Atif Mahmood
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Research Subjects
Atif Mahmood has a total of 15 co-authors. Here are the top co-authors by number of shared publications:
Hidayatullah Khan
2 shared publicationsMuhammad Amin
2 shared publicationsShahid Alam
Ghulam Ishaq Khan Institute of Engineering Sciences and Technology, Topi, Pakistan
2 shared publicationsFazal Muhammad
Department of Electrical Engineering, City University of Science and Information Technology, Peshawar, Pakistan
1 shared publication- Hao Yuan
College of Electrical Engineering, Sichuan University, Chengdu, China
1 shared publication Israr Ullah
1 shared publication
Latest Publications
- 25 February 2023
- Published by Springer Nature in Journal of Rubber Research
- Vol. 26 (1) , 55-70
Performance evaluation of micro/nano-silica filled silicone rubbers aged under multiple environmental stresses and bipolar DC voltage
- 25 February 2023
- Published by Springer Nature in Journal of Rubber Research
- Vol. 26 (1) , 55-70
Performance evaluation of micro/nano-silica filled silicone rubbers aged under multiple environmental stresses and bipolar DC voltage
- 27 November 2022
- Published by Springer Nature in Polymer Bulletin
- Vol. 80 (10) , 11069-11089
Performance and degradation analysis of HTV-SiR polymeric composites under the influence of bipolar DC voltages along with multiple stresses
- 27 November 2022
- Published by Springer Nature in Polymer Bulletin
- Vol. 80 (10) , 11069-11089
Performance and degradation analysis of HTV-SiR polymeric composites under the influence of bipolar DC voltages along with multiple stresses
- 30 September 2022
- Published by SAGE Publications in Journal of Elastomers & Plastics
- Vol. 54 (7) , 1091-1111
RTV-SiR based composites aged in a multi-stressed environment under AC and bipolar DC voltages
Silicone rubber-based polymers are gradually replacing traditional insulators in outdoor applications due to their numerous advantages, in particular high hydrophobicity that is important for suppressing leakage current and hence surface flashover. However, the main problem with polymeric composites is their aging when exposed to environmental stresses causing loss of their desired properties and expected lifetime. In this work, aging behavior of three types of room temperature vulcanized silicon rubber (RTV-SiR) loaded with nano-silica and micro-ATH is studied. Samples of the materials with different specifications were fabricated and exposed to various environmental stresses in two specially designed weather chambers under both AC and bipolar DC voltages for a time period of 9000 hours. Thereafter, diagnosis was performed for identifying the degree of deterioration using several techniques. These include hydrophobicity classification, measurements of leakage current and mechanical properties, Fourier transform infrared spectroscopy, and Thermogravimetric analysis. Results of the conducted experiments indicated stronger degradation of the desired properties under positive DC stress as compared to the AC and negative DC voltages. Moreover, silicone rubber doped with nano-sized particles of silica filler demonstrated better anti-aging performance as compared to its micro-ATH filled counterpart.
- 30 September 2022
- Published by SAGE Publications in Journal of Elastomers & Plastics
- Vol. 54 (7) , 1091-1111
RTV-SiR based composites aged in a multi-stressed environment under AC and bipolar DC voltages
Silicone rubber-based polymers are gradually replacing traditional insulators in outdoor applications due to their numerous advantages, in particular high hydrophobicity that is important for suppressing leakage current and hence surface flashover. However, the main problem with polymeric composites is their aging when exposed to environmental stresses causing loss of their desired properties and expected lifetime. In this work, aging behavior of three types of room temperature vulcanized silicon rubber (RTV-SiR) loaded with nano-silica and micro-ATH is studied. Samples of the materials with different specifications were fabricated and exposed to various environmental stresses in two specially designed weather chambers under both AC and bipolar DC voltages for a time period of 9000 hours. Thereafter, diagnosis was performed for identifying the degree of deterioration using several techniques. These include hydrophobicity classification, measurements of leakage current and mechanical properties, Fourier transform infrared spectroscopy, and Thermogravimetric analysis. Results of the conducted experiments indicated stronger degradation of the desired properties under positive DC stress as compared to the AC and negative DC voltages. Moreover, silicone rubber doped with nano-sized particles of silica filler demonstrated better anti-aging performance as compared to its micro-ATH filled counterpart.
- Open Access
- 1 October 2021
- Published by Elsevier in Polymer Testing
- Vol. 102
Healing of water tree aged cables using rejuvenation nanofluid
- 1 October 2021
- Published by Elsevier in Polymer Testing
- Vol. 102
Open AccessHealing of water tree aged cables using rejuvenation nanofluid
- 31 August 2020
- Published by SAGE Publications in Journal of Elastomers & Plastics
- Vol. 53 (5) , 489-503
Investigation of multiple-stresses on mechanical and thermal properties of 9000 h Aged RTV-SiR composites for high-voltage insulation
Due to many advantages, polymer composite insulators have been extensively used for high-voltage (HV) transmission lines and substation insulations. The in-service operation, various environmental and electrical stresses degrade their mechanical and thermal characteristics. In this study, nine thousand-hour (9000 h) multi-stress (HV, heat, acid rain, salt fog, ultraviolet (UV) radiation, and humidity) accelerated lab-weathering evaluation of alumina-trihydrate (ATH) and silicon dioxide (SiO2) filled silicone rubber (SiR) composites were utilized. Moreover, to quantify the influence of multiple stresses over 9000 h lab-aging, the tensile strength, elongation at break, hardness, and thermal properties were evaluated and compared with the characterization results of neat (un-aged) composites. Winter and summer-aging cycles were designed in accordance with the actual service environment of Islamabad (Pakistan). Mechanical results of SiR blends showed a decrease in the tensile strength and the elongation at break (EAB), whereas the hardness increased over 9000 h lab-aging. The maximum deviation of ∼57.1% in tensile strength was found for hybrid samples (micro-ATH+ nano-Silica blend: SMNC), whereas the minimum change of ∼25.73% was exhibited by micro-silica-filled SiR specimen SMC3. Compared to neat blends, the maximum variation in EAB was ∼61% for a neat sample (SiR), whereas minimum change was noticed for SMC2 (of ∼31%) over 9000 h lab-aging. Additionally, after 9000 h lab-aging, the maximum (of ∼79.6%) and minimum (of ∼24.4%) variation in hardness was found for hybrid and SiR samples, respectively. Moreover, thermogravimetric (TGA) analysis showed that relative to neat samples, the thermal stability of aged specimens was decreased over weathering. Among aged specimens, only ATH filled samples (SMC1, SMC2) exhibited superior performance for a given temperature range (from 0°C to 900°C) by leaving a higher residual weight of ∼68.6% for SMC2. Hence to simulate and quantify the influence of environmental stresses over insulant performance, accelerated lab weathering can be adopted as an efficient tool.
- 31 August 2020
- Published by SAGE Publications in Journal of Elastomers & Plastics
- Vol. 53 (5) , 489-503
Investigation of multiple-stresses on mechanical and thermal properties of 9000 h Aged RTV-SiR composites for high-voltage insulation
Due to many advantages, polymer composite insulators have been extensively used for high-voltage (HV) transmission lines and substation insulations. The in-service operation, various environmental and electrical stresses degrade their mechanical and thermal characteristics. In this study, nine thousand-hour (9000 h) multi-stress (HV, heat, acid rain, salt fog, ultraviolet (UV) radiation, and humidity) accelerated lab-weathering evaluation of alumina-trihydrate (ATH) and silicon dioxide (SiO2) filled silicone rubber (SiR) composites were utilized. Moreover, to quantify the influence of multiple stresses over 9000 h lab-aging, the tensile strength, elongation at break, hardness, and thermal properties were evaluated and compared with the characterization results of neat (un-aged) composites. Winter and summer-aging cycles were designed in accordance with the actual service environment of Islamabad (Pakistan). Mechanical results of SiR blends showed a decrease in the tensile strength and the elongation at break (EAB), whereas the hardness increased over 9000 h lab-aging. The maximum deviation of ∼57.1% in tensile strength was found for hybrid samples (micro-ATH+ nano-Silica blend: SMNC), whereas the minimum change of ∼25.73% was exhibited by micro-silica-filled SiR specimen SMC3. Compared to neat blends, the maximum variation in EAB was ∼61% for a neat sample (SiR), whereas minimum change was noticed for SMC2 (of ∼31%) over 9000 h lab-aging. Additionally, after 9000 h lab-aging, the maximum (of ∼79.6%) and minimum (of ∼24.4%) variation in hardness was found for hybrid and SiR samples, respectively. Moreover, thermogravimetric (TGA) analysis showed that relative to neat samples, the thermal stability of aged specimens was decreased over weathering. Among aged specimens, only ATH filled samples (SMC1, SMC2) exhibited superior performance for a given temperature range (from 0°C to 900°C) by leaving a higher residual weight of ∼68.6% for SMC2. Hence to simulate and quantify the influence of environmental stresses over insulant performance, accelerated lab weathering can be adopted as an efficient tool.