Qingliang Shan
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Previous Organizations / Institutes
The organizations / institutes from the scholar's other articles in the past ten years
Research Subjects
Qingliang Shan has a total of 27 co-authors. Here are the top co-authors by number of shared publications:
Qian Ma
School of Materials Science and Engineering South China University of Technology Guangzhou PR China
6 shared publications- Anze Shui
School of Materials Science and Engineering, South China University of Technology, Guangzhou 510641, PR China
5 shared publications Qiankun Xu
5 shared publicationsYewei Wang
5 shared publicationsHao Xiong
4 shared publicationsAnze Shui
School of Materials Science and Engineering South China University of Technology Guangzhou PR China
3 shared publications
Latest Publications
- 20 March 2024
- Published by Elsevier in Journal of Alloys and Compounds
- Vol. 987, 174189
High-performance electromagnetic wave absorbers based on hierarchically porous (Zn1/2Ni1/2)Co2O4 spinel clusters
- 20 March 2024
- Published by Elsevier in Journal of Alloys and Compounds
- Vol. 987, 174189
High-performance electromagnetic wave absorbers based on hierarchically porous (Zn1/2Ni1/2)Co2O4 spinel clusters
- 1 September 2023
- Published by Elsevier in Ceramics International
- Vol. 49 (22) , 36528-36535
Preparation of graded silicon nitride ceramics with high mechanical performance using β-Si3N4 seeds
- 1 September 2023
- Published by Elsevier in Ceramics International
- Vol. 49 (22) , 36528-36535
Preparation of graded silicon nitride ceramics with high mechanical performance using β-Si3N4 seeds
- 1 June 2022
- Published by Wiley in International Journal of Applied Ceramic Technology
- Vol. 19 (5) , 2675-2685
The fabrication of porous mullite ceramics based on the different sizes of aluminum hydroxide
- 1 June 2022
- Published by Wiley in International Journal of Applied Ceramic Technology
- Vol. 19 (5) , 2675-2685
The fabrication of porous mullite ceramics based on the different sizes of aluminum hydroxide
- 5 May 2022
- Published by Wiley in Journal of the American Ceramic Society
- Vol. 105 (9) , 5853-5867
The anti‐oxidation mechanism of SiC f /SiC–B 4 C modified with Al 2 O 3 in wet atmosphere based on machine learning
To study the anti‐oxidation mechanism of SiC f /SiC–B 4 C modified with Al 2 O 3 in wet atmosphere, the damage evolution of composites after oxidation was explored by unsupervised machine learning technology ( k ‐means). Results display that the mean feature values of cluster‐1 (some small cracks in oxidation layer and matrix as well as fiber debonding) in composites modified with Al 2 O 3 are larger than that in virgin after oxidation. Meanwhile, as the oxidation time increases, the concentrated area of cluster‐2 (fiber breakage, cracks in axial and transverse yarns) in both composites gradually shifts toward the direction of high mean feature values. Because Al 2 O 3 can protect the BN from oxidation, the increase of peak frequency and risetime of composites modified with Al 2 O 3 is less than that of virgin. Moreover, the proportion of cluster‐3 (big transverse matrix cracks) in composites modified with Al 2 O 3 is always more than that of virgin. Based on the research results, the corresponding relationship between each damage behavior and each cluster is thoroughly built.
- 5 May 2022
- Published by Wiley in Journal of the American Ceramic Society
- Vol. 105 (9) , 5853-5867
The anti‐oxidation mechanism of SiC f /SiC–B 4 C modified with Al 2 O 3 in wet atmosphere based on machine learning
To study the anti‐oxidation mechanism of SiC f /SiC–B 4 C modified with Al 2 O 3 in wet atmosphere, the damage evolution of composites after oxidation was explored by unsupervised machine learning technology ( k ‐means). Results display that the mean feature values of cluster‐1 (some small cracks in oxidation layer and matrix as well as fiber debonding) in composites modified with Al 2 O 3 are larger than that in virgin after oxidation. Meanwhile, as the oxidation time increases, the concentrated area of cluster‐2 (fiber breakage, cracks in axial and transverse yarns) in both composites gradually shifts toward the direction of high mean feature values. Because Al 2 O 3 can protect the BN from oxidation, the increase of peak frequency and risetime of composites modified with Al 2 O 3 is less than that of virgin. Moreover, the proportion of cluster‐3 (big transverse matrix cracks) in composites modified with Al 2 O 3 is always more than that of virgin. Based on the research results, the corresponding relationship between each damage behavior and each cluster is thoroughly built.
- 1 April 2022
- Published by Elsevier in Journal of the European Ceramic Society
- Vol. 42 (4) , 1712-1721
Foaming mechanism of polishing porcelain stoneware tile residues via adding C, Al and Si powder
- 1 April 2022
- Published by Elsevier in Journal of the European Ceramic Society
- Vol. 42 (4) , 1712-1721
Foaming mechanism of polishing porcelain stoneware tile residues via adding C, Al and Si powder
- 1 February 2022
- Published by Elsevier in Ceramics International
- Vol. 48 (3) , 3875-3883
Investigation on the microcrcaks strengthening effect in the damage behavior of Al2TiO5 flexible ceramics based on the AE
- 1 February 2022
- Published by Elsevier in Ceramics International
- Vol. 48 (3) , 3875-3883
Investigation on the microcrcaks strengthening effect in the damage behavior of Al2TiO5 flexible ceramics based on the AE
- 21 January 2022
- Published by Elsevier in Journal of the European Ceramic Society
- Vol. 42 (6) , 2618-2629
The oxidation resistance mechanism of SiC-B4C-xAl2O3 ceramics at 1400 ℃ in air atmosphere
- 21 January 2022
- Published by Elsevier in Journal of the European Ceramic Society
- Vol. 42 (6) , 2618-2629
The oxidation resistance mechanism of SiC-B4C-xAl2O3 ceramics at 1400 ℃ in air atmosphere
- 7 May 2021
- Published by Wiley in Advanced Engineering Materials
- Vol. 23 (9) , 2100170
Influence of Cooling Rates on the Microstructure and Mechanical Properties of Aluminum Titanate Flexible Ceramic
Herein, aluminum titanate (Al2TiO5, AT) flexible ceramics with different cooling rates (program‐controlling cooling (10 and 20 °C min−1), air cooling (≈400 °C min−1), and water cooling (>1000 °C min−1) are fabricated by reaction sintering of Al2O3 and TiO2. The effect of cooling rates on microstructures and the mechanical properties of AT ceramics are systematically investigated. The microcrack width and density of AT ceramics with different cooling rates are statistically calculated. In addition, the effect of a microcracks structure on the mechanical properties of AT ceramics is deeply studied. Results show that the increase in cooling rate will increase the width and density of microcrack, leading to a suitable increase in flexibility and a slight decrease in strength. When AT is cooled in air, the best bending strain of 1.10% can be obtained, with a median microcrack width of 0.533 μm and a density of 6831.88 ± 374.87 N mm−2. It is hopeful that through this research, the effect of cooling rate on the mechanical properties of AT flexible ceramics can be deeply understood, and the strategy used in this research can be used in other exploration of similar material.
- 7 May 2021
- Published by Wiley in Advanced Engineering Materials
- Vol. 23 (9) , 2100170
Influence of Cooling Rates on the Microstructure and Mechanical Properties of Aluminum Titanate Flexible Ceramic
Herein, aluminum titanate (Al2TiO5, AT) flexible ceramics with different cooling rates (program‐controlling cooling (10 and 20 °C min−1), air cooling (≈400 °C min−1), and water cooling (>1000 °C min−1) are fabricated by reaction sintering of Al2O3 and TiO2. The effect of cooling rates on microstructures and the mechanical properties of AT ceramics are systematically investigated. The microcrack width and density of AT ceramics with different cooling rates are statistically calculated. In addition, the effect of a microcracks structure on the mechanical properties of AT ceramics is deeply studied. Results show that the increase in cooling rate will increase the width and density of microcrack, leading to a suitable increase in flexibility and a slight decrease in strength. When AT is cooled in air, the best bending strain of 1.10% can be obtained, with a median microcrack width of 0.533 μm and a density of 6831.88 ± 374.87 N mm−2. It is hopeful that through this research, the effect of cooling rate on the mechanical properties of AT flexible ceramics can be deeply understood, and the strategy used in this research can be used in other exploration of similar material.
- 29 March 2021
- Published by Wiley in Journal of the American Ceramic Society
- Vol. 104 (8) , 4131-4144
The tensile damage behavior of SiC f /SiC–B 4 C after oxidation in wet atmosphere based on acoustic emission pattern recognition
In this research, SiC f /SiC–B 4 C composites were prepared through slurry impregnation and reaction melting infiltration (RMI). To explore the damage evolution of this composites after oxidation in wet atmosphere, the changes of damage behavior of composites before and after oxidation were studied using acoustic emission (AE) pattern recognition (PR) technology. Results show that since the damage behavior of the composites changes after oxidation, the optimal number of clusters transforms from 3 to 5. In addition, as the oxidation time increases, the area of concentration of damage events is gradually broadened towards lower stress direction due to the decrease of damage threshold of composites. Meanwhile, because the BN interface is gradually oxidized, the density of C3‐cracks (axial yarns cracks) near the fracture and the proportion of Cluster‐4 (the signals of transverse yarns cracks) will increase, for which the rising of interfacial shear stress should be responsible. Through this research, not only can the damage evolution of SiC f /SiC–B 4 C composites after oxidation be understood, but also the method employed in this research can be as guide for studying other similar materials.
- 29 March 2021
- Published by Wiley in Journal of the American Ceramic Society
- Vol. 104 (8) , 4131-4144
The tensile damage behavior of SiC f /SiC–B 4 C after oxidation in wet atmosphere based on acoustic emission pattern recognition
In this research, SiC f /SiC–B 4 C composites were prepared through slurry impregnation and reaction melting infiltration (RMI). To explore the damage evolution of this composites after oxidation in wet atmosphere, the changes of damage behavior of composites before and after oxidation were studied using acoustic emission (AE) pattern recognition (PR) technology. Results show that since the damage behavior of the composites changes after oxidation, the optimal number of clusters transforms from 3 to 5. In addition, as the oxidation time increases, the area of concentration of damage events is gradually broadened towards lower stress direction due to the decrease of damage threshold of composites. Meanwhile, because the BN interface is gradually oxidized, the density of C3‐cracks (axial yarns cracks) near the fracture and the proportion of Cluster‐4 (the signals of transverse yarns cracks) will increase, for which the rising of interfacial shear stress should be responsible. Through this research, not only can the damage evolution of SiC f /SiC–B 4 C composites after oxidation be understood, but also the method employed in this research can be as guide for studying other similar materials.
- 27 July 2020
- Published by Wiley in Journal of the American Ceramic Society
- Vol. 103 (12) , 7247-7258
More effective crack self‐healing capability of SiC f /SiC‐B 4 C with Al 2 O 3 modified under wet environment
Aluminum oxide has been introduced into SiC f /(SiC + B 4 C) composites to improve the crack self‐healing property in O 2 /H 2 O atmosphere. The observation of the surface and interior morphologies of the oxidized composites reveal that Al 2 O 3 can lead to rapid self‐healing of cracks, which will effectively block the oxidation of interior interphase and fiber. Further investigation reveals that Al 2 O 3 plays an important role in impeding the crystallization of SiO 2 and limiting the volatilization of B 2 O 3 . It is beneficial to form self‐healing fluid glass phase and improve glass phase stability. Under these circumstances, the pre‐crack can be healed more effectively, which is advantageous for composites to remain high strength retention rate.
- 27 July 2020
- Published by Wiley in Journal of the American Ceramic Society
- Vol. 103 (12) , 7247-7258
More effective crack self‐healing capability of SiC f /SiC‐B 4 C with Al 2 O 3 modified under wet environment
Aluminum oxide has been introduced into SiC f /(SiC + B 4 C) composites to improve the crack self‐healing property in O 2 /H 2 O atmosphere. The observation of the surface and interior morphologies of the oxidized composites reveal that Al 2 O 3 can lead to rapid self‐healing of cracks, which will effectively block the oxidation of interior interphase and fiber. Further investigation reveals that Al 2 O 3 plays an important role in impeding the crystallization of SiO 2 and limiting the volatilization of B 2 O 3 . It is beneficial to form self‐healing fluid glass phase and improve glass phase stability. Under these circumstances, the pre‐crack can be healed more effectively, which is advantageous for composites to remain high strength retention rate.