Aref Fakhrali
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Research Subjects
Aref Fakhrali has a total of 23 co-authors. Here are the top co-authors by number of shared publications:
- Dariush Semnani
Department of Textile Engineering Isfahan University of Technology Isfahan Iran
6 shared publications Sajjad Mohammadi
Kiananobiovista Laboratory, Tehran, Iran
3 shared publicationsHossein Salehi
Department of Anatomical Sciences and Molecular Biology, School of Medicine, Isfahan University of Medical Sciences, Isfahan 8174673461, Iran
2 shared publications- Mina Nasari
Department of Textile Engineering, Isfahan University of Technology, Isfahan, Iran
2 shared publications Abdolkarim Hossein Ravandi
Department of Textile Engineering Isfahan University of Technology Isfahan Iran
1 shared publicationAli Ghodsi
Department of Textile Engineering, Isfahan University of Technology, Isfahan 84156-83111, Iran
1 shared publication
Latest Publications
- 14 May 2024
- Published by American Chemical Society (ACS) in ACS Applied Polymer Materials
- Vol. 6 (10) , 5593-5607
Electroconductive Nanofiber/Myocardium Gel Scaffolds Applicable for Myocardial Infarction Therapy
- 14 May 2024
- Published by American Chemical Society (ACS) in ACS Applied Polymer Materials
- Vol. 6 (10) , 5593-5607
Electroconductive Nanofiber/Myocardium Gel Scaffolds Applicable for Myocardial Infarction Therapy
- 21 August 2022
- Published by Taylor & Francis in International Journal of Polymeric Materials and Polymeric Biomaterials
- Vol. 72 (18) , 1529-1545
Fabrication of novel PCL/PGS fibrous scaffold containing HA and GO through simultaneous electrospinning-electrospray technique
Herein, poly(caprolactone)/poly (glycerol sebacate) (PCL/PGS) fibrous structures incorporating hydroxyapatite (HA) and graphene oxide (GO) nanofillers were prepared through two procedures, including electrospinning and simultaneous electrospinning/electrospray procedures. Accordingly, introducing nanofillers into the structures through the simultaneous method led to improving the mechanical strength from 3.69 to 4.95 MPa. The electrospray nanofillers caused improvement of the amorphous regions (up to 83.4%) and increased the degradation rate. Furthermore, the filler-filled electrospun/electrospray sample illustrated the highest cell viability of 94.81 ± 0.5%. The results implied that the simultaneous procedure is promising for fabricating filler-loaded membranes as bone tissue scaffolds. Graphical Abstract
- 21 August 2022
- Published by Taylor & Francis in International Journal of Polymeric Materials and Polymeric Biomaterials
- Vol. 72 (18) , 1529-1545
Fabrication of novel PCL/PGS fibrous scaffold containing HA and GO through simultaneous electrospinning-electrospray technique
Herein, poly(caprolactone)/poly (glycerol sebacate) (PCL/PGS) fibrous structures incorporating hydroxyapatite (HA) and graphene oxide (GO) nanofillers were prepared through two procedures, including electrospinning and simultaneous electrospinning/electrospray procedures. Accordingly, introducing nanofillers into the structures through the simultaneous method led to improving the mechanical strength from 3.69 to 4.95 MPa. The electrospray nanofillers caused improvement of the amorphous regions (up to 83.4%) and increased the degradation rate. Furthermore, the filler-filled electrospun/electrospray sample illustrated the highest cell viability of 94.81 ± 0.5%. The results implied that the simultaneous procedure is promising for fabricating filler-loaded membranes as bone tissue scaffolds. Graphical Abstract
- 10 January 2022
- Published by Wiley in Journal of Applied Polymer Science
- Vol. 139 (19) , 52136
Electro‐conductive nanofibrous structure based on PGS/PCL coated with PPy by in situ chemical polymerization applicable as cardiac patch: Fabrication and optimization
As a special structure and due to the unique properties of submicron‐scale fibers and electrical conductivity, conductive nanofibers recently attracted further attention in various fields, especially tissue engineering. This study aimed to coat poly (glycerol sebacate) (PGS) nanofiber/poly(caprolactone) (PCL) as a widely used combination in the fields of medicine with poly(pyrrole) (PPy) as a conductive polymer, subsequently studying and optimizing production process variables using response surface methodology (RSM). The samples were examined for morphological and structural, and their electrical conductivity and electroactivity were measured using a four‐point probe system and a cyclic voltammetry, respectively. The electrospinning conditions for constructing the substrate nanofibers with the smallest diameter were optimized. The monomer concentration of 0.05M and the polymerization time of 3.3 h exploiting the RSM were also considered as the optimal conditions for obtaining coated‐nanofibers with the smallest diameter and desired electrical conductivity (0.001 S/cm). The structural findings confirmed the successful synthesis of PGS and PPy. The conductive‐nanofiber produced under optimal conditions revealed good mechanical properties (tensile strength = 3.12 ± 0.19 MPa and elongation at break = 80.26 ± 13.71%). The highest biocompatibility was observed for the sample synthesized with the pyrrole concentration of 0.05M, which can be a suitable candidate for application in cardiac tissue engineering.
- 10 January 2022
- Published by Wiley in Journal of Applied Polymer Science
- Vol. 139 (19) , 52136
Electro‐conductive nanofibrous structure based on PGS/PCL coated with PPy by in situ chemical polymerization applicable as cardiac patch: Fabrication and optimization
As a special structure and due to the unique properties of submicron‐scale fibers and electrical conductivity, conductive nanofibers recently attracted further attention in various fields, especially tissue engineering. This study aimed to coat poly (glycerol sebacate) (PGS) nanofiber/poly(caprolactone) (PCL) as a widely used combination in the fields of medicine with poly(pyrrole) (PPy) as a conductive polymer, subsequently studying and optimizing production process variables using response surface methodology (RSM). The samples were examined for morphological and structural, and their electrical conductivity and electroactivity were measured using a four‐point probe system and a cyclic voltammetry, respectively. The electrospinning conditions for constructing the substrate nanofibers with the smallest diameter were optimized. The monomer concentration of 0.05M and the polymerization time of 3.3 h exploiting the RSM were also considered as the optimal conditions for obtaining coated‐nanofibers with the smallest diameter and desired electrical conductivity (0.001 S/cm). The structural findings confirmed the successful synthesis of PGS and PPy. The conductive‐nanofiber produced under optimal conditions revealed good mechanical properties (tensile strength = 3.12 ± 0.19 MPa and elongation at break = 80.26 ± 13.71%). The highest biocompatibility was observed for the sample synthesized with the pyrrole concentration of 0.05M, which can be a suitable candidate for application in cardiac tissue engineering.
- 21 September 2021
- Published by Wiley in Polymers for Advanced Technologies
- Vol. 33 (1) , 81-95
Fabrication and characterization ofchitosan‐gelatin/single‐walledcarbon nanotubes electrospun composite scaffolds for cartilage tissue engineering applications
Cartilage is a connective tissue with a slow healing rate due to lack in blood circulation and slow metabolism. Designing tissue engineering scaffolds modified based on its specific features can assist its natural regeneration process. In this study, the chitosan‐gelatin/single‐walled carbon nanotubes functionalized by COOH (SWNTs‐COOH) nanocomposite scaffolds were fabricated through electrospinning. The effect of each component and different duration of cross‐linking were assessed in terms of morphology, porosity, chemical structure, thermal behavior, mechanical properties, wettability, biodegradability, and in vitro cell culture study. Adding SWNTs‐COOH decreased fiber diameter, water contact angle and degradation rate while increased tensile strength, hydrophilicity, stability and cell viability, due to their high intrinsic electrical conductivity, and mechanical properties and the presence of COOH functional groups in its structure. All the sample presented a porosity percentage of more than 80%, which is essential for tissue engineering scaffolds. The presence SWNTs‐COOH did not have any adverse effect on cytocompatibility. The optimal cross‐linking time increased the stability of the scaffolds in PBS. It can be concluded that the chitosan‐gelatin/1wt% SWNTs‐COOH scaffold can be appropriate for cartilage tissue engineering applications.
- 21 September 2021
- Published by Wiley in Polymers for Advanced Technologies
- Vol. 33 (1) , 81-95
Fabrication and characterization ofchitosan‐gelatin/single‐walledcarbon nanotubes electrospun composite scaffolds for cartilage tissue engineering applications
Cartilage is a connective tissue with a slow healing rate due to lack in blood circulation and slow metabolism. Designing tissue engineering scaffolds modified based on its specific features can assist its natural regeneration process. In this study, the chitosan‐gelatin/single‐walled carbon nanotubes functionalized by COOH (SWNTs‐COOH) nanocomposite scaffolds were fabricated through electrospinning. The effect of each component and different duration of cross‐linking were assessed in terms of morphology, porosity, chemical structure, thermal behavior, mechanical properties, wettability, biodegradability, and in vitro cell culture study. Adding SWNTs‐COOH decreased fiber diameter, water contact angle and degradation rate while increased tensile strength, hydrophilicity, stability and cell viability, due to their high intrinsic electrical conductivity, and mechanical properties and the presence of COOH functional groups in its structure. All the sample presented a porosity percentage of more than 80%, which is essential for tissue engineering scaffolds. The presence SWNTs‐COOH did not have any adverse effect on cytocompatibility. The optimal cross‐linking time increased the stability of the scaffolds in PBS. It can be concluded that the chitosan‐gelatin/1wt% SWNTs‐COOH scaffold can be appropriate for cartilage tissue engineering applications.
- 7 June 2021
- Published by Wiley in Journal of Applied Polymer Science
- Vol. 138 (40) , 51177
Biocompatible graphene‐embedded PCL/PGS‐based nanofibrous scaffolds: A potential application for cardiac tissue regeneration
Research in the field of tissue engineering, especially heart tissue engineering, is growing rapidly. Herein, the morphological, chemical, mechanical and biological properties of poly (caprolactone) (PCL)/poly (glycerol sebacate) (PGS) and PCL/PGS/graphene nanofibrous scaffolds are investigated. Initially, PGS pre‐polymer is synthesized and characterized by nuclear magnetic resonance and Fourier transform infrared spectroscopies. Then, in order to use the benefits of PGS, this polymer is mixed with PCL. Blending PGS with PCL resulted in the enhancement of ultimate elongation and reduction in the elastic modulus due to the intrinsic properties of PGS. The hydrophobicity of PCL nanofibers is reduced by adding PGS as hydrophilic polymer (105 ± 3° vs. 44 ± 2°). Also, the addition of graphene to the blend nanofibers is balanced the hydrophilicity. Degradation rate of pure PCL nanofibers is very slow but it is increased in the presence of PGS. All nanofibrous scaffolds are biocompatible and non‐toxic. The highest cell adhesion (covered area = 0.916 ± 0.032) and biocompatibility (98.79 ± 1%) are related to PCL/PGS loaded with 1% wt of graphene (PCL/PGS/graphene 1). Thus, this sample can be a good candidate for further examinations of cardiac tissue engineering.
- 7 June 2021
- Published by Wiley in Journal of Applied Polymer Science
- Vol. 138 (40) , 51177
Biocompatible graphene‐embedded PCL/PGS‐based nanofibrous scaffolds: A potential application for cardiac tissue regeneration
Research in the field of tissue engineering, especially heart tissue engineering, is growing rapidly. Herein, the morphological, chemical, mechanical and biological properties of poly (caprolactone) (PCL)/poly (glycerol sebacate) (PGS) and PCL/PGS/graphene nanofibrous scaffolds are investigated. Initially, PGS pre‐polymer is synthesized and characterized by nuclear magnetic resonance and Fourier transform infrared spectroscopies. Then, in order to use the benefits of PGS, this polymer is mixed with PCL. Blending PGS with PCL resulted in the enhancement of ultimate elongation and reduction in the elastic modulus due to the intrinsic properties of PGS. The hydrophobicity of PCL nanofibers is reduced by adding PGS as hydrophilic polymer (105 ± 3° vs. 44 ± 2°). Also, the addition of graphene to the blend nanofibers is balanced the hydrophilicity. Degradation rate of pure PCL nanofibers is very slow but it is increased in the presence of PGS. All nanofibrous scaffolds are biocompatible and non‐toxic. The highest cell adhesion (covered area = 0.916 ± 0.032) and biocompatibility (98.79 ± 1%) are related to PCL/PGS loaded with 1% wt of graphene (PCL/PGS/graphene 1). Thus, this sample can be a good candidate for further examinations of cardiac tissue engineering.
- 10 July 2020
- Published by IOP Publishing in Smart Materials and Structures
- Vol. 29 (8) , 085036
Overcoming the potential drop in conducting polymer artificial muscles through metallization of electrospun nanofibers by electroplating process
Electrochemical actuators made of conducting polymers are one of the major types of artificial muscles that have attracted much attention in recent years. However, these artificial muscles suffer from potential drop along the length, which undermines their performance in applications requiring longer muscles. This study is aimed at enhancing the performance of this type of artificial muscles through overcoming the potential drop along the length. This is implemented using copper electroplating and creating a full-length highly conductive nanofibrous layer. Polyurethane/copper/polypyrrole (PU/Cu/PPy) nanofibrous artificial muscles were fabricated by combining electrospinning, electroplating and electrochemical polymerization. The copper electroplating affected many features of the PU nanofibrous layer including surface morphology of nanofibers, thermal, mechanical and electrical properties. Average diameter of the PU nanofibers was measured as 306 ± 48 nm, which increased significantly by increasing the duration of copper electroplating. By copper electroplating for 20 s, the onset temperature of nanofibers thermal decomposition was increased from 249 to 302 °C. Additionally, using this process, the sample Young’s modulus was increased from 2.20 ± 0.21 to 62.32 ± 5.42 MPa while its elongation at break was decreased from 173.84 ± 14.22 to 94.81 ± 10.96. After copper electroplating for duration as low as 20 s, the electrical conductivity of nanofibers was increased by more than 200 times from 48.90 ± 1.10 to 10 103.06 ± 14.28 S cm −1 . Electrochemical polymerization of pyrrole on the surface of metalized nanofibers increased the average diameter of produced nanofibers to 1030 ± 102 nm. Providing an electrical connection along the entire length of artificial muscle resulted in enhanced electroactive property and hence final bending actuation of 88° for a cycle potential between −0.8 V and 0.5 V at a scan rate of 5 mV s −1 was observed. The nanofibrous artificial muscle fabricated by the proposed method has immense potential for use in practical applications.
- 10 July 2020
- Published by IOP Publishing in Smart Materials and Structures
- Vol. 29 (8) , 085036
Overcoming the potential drop in conducting polymer artificial muscles through metallization of electrospun nanofibers by electroplating process
Electrochemical actuators made of conducting polymers are one of the major types of artificial muscles that have attracted much attention in recent years. However, these artificial muscles suffer from potential drop along the length, which undermines their performance in applications requiring longer muscles. This study is aimed at enhancing the performance of this type of artificial muscles through overcoming the potential drop along the length. This is implemented using copper electroplating and creating a full-length highly conductive nanofibrous layer. Polyurethane/copper/polypyrrole (PU/Cu/PPy) nanofibrous artificial muscles were fabricated by combining electrospinning, electroplating and electrochemical polymerization. The copper electroplating affected many features of the PU nanofibrous layer including surface morphology of nanofibers, thermal, mechanical and electrical properties. Average diameter of the PU nanofibers was measured as 306 ± 48 nm, which increased significantly by increasing the duration of copper electroplating. By copper electroplating for 20 s, the onset temperature of nanofibers thermal decomposition was increased from 249 to 302 °C. Additionally, using this process, the sample Young’s modulus was increased from 2.20 ± 0.21 to 62.32 ± 5.42 MPa while its elongation at break was decreased from 173.84 ± 14.22 to 94.81 ± 10.96. After copper electroplating for duration as low as 20 s, the electrical conductivity of nanofibers was increased by more than 200 times from 48.90 ± 1.10 to 10 103.06 ± 14.28 S cm −1 . Electrochemical polymerization of pyrrole on the surface of metalized nanofibers increased the average diameter of produced nanofibers to 1030 ± 102 nm. Providing an electrical connection along the entire length of artificial muscle resulted in enhanced electroactive property and hence final bending actuation of 88° for a cycle potential between −0.8 V and 0.5 V at a scan rate of 5 mV s −1 was observed. The nanofibrous artificial muscle fabricated by the proposed method has immense potential for use in practical applications.