Kimiaki Nagatsuka
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Kimiaki Nagatsuka has a total of 14 co-authors. Here are the top co-authors by number of shared publications:
Bolyu Xiao
Joining and Welding Research Institute, Osaka University, Osaka, Japan
1 shared publicationK Nakata
Joining and Welding Research Institute, Osaka University, 11-1 Mihogaoka, Ibaraki, Osaka 567-0047, Japan
1 shared publicationK. Nakata
Joining and Welding Research Institute, Osaka University, 11-1, Mihogaoka, Ibaraki, Osaka, 567-0047, Japan
1 shared publicationKazuhiro Nakata
Joining and Welding Research Institute, Osaka University, Osaka, Japan
1 shared publication- Kazuhiro Nakata
Joining and Welding Research Institute, Osaka University, 11-1, Mihogaoka, Ibaraki, Osaka 567-0047, Japan
1 shared publication Lihui Wu
Joining and Welding Research Institute, Osaka University, Osaka, Japan
1 shared publication
Latest Publications
- 1 April 2018
- Published by SAGE Publications in Science and Technology of Welding and Joining
- Vol. 23 (3) , 181-186
Resistance spot welding of metal/carbon-fibre-reinforced plastics and applying silane coupling treatment
Dissimilar materials joining of SUS304 and carbon-fibre-reinforced plastics consisting of short fibres and thermoplastics was performed. The materials were joined by series resistance spot welding. The electrodes were pressed on the metal plate of the lap joint of metal/carbon-fibre-reinforced plastics. The SUS304 plate was heated by resistance heating, causing the thermoplastic near the interface to melt slightly because of heat conduction. SUS304 could be joined directly to carbon-fibre-reinforced polyamide and modified polypropylene, but not to polyphenylene sulphide. The joining area increased with an increase in the welding current and welding time, so did the tensile shear fracture load. Furthermore, the silane coupling agent treatment of SUS304 was highly effective in increasing the joining strength.
- 1 April 2018
- Published by SAGE Publications in Science and Technology of Welding and Joining
- Vol. 23 (3) , 181-186
Resistance spot welding of metal/carbon-fibre-reinforced plastics and applying silane coupling treatment
Dissimilar materials joining of SUS304 and carbon-fibre-reinforced plastics consisting of short fibres and thermoplastics was performed. The materials were joined by series resistance spot welding. The electrodes were pressed on the metal plate of the lap joint of metal/carbon-fibre-reinforced plastics. The SUS304 plate was heated by resistance heating, causing the thermoplastic near the interface to melt slightly because of heat conduction. SUS304 could be joined directly to carbon-fibre-reinforced polyamide and modified polypropylene, but not to polyphenylene sulphide. The joining area increased with an increase in the welding current and welding time, so did the tensile shear fracture load. Furthermore, the silane coupling agent treatment of SUS304 was highly effective in increasing the joining strength.
- 1 August 2014
- Published by SAGE Publications in Science and Technology of Welding and Joining
- Vol. 19 (6) , 521-526
Effect of Ti content in Ag–Cu–Ti activated filler metal on dissimilar joint formation of sialon and WC–Co alloy by laser brazing
Laser brazing was carried out for dissimilar joining of sialon and a WC–Co alloy. Eutectic type Ag–Cu alloys as filler metals with different Ti content ranging from 0 to 2·8 mass-% were used to investigate the effects of Ti on the interface structure and strength of the joint. The filler metal sheet was sandwiched between a sialon block and a WC–Co alloy plate, and a laser beam was irradiated selectively on the WC–Co alloy plate. The brazed joint was obtained using the filler metal containing >0·3 mass-%Ti. TiN, Ti5Si3, and Cu4Ti layers were formed at the interface of sialon and brazed metal as compound layers. The shear strength of the brazed joint increased with increasing Ti content in the filler metal in the range 0·3–1·7 mass-%, reaching a maximum value of 106 MPa. However, the strength decreased when the Ti content became higher than 1·7 mass-%.
- 1 August 2014
- Published by SAGE Publications in Science and Technology of Welding and Joining
- Vol. 19 (6) , 521-526
Effect of Ti content in Ag–Cu–Ti activated filler metal on dissimilar joint formation of sialon and WC–Co alloy by laser brazing
Laser brazing was carried out for dissimilar joining of sialon and a WC–Co alloy. Eutectic type Ag–Cu alloys as filler metals with different Ti content ranging from 0 to 2·8 mass-% were used to investigate the effects of Ti on the interface structure and strength of the joint. The filler metal sheet was sandwiched between a sialon block and a WC–Co alloy plate, and a laser beam was irradiated selectively on the WC–Co alloy plate. The brazed joint was obtained using the filler metal containing >0·3 mass-%Ti. TiN, Ti5Si3, and Cu4Ti layers were formed at the interface of sialon and brazed metal as compound layers. The shear strength of the brazed joint increased with increasing Ti content in the filler metal in the range 0·3–1·7 mass-%, reaching a maximum value of 106 MPa. However, the strength decreased when the Ti content became higher than 1·7 mass-%.
- 7 August 2012
- Published by IOP Publishing in Journal of Physics: Conference Series
- Vol. 379 (1) , 012047
Dissimilar joint characteristics of SiC and WC-Co alloy by laser brazing
- 7 August 2012
- Published by IOP Publishing in Journal of Physics: Conference Series
- Vol. 379 (1) , 012047
Dissimilar joint characteristics of SiC and WC-Co alloy by laser brazing
- 22 December 2011
- Published by Elsevier in Materials Science and Engineering: B
- Vol. 177 (7) , 520-523
Characteristics of dissimilar laser-brazed joints of isotropic graphite to WC–Co alloy
- 22 December 2011
- Published by Elsevier in Materials Science and Engineering: B
- Vol. 177 (7) , 520-523
Characteristics of dissimilar laser-brazed joints of isotropic graphite to WC–Co alloy