Haitao Li
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Haitao Li has a total of 39 co-authors. Here are the top co-authors by number of shared publications:
Qian Li
School of Materials Science and Engineering, Henan University of Science and Technology, Luoyang, People’s Republic of China
3 shared publicationsBo-Ping Zhang
University of Science and Technology Beijing
2 shared publicationsBoping Zhang
2 shared publications- Gong Xintai
Henan University of Science and Technology
2 shared publications Rui Zhang
2 shared publications- Yong-Jun Gu
School of Materials Science and Engineering, Henan University of Science and Technology, Luoyang, China
2 shared publications
Latest Publications
- 22 June 2026
- Published by Elsevier in Ceramics International
- Vol. 52 (20) , 35887-35896
Enhanced piezoelectric properties of KNN-based ceramics co-modified by CaZrO3 and LiSbO3
- 22 June 2026
- Published by Elsevier in Ceramics International
- Vol. 52 (20) , 35887-35896
Enhanced piezoelectric properties of KNN-based ceramics co-modified by CaZrO3 and LiSbO3
- Open Access
- 1 January 2023
- Published by Lab Academic Press in Materials Lab
- Vol. 2
Enhanced piezoelectric properties for potassium sodium niobate lead-free piezoelectric ceramics prepared by microwave technology
Potassium-sodium niobate (Na, K)NbO3 (NKN) powder was synthesized at low temperature via microwave-assisted hydrothermal solovthermal method (MHSM). The resultant powder was characterized by X-ray diffraction (XRD) and scanning electron microscope (SEM). XRD results showed that pure (Na, K)NbO3 powder with a single perovskite structure was successfully synthesized when the concentration of mineralization exceeded 1 M. In order to reduce the volatilization of alkaline elements, NKN ceramics derived from 5M-powder were prepared in a microwave furnace. Microstructure, stoichiometry, and electrical properties of the obtained ceramics were investigated. The piezoelectric coefficient (d33), electromechanical coupling coefficient (kp) and remnant polarization (Pr) of the sample sintered at 1050 ℃ show optimal values of 132 pC/N, 38% and 26.3 µC/cm2, respectively. The results indicate that the microwave heating is a promising method for synthesizing and sintering NKN-based ceramics.
- 1 January 2023
- Published by Lab Academic Press in Materials Lab
- Vol. 2
Open AccessEnhanced piezoelectric properties for potassium sodium niobate lead-free piezoelectric ceramics prepared by microwave technology
Potassium-sodium niobate (Na, K)NbO3 (NKN) powder was synthesized at low temperature via microwave-assisted hydrothermal solovthermal method (MHSM). The resultant powder was characterized by X-ray diffraction (XRD) and scanning electron microscope (SEM). XRD results showed that pure (Na, K)NbO3 powder with a single perovskite structure was successfully synthesized when the concentration of mineralization exceeded 1 M. In order to reduce the volatilization of alkaline elements, NKN ceramics derived from 5M-powder were prepared in a microwave furnace. Microstructure, stoichiometry, and electrical properties of the obtained ceramics were investigated. The piezoelectric coefficient (d33), electromechanical coupling coefficient (kp) and remnant polarization (Pr) of the sample sintered at 1050 ℃ show optimal values of 132 pC/N, 38% and 26.3 µC/cm2, respectively. The results indicate that the microwave heating is a promising method for synthesizing and sintering NKN-based ceramics.
- 12 July 2022
- Published by Trans Tech Publications, Ltd. in Journal of Nano Research
- Vol. 74, 83-96
Enhancing Dispersion of Yttria-Stabilized Tetragonal Zirconia Nanopowders with Microwave Solvothermal Synthesis
Yttria stabilized tetragonal zirconia (Y0.08Zr0.94O2, YSZ) nanopowders were successfully synthesized by microwave solvothermal method (MSM). The synthesizing temperature, holding time and mineralizer concentration were optimized. The crystallization and particle distribution of as-prepared YSZ nanopowders were identified by DSC/TG, XRD, FESEM, TEM, FTIR, DLS, and BET. The dispersion of YSZ nanopowders dried by different methods and modified by polyethyleneimine (PEI) was analyzed and discussed. The results show that the PEI modified samples have the best dispersion, and the dispersion of freeze-dried samples is better than that of traditional dried ones. The particle size of the PEI modified samples calculated from the surface area determined by BET is 15.7 nm, which is consistent with that determined by TEM (16.5 nm), but slightly smaller than that calculated by the Scherrer formula according to XRD (22.3 nm). This may be attributed to the different testing principles in these methods.
- 12 July 2022
- Published by Trans Tech Publications, Ltd. in Journal of Nano Research
- Vol. 74, 83-96
Enhancing Dispersion of Yttria-Stabilized Tetragonal Zirconia Nanopowders with Microwave Solvothermal Synthesis
Yttria stabilized tetragonal zirconia (Y0.08Zr0.94O2, YSZ) nanopowders were successfully synthesized by microwave solvothermal method (MSM). The synthesizing temperature, holding time and mineralizer concentration were optimized. The crystallization and particle distribution of as-prepared YSZ nanopowders were identified by DSC/TG, XRD, FESEM, TEM, FTIR, DLS, and BET. The dispersion of YSZ nanopowders dried by different methods and modified by polyethyleneimine (PEI) was analyzed and discussed. The results show that the PEI modified samples have the best dispersion, and the dispersion of freeze-dried samples is better than that of traditional dried ones. The particle size of the PEI modified samples calculated from the surface area determined by BET is 15.7 nm, which is consistent with that determined by TEM (16.5 nm), but slightly smaller than that calculated by the Scherrer formula according to XRD (22.3 nm). This may be attributed to the different testing principles in these methods.
- 2 July 2022
- Published by Elsevier in Solid State Communications
- Vol. 353
(K, Na)NbO3 lead-free piezoceramics prepared by microwave sintering and solvothermal powder synthesis
- 2 July 2022
- Published by Elsevier in Solid State Communications
- Vol. 353
(K, Na)NbO3 lead-free piezoceramics prepared by microwave sintering and solvothermal powder synthesis
- Open Access
- 1 January 2022
- Published by Elsevier in SSRN Electronic Journal
(K, Na)Nbo 3 Lead-Free Piezoceramics Prepared by Microwave Sintering and Solvothermal Powder Synthesis
Low temperature and short processing time are benefical for fabricating (K, Na)NbO 3 (KNN) lead-free piezoelectric ceramics with a drawback of easy alkali metal volatilization during the powder synthesis and sintering processes. This study revealed that microwave sintering in addition to microwave solvothermal powder synthesis can lead to short-time fabrication of KNN ceramics with high density and fine grains. It was found that KNN powder with a single perovskite structure can be synthesized successfully by microwave solvothermal method if the KOH/NaOH concentration exceeds 1 M, which can be densified by microwave sintering to a high relative density close to 97% at 1050 o C even using 2/9 shorter soak time than normal sintering at the same temperature. Importantly, the microwave-sintered KNN ceramics show better piezoelectric and ferroelectric properties than that by normal sintering. Despite nonexistence of any dopants, a high-level piezoelectric coefficient ( d 33 ) reaching 132 pC/N was obtained in the MS-processed pure KNN ceramics that also possess better ferroelectric properties with a high remnant polarization ( P r ) up to 26.3 µC/cm 2 . The present work indicate that the microwave solvothermal method is a promising method for preparing KNN-based ceramics.
- 1 January 2022
- Published by Elsevier in SSRN Electronic Journal
Open Access(K, Na)Nbo 3 Lead-Free Piezoceramics Prepared by Microwave Sintering and Solvothermal Powder Synthesis
Low temperature and short processing time are benefical for fabricating (K, Na)NbO 3 (KNN) lead-free piezoelectric ceramics with a drawback of easy alkali metal volatilization during the powder synthesis and sintering processes. This study revealed that microwave sintering in addition to microwave solvothermal powder synthesis can lead to short-time fabrication of KNN ceramics with high density and fine grains. It was found that KNN powder with a single perovskite structure can be synthesized successfully by microwave solvothermal method if the KOH/NaOH concentration exceeds 1 M, which can be densified by microwave sintering to a high relative density close to 97% at 1050 o C even using 2/9 shorter soak time than normal sintering at the same temperature. Importantly, the microwave-sintered KNN ceramics show better piezoelectric and ferroelectric properties than that by normal sintering. Despite nonexistence of any dopants, a high-level piezoelectric coefficient ( d 33 ) reaching 132 pC/N was obtained in the MS-processed pure KNN ceramics that also possess better ferroelectric properties with a high remnant polarization ( P r ) up to 26.3 µC/cm 2 . The present work indicate that the microwave solvothermal method is a promising method for preparing KNN-based ceramics.
- 9 October 2017
- Published by Springer Nature in Journal of Materials Science: Materials in Electronics
- Vol. 29 (1) , 746-752
Hydrothermal solvothermal synthesis potassium sodium niobate lead-free piezoelectric ceramics assisted with microwave
- 9 October 2017
- Published by Springer Nature in Journal of Materials Science: Materials in Electronics
- Vol. 29 (1) , 746-752
Hydrothermal solvothermal synthesis potassium sodium niobate lead-free piezoelectric ceramics assisted with microwave
- Open Access
- 1 January 2015
- Published by Shanghai Institute of Ceramics in Journal of Inorganic Materials
- Vol. 30 (4) , 369-373
Effect of ZnO-doping on Sinterability and Microwave Dielectric Property of Ca$lt;inf$gt;0.25$lt;/inf$gt;(Li$lt;inf$gt;0.43$lt;/inf$gt;Sm$lt;inf$gt;0.57$lt;/inf$gt;)$lt;inf$gt;0.75$lt;/inf$gt;TiO$lt;inf$gt;3$lt;/inf$gt; Ceramics
ZnO 掺杂对 Ca 0.25 (Li 0.43 Sm 0.57) 0.75 TiO 3 陶瓷烧结性能 和微波介电性能的影响 李海涛, 李 谦, 闫焉服, 许荣辉 (河南科技大学 材料科学与工程学院, 洛阳 471003) 摘 要: 采用溶胶-凝胶法制备 Ca 0.25 (Li 0.43 Sm 0.57) 0.75 TiO 3 (CLST)微波介质陶瓷纳米粉体, 研究了 ZnO 掺杂量和烧结 温度对 CLST+ xmol% ZnO 陶瓷烧结性能和微波介电性能的影响。XRD 分析结果表明: 随着 ZnO 掺杂量 x 的增加, 陶瓷的晶体结构从正交相变为伪立方相, 并在 x≥1.5 的样品中出现了杂相。CLST+ xmol% ZnO 陶瓷的致密化烧结 温度随 x 的增加而降低, x=1.0 的样品的致密化烧结温度比 x=0 的降低了 200 ℃。 介电常数 ε r 和频率品质因数 Qf 随 x 增加和烧结温度的升高具有最优值, 频率温度系数则单调降低。x=1.0 的样品在 1100 ℃烧结时具有优异的综合性 能: ρ = 4.85 g/cm 3 , ε r =102.8, Qf = 5424 GHz, τ f =-8.2×10-6 /℃。 表明 ZnO 掺杂的 CLST 陶瓷是一种很有发展潜力的 微波介质陶瓷。
- 1 January 2015
- Published by Shanghai Institute of Ceramics in Journal of Inorganic Materials
- Vol. 30 (4) , 369-373
Open AccessEffect of ZnO-doping on Sinterability and Microwave Dielectric Property of Ca$lt;inf$gt;0.25$lt;/inf$gt;(Li$lt;inf$gt;0.43$lt;/inf$gt;Sm$lt;inf$gt;0.57$lt;/inf$gt;)$lt;inf$gt;0.75$lt;/inf$gt;TiO$lt;inf$gt;3$lt;/inf$gt; Ceramics
ZnO 掺杂对 Ca 0.25 (Li 0.43 Sm 0.57) 0.75 TiO 3 陶瓷烧结性能 和微波介电性能的影响 李海涛, 李 谦, 闫焉服, 许荣辉 (河南科技大学 材料科学与工程学院, 洛阳 471003) 摘 要: 采用溶胶-凝胶法制备 Ca 0.25 (Li 0.43 Sm 0.57) 0.75 TiO 3 (CLST)微波介质陶瓷纳米粉体, 研究了 ZnO 掺杂量和烧结 温度对 CLST+ xmol% ZnO 陶瓷烧结性能和微波介电性能的影响。XRD 分析结果表明: 随着 ZnO 掺杂量 x 的增加, 陶瓷的晶体结构从正交相变为伪立方相, 并在 x≥1.5 的样品中出现了杂相。CLST+ xmol% ZnO 陶瓷的致密化烧结 温度随 x 的增加而降低, x=1.0 的样品的致密化烧结温度比 x=0 的降低了 200 ℃。 介电常数 ε r 和频率品质因数 Qf 随 x 增加和烧结温度的升高具有最优值, 频率温度系数则单调降低。x=1.0 的样品在 1100 ℃烧结时具有优异的综合性 能: ρ = 4.85 g/cm 3 , ε r =102.8, Qf = 5424 GHz, τ f =-8.2×10-6 /℃。 表明 ZnO 掺杂的 CLST 陶瓷是一种很有发展潜力的 微波介质陶瓷。
- 20 April 2012
- Published by China Science Publishing & Media Ltd. in Journal of Inorganic Materials
- Vol. 27 (4) , 385-389
Influence of Compensated Li Content on Microstructure, Crystalline Phase and Electrical Properties of NKN-based Lead-free Piezoelectric Ceramics
High dense Li0.05+x(Na0.535K0.48)0.95NbO3 (LxNKN) lead―free piezoelectric ceramics with fine morphology were synthesised by conventional mixed―oxide method at 1000¡䪠and its microstructure, phase structure and electrical properties were investigated as a function of excessive Li addition. The results revealed that the excess Li content facilitated the sinterability and improved the piezoelectric properties for LxNKN ceramics. A PPT bridging tetragonal and orthorhombic symmetry was found at x= 0.01―0.015 by using the X―ray diffraction patterns and the corresponding calculation of lattice parameters. Owing to such transitional behavior, the piezoelectric coefficient (d33), electromechanical coupling coefficient (kp), dielectric constant (εr) and remanent polarization (Pr) were enhanced to peak values, 282 pC/N, 44%, 942 and 27 μC/cm2, respectively. Compared with LNKN ceramics, the variation in Curie temperature (Tc) by the compensation amount of Li was much smaller for LxNKN ceramics. The reason is that the amount of Li that entered into crystal lattice is relatively rare for LxNKN ceramics. The results provide a way to low―temperature sintering of LNKN―based lead―free piezoceramics with high performance
- 20 April 2012
- Published by China Science Publishing & Media Ltd. in Journal of Inorganic Materials
- Vol. 27 (4) , 385-389
Influence of Compensated Li Content on Microstructure, Crystalline Phase and Electrical Properties of NKN-based Lead-free Piezoelectric Ceramics
High dense Li0.05+x(Na0.535K0.48)0.95NbO3 (LxNKN) lead―free piezoelectric ceramics with fine morphology were synthesised by conventional mixed―oxide method at 1000¡䪠and its microstructure, phase structure and electrical properties were investigated as a function of excessive Li addition. The results revealed that the excess Li content facilitated the sinterability and improved the piezoelectric properties for LxNKN ceramics. A PPT bridging tetragonal and orthorhombic symmetry was found at x= 0.01―0.015 by using the X―ray diffraction patterns and the corresponding calculation of lattice parameters. Owing to such transitional behavior, the piezoelectric coefficient (d33), electromechanical coupling coefficient (kp), dielectric constant (εr) and remanent polarization (Pr) were enhanced to peak values, 282 pC/N, 44%, 942 and 27 μC/cm2, respectively. Compared with LNKN ceramics, the variation in Curie temperature (Tc) by the compensation amount of Li was much smaller for LxNKN ceramics. The reason is that the amount of Li that entered into crystal lattice is relatively rare for LxNKN ceramics. The results provide a way to low―temperature sintering of LNKN―based lead―free piezoceramics with high performance
- 21 May 2010
- Published by Wiley in Rare Metals
- Vol. 29 (3) , 243-247
Microstructure and microwave dielectric properties of ZnO‐B 2 O 3 added (Ca 0.254 Li 0.19 Sm 0.14 )TiO 3 ceramics
The effects of ZnO‐B 2 O 3 (ZB 2 ) on the sintering behavior and microwave dielectric properties of (Ca 0.254 Li 0.19 Sm 0.14 )TiO 3 ceramics were investigated. The densities of the specimens reached the maximum value by adding 3 wt.% ZB 2 and then decreased. The sintering temperature of the specimens was lowered from 1300 to 1100°C without degradation of the microwave dielectric properties. The (Ca 0.254 Li 0.19 Sm 0.14 )‐TiO 3 + 3 wt.% ZB 2 sintered at 1100°C for 3 h showed good microwave dielectric properties, ɛ r = 108.2, Q f = 6545 GHz, and τ f = 6.5 ppm/°C, respectively, indicating that ZB 2 was an effective sintering aid to improve the densification and microwave dielectric properties of (Ca 0.254 Li 0.19 Sm 0.14 )TiO 3 ceramics.
- 21 May 2010
- Published by Wiley in Rare Metals
- Vol. 29 (3) , 243-247
Microstructure and microwave dielectric properties of ZnO‐B 2 O 3 added (Ca 0.254 Li 0.19 Sm 0.14 )TiO 3 ceramics
The effects of ZnO‐B 2 O 3 (ZB 2 ) on the sintering behavior and microwave dielectric properties of (Ca 0.254 Li 0.19 Sm 0.14 )TiO 3 ceramics were investigated. The densities of the specimens reached the maximum value by adding 3 wt.% ZB 2 and then decreased. The sintering temperature of the specimens was lowered from 1300 to 1100°C without degradation of the microwave dielectric properties. The (Ca 0.254 Li 0.19 Sm 0.14 )‐TiO 3 + 3 wt.% ZB 2 sintered at 1100°C for 3 h showed good microwave dielectric properties, ɛ r = 108.2, Q f = 6545 GHz, and τ f = 6.5 ppm/°C, respectively, indicating that ZB 2 was an effective sintering aid to improve the densification and microwave dielectric properties of (Ca 0.254 Li 0.19 Sm 0.14 )TiO 3 ceramics.