Chaou Choak Tan
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Chaou Choak Tan has a total of 20 co-authors. Here are the top co-authors by number of shared publications:
Guillaume Remy
University of Warwick
2 shared publicationsMark A Williams
University of Warwick
2 shared publicationsMelanie J Loveridge
University of Warwick
2 shared publicationsRohit Bhagat
University of Warwick
2 shared publicationsShaun Dixon
University of Warwick
2 shared publicationsAnup Barai
University of Warwick
1 shared publication
Latest Publications
- Open Access
A Study on the Influence of Lithium Plating on Battery Degradation
Within Li-ion batteries, lithium plating is considered as one of the main reasons behind the capacity fade that occurs during low temperature and fast charging conditions. Previous studies indicate that plating is influenced by the levels of loss of lithium inventory (LLI) and the loss of active material (LAM) present in a battery. However, it is not clear from the literature on how lithium plating influences battery degradation in terms of LAM and LLI. Quantifying the undesirable impacts of lithium plating can help in understanding its impact on battery degradation and feedback effects of previous lithium plating on the formation of present plating. This study aims to quantify the degradation modes of lithium plating: LLI, LAM at the electrode level. A commercial Li-ion cell was first, aged using two different cases: with and without lithium plating. Second, a degradation diagnostic method is developed to quantify the degradation modes based on their measurable effects on open-circuit voltage (OCV) and cell capacity. The results highlight that LAMNE and LLI levels under the fast charge profile are increased by 10% and 12%, respectively, compared to those under the less aggressive charge profile. Further, limitations of the degradation analysis methods are discussed.
Open AccessA Study on the Influence of Lithium Plating on Battery Degradation
Within Li-ion batteries, lithium plating is considered as one of the main reasons behind the capacity fade that occurs during low temperature and fast charging conditions. Previous studies indicate that plating is influenced by the levels of loss of lithium inventory (LLI) and the loss of active material (LAM) present in a battery. However, it is not clear from the literature on how lithium plating influences battery degradation in terms of LAM and LLI. Quantifying the undesirable impacts of lithium plating can help in understanding its impact on battery degradation and feedback effects of previous lithium plating on the formation of present plating. This study aims to quantify the degradation modes of lithium plating: LLI, LAM at the electrode level. A commercial Li-ion cell was first, aged using two different cases: with and without lithium plating. Second, a degradation diagnostic method is developed to quantify the degradation modes based on their measurable effects on open-circuit voltage (OCV) and cell capacity. The results highlight that LAMNE and LLI levels under the fast charge profile are increased by 10% and 12%, respectively, compared to those under the less aggressive charge profile. Further, limitations of the degradation analysis methods are discussed.
- 30 June 2019
- Published by The Electrochemical Society in ECS Meeting Abstracts
- Vol. MA2019-04 (1) , 70
Ageing Analysis of Miniature Cylindrical Cell for Fitbit Flex 2 Wristband
Lithium ion battery (LIB) is gaining popularity in energy storage device due to its high energy density per unit mass and has found application in mobile phone, laptops, power tools and electric vehicle. More recently, LIB has also been utilised to power smart wearable devices such as fitness tracker, smart watches and smart glasses. Wearable device is gaining popularity and the market will continue to grow1. With devices shrinking so drastically, the need for smaller but higher energy density battery and good cycle life is more demanding than ever. Understanding battery performance and its degradation process are therefore crucial to give insights on how to extend battery life and reduce capacity-fading. Here, we performed cell assessment on miniature cylindrical cell extracted from Fitbit Flex 2 fitness tracker and with an attempt to understand capacity-fading process of Fitbit cell utilising electrochemical, teardown and materials analysis. This miniature cylindrical cell is 3.65 x 20 mm in size with energy density of 503Wh/L and nominal capacity of 15mAh. Teardown analysis on several numbers of non-cycled Fitbit cells have shown severe anode coating delamination from the copper current collector when the jelly roll were unravelled and with anode materials transferred to the separator. Nevertheless, Fitbit cell shows 82 % cell capacity retention after 500 continuous charging and discharging cycles at 3.0-4.35 V, 0.75C rate at 20 °C. Electrochemical Impedance Spectroscopy (EIS) shows increase in internal cell resistance, in which Li+ ion charge-transfer resistance (Rct) is the main contributor. Scanning electron microscope (SEM) with energy dispersive spectroscopy (EDS) shows no visible morphological and compositional changes between fresh and aged cathode, anode and separator. X-ray photoelectron spectroscopy (XPS) reveals surface film contains organic compounds as well as lithium fluoride (LiF) and phosphates other than LiPF6 forming on both cathode and anode surface. XPS also shows increasing LiF and phosphates in cathode and anode surface film. The cause of increasing Rct and the possible source of LiF will be discussed. 1. https://www.statista.com/statistics/610447/wearable-device-revenue-worldwide/ [assessed on 17 January 2019] Figure 1
- 30 June 2019
- Published by The Electrochemical Society in ECS Meeting Abstracts
- Vol. MA2019-04 (1) , 70
Ageing Analysis of Miniature Cylindrical Cell for Fitbit Flex 2 Wristband
Lithium ion battery (LIB) is gaining popularity in energy storage device due to its high energy density per unit mass and has found application in mobile phone, laptops, power tools and electric vehicle. More recently, LIB has also been utilised to power smart wearable devices such as fitness tracker, smart watches and smart glasses. Wearable device is gaining popularity and the market will continue to grow1. With devices shrinking so drastically, the need for smaller but higher energy density battery and good cycle life is more demanding than ever. Understanding battery performance and its degradation process are therefore crucial to give insights on how to extend battery life and reduce capacity-fading. Here, we performed cell assessment on miniature cylindrical cell extracted from Fitbit Flex 2 fitness tracker and with an attempt to understand capacity-fading process of Fitbit cell utilising electrochemical, teardown and materials analysis. This miniature cylindrical cell is 3.65 x 20 mm in size with energy density of 503Wh/L and nominal capacity of 15mAh. Teardown analysis on several numbers of non-cycled Fitbit cells have shown severe anode coating delamination from the copper current collector when the jelly roll were unravelled and with anode materials transferred to the separator. Nevertheless, Fitbit cell shows 82 % cell capacity retention after 500 continuous charging and discharging cycles at 3.0-4.35 V, 0.75C rate at 20 °C. Electrochemical Impedance Spectroscopy (EIS) shows increase in internal cell resistance, in which Li+ ion charge-transfer resistance (Rct) is the main contributor. Scanning electron microscope (SEM) with energy dispersive spectroscopy (EDS) shows no visible morphological and compositional changes between fresh and aged cathode, anode and separator. X-ray photoelectron spectroscopy (XPS) reveals surface film contains organic compounds as well as lithium fluoride (LiF) and phosphates other than LiPF6 forming on both cathode and anode surface. XPS also shows increasing LiF and phosphates in cathode and anode surface film. The cause of increasing Rct and the possible source of LiF will be discussed. 1. https://www.statista.com/statistics/610447/wearable-device-revenue-worldwide/ [assessed on 17 January 2019] Figure 1
- 23 July 2018
- Published by The Electrochemical Society in ECS Meeting Abstracts
- Vol. MA2018-02 (7) , 482
Pushing to the Limit: Samsung Galaxy Note 7 and Fitbit Flex 2
The ongoing demand for smaller and lighter devices, with batteries having longer usage times, has put increasing operational pressure on the batteries. The use of higher capacity cathodes, increasing areal capacity and thinner separators are some of the approaches used to achieve higher energy densities. Here we report two case studies on batteries from the Samsung Galaxy Note 7 phone and fitness tracker wristband, Fitbit Flex 2, highlighting where the device manufacturers were pushing the boundaries to achieve this higher energy density. In September 2016, several reports were published of the Samsung Galaxy Note 7 phone batteries overheating, exploding or catching fire, which led to a total product recall of the Samsung Galaxy Note 7 phone. “The launch of what was supposed to be its flagship model has turned into a fiasco for the world's largest smartphone maker”, the BBC reported1. We carried out a more in-depth investigation, “Looking Deeper into the Galaxy (Note 7)2”, inspecting each of the battery components. The study incorporated X-ray computed tomography, thermal imaging and scanning electron microscopy (with energy dispersive spectroscopy), to identify the most likely root causes of the battery failure. The findings reveal that thermal properties of the battery is not thought to be a contributing factor to battery failure but are from battery design/cell manufacturing defects: (1) Unintended folding of the anode coating at the corner near to the anode tab resulted from insufficient space to safely accommodate the electrodes; (2) No Insulating tape on the cathode tab, and (3) un-bonded welding sections with protrusion features observed at the cathode tab which may penetrate the separator. Such flaws can lead to internal short circuit between the cathode and anode; (4) A much thinner separator (≤ 5 µm, with 2O3 coating on both sides) used in Galaxy Note 7 also increased the likelihood of separator damage which can lead to short circuit. The ceramic coating layer detached itself quite easily when the cell was unravelled, indicating a lack of interfacial integrity. We also report another forensic investigation on a miniature lithium ion rechargeable cylindrical cell with a diameter of 3.65 mm and length in 20 mm, and nominal capacity of 15 mAh, which is fitted in Fitbit Flex 2 fitness tracker. This miniature cylindrical cell shows an impressive volumetric energy density of 503 Wh/L despite having a limited space. The unravelling of the jelly roll shows severe anode coating delamination from the copper current collector, transferring unto the separator. The high bending stress exert on the cell components when rolled up to a 3 mm diameter jelly roll has resulted severe delamination of the anode coating. 1. http://www.bbc.co.uk/news/technology-37615496 2. Melanie J. Loveridge, Guillaume Remy, Nadia Kourra, Ronny Genieser, Anup Barai, Mike J. Lain, Yue Guo, Mark Amor-Segan, Mark A. Williams, Tazdin Amietszajew, Mark Ellis, Rohit Bhagat and David Greenwood, Looking Deeper into the Galaxy (Note 7). Batteries 2018, 4 (1), 3. Figure 1
- 23 July 2018
- Published by The Electrochemical Society in ECS Meeting Abstracts
- Vol. MA2018-02 (7) , 482
Pushing to the Limit: Samsung Galaxy Note 7 and Fitbit Flex 2
The ongoing demand for smaller and lighter devices, with batteries having longer usage times, has put increasing operational pressure on the batteries. The use of higher capacity cathodes, increasing areal capacity and thinner separators are some of the approaches used to achieve higher energy densities. Here we report two case studies on batteries from the Samsung Galaxy Note 7 phone and fitness tracker wristband, Fitbit Flex 2, highlighting where the device manufacturers were pushing the boundaries to achieve this higher energy density. In September 2016, several reports were published of the Samsung Galaxy Note 7 phone batteries overheating, exploding or catching fire, which led to a total product recall of the Samsung Galaxy Note 7 phone. “The launch of what was supposed to be its flagship model has turned into a fiasco for the world's largest smartphone maker”, the BBC reported1. We carried out a more in-depth investigation, “Looking Deeper into the Galaxy (Note 7)2”, inspecting each of the battery components. The study incorporated X-ray computed tomography, thermal imaging and scanning electron microscopy (with energy dispersive spectroscopy), to identify the most likely root causes of the battery failure. The findings reveal that thermal properties of the battery is not thought to be a contributing factor to battery failure but are from battery design/cell manufacturing defects: (1) Unintended folding of the anode coating at the corner near to the anode tab resulted from insufficient space to safely accommodate the electrodes; (2) No Insulating tape on the cathode tab, and (3) un-bonded welding sections with protrusion features observed at the cathode tab which may penetrate the separator. Such flaws can lead to internal short circuit between the cathode and anode; (4) A much thinner separator (≤ 5 µm, with 2O3 coating on both sides) used in Galaxy Note 7 also increased the likelihood of separator damage which can lead to short circuit. The ceramic coating layer detached itself quite easily when the cell was unravelled, indicating a lack of interfacial integrity. We also report another forensic investigation on a miniature lithium ion rechargeable cylindrical cell with a diameter of 3.65 mm and length in 20 mm, and nominal capacity of 15 mAh, which is fitted in Fitbit Flex 2 fitness tracker. This miniature cylindrical cell shows an impressive volumetric energy density of 503 Wh/L despite having a limited space. The unravelling of the jelly roll shows severe anode coating delamination from the copper current collector, transferring unto the separator. The high bending stress exert on the cell components when rolled up to a 3 mm diameter jelly roll has resulted severe delamination of the anode coating. 1. http://www.bbc.co.uk/news/technology-37615496 2. Melanie J. Loveridge, Guillaume Remy, Nadia Kourra, Ronny Genieser, Anup Barai, Mike J. Lain, Yue Guo, Mark Amor-Segan, Mark A. Williams, Tazdin Amietszajew, Mark Ellis, Rohit Bhagat and David Greenwood, Looking Deeper into the Galaxy (Note 7). Batteries 2018, 4 (1), 3. Figure 1