Andrey Balyakin
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Andrey Balyakin has a total of 36 co-authors. Here are the top co-authors by number of shared publications:
- Alexander I. Khaimovich
Department of Engine Production Technology, Samara National Research University, Moskovskoye shosse 34, 443086 Samara, Russia
6 shared publications - Ekaterina A. Nosova
Самарский национальный исследовательский университет имени академика С.П. Королёва
5 shared publications Natalia V. Galkina
Samara State Aerospace University
4 shared publications- Evgeniy P. Zlobin
Samara National Research University
3 shared publications - M. A. Oleynik
Samara University, 34, Moskovskoe sh., Samara, 443086, Russia
3 shared publications Alexander I. Khaimovich
Samara National Research University
2 shared publications
Latest Publications
- Open Access
In-Situ Monitoring of Directed Energy Deposition Laser Beam of Nickel-Based Superalloy via Built-in Optical Coaxial Camera
This study presents the development and validation of an in situ monitoring method for the laser direct energy deposition (DED) process, utilizing an integrated optical camera (720 HD, 60 fps) to analyze melt pool imagery. The approach is grounded in an experimental framework employing Taguchi orthogonal arrays, which ensures a stable dataset by controlling process variability and enabling reliable extraction of relevant features. The monitoring system focuses on analyzing brightness distribution regions within the melt pool image, identified as specific clusters that reflect external process conditions. The method emphasizes precise segmentation of the melt pool area, combined with automatic detection and classification of cluster features associated with key process parameters—such as focus distance, the number of deposited layers, powder feed rate, and scanning speed. The main contribution of this work is demonstrating the effectiveness of using an optical camera for DED monitoring, based on an algorithm that processes a set of melt pool identification features through computer vision and machine learning techniques, including Random Forest and HistGradient Boosting, achieving classification accuracies exceeding 95%. By continuously tracking the evolution of these features within a closed-loop control system, the process can be maintained in a stable, defect-free state, effectively preventing the formation of common process defects.
Open AccessIn-Situ Monitoring of Directed Energy Deposition Laser Beam of Nickel-Based Superalloy via Built-in Optical Coaxial Camera
This study presents the development and validation of an in situ monitoring method for the laser direct energy deposition (DED) process, utilizing an integrated optical camera (720 HD, 60 fps) to analyze melt pool imagery. The approach is grounded in an experimental framework employing Taguchi orthogonal arrays, which ensures a stable dataset by controlling process variability and enabling reliable extraction of relevant features. The monitoring system focuses on analyzing brightness distribution regions within the melt pool image, identified as specific clusters that reflect external process conditions. The method emphasizes precise segmentation of the melt pool area, combined with automatic detection and classification of cluster features associated with key process parameters—such as focus distance, the number of deposited layers, powder feed rate, and scanning speed. The main contribution of this work is demonstrating the effectiveness of using an optical camera for DED monitoring, based on an algorithm that processes a set of melt pool identification features through computer vision and machine learning techniques, including Random Forest and HistGradient Boosting, achieving classification accuracies exceeding 95%. By continuously tracking the evolution of these features within a closed-loop control system, the process can be maintained in a stable, defect-free state, effectively preventing the formation of common process defects.
- 30 September 2025
- Published by Nosov Magnitogorsk State Technical University in Vestnik of Nosov Magnitogorsk State Technical University
- Vol. 23 (3)
Manufacturing of Branch Tubes for Nuclear Industry by Direct Energy Deposition Made of Metal Powder Composition 08Cr18Ni10T
Traditionally, branch tubes for process pipeline systems at nuclear power plants are made by stamping. However, when using this method, a serious problem arises such as a high percentage of defects due to the uneven distribution of material over the product. This leads to a decrease in product quality and an increase in production costs. In this regard, there is a need to search for alternative manufacturing methods. One of the promising areas is the use of additive technologies, namely direct energy deposition. The purpose of this work is to study the possibility of using direct energy deposition as a new technology for the production of branch tubes. As part of the research, a pilot batch of parts and test samples were produced. The accuracy of the geometric parameters of the obtained branch tubes was monitored, as well as the assessment of the physical and mechanical properties and quality of the surface layer. The results of the study showed that the chemical composition of the sample material meets the requirements for the 08Cr18Ni10T steel grade. However, mechanical tests revealed some inconsistencies in the field of yield strength. The samples have high resistance to intercrystalline corrosion, as well as a low degree of contamination with non-metallic inclusions, the con-tent of the ferrite phase does not exceed 5%. The control of the geometric parameters of the branch tubes showed that all dimensions meet the design requirements, and there are no unacceptable defects on the surface. Based on the data obtained, recommendations were made on possible adjustments to the technology to ensure compliance with all GOST requirements for mechanical properties. The practical significance of the research lies in the possibility of using the results obtained to optimize production processes and improve product quality in the nuclear industry.
- 30 September 2025
- Published by Nosov Magnitogorsk State Technical University in Vestnik of Nosov Magnitogorsk State Technical University
- Vol. 23 (3)
Manufacturing of Branch Tubes for Nuclear Industry by Direct Energy Deposition Made of Metal Powder Composition 08Cr18Ni10T
Traditionally, branch tubes for process pipeline systems at nuclear power plants are made by stamping. However, when using this method, a serious problem arises such as a high percentage of defects due to the uneven distribution of material over the product. This leads to a decrease in product quality and an increase in production costs. In this regard, there is a need to search for alternative manufacturing methods. One of the promising areas is the use of additive technologies, namely direct energy deposition. The purpose of this work is to study the possibility of using direct energy deposition as a new technology for the production of branch tubes. As part of the research, a pilot batch of parts and test samples were produced. The accuracy of the geometric parameters of the obtained branch tubes was monitored, as well as the assessment of the physical and mechanical properties and quality of the surface layer. The results of the study showed that the chemical composition of the sample material meets the requirements for the 08Cr18Ni10T steel grade. However, mechanical tests revealed some inconsistencies in the field of yield strength. The samples have high resistance to intercrystalline corrosion, as well as a low degree of contamination with non-metallic inclusions, the con-tent of the ferrite phase does not exceed 5%. The control of the geometric parameters of the branch tubes showed that all dimensions meet the design requirements, and there are no unacceptable defects on the surface. Based on the data obtained, recommendations were made on possible adjustments to the technology to ensure compliance with all GOST requirements for mechanical properties. The practical significance of the research lies in the possibility of using the results obtained to optimize production processes and improve product quality in the nuclear industry.
- Open Access
- 30 June 2025
- Published by Siberian State Industrial University in Bulletin of the Siberian State Industrial University
- Vol. 1 (2) , 44-51
INVESTIGATION OF THE INFLUENCE OF THE PARAMETERS OF THE DEPOSITION MODE ON THE HARDNESS OF 12CR18NI10TI STEEL AFTER DIRECT LASER CULTIVATION
ИССЛЕДОВАНИЕ ВЛИЯНИЯ ПАРАМЕТРОВ РЕЖИМА НАПЛАВЛЕНИЯ НА ТВЕРДОСТЬ СТАЛИ 12Х18Н10Т ПОСЛЕ ПРЯМОГО ЛАЗЕРНОГО ВЫРАЩИВАНИЯ
- 30 June 2025
- Published by Siberian State Industrial University in Bulletin of the Siberian State Industrial University
- Vol. 1 (2) , 44-51
Open AccessINVESTIGATION OF THE INFLUENCE OF THE PARAMETERS OF THE DEPOSITION MODE ON THE HARDNESS OF 12CR18NI10TI STEEL AFTER DIRECT LASER CULTIVATION
ИССЛЕДОВАНИЕ ВЛИЯНИЯ ПАРАМЕТРОВ РЕЖИМА НАПЛАВЛЕНИЯ НА ТВЕРДОСТЬ СТАЛИ 12Х18Н10Т ПОСЛЕ ПРЯМОГО ЛАЗЕРНОГО ВЫРАЩИВАНИЯ
- Open Access
Effect of Interface Relief on the Occurrence of Cracks at the Contact Point of Laser-Direct-Energy-Deposited Copper Alloy and Nickel Base Superalloy
The relevance of the study is related to the need to join dissimilar copper and nickel alloys by laser direct energy and material deposition (LDED). The purpose of research is studying the distribution of elements, structure, and properties of contact zone of nickel-based super alloy and CuCr1 bronze obtained by direct energy and material deposition with preliminary formation of relief of contact surface. For the purposes of research, samples were made from UNS C18200 copper alloy CuCr1 without relief, with a relief of 0.5 mm depth, and with a relief of 1 mm depth. The Ni50Cr33W4.5Mo2.8TiAlNb (EP648) alloy powder was deposited onto the bronze samples with a micro-relief. The deposition was produced by direct injection of energy and material. The influence of interphase interaction of CuCr-chromium carbide system on the possibility of initiation of a crack in the area of carbide secretions is not significant and does not exceed 3.1% according to CIC criterion from the background level for CuCr1 (CIC = 1.54% for CuCr1-Al4C3 interface and CIC = 3.1% for CuCr1-Cr23C6 interface). An X-ray analysis revealed the presence of tensile residual macro-stresses, arising from differences in thermal expansion coefficients in the CuCr1-EP648 interface area, which may be the main cause of crack formation. Cracks are generated and run along the grain boundaries, on which traces of excretion are visible. The contact surface in the CuCr1-EP648 interface area has no visible defects, which indicates the good adhesion of materials when applying an initial layer of EP648 by LDED. The presence of a 0.5-mm micro-relief on CuCr1 has a positive effect on the strength of the connection, as it increases the surface area of the contact CuCr1-EP648 and therefore reduces the contact stress of the breakout.
Open AccessEffect of Interface Relief on the Occurrence of Cracks at the Contact Point of Laser-Direct-Energy-Deposited Copper Alloy and Nickel Base Superalloy
The relevance of the study is related to the need to join dissimilar copper and nickel alloys by laser direct energy and material deposition (LDED). The purpose of research is studying the distribution of elements, structure, and properties of contact zone of nickel-based super alloy and CuCr1 bronze obtained by direct energy and material deposition with preliminary formation of relief of contact surface. For the purposes of research, samples were made from UNS C18200 copper alloy CuCr1 without relief, with a relief of 0.5 mm depth, and with a relief of 1 mm depth. The Ni50Cr33W4.5Mo2.8TiAlNb (EP648) alloy powder was deposited onto the bronze samples with a micro-relief. The deposition was produced by direct injection of energy and material. The influence of interphase interaction of CuCr-chromium carbide system on the possibility of initiation of a crack in the area of carbide secretions is not significant and does not exceed 3.1% according to CIC criterion from the background level for CuCr1 (CIC = 1.54% for CuCr1-Al4C3 interface and CIC = 3.1% for CuCr1-Cr23C6 interface). An X-ray analysis revealed the presence of tensile residual macro-stresses, arising from differences in thermal expansion coefficients in the CuCr1-EP648 interface area, which may be the main cause of crack formation. Cracks are generated and run along the grain boundaries, on which traces of excretion are visible. The contact surface in the CuCr1-EP648 interface area has no visible defects, which indicates the good adhesion of materials when applying an initial layer of EP648 by LDED. The presence of a 0.5-mm micro-relief on CuCr1 has a positive effect on the strength of the connection, as it increases the surface area of the contact CuCr1-EP648 and therefore reduces the contact stress of the breakout.
- Open Access
- 17 December 2024
- Published by Samara National Research University in VESTNIK of Samara University. Aerospace and Mechanical Engineering
- Vol. 23 (4) , 99-111
Model of interaction between laser radiation and metal powder composition during direct laser growth
This paper presents a model for analyzing the interaction of laser radiation and a metal-powder composition in the process of direct laser growing of large-sized combustion chambers of gas turbine engines. The metal-powder composition is fed into the melting zone coaxially with laser radiation; the task is to completely melt the powder with laser radiation before it enters the melt bath on the construction platform. The laser radiation is absorbed as it passes through the gas-powder jet, and its energy is also used to melt the construction platform or the previous layer. Thus, in order to determine the parameters of the operating conditions that provide the possibility of melting powder particles, it is necessary to determine the boundaries of the parameters at which each particle of the metal-powder composition completely melts in a gas-powder jet. To simulate heat transfer inside a particle, the Beer – Lambert laser radiation absorption law was used using the lumped parameter approach. The required energy for melting the powder material was determined through enthalpy. The resulting one-dimensional differential equation of enthalpy increment is solved numerically by the Euler method. Using this model, the distance from the point of origin of the interaction of the laser beam with a metal-powder composition to the zone of its complete melting was determined and the effect of the velocity of the gas-powder jet, the power of laser radiation, the bulk density of the metal-powder composition and the average radius of the powder particles on the distance to the zone of complete melting was studied.
- 17 December 2024
- Published by Samara National Research University in VESTNIK of Samara University. Aerospace and Mechanical Engineering
- Vol. 23 (4) , 99-111
Open AccessModel of interaction between laser radiation and metal powder composition during direct laser growth
This paper presents a model for analyzing the interaction of laser radiation and a metal-powder composition in the process of direct laser growing of large-sized combustion chambers of gas turbine engines. The metal-powder composition is fed into the melting zone coaxially with laser radiation; the task is to completely melt the powder with laser radiation before it enters the melt bath on the construction platform. The laser radiation is absorbed as it passes through the gas-powder jet, and its energy is also used to melt the construction platform or the previous layer. Thus, in order to determine the parameters of the operating conditions that provide the possibility of melting powder particles, it is necessary to determine the boundaries of the parameters at which each particle of the metal-powder composition completely melts in a gas-powder jet. To simulate heat transfer inside a particle, the Beer – Lambert laser radiation absorption law was used using the lumped parameter approach. The required energy for melting the powder material was determined through enthalpy. The resulting one-dimensional differential equation of enthalpy increment is solved numerically by the Euler method. Using this model, the distance from the point of origin of the interaction of the laser beam with a metal-powder composition to the zone of its complete melting was determined and the effect of the velocity of the gas-powder jet, the power of laser radiation, the bulk density of the metal-powder composition and the average radius of the powder particles on the distance to the zone of complete melting was studied.
- 22 February 2024
- Published by Pleiades Publishing Ltd in Russian Journal of Non-Ferrous Metals
- Vol. 65 (1) , 34-41
Heat Treatment Effect on the Structure and Properties of Workpieces from Heat-Resistant Nickel Alloys Obtained by Additive Technologies
Both conventional technologies for obtaining workpieces and the additive technological process of direct energy and material feeding (direct energy deposition, DED) are employed for manufacturing bulky workpieces for gas turbine engine parts from heat-resistant nickel-based alloys. The DED technology allows managing a highly coordinated energy impact on the microvolume of the alloy, which ensures obtaining the material structure with higher working characteristics compared to castings. At present, application of nickel material in additive technologies is limited by the ultrafast crystallization processes that cause accumulation of significant internal stresses, which leads to formation of micro- and macrodefects. Heat treatment is recommended for residual stress reduction in the products after the DED process, but optimal modes of such processing of a workpiece are not specified. On the other hand, heat treatment implies obtaining high mechanical properties. For products fabricated by additive methods of surfacing powders with nonequilibrium structure, similar recommendations are insufficient. The place of heat treatment in the general cycle of manufacturing parts is set depending on the requirements for the properties of the product. In most cases, heat treatment is performed after mechanical post-treatment. This is associated with the requirements for high strength, hardness, and wear resistance of the product material. The article studies the effect of various heat treatment modes on the hardness, microstructure, and residual stresses of the samples made of the KhN50VMTYuB heat-resistant nickel-based alloy obtained by the DED technology. The DED technology of workpiece manufacturing from the KhN50VMTYuB alloy leads to a fairly high hardness of about 190 HB. It is well known that the growth of products from the highly alloyed powder of nonequilibrium structure proceeds by rapid cooling, which causes structural changes similar to the aging while heating by a laser beam. Heat treatment of the grown products may be aimed at increasing the machinability by cutting and reducing the warping of products, as a result of the redistribution of residual stresses. In this case, the decrease in hardness may be the criterion of goal achieving. The results of the presented study demonstrate that the most cost-efficient mode of heat treatment for the residual stress removal is the mode consisting in heating up to 1180°C and holding for 4 h with subsequent air cooling, which allows reducing hardness from 191 ± 1 HВ to 135 ± 1 HВ. The lowest hardness values of HB 128 ± 1 were obtained after heating to 1140°C, holding for 4 h, and cooling with a furnace. Air cooling allows obtaining the hardness of HB 130 ± 18. On one hand, this indicates slightly higher hardness values, but deviations are of a higher level, and the level of residual stresses in the annular samples herewith are of the lowest values, which follows from the results of change in the geometry of samples after cutting. The highest hardness of 311 ± 8 HB was obtained at the end of heat treatment, which includes heating up to 1100°C, holding for 4 h, and air cooling; then heating up to 950°C, holding for 3.5 h, and air cooling; then heating up to 800°C, holding for 7.5 h, and air cooling; then heating up to 700°C, holding for 14 h, and air cooling. The microstructure analysis of the grown samples reveals that, after all types of heat treatment, an inequigranular structure is formed in the samples, and the layered structure characteristic of the deposited particles is lost.
- 22 February 2024
- Published by Pleiades Publishing Ltd in Russian Journal of Non-Ferrous Metals
- Vol. 65 (1) , 34-41
Heat Treatment Effect on the Structure and Properties of Workpieces from Heat-Resistant Nickel Alloys Obtained by Additive Technologies
Both conventional technologies for obtaining workpieces and the additive technological process of direct energy and material feeding (direct energy deposition, DED) are employed for manufacturing bulky workpieces for gas turbine engine parts from heat-resistant nickel-based alloys. The DED technology allows managing a highly coordinated energy impact on the microvolume of the alloy, which ensures obtaining the material structure with higher working characteristics compared to castings. At present, application of nickel material in additive technologies is limited by the ultrafast crystallization processes that cause accumulation of significant internal stresses, which leads to formation of micro- and macrodefects. Heat treatment is recommended for residual stress reduction in the products after the DED process, but optimal modes of such processing of a workpiece are not specified. On the other hand, heat treatment implies obtaining high mechanical properties. For products fabricated by additive methods of surfacing powders with nonequilibrium structure, similar recommendations are insufficient. The place of heat treatment in the general cycle of manufacturing parts is set depending on the requirements for the properties of the product. In most cases, heat treatment is performed after mechanical post-treatment. This is associated with the requirements for high strength, hardness, and wear resistance of the product material. The article studies the effect of various heat treatment modes on the hardness, microstructure, and residual stresses of the samples made of the KhN50VMTYuB heat-resistant nickel-based alloy obtained by the DED technology. The DED technology of workpiece manufacturing from the KhN50VMTYuB alloy leads to a fairly high hardness of about 190 HB. It is well known that the growth of products from the highly alloyed powder of nonequilibrium structure proceeds by rapid cooling, which causes structural changes similar to the aging while heating by a laser beam. Heat treatment of the grown products may be aimed at increasing the machinability by cutting and reducing the warping of products, as a result of the redistribution of residual stresses. In this case, the decrease in hardness may be the criterion of goal achieving. The results of the presented study demonstrate that the most cost-efficient mode of heat treatment for the residual stress removal is the mode consisting in heating up to 1180°C and holding for 4 h with subsequent air cooling, which allows reducing hardness from 191 ± 1 HВ to 135 ± 1 HВ. The lowest hardness values of HB 128 ± 1 were obtained after heating to 1140°C, holding for 4 h, and cooling with a furnace. Air cooling allows obtaining the hardness of HB 130 ± 18. On one hand, this indicates slightly higher hardness values, but deviations are of a higher level, and the level of residual stresses in the annular samples herewith are of the lowest values, which follows from the results of change in the geometry of samples after cutting. The highest hardness of 311 ± 8 HB was obtained at the end of heat treatment, which includes heating up to 1100°C, holding for 4 h, and air cooling; then heating up to 950°C, holding for 3.5 h, and air cooling; then heating up to 800°C, holding for 7.5 h, and air cooling; then heating up to 700°C, holding for 14 h, and air cooling. The microstructure analysis of the grown samples reveals that, after all types of heat treatment, an inequigranular structure is formed in the samples, and the layered structure characteristic of the deposited particles is lost.
- Open Access
- 30 December 2023
- Published by Siberian State Industrial University in Bulletin of the Siberian State Industrial University
- No. 4,p. 64-78
PROCESS OF DIRECT LASER GROWTH OF HEAT-RESISTANT ALLOY: INFLUENCE OF POWER AND HEAT TREATMENT ON MICROSTRUCTURE AND MECHANICALCHARACTERISTICS
The microstructure and tensile mechanical properties of samples made of a heat-resistant nickel-based alloy obtained using the direct energy and material supply (LP-DED) process have been studied. The power of the laser radiation varied from 1200 to 2000 watts. It was noted that low laser power can lead to higher cooling rates and defects in the microstructure of the samples. The radiation power of 2000 W resulted in the highest mechanical properties under tension. The effect of heat treatment on microstructure, hardness and tensile properties was investigated. When examining the samples after destruction, it was found that defects in the form of non‒melts and cracks are present in the fractures of the samples obtained at a power of 1400 -1800 watts. In the fractures of the samples made at a laser power of 1200 and 1600 W, there are non-molten powder particles. On the fracture surfaces of all samples, pits and the classic shape of a cup and cone were present, indicating a viscous fracture mechanism. It was found that heat treatment can completely homogenize the microstructure, lead to relatively homogeneous, equiaxed grains and increase the hardness of the material. Heat treatment reduces the anisotropy of properties, leads to an increase in the level of tensile properties at different laser power. The study provides an initial basis to help designers and specialists with the choice of laser power, aswell as to understand its effect on a heat-resistant alloy, its effect on microstructure and mechanical properties at room temperature. Изучены микроструктура и механические свойства при растяжении образцов из жаропрочного сплава на никелевой основе, полученных с использованием процесса прямого подвода энергии и материала (LP-DED). Мощность лазерного излучения варьировали от 1200 до 2000 Вт. Было отмечено, что низкая мощность лазера может привести к более высоким скорости охлаждения и дефектности в микроструктуре образцов. Мощность излучения 2000 Вт привела к получению самых высоких механических свойств при растяжении. Было исследовано влияние термической обработки на микроструктуру, твердость и свойства при растяжении. При исследовании образцов после разрушения обнаружено, что в изломах образцов, полученных при мощности 1400 ‒ 1800 Вт, присутствуют дефекты в виде непроплавов и трещин. В изломах образцов,изготовленных при мощности лазера 1200 и 1600 Вт, присутствуют не расплавившиеся частицы порошка. На поверхностях излома всех образцов присутствовали ямки и классическая форма чашечки и конуса, указывающие на вязкий механизм разрушения. Было обнаружено, что термическая обработка может полностью гомогенизировать микроструктуру, привести к относительно однородным, равноосным зернам и увеличить твердость материала. Термическая обработка снижает анизотропию свойств, приводит к повышению уровня свойств на растяжение при разной мощности лазера. Исследование предоставляет первоначальную основу, чтобы помочь конструкторам и специалистам с выбором мощности лазера, а также понимать его воздействие на жаропрочный сплав, влияние на микроструктуру и механические свойства при комнатной температуре.
- 30 December 2023
- Published by Siberian State Industrial University in Bulletin of the Siberian State Industrial University
- No. 4,p. 64-78
Open AccessPROCESS OF DIRECT LASER GROWTH OF HEAT-RESISTANT ALLOY: INFLUENCE OF POWER AND HEAT TREATMENT ON MICROSTRUCTURE AND MECHANICALCHARACTERISTICS
The microstructure and tensile mechanical properties of samples made of a heat-resistant nickel-based alloy obtained using the direct energy and material supply (LP-DED) process have been studied. The power of the laser radiation varied from 1200 to 2000 watts. It was noted that low laser power can lead to higher cooling rates and defects in the microstructure of the samples. The radiation power of 2000 W resulted in the highest mechanical properties under tension. The effect of heat treatment on microstructure, hardness and tensile properties was investigated. When examining the samples after destruction, it was found that defects in the form of non‒melts and cracks are present in the fractures of the samples obtained at a power of 1400 -1800 watts. In the fractures of the samples made at a laser power of 1200 and 1600 W, there are non-molten powder particles. On the fracture surfaces of all samples, pits and the classic shape of a cup and cone were present, indicating a viscous fracture mechanism. It was found that heat treatment can completely homogenize the microstructure, lead to relatively homogeneous, equiaxed grains and increase the hardness of the material. Heat treatment reduces the anisotropy of properties, leads to an increase in the level of tensile properties at different laser power. The study provides an initial basis to help designers and specialists with the choice of laser power, aswell as to understand its effect on a heat-resistant alloy, its effect on microstructure and mechanical properties at room temperature. Изучены микроструктура и механические свойства при растяжении образцов из жаропрочного сплава на никелевой основе, полученных с использованием процесса прямого подвода энергии и материала (LP-DED). Мощность лазерного излучения варьировали от 1200 до 2000 Вт. Было отмечено, что низкая мощность лазера может привести к более высоким скорости охлаждения и дефектности в микроструктуре образцов. Мощность излучения 2000 Вт привела к получению самых высоких механических свойств при растяжении. Было исследовано влияние термической обработки на микроструктуру, твердость и свойства при растяжении. При исследовании образцов после разрушения обнаружено, что в изломах образцов, полученных при мощности 1400 ‒ 1800 Вт, присутствуют дефекты в виде непроплавов и трещин. В изломах образцов,изготовленных при мощности лазера 1200 и 1600 Вт, присутствуют не расплавившиеся частицы порошка. На поверхностях излома всех образцов присутствовали ямки и классическая форма чашечки и конуса, указывающие на вязкий механизм разрушения. Было обнаружено, что термическая обработка может полностью гомогенизировать микроструктуру, привести к относительно однородным, равноосным зернам и увеличить твердость материала. Термическая обработка снижает анизотропию свойств, приводит к повышению уровня свойств на растяжение при разной мощности лазера. Исследование предоставляет первоначальную основу, чтобы помочь конструкторам и специалистам с выбором мощности лазера, а также понимать его воздействие на жаропрочный сплав, влияние на микроструктуру и механические свойства при комнатной температуре.
- 1 January 2023
- Published by FSB EIHE Omsk State Technical University in Omsk Scientific Bulletin. Series Aviation-Rocket and Power Engineering
- Vol. 7 (4)
Investigation of the process of vibration processing of AlSi10Mg aluminum alloy samples obtained by SLS technology
The results of the experiment aimed at studying the effect of vibration treatment on samples of various sizes made of AlSi10Mg alloy obtained by selective laser melting are presented. During the investigation, changes in the roughness and rounding of sharp edges are monitored depending on the size of the samples and the angle of inclination of the wall. Also, the formation of low contact zones and untreated zones during processing is studied. As a result of the experiment, a minimum surface roughness of Ra 1,2 microns is achieved. The length of the untreated zones, depending on the geometry, ranged from 0,5 mm to 6 mm. Rounding occurred most effectively in the first 4 hours of processing on the edges formed by an obtuse angle. The results obtained allow us to better understand the features of vibration processing of aluminum alloy products and optimize the process to achieve the required surface characteristics. Thus, the results of the study can be useful for various industrial sectors where aluminum alloys are used, and contribute to the further development of processing technologies for products obtained using SLM technology.
- 1 January 2023
- Published by FSB EIHE Omsk State Technical University in Omsk Scientific Bulletin. Series Aviation-Rocket and Power Engineering
- Vol. 7 (4)
Investigation of the process of vibration processing of AlSi10Mg aluminum alloy samples obtained by SLS technology
The results of the experiment aimed at studying the effect of vibration treatment on samples of various sizes made of AlSi10Mg alloy obtained by selective laser melting are presented. During the investigation, changes in the roughness and rounding of sharp edges are monitored depending on the size of the samples and the angle of inclination of the wall. Also, the formation of low contact zones and untreated zones during processing is studied. As a result of the experiment, a minimum surface roughness of Ra 1,2 microns is achieved. The length of the untreated zones, depending on the geometry, ranged from 0,5 mm to 6 mm. Rounding occurred most effectively in the first 4 hours of processing on the edges formed by an obtuse angle. The results obtained allow us to better understand the features of vibration processing of aluminum alloy products and optimize the process to achieve the required surface characteristics. Thus, the results of the study can be useful for various industrial sectors where aluminum alloys are used, and contribute to the further development of processing technologies for products obtained using SLM technology.
- 1 January 2023
- Published by Pleiades Publishing Ltd in Physics of the Solid State
- Vol. 65 (1) , 32-35
Effect of Annealing on the Microstructure and Hardness of EP648 Alloy after Direct Metal Deposition
Samples of Ni-based super alloy are received by the method of direct metal deposition. Annealing at temperature 1180°С during 4 h is provided. Measurements of hardness, optical metallography, X-ray analysis are carried out. It was found that direct metal deposition of samples from Ni-based super alloy EP648 lead to Ni solid solution of alloying elements with face-centered cubic structure having lattice period a = 7.11 Å, also structure of Ni2Cr, is slightly revealed by optical metallography. Annealing at temperature 1180°С during 4 h of the direct metal deposited samples of super alloy EP648 lead to hardness increasing from от 19 ± 4 HRC to 34 ± 0.3 HRС, the uniformity of values are observed. After annealing the face-centered cubic structure is revealed, high value of lattice period is saving; presence of the phase Ni2Cr and sedimentation of Ni3Cr2 are found. Residual tensile macro stresses are found.
- 1 January 2023
- Published by Pleiades Publishing Ltd in Physics of the Solid State
- Vol. 65 (1) , 32-35
Effect of Annealing on the Microstructure and Hardness of EP648 Alloy after Direct Metal Deposition
Samples of Ni-based super alloy are received by the method of direct metal deposition. Annealing at temperature 1180°С during 4 h is provided. Measurements of hardness, optical metallography, X-ray analysis are carried out. It was found that direct metal deposition of samples from Ni-based super alloy EP648 lead to Ni solid solution of alloying elements with face-centered cubic structure having lattice period a = 7.11 Å, also structure of Ni2Cr, is slightly revealed by optical metallography. Annealing at temperature 1180°С during 4 h of the direct metal deposited samples of super alloy EP648 lead to hardness increasing from от 19 ± 4 HRC to 34 ± 0.3 HRС, the uniformity of values are observed. After annealing the face-centered cubic structure is revealed, high value of lattice period is saving; presence of the phase Ni2Cr and sedimentation of Ni3Cr2 are found. Residual tensile macro stresses are found.
- Open Access
Optimization of Process Parameters for Powder Bed Fusion Additive Manufacturing Using a Linear Programming Method: A Conceptual Framework
At present, the selection of optimal technological parameters for laser powder bed fusion (LPBF) is determined by the requirements of the fusion process. The main parameters that are commonly varied include laser power (P), scanning speed (v), hatch spacing (h), and layer thickness (t). The productivity of the LPBF process (the increment in the fused volume of the material) is equal to the product of the last three parameters, and the mechanical properties are largely determined by the volumetric fusion energy density, which is equal to the ratio of laser power to productivity. While ensuring maximum process productivity, it is possible to obtain acceptable quality characteristics—mechanical properties, surface roughness, etc.—for a certain range of LPBF technological parameters. In these cases, several quality characteristics act as constraints on the optimization process, and productivity and the key quality characteristics become components of the objective function. Therefore, this article proposes a formalized representation of the optimization problem for the LPBF process, including the derivation of the objective function with the constraint matrix, and provides a solution to the problem using the linear programming (LP) method. The advantages of the proposed method include the guaranteed convergence of the solution with an unlimited number of constraints; the disadvantage concerns the adequacy of the solution, which is limited by a relatively narrow range of parameter changes. The proposed method was tested in determining the optimal LPBF parameters for an HN58MBYu powder LP model that included 13 constraints and an objective function with two target parameters. The obtained results made it possible to increase the productivity by 15% relative to the basic technological parameters.
Open AccessOptimization of Process Parameters for Powder Bed Fusion Additive Manufacturing Using a Linear Programming Method: A Conceptual Framework
At present, the selection of optimal technological parameters for laser powder bed fusion (LPBF) is determined by the requirements of the fusion process. The main parameters that are commonly varied include laser power (P), scanning speed (v), hatch spacing (h), and layer thickness (t). The productivity of the LPBF process (the increment in the fused volume of the material) is equal to the product of the last three parameters, and the mechanical properties are largely determined by the volumetric fusion energy density, which is equal to the ratio of laser power to productivity. While ensuring maximum process productivity, it is possible to obtain acceptable quality characteristics—mechanical properties, surface roughness, etc.—for a certain range of LPBF technological parameters. In these cases, several quality characteristics act as constraints on the optimization process, and productivity and the key quality characteristics become components of the objective function. Therefore, this article proposes a formalized representation of the optimization problem for the LPBF process, including the derivation of the objective function with the constraint matrix, and provides a solution to the problem using the linear programming (LP) method. The advantages of the proposed method include the guaranteed convergence of the solution with an unlimited number of constraints; the disadvantage concerns the adequacy of the solution, which is limited by a relatively narrow range of parameter changes. The proposed method was tested in determining the optimal LPBF parameters for an HN58MBYu powder LP model that included 13 constraints and an objective function with two target parameters. The obtained results made it possible to increase the productivity by 15% relative to the basic technological parameters.