Ying Yan
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Previous Organizations / Institutes
The organizations / institutes from the scholar's other articles in the past ten years
Ying Yan has a total of 16 co-authors. Here are the top co-authors by number of shared publications:
Cheng Chen
State Environmental Protection Key Laboratory of Environmental Risk Assessment and Control on Chemical Process, College of Resources and Environmental Engineering East China University of Science and Technology Shanghai China
2 shared publicationsHao Zhou
Shanghai Museum Shanghai China
2 shared publicationsLaiming Wu
Shanghai Museum Shanghai China
2 shared publicationsLehua Zhang
State Environmental Protection Key Laboratory of Environmental Risk Assessment and Control on Chemical Process, College of Resources and Environmental Engineering East China University of Science and Technology Shanghai China
2 shared publicationsBao-Rong Hou
Institute of Oceanology, Chinese Academy of Sciences, Qingdao ShanDong 266071, People's Republic of China
1 shared publicationChengyu Gu
State Environmental Protection Key Laboratory of Environmental Risk Assessment and Control on Chemical Process, East China University of Science and Technology, Shanghai 200237, China
1 shared publication
Latest Publications
- Open Access
- 27 September 2021
- Published by Royal Society of Chemistry (RSC) in RSC Advances
- Vol. 11 (51) , 32038-32046
Fabrication of a superhydrophobic surface by straightforward immersion for copperplate artwork protection
With the background of contemporary art, using comprehensive materials to create artworks is becoming more and more common. The new era of digital image-based copperplate artworks, using photosensitive lithography, has given traditional art forms new life and greater popularity in the digital age. However, the patterns and textures of the works created by the new techniques are generally shallow, and the copper surface is easily damaged and loses its aesthetic value, which makes it a practical problem to protect such works more effectively. In this paper, a facile method is adopted, wherein a superhydrophobic film is constructed on the surface of copperplate images by straightforward immersion in (heptadecafluoro-1,1,2,2-tetradecyl)trimethoxysilane (FAS-17) solution to achieve the anticorrosive protection of copperplate artworks. The hydrophobicity of the copper surface was analyzed using an instrument that measures contact angles. The superhydrophobic surface morphology and composition were analyzed with a scanning electron microscope coupled with an energy-dispersive spectrometer, and the corrosion resistance was analyzed using an electrochemical workstation. A systematic study is presented on the effect of the immersion time in FAS-17 and the concentration of FAS-17, and the optimal preparation conditions of the superhydrophobic film were determined, which means that the copper substrates were immersed in 0.7 mol L−1 FAS-17 for 40 min. After the treatment of the surface to make it superhydrophobic, the contact angle and the corrosion inhibition efficiency of the copperplate etching surface reached 161.2° and 95.7%, respectively. The results show that the superhydrophobic film was successfully prepared on the surface of the artwork based on copper, which can effectively improve the corrosion resistance and is beneficial for the long-term protection of artwork.
- 27 September 2021
- Published by Royal Society of Chemistry (RSC) in RSC Advances
- Vol. 11 (51) , 32038-32046
Open AccessFabrication of a superhydrophobic surface by straightforward immersion for copperplate artwork protection
With the background of contemporary art, using comprehensive materials to create artworks is becoming more and more common. The new era of digital image-based copperplate artworks, using photosensitive lithography, has given traditional art forms new life and greater popularity in the digital age. However, the patterns and textures of the works created by the new techniques are generally shallow, and the copper surface is easily damaged and loses its aesthetic value, which makes it a practical problem to protect such works more effectively. In this paper, a facile method is adopted, wherein a superhydrophobic film is constructed on the surface of copperplate images by straightforward immersion in (heptadecafluoro-1,1,2,2-tetradecyl)trimethoxysilane (FAS-17) solution to achieve the anticorrosive protection of copperplate artworks. The hydrophobicity of the copper surface was analyzed using an instrument that measures contact angles. The superhydrophobic surface morphology and composition were analyzed with a scanning electron microscope coupled with an energy-dispersive spectrometer, and the corrosion resistance was analyzed using an electrochemical workstation. A systematic study is presented on the effect of the immersion time in FAS-17 and the concentration of FAS-17, and the optimal preparation conditions of the superhydrophobic film were determined, which means that the copper substrates were immersed in 0.7 mol L−1 FAS-17 for 40 min. After the treatment of the surface to make it superhydrophobic, the contact angle and the corrosion inhibition efficiency of the copperplate etching surface reached 161.2° and 95.7%, respectively. The results show that the superhydrophobic film was successfully prepared on the surface of the artwork based on copper, which can effectively improve the corrosion resistance and is beneficial for the long-term protection of artwork.
- 13 October 2019
- Published by Wiley in Materials and Corrosion
- Vol. 71 (3) , 464-473
Electrochemical corrosion behavior of bronze materials in an acid‐containing simulated atmospheric environment
The present work investigates the corrosion behavior of bronze materials under thin electrolyte layers (TELs) in a simulated atmospheric environment containing formic and acetic acid by electrochemical measurements as well as surface characterization. The results show that the corrosion of bronze under TEL is significantly faster than that in the bulk solution, and the corrosion rate of bronze is the highest when the thickness of TEL is about 100 μm. Formic acid is observed to be more corrosive than acetic acid. Copper formate and copper acetate hydrate appear in the corrosion products formed on the surface of bronze, suggesting that the organic acid participates in the corrosion process of bronze materials in the simulated atmospheric environment.
- 13 October 2019
- Published by Wiley in Materials and Corrosion
- Vol. 71 (3) , 464-473
Electrochemical corrosion behavior of bronze materials in an acid‐containing simulated atmospheric environment
The present work investigates the corrosion behavior of bronze materials under thin electrolyte layers (TELs) in a simulated atmospheric environment containing formic and acetic acid by electrochemical measurements as well as surface characterization. The results show that the corrosion of bronze under TEL is significantly faster than that in the bulk solution, and the corrosion rate of bronze is the highest when the thickness of TEL is about 100 μm. Formic acid is observed to be more corrosive than acetic acid. Copper formate and copper acetate hydrate appear in the corrosion products formed on the surface of bronze, suggesting that the organic acid participates in the corrosion process of bronze materials in the simulated atmospheric environment.
- 26 August 2018
- Published by Wiley in Materials and Corrosion
- Vol. 70 (2) , 319-327
Corrosion behavior of bronze under organic acid‐containing thin electrolyte layer
The corrosion process and mechanism of three kinds of bronze materials under organic acid‐containing thin electrolyte layer (TEL) are investigated by electrochemical impedance spectroscopy (EIS) and Tafel polarization curves. It can be seen from the results that the corrosion rate of three specimens under TELs is lower than that in bulk solution. For bare bronze, the corrosion rate increases with the thickness of TEL, while for Cu2O patina bronze and CuCl patina bronze, there exists a critical thickness under TELs where the patina bronze have the maximum corrosion rate. In addition, the results show that Cu2O patina could increase the corrosion resistance, while CuCl patina, as a harmful patina, can accelerate the corrosion process. The principal corrosion products identified on the surface of bare bronze and Cu2O patina bronze are CuO, Cu(OH)2, and Cu(COOH)2, while the principal corrosion products identified on the surface of CuCl patina bronze is Cu2Cl(OH)3.
- 26 August 2018
- Published by Wiley in Materials and Corrosion
- Vol. 70 (2) , 319-327
Corrosion behavior of bronze under organic acid‐containing thin electrolyte layer
The corrosion process and mechanism of three kinds of bronze materials under organic acid‐containing thin electrolyte layer (TEL) are investigated by electrochemical impedance spectroscopy (EIS) and Tafel polarization curves. It can be seen from the results that the corrosion rate of three specimens under TELs is lower than that in bulk solution. For bare bronze, the corrosion rate increases with the thickness of TEL, while for Cu2O patina bronze and CuCl patina bronze, there exists a critical thickness under TELs where the patina bronze have the maximum corrosion rate. In addition, the results show that Cu2O patina could increase the corrosion resistance, while CuCl patina, as a harmful patina, can accelerate the corrosion process. The principal corrosion products identified on the surface of bare bronze and Cu2O patina bronze are CuO, Cu(OH)2, and Cu(COOH)2, while the principal corrosion products identified on the surface of CuCl patina bronze is Cu2Cl(OH)3.
- Open Access
- 15 June 2007
- Published by International Union of Crystallography (IUCr) in Acta Crystallographica Section E Crystallographic Communications
- Vol. 63 (7) , m1921-m1922
catena-Poly[[[tetra-μ2-aqua-heptaaqua(μ2-benzene-1,3,5-tricarboxylato)-μ3-hydroxido-trinickel(II)sodium]-μ4-benzene-1,3,5-tricarboxylato] sesquihydrate]
- 15 June 2007
- Published by International Union of Crystallography (IUCr) in Acta Crystallographica Section E Crystallographic Communications
- Vol. 63 (7) , m1921-m1922
Open Accesscatena-Poly[[[tetra-μ2-aqua-heptaaqua(μ2-benzene-1,3,5-tricarboxylato)-μ3-hydroxido-trinickel(II)sodium]-μ4-benzene-1,3,5-tricarboxylato] sesquihydrate]