Zhaohui Jiang
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Research Subjects
Zhaohui Jiang has a total of 31 co-authors. Here are the top co-authors by number of shared publications:
Zengge Guo
Lutai School of Textile and Apparel, Shandong University of Technology, Zibo, China
8 shared publicationsZhao Jia
Lutai School of Textile and Apparel, Shandong University of Technology, Zibo, China
8 shared publicationsChangfa Xiao
Key Laboratory of Fiber Modification and Functional Fiber, Tianjin Polytechnic University, China
6 shared publicationsCongcong Pu
Lutai School of Textile and Apparel, Shandong University of Technology, China
4 shared publicationsJian Jin
State Key Laboratory of Biobased Fiber Manufacture Technology, China Textile Academy, Beijing, China
4 shared publicationsMingyue Tian
Lutai School of Textile and Apparel, Shandong University of Technology, Zibo, China
3 shared publications
Latest Publications
- 25 August 2020
- Published by Springer Nature in Polymer Bulletin
- Vol. 78 (9) , 4947-4958
Corrosion degradation behavior of PBO fibers under strong inorganic acid
- 25 August 2020
- Published by Springer Nature in Polymer Bulletin
- Vol. 78 (9) , 4947-4958
Corrosion degradation behavior of PBO fibers under strong inorganic acid
- 14 July 2020
- Published by SAGE Publications in High Performance Polymers
- Vol. 33 (1) , 33-39
Evaluation of the alkali and oxidation resistance of PBO fibers
Poly( p-phenylene benzobisoxazole) (PBO) fiber, well-known for its super high strength, is a novel fiber with excellent heat resistance and flame retardancy. However, chemical stability appears to be one of its few weaknesses. In this study, PBO fibers were treated with sodium hydroxide (NaOH) and potassium permanganate (KMnO4) solutions under various conditions. Scanning electron microscopy, optical microscopy, tensile testing, Fourier-transform infrared spectroscopy, differential scanning calorimetry (DSC), and thermogravimetric analysis were employed to characterize the variations of its structure and properties. The results show that many longitudinal corrosion grooves appeared on the surface of PBO fibers treated with KMnO4, while only subtle microcracks occurred after treatment with NaOH. The breaking tenacity of the fiber decreased from 38.13 cN dtex−1 to 2.76 cN dtex−1 after treatment with KMnO4 for 6 h, while it remained at a higher level (27.67cN dtex−1) when treated with NaOH. After treatment with KMnO4 solution, a more obvious absorption peak appeared in the vicinity of 1448.3 cm−1, inferring an occurrence of chemical changes for oxazole ring. Moreover, the remaining mass and initial degradation temperature are significantly improved, also indicating that the cyclic or cross-linked structure is rebuilt. Furthermore, the cyclization or cross-linking of macromolecules destroyed the highly ordered structure of PBO fibers, demonstrated by acromion melting peaks at low temperature in the DSC curves. However, the aggregation and chemical structures of PBO fibers have no obvious changes after treatment with NaOH.
- 14 July 2020
- Published by SAGE Publications in High Performance Polymers
- Vol. 33 (1) , 33-39
Evaluation of the alkali and oxidation resistance of PBO fibers
Poly( p-phenylene benzobisoxazole) (PBO) fiber, well-known for its super high strength, is a novel fiber with excellent heat resistance and flame retardancy. However, chemical stability appears to be one of its few weaknesses. In this study, PBO fibers were treated with sodium hydroxide (NaOH) and potassium permanganate (KMnO4) solutions under various conditions. Scanning electron microscopy, optical microscopy, tensile testing, Fourier-transform infrared spectroscopy, differential scanning calorimetry (DSC), and thermogravimetric analysis were employed to characterize the variations of its structure and properties. The results show that many longitudinal corrosion grooves appeared on the surface of PBO fibers treated with KMnO4, while only subtle microcracks occurred after treatment with NaOH. The breaking tenacity of the fiber decreased from 38.13 cN dtex−1 to 2.76 cN dtex−1 after treatment with KMnO4 for 6 h, while it remained at a higher level (27.67cN dtex−1) when treated with NaOH. After treatment with KMnO4 solution, a more obvious absorption peak appeared in the vicinity of 1448.3 cm−1, inferring an occurrence of chemical changes for oxazole ring. Moreover, the remaining mass and initial degradation temperature are significantly improved, also indicating that the cyclic or cross-linked structure is rebuilt. Furthermore, the cyclization or cross-linking of macromolecules destroyed the highly ordered structure of PBO fibers, demonstrated by acromion melting peaks at low temperature in the DSC curves. However, the aggregation and chemical structures of PBO fibers have no obvious changes after treatment with NaOH.
- 16 April 2018
- Published by SAGE Publications in Textile Research Journal
- Vol. 89 (7) , 1207-1214
Preparation and properties of bottle-recycled polyethylene terephthalate (PET) filaments
Bottle-recycled polyethylene terephthalate (R-PET) fibers were fabricated by the melt spinning method. Based on characteristics of R-PET chips, this study involved a primary exploration of the spinning parameters, including spinning temperature, spinning speed and spinneret plate. The properties of R-PET and original PET (O-PET) fibers were compared using scanning electron microscopy (SEM), tensile testing, sonic orientation, differential scanning calorimetry (DSC), thermogravimetric analysis (TGA) and Fourier transform infrared spectroscopy (FTIR). Apparent morphological observation displays an irregular cross-sectional shape and a scattered diameter distribution for R-PET fibers. Compared with O-PET fibers, R-PET fibers demonstrate a greater breaking strength and smaller elongation at break, resulting from the lower crystallinity and higher degree of orientation. Furthermore, the R-PET fibers have the same chemical structure as that of O-PET fibers demonstrated by FTIR spectroscopy, but TGA results show that thermal stability of R-PET fibers is significantly inferior to that of O-PET fibers, as a result of too many impurities and oligomers during the recycling process.
- 16 April 2018
- Published by SAGE Publications in Textile Research Journal
- Vol. 89 (7) , 1207-1214
Preparation and properties of bottle-recycled polyethylene terephthalate (PET) filaments
Bottle-recycled polyethylene terephthalate (R-PET) fibers were fabricated by the melt spinning method. Based on characteristics of R-PET chips, this study involved a primary exploration of the spinning parameters, including spinning temperature, spinning speed and spinneret plate. The properties of R-PET and original PET (O-PET) fibers were compared using scanning electron microscopy (SEM), tensile testing, sonic orientation, differential scanning calorimetry (DSC), thermogravimetric analysis (TGA) and Fourier transform infrared spectroscopy (FTIR). Apparent morphological observation displays an irregular cross-sectional shape and a scattered diameter distribution for R-PET fibers. Compared with O-PET fibers, R-PET fibers demonstrate a greater breaking strength and smaller elongation at break, resulting from the lower crystallinity and higher degree of orientation. Furthermore, the R-PET fibers have the same chemical structure as that of O-PET fibers demonstrated by FTIR spectroscopy, but TGA results show that thermal stability of R-PET fibers is significantly inferior to that of O-PET fibers, as a result of too many impurities and oligomers during the recycling process.
- 30 November 2016
- Published by Springer Nature in Polymer Bulletin
- Vol. 74 (7) , 2787-2797
Rheological properties of PA6 chips with different spinnability in high-speed spinning
- 30 November 2016
- Published by Springer Nature in Polymer Bulletin
- Vol. 74 (7) , 2787-2797
Rheological properties of PA6 chips with different spinnability in high-speed spinning
- 27 May 2016
- Published by SAGE Publications in High Performance Polymers
- Vol. 29 (4) , 476-483
Preparation and properties of melt-spinning fluorinated ethylene propylene fibres
In this work, a novel fibre, fluorinated ethylene propylene (FEP) filament, was fabricated by melt-spinning. In addition, the properties of FEP fibres were investigated through apparent morphological observation, tensile testing, dry-hot shrinkage, differential scanning calorimetry, thermogramitric analysis (TGA) and Fourier transform infrared spectroscopy. Apparent morphological observation shows that FEP fibres present circular cross-sections and smooth surfaces. Just like the conventional fibres prepared by melt-spinning, such as poly (ethylene terephthalate) (PET) and polyamide 6, the stress–strain curves of FEP fibres show obvious stress yield points. The elastic recovery ratio of FEP fibres (80%) is much greater than that of polytetrafluoroethylene (PTFE) fibres (40%), endowing FEP textiles good wrinkle resistance. When FEP fibres are deposited in flame, smoke and droplets do not appear but shrinkage does occur. After treatment in hot air, the breaking strength of FEP fibres decreases, but the elongation at break increases. The melting temperature of FEP fibres is as closely high as that of the PET fibres, while the crystallization temperature is much higher, which puts forward greater challenges for FEP spinning. Compared with PTFE fibres, the crystallinity and the melting temperature of FEP fibres are much lower. TGA results demonstrate that FEP fibres present excellent thermal stability that is as stable as that of the PTFE fibres.
- 27 May 2016
- Published by SAGE Publications in High Performance Polymers
- Vol. 29 (4) , 476-483
Preparation and properties of melt-spinning fluorinated ethylene propylene fibres
In this work, a novel fibre, fluorinated ethylene propylene (FEP) filament, was fabricated by melt-spinning. In addition, the properties of FEP fibres were investigated through apparent morphological observation, tensile testing, dry-hot shrinkage, differential scanning calorimetry, thermogramitric analysis (TGA) and Fourier transform infrared spectroscopy. Apparent morphological observation shows that FEP fibres present circular cross-sections and smooth surfaces. Just like the conventional fibres prepared by melt-spinning, such as poly (ethylene terephthalate) (PET) and polyamide 6, the stress–strain curves of FEP fibres show obvious stress yield points. The elastic recovery ratio of FEP fibres (80%) is much greater than that of polytetrafluoroethylene (PTFE) fibres (40%), endowing FEP textiles good wrinkle resistance. When FEP fibres are deposited in flame, smoke and droplets do not appear but shrinkage does occur. After treatment in hot air, the breaking strength of FEP fibres decreases, but the elongation at break increases. The melting temperature of FEP fibres is as closely high as that of the PET fibres, while the crystallization temperature is much higher, which puts forward greater challenges for FEP spinning. Compared with PTFE fibres, the crystallinity and the melting temperature of FEP fibres are much lower. TGA results demonstrate that FEP fibres present excellent thermal stability that is as stable as that of the PTFE fibres.
- 11 May 2016
- Published by Wiley in Journal of Applied Polymer Science
- Vol. 133 (34)
Effect of coupling agent on structure and properties of micro–nano composite fibers based on PET
Poly(ethylene terephthalate) (PET)/carbon black (CB) micro–nano composite fibers were manufactured by melt spinning method. To achieve good dispersion, nano‐CB particles were modified by coupling agent (CA). The effect of CA on structure and properties of the fibers were investigated via scanning electron microscopy (SEM), tensile testing, differential scanning calorimetry (DSC), wide‐angle X‐ray diffraction (WAXD), sonic orientation, and birefringence, respectively. At 2 wt % CA dosage, CB particles present the optimal dispersion in the fibers, shown in SEM images. Besides, the fibers possess the maximum breaking strength, the lowest crystallization temperature, and the highest crystallinity. After CA modification, the superior interfacial structure between PET and CB is beneficial to improve mechanical properties of the fibers. The well dispersed CB particles provide more heterogeneous nucleation points, resulting in the highest crystallinity. Furthermore, the fibers with 2 wt % CA dosage possess the maximum orientation and shrinkage ratio. According to Viogt–Kelvin model, the thermal shrinkage curves of the fibers can be well fitted using single exponential function. The three‐phase structure model of crystal phase–amorphous phase–CB phase was established to interpret the relationship among shrinkage, orientation, and dispersion of CB particles. © 2016 Wiley Periodicals, Inc. J. Appl. Polym. Sci. 2016, 133, 43846.
- 11 May 2016
- Published by Wiley in Journal of Applied Polymer Science
- Vol. 133 (34)
Effect of coupling agent on structure and properties of micro–nano composite fibers based on PET
Poly(ethylene terephthalate) (PET)/carbon black (CB) micro–nano composite fibers were manufactured by melt spinning method. To achieve good dispersion, nano‐CB particles were modified by coupling agent (CA). The effect of CA on structure and properties of the fibers were investigated via scanning electron microscopy (SEM), tensile testing, differential scanning calorimetry (DSC), wide‐angle X‐ray diffraction (WAXD), sonic orientation, and birefringence, respectively. At 2 wt % CA dosage, CB particles present the optimal dispersion in the fibers, shown in SEM images. Besides, the fibers possess the maximum breaking strength, the lowest crystallization temperature, and the highest crystallinity. After CA modification, the superior interfacial structure between PET and CB is beneficial to improve mechanical properties of the fibers. The well dispersed CB particles provide more heterogeneous nucleation points, resulting in the highest crystallinity. Furthermore, the fibers with 2 wt % CA dosage possess the maximum orientation and shrinkage ratio. According to Viogt–Kelvin model, the thermal shrinkage curves of the fibers can be well fitted using single exponential function. The three‐phase structure model of crystal phase–amorphous phase–CB phase was established to interpret the relationship among shrinkage, orientation, and dispersion of CB particles. © 2016 Wiley Periodicals, Inc. J. Appl. Polym. Sci. 2016, 133, 43846.
- 1 March 2016
- Published by ASTM International in Journal of Testing and Evaluation
- Vol. 44 (2) , 1019-1026
Study on the Characterization and Evaluation Methods of PA6 Chips for High-Speed Spinning
The reasons for the significant difference of PA6 spinnability are discussed. For this research project, BASF PA6 chips (BASF, Germany) and PA6 chips (GC, China) were chosen as research objects. We chose these two different chips because BASF PA6 chips are stable and GC PA6 chips are unstable in high-speed spinning. The measurement of relative viscosity, crystallization rate, content of extractable matter, molecular weight and its distribution, and Fourier transform infrared (FTIR) spectroscopy of extractable matter were systematically investigated. Moreover, the screw extrusion process of PA6 melt in high-speed melt spinning was simulated by a capillary rheometer, in which PA6 samples with different melting times were prepared to conduct the above-mentioned tests. Compared to BASF chips, the GC chips have the higher content of extractable matter, the greater and more variable relative viscosity, the greater molecular weight, and the wider distribution, causing the poorer spinnability in high-speed spinning. Furthermore, the extractable matter in GC chips is the same as that in BASF chips, which is confirmed by FTIR spectra.
- 1 March 2016
- Published by ASTM International in Journal of Testing and Evaluation
- Vol. 44 (2) , 1019-1026
Study on the Characterization and Evaluation Methods of PA6 Chips for High-Speed Spinning
The reasons for the significant difference of PA6 spinnability are discussed. For this research project, BASF PA6 chips (BASF, Germany) and PA6 chips (GC, China) were chosen as research objects. We chose these two different chips because BASF PA6 chips are stable and GC PA6 chips are unstable in high-speed spinning. The measurement of relative viscosity, crystallization rate, content of extractable matter, molecular weight and its distribution, and Fourier transform infrared (FTIR) spectroscopy of extractable matter were systematically investigated. Moreover, the screw extrusion process of PA6 melt in high-speed melt spinning was simulated by a capillary rheometer, in which PA6 samples with different melting times were prepared to conduct the above-mentioned tests. Compared to BASF chips, the GC chips have the higher content of extractable matter, the greater and more variable relative viscosity, the greater molecular weight, and the wider distribution, causing the poorer spinnability in high-speed spinning. Furthermore, the extractable matter in GC chips is the same as that in BASF chips, which is confirmed by FTIR spectra.
- Open Access
- 9 January 2016
- Published by Walter de Gruyter GmbH in e-Polymers
- Vol. 16 (2) , 171-176
Chemical stability of novel melt spinning FEP fibers
Fluorinated ethylene propylene (FEP) and polytetrafluoroethylene (PTFE) are both perfluorinated polymer, thus endowing FEP fibers excellent chemical stability. Compared with the difficult processing of PTFE, FEP fibers can be fabricated by melt spinning. The FEP fibers were treated by H 2 SO 4 and NaOH. After treatment, FEP fibers have a slight swelling observed by optical microscope (OM). Meanwhile, the strength of treated FEP fibers decreases slightly, while tensile modulus and elongation at break increases because of the infiltration of H 2 SO 4 and NaOH. Differential scanning calorimeter (DSC) results show that the crystallinity of FEP fibers decreases, due to the regularity of macromolecules destroyed by H 2 SO 4 and NaOH, which enter into crystalline region. This is consistent with WAXD results, indicating crystal size and crystal plane space decreases, owing to the infiltration of H 2 SO 4 and NaOH. However, chemical bonds of FEP fibers are unaffected, which is confirmed by FTIR spectra. Therefore, FEP fibers possess excellent chemical stability.
- 9 January 2016
- Published by Walter de Gruyter GmbH in e-Polymers
- Vol. 16 (2) , 171-176
Open AccessChemical stability of novel melt spinning FEP fibers
Fluorinated ethylene propylene (FEP) and polytetrafluoroethylene (PTFE) are both perfluorinated polymer, thus endowing FEP fibers excellent chemical stability. Compared with the difficult processing of PTFE, FEP fibers can be fabricated by melt spinning. The FEP fibers were treated by H 2 SO 4 and NaOH. After treatment, FEP fibers have a slight swelling observed by optical microscope (OM). Meanwhile, the strength of treated FEP fibers decreases slightly, while tensile modulus and elongation at break increases because of the infiltration of H 2 SO 4 and NaOH. Differential scanning calorimeter (DSC) results show that the crystallinity of FEP fibers decreases, due to the regularity of macromolecules destroyed by H 2 SO 4 and NaOH, which enter into crystalline region. This is consistent with WAXD results, indicating crystal size and crystal plane space decreases, owing to the infiltration of H 2 SO 4 and NaOH. However, chemical bonds of FEP fibers are unaffected, which is confirmed by FTIR spectra. Therefore, FEP fibers possess excellent chemical stability.
- 28 September 2015
- Published by Wiley in Polymer Composites
- Vol. 38 (11) , 2358-2367
Effect of coupling agent on crystallization and rheological properties of poly(ethylene terephthalate) composite masterbatches
Poly(ethylene terephthalate)/carbon black/coupling agent composite masterbatches were fabricated using separate feeding technique. The effect of coupling agent on crystallization of composite masterbatches was investigated by differential scanning calorimetry, wide‐angle X‐ray diffraction, and Fourier transform‐infrared spectroscopy, respectively. The results show that the strong interfacial interaction among poly(ethylene terephthalate) (PET), coupling agent and carbon black hinders chains mobility in process of PET crystallization, which is illustrated by interfical structure model. Whereas, the crystallinity of composite masterbatch increases due to uniform dispersion of carbon black modified by coupling agent. Activation energy of viscous flow of the composite masterbatches is closer to that of virgin PET, so the spinning parameters can be controlled according to each other. Besides, structural viscosity index of composite masterbatches is greater due to strong interfacial interaction among PET, coupling agent and carbon black. Thus, in order to smooth spinning, the composite masterbatches need greater shear rate compared with PET/carbon black masterbatch. POLYM. COMPOS., 38:2358–2367, 2017. © 2015 Society of Plastics Engineers
- 28 September 2015
- Published by Wiley in Polymer Composites
- Vol. 38 (11) , 2358-2367
Effect of coupling agent on crystallization and rheological properties of poly(ethylene terephthalate) composite masterbatches
Poly(ethylene terephthalate)/carbon black/coupling agent composite masterbatches were fabricated using separate feeding technique. The effect of coupling agent on crystallization of composite masterbatches was investigated by differential scanning calorimetry, wide‐angle X‐ray diffraction, and Fourier transform‐infrared spectroscopy, respectively. The results show that the strong interfacial interaction among poly(ethylene terephthalate) (PET), coupling agent and carbon black hinders chains mobility in process of PET crystallization, which is illustrated by interfical structure model. Whereas, the crystallinity of composite masterbatch increases due to uniform dispersion of carbon black modified by coupling agent. Activation energy of viscous flow of the composite masterbatches is closer to that of virgin PET, so the spinning parameters can be controlled according to each other. Besides, structural viscosity index of composite masterbatches is greater due to strong interfacial interaction among PET, coupling agent and carbon black. Thus, in order to smooth spinning, the composite masterbatches need greater shear rate compared with PET/carbon black masterbatch. POLYM. COMPOS., 38:2358–2367, 2017. © 2015 Society of Plastics Engineers