in the annealed samples, indicating that the grains are refined under the action of dislocations. During cold rolling, high-density dislocations are initially introduced in the samples, which contributes to a large number of dislocations remaining after annealing. With the sustaining increase in cold-rolled deformation, the samples exhibit more excellent tensile strength and hardness due to the decrease in grain size and increase in dislocation density, especially for the samples subjected to 30% cold-rolling reduction. The contribution of dislocations on yield strength is more than 60%.