Chenchy J. Lin
Research Subjects
Chenchy J. Lin has a total of 7 co-authors. Here are the top co-authors by number of shared publications:
William L. Hergenrother
Bridgestone Americas Center for Research and Technology, 1200 Firestone Parkway, Akron, Ohio 44317
4 shared publicationsAshley S. Hilton
Bridgestone Americas Center for Research and Technology, 1200 Firestone Parkway, Akron, Ohio 44317
3 shared publicationsTerrence E. Hogan
Bridgestone Americas Center for Research and Technology, 1200 Firestone Parkway, Akron, Ohio 44317
2 shared publicationsAlberto Scurati
Bridgestone Americas Center for Research and Technology, 1200 Firestone Parkway, Akron, Ohio 44317
1 shared publicationDennis R. Brumbaugh
Bridgestone Americas Center for Research and Technology, 1200 Firestone Parkway, Akron, Ohio 44317
1 shared publication- William L. Hergenrother
Bridgestone Americas Center for Research and Technology, 1200 Firestone Parkway, Akron, Ohio 44317
1 shared publication
Latest Publications
- 27 July 2010
- Published by Wiley in Journal of Applied Polymer Science
- Vol. 119 (2) , 768-775
Tailoring the polymeric nanoparticles for rubber reinforcement
- 27 July 2010
- Published by Wiley in Journal of Applied Polymer Science
- Vol. 119 (2) , 768-775
Tailoring the polymeric nanoparticles for rubber reinforcement
- 10 September 2009
- Published by Wiley in Journal of Applied Polymer Science
- Vol. 115 (2) , 655-664
Reduction of volatile organic compound emission. II. Use of alkoxy‐modified silsesquioxane for compounding silica‐filled rubbers
A class of alkoxy‐modified silsesquioxane (AMS) containing less than 5 wt % of latent alcohol that can be used for compounding silica‐filled rubbers is described. The AMS derived from octyl‐triethoxysilane (OTES) behaves as a good shielding agent in silica‐filled rubber to significantly reduce the compound Mooney viscosity and filler flocculation. The co‐AMS prepared from OTES and 3‐mercaptopropyl‐trimethoxysilane yielded an effective shielding and coupling agent for reinforcing the silica‐filled vulcanizates. The alcohols released as volatile organic compounds (VOC) are quantified during compounding and processing along with the compound properties of silica‐filled vulcanizates containing various silicon compounds such as bis‐(triethoxysilyl propyl) disulfide (TESPD), a polyhedral oligomeric silsesquioxanes (POSS), OTES, AMS, or co‐AMS. Dynamic mechanical properties such as dependences of hysteresis on temperature (HTD) and storage modulus on strain (MSD) are discussed. Stronger HTD and weaker MSD were found in stocks containing co‐AMS or a combination of AMS and a coupling agent when compared with that with TESPD. Stronger HTD and weaker MSD may benefit a tire compound with lower rolling resistance, more stable handling performance, as well as better wet traction. More importantly, the VOC released during the manufacture of rubber articles are significantly reduced in stocks containing AMS (or co‐AMS) when compared with those with a silane. © 2009 Wiley Periodicals, Inc. J Appl Polym Sci, 2010
- 10 September 2009
- Published by Wiley in Journal of Applied Polymer Science
- Vol. 115 (2) , 655-664
Reduction of volatile organic compound emission. II. Use of alkoxy‐modified silsesquioxane for compounding silica‐filled rubbers
A class of alkoxy‐modified silsesquioxane (AMS) containing less than 5 wt % of latent alcohol that can be used for compounding silica‐filled rubbers is described. The AMS derived from octyl‐triethoxysilane (OTES) behaves as a good shielding agent in silica‐filled rubber to significantly reduce the compound Mooney viscosity and filler flocculation. The co‐AMS prepared from OTES and 3‐mercaptopropyl‐trimethoxysilane yielded an effective shielding and coupling agent for reinforcing the silica‐filled vulcanizates. The alcohols released as volatile organic compounds (VOC) are quantified during compounding and processing along with the compound properties of silica‐filled vulcanizates containing various silicon compounds such as bis‐(triethoxysilyl propyl) disulfide (TESPD), a polyhedral oligomeric silsesquioxanes (POSS), OTES, AMS, or co‐AMS. Dynamic mechanical properties such as dependences of hysteresis on temperature (HTD) and storage modulus on strain (MSD) are discussed. Stronger HTD and weaker MSD were found in stocks containing co‐AMS or a combination of AMS and a coupling agent when compared with that with TESPD. Stronger HTD and weaker MSD may benefit a tire compound with lower rolling resistance, more stable handling performance, as well as better wet traction. More importantly, the VOC released during the manufacture of rubber articles are significantly reduced in stocks containing AMS (or co‐AMS) when compared with those with a silane. © 2009 Wiley Periodicals, Inc. J Appl Polym Sci, 2010
- 27 August 2009
- Published by Wiley in Journal of Applied Polymer Science
- Vol. 115 (1) , 79-90
Reduction of volatile organic compound emission. I. Synthesis and characterization of alkoxy‐modified silsesquioxane
The preparation and characterization of a class of alkoxy‐modified silsesquioxane (AMS) compounds containing less than 5 wt % of latent alcohol is described. The AMS derived from octyl triethoxysilane (OTES) behaves as a shielding agent in silica‐filled rubbers while significantly reducing the volatile organic compounds that are released during the manufacture of rubber articles. Analysis of AMS by high pressure liquid chromatography and 29Si NMR shows that it has a plethora of structures present that can best be described as a highly condensed opened oligomeric, branched arrangement of silsesquioxanes units. This structure is moisture stable, hydrocarbon soluble, and reactive with silica at compounding temperatures. The AMS has been prepared by acid‐ or base‐catalyzed hydrolysis and condensation in alcohol solution to form a product that often separates from the lower density reaction mixture. The kinetics of the AMS formation was examined and showed two separate rate processes occurring. The co‐AMS prepared from OTES and 3‐mercaptopropyl trimethoxysilane yielded an effective shielding agent and coupling agent when used in silica‐filled vulcanizates. © 2009 Wiley Periodicals, Inc. J Appl Polym Sci, 2010
- 27 August 2009
- Published by Wiley in Journal of Applied Polymer Science
- Vol. 115 (1) , 79-90
Reduction of volatile organic compound emission. I. Synthesis and characterization of alkoxy‐modified silsesquioxane
The preparation and characterization of a class of alkoxy‐modified silsesquioxane (AMS) compounds containing less than 5 wt % of latent alcohol is described. The AMS derived from octyl triethoxysilane (OTES) behaves as a shielding agent in silica‐filled rubbers while significantly reducing the volatile organic compounds that are released during the manufacture of rubber articles. Analysis of AMS by high pressure liquid chromatography and 29Si NMR shows that it has a plethora of structures present that can best be described as a highly condensed opened oligomeric, branched arrangement of silsesquioxanes units. This structure is moisture stable, hydrocarbon soluble, and reactive with silica at compounding temperatures. The AMS has been prepared by acid‐ or base‐catalyzed hydrolysis and condensation in alcohol solution to form a product that often separates from the lower density reaction mixture. The kinetics of the AMS formation was examined and showed two separate rate processes occurring. The co‐AMS prepared from OTES and 3‐mercaptopropyl trimethoxysilane yielded an effective shielding agent and coupling agent when used in silica‐filled vulcanizates. © 2009 Wiley Periodicals, Inc. J Appl Polym Sci, 2010
- 29 January 2008
- Published by Wiley in Journal of Applied Polymer Science
- Vol. 108 (3) , 1722-1736
Hysteresis temperature dependence in filled rubbers. II. Mechanical mixing, filler microdispersion, and polymer–filler interactions
The effects of mechanical mixing and filler–filler (F–F) and polymer–filler (P–F) interactions on the normalized state of a filler microdispersion [d(x)] and the viscoelastic properties of silica‐filled rubbers were studied. The rubbers were prepared with or without the addition of n‐octyl‐triethoxysilane (OTES) to modify F–F interactions or coupling agents such as 3‐mercaptopropyl‐trimethoxysilane and 3‐mercaptopropyl‐triethoxysilane (MPTES) to increase P–F interactions. Increased mixing improved d(x) and enhanced the hysteresis temperature dependence (HTD) by giving a higher tan δ value near the compound glass‐transition temperature (Tg) but lowered tan δ at elevated temperatures for stocks containing a coupling agent. The changes in P–F and F–F interactions in rubbers with mixing and subsequent thermal treatment were shown to be responsible for the property differences observed among stocks containing different silanes. Attempts were made to quantify the efficiency for improving d(x) with various silanes. The increased P–F interactions in compounds containing MPTES showed better efficiency for improving d(x) and enhancing HTD in comparison with OTES. It was also demonstrated that the change in hysteresis near Tg was mainly governed by the degree of filler networking, whereas elevated‐temperature hysteresis was strongly influenced by the P–F interactions in compounds. © 2008 Wiley Periodicals, Inc. J Appl Polym Sci, 2008
- 29 January 2008
- Published by Wiley in Journal of Applied Polymer Science
- Vol. 108 (3) , 1722-1736
Hysteresis temperature dependence in filled rubbers. II. Mechanical mixing, filler microdispersion, and polymer–filler interactions
The effects of mechanical mixing and filler–filler (F–F) and polymer–filler (P–F) interactions on the normalized state of a filler microdispersion [d(x)] and the viscoelastic properties of silica‐filled rubbers were studied. The rubbers were prepared with or without the addition of n‐octyl‐triethoxysilane (OTES) to modify F–F interactions or coupling agents such as 3‐mercaptopropyl‐trimethoxysilane and 3‐mercaptopropyl‐triethoxysilane (MPTES) to increase P–F interactions. Increased mixing improved d(x) and enhanced the hysteresis temperature dependence (HTD) by giving a higher tan δ value near the compound glass‐transition temperature (Tg) but lowered tan δ at elevated temperatures for stocks containing a coupling agent. The changes in P–F and F–F interactions in rubbers with mixing and subsequent thermal treatment were shown to be responsible for the property differences observed among stocks containing different silanes. Attempts were made to quantify the efficiency for improving d(x) with various silanes. The increased P–F interactions in compounds containing MPTES showed better efficiency for improving d(x) and enhancing HTD in comparison with OTES. It was also demonstrated that the change in hysteresis near Tg was mainly governed by the degree of filler networking, whereas elevated‐temperature hysteresis was strongly influenced by the P–F interactions in compounds. © 2008 Wiley Periodicals, Inc. J Appl Polym Sci, 2008
- 1 March 2004
- Published by Rubber Division, ACS in Rubber Chemistry and Technology
- Vol. 77 (1) , 90-114
On the Filler Flocculation in Silica and Carbon Black Filled Rubbers: Part II. Filler Flocculation and Polymer-Filler Interaction
Filler flocculation and polymer-filler interaction in silica and carbon black filled rubbers containing different functional end-groups were investigated. Lithium-hexamethyleneimine initiated polymers terminated with a proton (HMI-P-H), SnCl4 (HMI-P-Sn), and a mixture of SnCl4 and tetraethyl orthosilicate (HMI-P-TEOS) were employed to determine the affinities of various functionalities toward fillers. Reduced filler flocculation was found for compounds of HMI-P-Sn and HMI-P-TEOS after thermal annealing at 171 °C for 15 minutes when compared to the annealed HMI-P-H stock. Curing at the same condition used for annealing gave further suppression of filler flocculation for HMI-P-TEOS stock by increased polymer-filler interaction during cure. Polymer-filler interaction was followed by examining G′ strain dependence and the differences in G′ obtained between HMI-P-Sn or HMI-P-TEOS and HMI-P-H (δG′). This treatment gave a peak maximum in the δG′ plot as a function of strain. The magnitude of the maximum in HMI-P-TEOS stock is double that of HMI-P-Sn stock and increased after thermal annealing. The compound tanδ temperature dependence showed higher hysteresis around the Tg transition and strong dependence at elevated temperatures was found for HMI-P-TEOS stocks. This increased polymer-filler interaction is manifested with increased 0 °C tanδ and reduced 50 °C tanδ which relates to the improved wet traction and rolling resistance for tires.
- 1 March 2004
- Published by Rubber Division, ACS in Rubber Chemistry and Technology
- Vol. 77 (1) , 90-114
On the Filler Flocculation in Silica and Carbon Black Filled Rubbers: Part II. Filler Flocculation and Polymer-Filler Interaction
Filler flocculation and polymer-filler interaction in silica and carbon black filled rubbers containing different functional end-groups were investigated. Lithium-hexamethyleneimine initiated polymers terminated with a proton (HMI-P-H), SnCl4 (HMI-P-Sn), and a mixture of SnCl4 and tetraethyl orthosilicate (HMI-P-TEOS) were employed to determine the affinities of various functionalities toward fillers. Reduced filler flocculation was found for compounds of HMI-P-Sn and HMI-P-TEOS after thermal annealing at 171 °C for 15 minutes when compared to the annealed HMI-P-H stock. Curing at the same condition used for annealing gave further suppression of filler flocculation for HMI-P-TEOS stock by increased polymer-filler interaction during cure. Polymer-filler interaction was followed by examining G′ strain dependence and the differences in G′ obtained between HMI-P-Sn or HMI-P-TEOS and HMI-P-H (δG′). This treatment gave a peak maximum in the δG′ plot as a function of strain. The magnitude of the maximum in HMI-P-TEOS stock is double that of HMI-P-Sn stock and increased after thermal annealing. The compound tanδ temperature dependence showed higher hysteresis around the Tg transition and strong dependence at elevated temperatures was found for HMI-P-TEOS stocks. This increased polymer-filler interaction is manifested with increased 0 °C tanδ and reduced 50 °C tanδ which relates to the improved wet traction and rolling resistance for tires.
- 1 May 2002
- Published by Rubber Division, ACS in Rubber Chemistry and Technology
- Vol. 75 (2) , 215-245
Mooney Viscosity Stability and Polymer Filler Interactions in Silica Filled Rubbers
The change in Mooney viscosity (ML1+4) with aging was followed for silica filled compounds containing various silanes and polar additives. Several mechanisms for the aging stability are postulated and evaluated through experimentation. The type of silane or polar additive used can cause the ML1+4 to increase or even decrease during aging. When bis(triethoxy silanes) are used in silica filled rubbers, the ML1+4 growth during aging is caused by hydrolysis. Silica-silica bridging was found to be responsible for the ML1+4 growth in rubber compounds containing a more thermally stable polysulfide or a sulfur-free bis(triethoxy silane). When the bis(triethoxy silane) is bis(3-triethoxysilylpropyl) tetrasulfide (TESPT), a fraction of TESPT is attached to the unsaturated rubber to give polymer-silica attachments. These attachments further enhance the hydrolytic ML1+4 increase during aging. Chemical coating of the silica with a monofunctional silane or a physical coating with a trialkyl amine compound effectively stops the ML1+4 increase upon aging. The prevention of ML1+4 growth is so efficient that a reduction in the ML1+4 can be realized by absorption of ambient moisture. The extent of ML1+4 reduction caused by moisture depends on the degree of hydrophobation of the coated silicas. Hydrolytic stability was also studied with an amine or a sugar fatty acid ester that formed either strong or weak polar associations to the silica.
- 1 May 2002
- Published by Rubber Division, ACS in Rubber Chemistry and Technology
- Vol. 75 (2) , 215-245
Mooney Viscosity Stability and Polymer Filler Interactions in Silica Filled Rubbers
The change in Mooney viscosity (ML1+4) with aging was followed for silica filled compounds containing various silanes and polar additives. Several mechanisms for the aging stability are postulated and evaluated through experimentation. The type of silane or polar additive used can cause the ML1+4 to increase or even decrease during aging. When bis(triethoxy silanes) are used in silica filled rubbers, the ML1+4 growth during aging is caused by hydrolysis. Silica-silica bridging was found to be responsible for the ML1+4 growth in rubber compounds containing a more thermally stable polysulfide or a sulfur-free bis(triethoxy silane). When the bis(triethoxy silane) is bis(3-triethoxysilylpropyl) tetrasulfide (TESPT), a fraction of TESPT is attached to the unsaturated rubber to give polymer-silica attachments. These attachments further enhance the hydrolytic ML1+4 increase during aging. Chemical coating of the silica with a monofunctional silane or a physical coating with a trialkyl amine compound effectively stops the ML1+4 increase upon aging. The prevention of ML1+4 growth is so efficient that a reduction in the ML1+4 can be realized by absorption of ambient moisture. The extent of ML1+4 reduction caused by moisture depends on the degree of hydrophobation of the coated silicas. Hydrolytic stability was also studied with an amine or a sugar fatty acid ester that formed either strong or weak polar associations to the silica.