Shumei Lou
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Research Subjects
Shumei Lou has a total of 78 co-authors. Here are the top co-authors by number of shared publications:
Chunjian Su
8 shared publicationsBaojia Cheng
6 shared publicationsLingwei Ran
College of Mechanical and Electronic Engineering, Shandong University of Science and Technology, Qingdao, People’s Republic of China
5 shared publicationsLeyao Xu
4 shared publicationsPeng Chen
College of Intelligent Equipment, Shandong University of Science and Technology, Tai ‘An, Shandong province, China
4 shared publicationsYiming Li
College of Mechanical and Electronic Engineering, Shandong University of Science and Technology, Qingdao, People’s Republic of China
4 shared publications
Latest Publications
- 11 May 2026
- Published by Springer Nature in Journal of Materials Engineering and Performance
- Vol. 35 (32) , 1-11
Fracture Prediction of Nonuniform-Thickness 7050 Aluminum Alloy Plates by Quasi-Static Three-Point Bending
- 11 May 2026
- Published by Springer Nature in Journal of Materials Engineering and Performance
- Vol. 35 (32) , 1-11
Fracture Prediction of Nonuniform-Thickness 7050 Aluminum Alloy Plates by Quasi-Static Three-Point Bending
- 23 October 2025
- Published by Elsevier in Applied Surface Science
- Vol. 718
Enhancing 30 wt% GF/PET-A2024 joint performance via in situ Cu2+ coordination and multiscale interface
- 23 October 2025
- Published by Elsevier in Applied Surface Science
- Vol. 718
Enhancing 30 wt% GF/PET-A2024 joint performance via in situ Cu2+ coordination and multiscale interface
- 4 October 2025
- Published by Wiley in Polymer Composites
- Vol. 47 (6) , 5456-5476
Interfacial Strength Improvement of 30 wt% GF / PET ‐ A2024 by the Combination of Multiscale Mechanical Interlocking and π–π Stacking/Hydrogen Bonds
The interfacial strength of 30 wt% GF/PET‐A2024 joint was enhanced via surface treatment of ultrasonic‐assisted N 2 H 4 solution corrosion and phenolic resin interlayer. N 2 H 4 corrosion forms a multiscale “crater + nanopore” morphology on the A2024 surface, enabling multiscale mechanical interlocking. PR forms AO bonds with A2024 and π–π stacking/hydrogen bonds with PET, creating a chemical “bridge” between the joining surface of PET and A2024. This synergistic effect increases the interface strength from 3.45 MPa (sandpapered) to 29.15 MPa. Density functional theory confirms the stability of π–π stacking interactions, and molecular dynamics simulation reveals that the morphology on the A2024 surface enhances the mechanical interlocking of the joint. This work provides theoretical guidance for improving resin/aluminum interfaces and highlights the potential of micro‐nano morphology and supramolecular interactions in strengthening interface adhesion.
- 4 October 2025
- Published by Wiley in Polymer Composites
- Vol. 47 (6) , 5456-5476
Interfacial Strength Improvement of 30 wt% GF / PET ‐ A2024 by the Combination of Multiscale Mechanical Interlocking and π–π Stacking/Hydrogen Bonds
The interfacial strength of 30 wt% GF/PET‐A2024 joint was enhanced via surface treatment of ultrasonic‐assisted N 2 H 4 solution corrosion and phenolic resin interlayer. N 2 H 4 corrosion forms a multiscale “crater + nanopore” morphology on the A2024 surface, enabling multiscale mechanical interlocking. PR forms AO bonds with A2024 and π–π stacking/hydrogen bonds with PET, creating a chemical “bridge” between the joining surface of PET and A2024. This synergistic effect increases the interface strength from 3.45 MPa (sandpapered) to 29.15 MPa. Density functional theory confirms the stability of π–π stacking interactions, and molecular dynamics simulation reveals that the morphology on the A2024 surface enhances the mechanical interlocking of the joint. This work provides theoretical guidance for improving resin/aluminum interfaces and highlights the potential of micro‐nano morphology and supramolecular interactions in strengthening interface adhesion.
- 8 June 2023
- Published by Springer Nature in Metals and Materials International
- Vol. 29 (12) , 3607-3617
Effects of Extrusion Temperature on the Properties of a 0.5 wt% GNP/Al Composite in Porthole Die Extrusion
- 8 June 2023
- Published by Springer Nature in Metals and Materials International
- Vol. 29 (12) , 3607-3617
Effects of Extrusion Temperature on the Properties of a 0.5 wt% GNP/Al Composite in Porthole Die Extrusion
- Open Access
Microstructural and Mechanical Properties of Longitudinal Welds in Porthole Die Extrudates of a 0.5 wt.% GNP/Al Composite
In this study, porthole die extrusion was performed on a graphene-nanoplatelet-reinforced aluminum composite (0.5 wt.% GNP/Al) prepared by powder metallurgy. The microstructure, grain size, microtexture, and mechanical properties of the composite extruded by the porthole die were studied. Along the extrusion direction, the tensile strength of the extruded composite was 139.7 MPa, and the elongation was 27.1%. Along the transverse direction, which included the weld zone, the tensile strength was 126.4 MPa, and the elongation was 24.1%. These values were 6.65% and 54.63% higher than those obtained for pure aluminum, respectively. Fractography along the extrusion direction revealed obvious ductile fracture characteristics; however, these were not so obvious along the transverse direction, mainly due to the anisotropy caused by the grain orientation of the extruded composite, thereby indicating that the composite exhibited excellent weld performance, which was further verified by Optical Microscope, Electron Backscattered Diffraction, and Transmission Electron Microscopeimages. Overall, these results indicate that GNP can contribute to the strength and toughness of composites in the weld zone in porthole die extrusions.
Open AccessMicrostructural and Mechanical Properties of Longitudinal Welds in Porthole Die Extrudates of a 0.5 wt.% GNP/Al Composite
In this study, porthole die extrusion was performed on a graphene-nanoplatelet-reinforced aluminum composite (0.5 wt.% GNP/Al) prepared by powder metallurgy. The microstructure, grain size, microtexture, and mechanical properties of the composite extruded by the porthole die were studied. Along the extrusion direction, the tensile strength of the extruded composite was 139.7 MPa, and the elongation was 27.1%. Along the transverse direction, which included the weld zone, the tensile strength was 126.4 MPa, and the elongation was 24.1%. These values were 6.65% and 54.63% higher than those obtained for pure aluminum, respectively. Fractography along the extrusion direction revealed obvious ductile fracture characteristics; however, these were not so obvious along the transverse direction, mainly due to the anisotropy caused by the grain orientation of the extruded composite, thereby indicating that the composite exhibited excellent weld performance, which was further verified by Optical Microscope, Electron Backscattered Diffraction, and Transmission Electron Microscopeimages. Overall, these results indicate that GNP can contribute to the strength and toughness of composites in the weld zone in porthole die extrusions.
- 2 January 2023
- Published by Taylor & Francis in The Journal of Adhesion
- Vol. 99 (12) , 1916-1932
Effect of adhesive modification and surface treatment of laminates on the single lap bonding joint properties of carbon fibre composites
In this study, the effects of adhesive modification, surface treatment of laminates, and their combined effects on the bonding properties of adhesive joints were studied using tensile shear tests, SEM micro-morphology characterisation, EDS energy spectra, analysis of the load-displacement curve, failure mode, and element content on the bonding surface. The test group corresponding to surface treatment of the laminate exhibited the best tensile shear performance. Surface treatment by 20% NaOH increased the tensile shear strength and failure displacement by 30.41% and 106.72%, respectively, compared to that obtained with only surface polishing using 320# sandpaper. In the adhesive modification test group, the tensile shear strength of the joint was the largest with an adhesive modification by 3 wt.% short glass fibres, while the tensile shear strength and failure displacement increased by 7.96% (18.63 MPa) and 10.2%, respectively, compared with those without adhesive modification. To further improve the wettability and interfacial bonding strength between the glass fibre and adhesive, a 3 wt.% short glass fibre was pretreated with KH-550 silane coupling agent. The tensile shear strength of the joint improved to 19.06 MPa, and the maximum failure displacement was 1.59 mm, which were 2.31% and 2.58% higher than those without KH-550 silane coupling agent pretreatment on the glass fibre, respectively. Furthermore, adhesive modification by KH-550 treated 3 wt.% short glass fibre was underwent combining with laminate surface treatment with 20% NaOH. The bonding strength was higher than that obtained using 3 wt.% GF adhesive modification pretreated with KH-550, while lower by 10.49% compared with that corresponding to the surface treatment of the laminate by 20% NaOH. This was primarily attributed to the pores produced by the hydrolysis reaction between NaOH and the KH-550 silane coupling agent, which weakened the load-bearing capacity of the joint.
- 2 January 2023
- Published by Taylor & Francis in The Journal of Adhesion
- Vol. 99 (12) , 1916-1932
Effect of adhesive modification and surface treatment of laminates on the single lap bonding joint properties of carbon fibre composites
In this study, the effects of adhesive modification, surface treatment of laminates, and their combined effects on the bonding properties of adhesive joints were studied using tensile shear tests, SEM micro-morphology characterisation, EDS energy spectra, analysis of the load-displacement curve, failure mode, and element content on the bonding surface. The test group corresponding to surface treatment of the laminate exhibited the best tensile shear performance. Surface treatment by 20% NaOH increased the tensile shear strength and failure displacement by 30.41% and 106.72%, respectively, compared to that obtained with only surface polishing using 320# sandpaper. In the adhesive modification test group, the tensile shear strength of the joint was the largest with an adhesive modification by 3 wt.% short glass fibres, while the tensile shear strength and failure displacement increased by 7.96% (18.63 MPa) and 10.2%, respectively, compared with those without adhesive modification. To further improve the wettability and interfacial bonding strength between the glass fibre and adhesive, a 3 wt.% short glass fibre was pretreated with KH-550 silane coupling agent. The tensile shear strength of the joint improved to 19.06 MPa, and the maximum failure displacement was 1.59 mm, which were 2.31% and 2.58% higher than those without KH-550 silane coupling agent pretreatment on the glass fibre, respectively. Furthermore, adhesive modification by KH-550 treated 3 wt.% short glass fibre was underwent combining with laminate surface treatment with 20% NaOH. The bonding strength was higher than that obtained using 3 wt.% GF adhesive modification pretreated with KH-550, while lower by 10.49% compared with that corresponding to the surface treatment of the laminate by 20% NaOH. This was primarily attributed to the pores produced by the hydrolysis reaction between NaOH and the KH-550 silane coupling agent, which weakened the load-bearing capacity of the joint.
- 27 December 2022
- Published by Springer Nature in Journal of Materials Engineering and Performance
- Vol. 32 (20) , 9344-9356
Influence of Extrusion Temperature on the Microstructure and Mechanical Properties of a 0.5 wt.% Graphene Nanoplatelet-Reinforced Aluminum Composite
- 27 December 2022
- Published by Springer Nature in Journal of Materials Engineering and Performance
- Vol. 32 (20) , 9344-9356
Influence of Extrusion Temperature on the Microstructure and Mechanical Properties of a 0.5 wt.% Graphene Nanoplatelet-Reinforced Aluminum Composite