Shuixian Yang
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Research Subjects
Research Interests
Shuixian Yang has a total of 7 co-authors. Here are the top co-authors by number of shared publications:
Hao Guo
State Key Laboratory of High Performance Ceramics and Superfine Microstructure Shanghai Institute of Ceramics Chinese Academy of Sciences Shanghai China
2 shared publicationsJian Zhang
State Key Laboratory of High Performance Ceramics and Superfine Microstructure Shanghai Institute of Ceramics Chinese Academy of Sciences Shanghai China
2 shared publicationsJianmin Li
State Key Laboratory of High Performance Ceramics and Superfine Microstructure Shanghai Institute of Ceramics Chinese Academy of Sciences Shanghai China
2 shared publicationsRun Tian
State Key Laboratory of High Performance Ceramics and Superfine Microstructure Shanghai Institute of Ceramics Chinese Academy of Sciences Shanghai China
2 shared publications- Shiwei Wang
State Key Laboratory of High Performance Ceramics and Superfine Microstructure Shanghai Institute of Ceramics Chinese Academy of Sciences 200050 Shanghai China
2 shared publications - Xiaojian Mao
State Key Laboratory of High Performance Ceramics and Superfine Microstructures Shanghai Institute of Ceramics Chinese Academy of Sciences 200050 Shanghai China
2 shared publications
Latest Publications
- 4 April 2021
- Published by Wiley in Journal of the American Ceramic Society
- Vol. 104 (9) , 4304-4308
Reactive sintered highly transparent AlON ceramics with Y2O3‐MgAl2O4‐H3BO3 ternary additive
In this study, highly transparent aluminate oxynitride (AlON) ceramics were prepared via the reactive sintering of Al2O3 and AlN powders using a Y2O3‐MgAl2O4‐H3BO3 ternary sintering additive. The ternary doping process resulted in the efficient preparation of transparent AlON ceramics with small grains and high transmittance as compared to the binary doping (Y2O3‐MgAl2O4) process. The addition of 0.1 wt.% Y2O3‐0.4 wt.% MgAl2O4‐0.12 wt.% H3BO3 resulted in the formation of a 4‐mm‐thick AlON ceramic with high transmittance (81% at 600 nm) and low haze (3.46%). This is the best performance in terms of the thickness and transmittance reported for AlON transparent ceramics prepared by the reactive sintering method.
- 4 April 2021
- Published by Wiley in Journal of the American Ceramic Society
- Vol. 104 (9) , 4304-4308
Reactive sintered highly transparent AlON ceramics with Y2O3‐MgAl2O4‐H3BO3 ternary additive
In this study, highly transparent aluminate oxynitride (AlON) ceramics were prepared via the reactive sintering of Al2O3 and AlN powders using a Y2O3‐MgAl2O4‐H3BO3 ternary sintering additive. The ternary doping process resulted in the efficient preparation of transparent AlON ceramics with small grains and high transmittance as compared to the binary doping (Y2O3‐MgAl2O4) process. The addition of 0.1 wt.% Y2O3‐0.4 wt.% MgAl2O4‐0.12 wt.% H3BO3 resulted in the formation of a 4‐mm‐thick AlON ceramic with high transmittance (81% at 600 nm) and low haze (3.46%). This is the best performance in terms of the thickness and transmittance reported for AlON transparent ceramics prepared by the reactive sintering method.
- 18 October 2020
- Published by Wiley in Journal of the American Ceramic Society
- Vol. 104 (2) , 1040-1046
Oxidation behavior and mechanism of aluminum oxynitride (AlON) at elevated temperatures
The oxidation behavior and mechanism of aluminum oxynitride (AlON) powder exposed to air at elevated temperatures between 800°C and 1300°C was investigated by X‐ray diffractometry (XRD), scanning electron microscope (SEM), electron spin resonance (ESR), nuclear magnetic resonance (NMR), and simultaneous thermogravimetry, differential thermal analysis, and mass spectrometry techniques (TG‐DTA‐MS). The weight of AlON gradually increases to a maximum value at 1150°C and then decreases with further heating. Meanwhile, AlON powder undergoes chemical changes, as evidenced by lattice expansion, and turns eventually into alumina. ESR spectra reveal the occurrence of lone pair electrons in the oxidized products and the intensity of corresponding resonance signal increases before disappearing with the increase in temperature. Combined with the results of NMR and TG‐DTA‐MS, the measured data suggest that Al‐N in [AlO 3 N] tetrahedron and [AlO 5 N] octahedron are gradually oxidized into Al‐O‐N group with lone pair electrons, which causes continuous weight gain and lattice expansion. Further oxidation at higher temperatures results in alumina and N 2 .
- 18 October 2020
- Published by Wiley in Journal of the American Ceramic Society
- Vol. 104 (2) , 1040-1046
Oxidation behavior and mechanism of aluminum oxynitride (AlON) at elevated temperatures
The oxidation behavior and mechanism of aluminum oxynitride (AlON) powder exposed to air at elevated temperatures between 800°C and 1300°C was investigated by X‐ray diffractometry (XRD), scanning electron microscope (SEM), electron spin resonance (ESR), nuclear magnetic resonance (NMR), and simultaneous thermogravimetry, differential thermal analysis, and mass spectrometry techniques (TG‐DTA‐MS). The weight of AlON gradually increases to a maximum value at 1150°C and then decreases with further heating. Meanwhile, AlON powder undergoes chemical changes, as evidenced by lattice expansion, and turns eventually into alumina. ESR spectra reveal the occurrence of lone pair electrons in the oxidized products and the intensity of corresponding resonance signal increases before disappearing with the increase in temperature. Combined with the results of NMR and TG‐DTA‐MS, the measured data suggest that Al‐N in [AlO 3 N] tetrahedron and [AlO 5 N] octahedron are gradually oxidized into Al‐O‐N group with lone pair electrons, which causes continuous weight gain and lattice expansion. Further oxidation at higher temperatures results in alumina and N 2 .